The surface composition of mica substrates
Muscovite mica substrate surface composition as function of preparation and processing, using Auger electron spectroscopy
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Muscovite mica substrate surface composition as function of preparation and processing, using Auger electron spectroscopy
Epitaxial deposition of Au on ultrahigh vacuum cleaved mica during early nucleation and growth
Measurements of crystalline sizes during nucleation of gold on mica surfaces cleaved in ultra-high vacuum (UHV) reveal the presence of symmetric, sharply peaked distributions which flatten and broaden with increasing nucleation time. When the number density of nuclei increases, the growth rate is suppressed. The time taken to reach a given size increases with increasing temperature when the nuclei are growing as isolated particles. When the nuclei are spaced so far that their diffusion fields overlap, then the time taken to reach a given size decreases with increasing temperature.
A UHV technique is presented for evaluating the adsorption-desorption properties of UHV vapor-deposited metal particles supported on insulating substrates. Desorption studies of CO from particulate and continuous Pd films supported on mica were performed. The desorption results indicate that: the CO desorption energies from the deposited metals are much lower than those from bulk single crystals; two desorption states exist for the vapor-deposited films; and the lower energy desorption peak of the vapor-deposited films is coverage dependent. Possible reasons for the difference between previously reported CO desorption studies on bulk substrates and the present results are discussed.
The structure of small platinum particles condensed in vacuum onto NaCl (001), NaCl (111) and mica substrates was studied by electron diffraction and electron microscopy. Results show that above a certain substrate temperature decahedral or icosahedral particles are formed. These particles are practically absent with substrates cleaved in high vacuum. They are always much less numerous than in gold films prepared under the same conditions. Assumptions made to explain this phenomenon are: (1) the initial growth of an abnormal structure of the nuclei as opposed by the substrate; (2) the particles disappear before they attain a size which corresponds to the observations; and (3) the particles result from a coalescence mechanism leading to multiple twinned particles.
High resolution transmission electron microscopy (HRTEM) observations were made of a mixture of mica and montmorillonite from fine-grained calcium, aluminum inclusions (CAI) in the Allende C3(V) meteorite. A petrographic thin section having a diameter of 4 mm contained CAI fragments ranging from less than 1 to 50 microns. The observed textural and chemical characteristics placed the inclusion in the fine-grained alkali-rich spinel aggregate category of Warks' (1979) classifications of CAIs and as type 3 in Kornacki's classifications of fine grains in Allende. Chemical analyses were performed on the phyllosilicate grains observed in the TEM scan by means of an X ray observed, and the proximity to the matrix boundary suggests a metamorphism which included aqueous alteration at a relatively low temperature.
The survival of the Galactic magnetic field almost certainly sets an astrophysical upper bound of approx. 10 to the minus 15th power cm(-2) sr(-1) s(-1) on the flux of monopoles. To improve significantly upon this Parker limit with direct, real time searches would require a detector area of approx. 10,000 square meters and a collection time of years. Several such searches are being contemplated. A novel alternative scheme using large mica crystals capable of recording and storing tracks of slow monopoles over a time scale of approx. 10 to the 9th power years was proposed.
Au was implanted into the (001) surface of Muscovite mica at an energy of 1.1 MeV and at doses of 1, 3, 6, and 10 x 10(exp 16) ions/cu cm. Optical spectra of the as-implanted samples revealed a peak at 2.28 eV (545 nm) which is attributed to the surface plasmon absorption of Au colloids. The infrared reflectance measurements show a decreasing reflectivity with increasing ion dose in the Si-O stretching region (900-1200 /cm). A new peak observed at 967 /cm increases with the ion dose and is assigned to an Si-O dangling bond. Atomic force microscopy images of freshly cleaved samples implanted with 6 and 10 x 10(exp 16) ions/sq cm indicated metal colloids with diameters between 0.9- 1.5 nm. AFM images of the annealed samples showed irregularly shaped structures with a topology that results from the fusion of smaller colloids.
Not Available
Explore the source record for details and available documents.
Not Available
Abstract not provided
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.