Search NASA⌕ Search

SEARCH · Search NASA

Results for “Martensite”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Hydrogen adsorption and diffusion, and subcritical-crack growth in high strength steels and nickel base alloys

Embrittlement, or the enhancement of crack growth by gaseous hydrogen in high strength alloys, is of primary interest in selecting alloys for various components in the space shuttle. Embrittlement is known to occur at hydrogen gas pressures ranging from fractions to several hundred atmospheres, and is most severe in the case of martensitic high strength steels. Kinetic information on subcritical crack growth in gaseous hydrogen is sparse at this time. Corroborative information on hydrogen adsorption and diffusion is inadequate to permit a clear determination of the rate controlling process and possible mechanism in hydrogen enhanced crack growth, and for estimating behavior over a range of temperatures and pressures. Therefore, coordinated studies of the kinetics of crack growth, and adsorption and diffusion of hydrogen, using identical materials, have been initiated. Comparable conditions of temperature and pressure will be used in the chemical and mechanical experiments. Inconel 718 alloy and 18Ni(200) maraging steel have been selected for these studies. Results from these studies are expected to provide not only a better understanding of the gaseous hydrogen embrittlement phenomenon itself, but also fundamental information on hydrogen adsorption and diffusion, and crack growth information that can be used directly for design.

Wei, R. P.↗

Gas-phase hydrogen permeation through alpha iron, 4130 steel, and 304 stainless steel from less than 100 C to near 600 C

Gas phase hydrogen permeation studies were conducted on hollow, cylindrical membranes of triply zone-refined alpha iron, AISI 304 austenitic stainless steel, and AISI-SAE 4130 steel in both the normalized (ferrite and carbide) and quenched and tempered (martensite) conditions. Membrane temperature was varied from less than 100 C to near 600 C and hydrogen pressure was varied. For one membrane material, normalized 4130 steel, gas phase hydrogen transport under both steady state and nonsteady state conditions was demonstrated to be controlled by lattice diffusion. Additionally, Sievert's law was shown to be applicable. For all membrane materials, expressions for the coefficients for hydrogen permeation were determined by analysis of steady state transport; the coefficients for diffusion were determined by the lag time technique applied to nonsteady state transport; and through a knowledge of the Sievert's constants, the subsurface equilibrium lattice hydrogen concentrations were determined.

Nelson, H. G.↗

The resistance of selected high strength alloys to embrittlement by a hydrogen environment

Selected high strength iron base and cobalt base alloys with yield strengths in the range from 1233 to 2129 MN per sq m (179 to 309 KSI) were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature. These alloys were strengthened initially by cold working which produced strain induced epsilon prime-hcp martensite and fcc mechanical twins in an fcc matrix. Heat treatment of the cobalt base alloy after cold working produced carbide precipitates with retention of an hcp epsilon phase which increased the yield strength level to a maximum of 2129 MN per sq m (309 KSI). High-strength alloys can be produced which have some resistance to degradation of mechanical properties by a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

Metallographic study of metallic fragment of lunar surface material

A high precision investigation of a metallic fragment from the lunar material returned by the Soviet Luna 16 automatic station revealed three characteristic temperature intervals with different kinetics of solid solution decomposition. The following were found in the structure of the iron-nickel-cobalt alloy: (1) delta-phase and alpha-ferrite of diffusional, displacement origin in the grain boundary and acicular forms; and (2) martensite of isothermal and athermal nature, acicular, lamellar, massive, and dendritic. The diversity of the shapes of structural constituents is associated with the effect on their formation of elastic distortions and various mechanisms of deformation relaxation processes.

Mints, R. I.↗

The resistance of selected high strength alloys to embrittlement by a hydrogen environment

Selected high strength iron base and cobalt base alloys were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature. These alloys were strengthened initially by cold working which produced strain induced martensite and fcc mechanical twins in an fcc matrix. Heat treatment of the cobalt base alloy after cold working produced carbide precipitates with retention of an hcp epsilon phase which increased the yield strength level. High strength alloys can be produced which have some resistance to degradation of mechanical properties by a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

The resistance to embrittlement by a hydrogen environment of selected high strength iron-manganese base alloys

Fe-16Mn and Fe-25Mn base alloys, which had been cold worked to yield strength levels of 201 and 178 KSI, were resistant to degradation of mechanical properties in a one atmosphere hydrogen environment at ambient temperature under the loading conditions employed in this investigation. Transmission electron microscopy established that bands of epsilon phase martensite and fcc mechanical twins were formed throughout the fcc matrix when these alloys were cold worked. In the cold worked alloys a high density of crystal defects were observed associated with both types of strain induced structures, which should contribute significantly to the strengthening of these alloys. High strength iron base alloys can be produced which appear to have some resistance to degradation of mechanical properties in a hydrogen environment under certain conditions.

Benson, R. B., Jr.↗

Tough cryogenic alloys from the Fe-Mn and Fe-Mn-Cr systems

By adjusting composition, metastable gamma (austenite) and epsilon (hexagonal) martensite may be retained in Fe-Mn and Fe-Mn-Cr alloys and used to impact toughness through the TRIP mechanism. The resulting alloys have excellent toughness at cryogenic temperatures. The best alloys obtained to date are: Fe-20Mn, with sigma (sub y) = 79ksi and K sub IC = 275ksi square root of (in) at 77 K, and Fc-16Mn-8Cr, with sigma sub y = 85ksi and K sub IC = 72ksi square root of (in) at 77 K.

Schanfein, M. J.↗

Fatigue failure of hydrogen embrittled high strength steels

Results of an experimental investigation are presented concerning the fracture behavior of cathodically charged, quenched and tempered martensitic steels under cyclic load conditions. Introduction of H2 by cathodic charging reduced fatigue life by as much as 60%. It is proposed that subsurface transverse fatigue cracks nucleate simultaneously at multiple sites, such as at microcracks, voids, or inclusions. Fatigue crack growth then occurs on planes perpendicular to the major applied stress axis in the presence of the critical combination of applied external stress and hydrogen.

Kim, Y. G.↗

The metallic microstructures and thermal histories of severely reheated chondrites

The metallographic structures of eight severely reheated chondrites - Farmington, Ramsdorf, Orvinio, Wickenburg, Lubbock, Rose City, Arapahoe, and Tadjera - were studied using optical, SEM and electron microprobe techniques. The following metallographic criteria were used to estimate the post-shock residual temperature of the chondrites: melted metal-troilite appearance, presence of martensite, phosphorus enrichment of metal and averaging of central metal grain compositions. The presence of phosphides and secondary kamacite are due to slow post-shock cooling rates. Ni rim gradients indicate both extensive remelting of metal grains and relatively fast cooling.

Smith, B. A.↗

The design of an Fe-12Mn-O.2Ti alloy steel for low temperature use

An investigation was made to improve the low temperature mechanical properties of Fe-8 approximately 12% Mn-O 2Ti alloy steels. A two-phase(alpha + gamma) tempering in combination with cold working or hot working was identified as an effective treatment. A potential application as a Ni-free cryogenic steel was shown for this alloy. It was also shown that an Fe-8Mn steel could be grain-refined by a purely thermal treatment because of its dislocated martensitic structure and absence of epsilon phase. A significant reduction of the ductile-brittle transition temperature was obtained in this alloy. The nature and origin of brittle fracture in Fe-Mn alloys were also investigated. Two embrittling regions were found in a cooling curve of an Fe-12Mn-O 2Ti steel which was shown to be responsible for intergranular fracture. Auger electron spectroscopy identified no segregation during solution-annealing treatment. Avoiding the embrittling zones by controlled cooling led to a high cryogenic toughness in a solution-annealed condition.

Hwang, S. K.↗

The suppression of low-temperature intergranular brittleness in ferritic Fe-Mn alloys

A method for obtaining cryogenic toughness in an Fe-12Mn-0.2Ti alloy by a controlled cooling technique is presented. The intergranular fracture surface of the quenched alloy, using an AES, revealed no significant difference from that obtained by the bulk transgranular fracture surface, indicating the absence of large-scale grain boundary segregation during the austenitizing treatment. Attention is given to the step cooling method, using a furnace at temperatures of 100 to 120 C, followed by fast cooling to ambient temperature, which in turn produces a high-impact toughness without intergranular brittleness. It is concluded that the sources of brittle intergranular fracture in the alloy are both chemical, operating in martensitic structure, and nonchemical, active during quenching from the austenitizing treatment.

Hwang, S. K.↗

An electron-microscope study of alpha to gamma transformation in an iron-nickel alloy

Procedures used to study the alpha to gamma conversion in thin foils of an iron alloy with 32% nickel concentration and initial martensite conversion temperature of -60 C are described. Photomicrographs show deformation twinning as well as changes in samples after they were heated. Reverse conversion is discussed and results are examined.

Lobodyuk, V. A.↗

Magnetization of small iron-nickel spheres

Magnetic properties of small iron-nickel alloy spheres, having compositions which cover the entire Fe-Ni binary, are presented. The spheres were formed during solidification in free fall following the melting of electropolished wires of appropriate composition. The spheres with Ni not greater than 25% acquired a martensitic thermal remanence while those with Ni not less than 30% acquired a thermoremanent magnetization. A magnetic remanence-composition diagram and a coercive force-composition diagram are constructed. Magnetic hysteresis loops and derived parameters demonstrate the difference between metal-bearing and oxide-bearing natural samples. The magnetic remanence varies as the sphere size in conjunction with the microstructure. These results help to explain why coercive force is generally low, remanent coercive force is generally high, and their ratio (R/C) is always large in fine metal dispersions, such as lunar samples and chondrite meteorites.

Wasilewski, P.↗

Mechanical properties of weldments in experimental Fe-12Mn-0.2Ti and Fe-12Mn-1Mo-0.2Ti alloys for cryogenic service

Mechanical properties of weldments in two Fe-12Mn experimental alloys designed for cryogenic service were evaluated. Weldments were made using the GTA welding process. Tests to evaluate the weldments were conducted at -196 C and included: equivalent energy fracture toughness tests; autogenous transverse weld, notched transverse weld, and longitudinal weld tensile tests; and all-weld-metal tensile tests. The Fe-12Mn-0.2Ti and Fe-12Mn-1Mo-0.2Ti alloys proved weldable for cryogenic service, with weld metal and heat-affected zone properties comparable with those of the base metal. Optimum properties were achieved in the base alloys, weld metals, and heat-affected zones after a two-step heat treatment consisting of austenitizing at 900 C followed by tempering at 500 C. The Mo-containing alloy offered a marked improvement in cryogenic properties over those of the Mo-free alloy. Molybdenum increased the amount of retained austenite and reduced the amount of epsilon martensite observed in the microstructure of the two alloys.

Stephens, J. R.↗

Crack tip deformation and fatigue crack growth

Recent research on fatigue crack growth is summarized. Topics discussed include the use of the differential stress intensity factor to characterize crack tip deformation, the use of the unzipping model to study the growth of microcracks and the fatigue crack growth in a ferritic-martensitic steel, and the development of a model of fatige crack growth threshold. It is shown that in the case of small yielding, the differential stress intensity factor provides an adequate description of cyclic plastic deformation at the crack tip and correlates well with the crack growth rate. The unzipping model based on crack tip shear decohesion process is found to be in good agreement with the measured crack growth and striation spacing measurements. The proposed model of crack growth threshold gives correct predictions of the crack growth behavior in the near-threshold region.

Liu, H.-W.↗

Metallic alloy stability studies

The dimensional stability of candidate cryogenic wind tunnel model materials was investigated. Flat specimens of candidate materials were fabricated and cryo-cycled to assess relative dimensional stability. Existing 2-dimensional airfoil models as well as models in various stages of manufacture were also cryo-cycled. The tests indicate that 18 Ni maraging steel offers the greatest dimensional stability and that PH 13-8 Mo stainless steel is the most stable of the stainless steels. Dimensional stability is influenced primarily by metallurgical transformations (austenitic to martensitic) and manufacturing-induced stresses. These factors can be minimized by utilization of stable alloys, refinement of existing manufacturing techniques, and incorporation of new manufacturing technologies.

Firth, G. C.↗

Grain-refining heat treatments to improve cryogenic toughness of high-strength steels

The development of two high Reynolds number wind tunnels at NASA Langley Research Center which operate at cryogenic temperatures with high dynamic pressures has imposed severe requirements on materials for model construction. Existing commercial high strength steels lack sufficient toughness to permit their safe use at temperatures approaching that of liquid nitrogen (-320 F). Therefore, a program to improve the cryogenic toughness of commercial high strength steels was conducted. Significant improvement in the cryogenic toughness of commercial high strength martensitic and maraging steels was demonstrated through the use of grain refining heat treatments. Charpy impact strength at -320 F was increased by 50 to 180 percent for the various alloys without significant loss in tensile strength. The grain sizes of the 9 percent Ni-Co alloys and 200 grade maraging steels were reduced to 1/10 of the original size or smaller, with the added benefit of improved machinability. This grain refining technique should permit these alloys with ultimate strengths of 220 to 270 ksi to receive consideration for cryogenic service.

Rush, H. F.↗

Studies of an artificially shock-loaded H group chondrite

SEM and TEM, together with thermoluminescence (TL), are used to study five samples of the naturally unshocked Kernouve (H6) meteorite that were shock-loaded to pressures of 70, 165, 270, and 390 kbar. Attention is given to olivine and orthopyroxene deformation mechanisms at these pressure levels. The microhardness of the kamacite in the samples increases with shock pressure, and it is noted that annealed kamacite displays incipient crystallinity, while alpha-martensite and taenite sometimes contain slip lines. At pressures over 200 kbar, there was a systematic decrease in both natural TL and TL sensitivity. Changes in the ratio of these two values for various regions of the TL glow curve suggest that two processes were effective during shock: thermal drainage of electron traps and a reduction in the effective trap density. Thermal effects with widespread annealing are noted in the case of a sample subjected to shock pulse.

Sears, D. W.↗