Search NASA⌕ Search

SEARCH · Search NASA

Results for “Polyolefin”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

PET and polyolefin plastics supply chains in Michigan: present and future systems analysis of environmental and socio-economic impacts

Many actions are underway at global, national, and local levels to increase plastics circularity. However, studies evaluating the environmental and socio-economic impacts of such a transition are lacking at regional levels in the United States. In this work, the existing polyethylene terephthalate and polyolefin plastics supply chains in Michigan were compared to a potential future (‘NextCycle’) scenario that looks at increasing Michigan’s overall recycling rate to 45%. Material flow analysis data was combined with environmental and socio-economic metrics to evaluate the sustainability of these supply chains for the modeled scenarios. Overall, the NextCycle scenario for these supply chains achieved a net 14% and 34% savings of greenhouse gas (GHG) emissions and energy impacts, when compared with their respective baseline values. Additionally, the NextCycle scenario showed a net gain in employment and wages, however, it showed a net loss of revenue generation outside of Michigan due to the avoided use of virgin resins in Michigan.

54 ENVIRONMENTAL SCIENCES↗

Recycling of Pretreated Polyolefin-Based Ocean-Bound Plastic Waste by Incorporating Clay and Rubber

Plastic waste found in oceans has become a major concern because of its impact on marine organisms and human health. There is significant global interest in recycling these materials, but their reclamation, sorting, cleaning, and reprocessing, along with the degradation that occurs in the natural environment, all make it difficult to achieve high quality recycled resins from ocean plastic waste. To mitigate these limitations, various additives including clay and rubber were explored. In this study, we compounded different types of ocean-bound (o-HDPE and o-PP) and virgin polymers (v-LDPE and v-PS) with various additives including a functionalized clay, styrene-multi-block-copolymer (SMB), and ethylene-propylene-based rubber (EPR). Physical observation showed that all blends containing PS were brittle due to the weak interfaces between the polyolefin regions and the PS domains within the polymer blend matrix. Blends containing clay showed rough surfaces and brittleness because of the non-uniform distribution of clay particles in the polymer matrix. To evaluate the properties and compatibility of the blends, characterizations using differential scanning calorimetry (DSC), scanning electron microscopy (SEM), and small-amplitude oscillatory shear (SAOS) rheology were carried out. The polymer blend (v-LDPE, o-HDPE, o-PP) containing EPR showed improved elasticity. Incorporating additives such as rubber could improve the mechanical properties of polymer blends for recycling purposes.

42 ENGINEERING↗

Minimum GHG emissions and energy consumption of U.S. PET and polyolefin packaging supply chains in a circular economy

There is a wide agreement on the urgency of transforming linear management of plastics towards a circular economy model. However, no clear pathways exist as to required recycling technologies involved and system-wide environmental impacts. This study explores such pathways in the U.S. for the most commonly used packaging plastics through a combination of mechanical and emerging advanced recycling technologies. A system optimization model aimed at minimizing environmental impacts was developed to determine optimal end-of-life (EOL) management and locations of existing and emerging U.S. recycling infrastructures. Our study includes material flows from virgin resin production through semi-manufacturing processes to existing EOL disposal and recycling processes. An optimized circular plastics packaging system achieved greenhouse gas (GHG) emission savings of up to 28% and cumulative energy demand (CED) savings of up to 46%, compared to the linear economy. Moreover, these savings of GHG emissions and CED impacts represent a reduction of 0.16% and 0.49% compared to annual U.S. GHG emissions and energy consumption in 2022, respectively. The optimal recycling rates and systems-level circularity ranged from 78–99% and 57–75%, respectively. Increased energy savings led to increased GHG emissions showing a potential trade-off between GHG emissions and energy. Analysis of 40 scenarios showed the importance of material collection distances, blend limit of mechanically recycled resins, process yields, and mandated recycling rates for achieving a sustainable circular economy of plastics.

09 - BIOMASS FUELS↗

The role of the Pt-group dehydrogenation catalyst in alkane metathesis for polyolefin deconstruction

Recent proposed approaches in the depolymerization of waste plastics employ an olefin intermediate to produce alkanes or alkenes using olefin metathesis in tandem chemistry. Here, in this study, we investigated the role of the dehydrogenation catalyst on reaction rate, kinetics, and product distribution in heterogeneous tandem dehydrogenation and olefin metathesis (alkane metathesis) of three different alkane reactants, including polyethylene. We found that many properties to which alkane dehydrogenation rates were sensitive-including metal composition, nanoparticle size, and surface doping of Re species also controlled activity in Tandem D/OM. When comparing Pd, Pt, and Pt 3 Sn 1 , supported Pd in tandem with a Re 2 O 7 olefin metathesis catalyst showed four-fold higher activity (surface area basis) compared to Pt or Pt 3 Sn 1 catalysts on the same support, mainly due to differences in the rate of hydrogenation. Catalyst preparation resulted in metal nanoparticles partially covered by ReO x , as seen from elemental mapping. Co-location of Re 2 O 7 and Pd correlated with increased rates of hydrogenation (i.e., an increase in the rate of alkane formation and simultaneous lowering of the rate of alkene formation), with a reaction order in catalyst study that further supported this conclusion. The Pd and Re 2 O 7 system displayed marked improvement compared to Pt or Pt 3 Sn 1 with Re 2 O 7 , and previous work, in the depolymerization rate of a linear polyethylene feedstock, with over 94 % reduction in polymer molecular weight in 15 h at 190 °C using less catalyst and increased reactant loadings, while keeping solvent to polymer consumption below 2.5.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Delamination recycling of multilayer plastic films: Solvent-assisted separation pathways and recovery of solid polyolefins

Multilayer plastic films are excellent packaging materials due to the bound layers of multiple polymers, with each different polymer contributing to the film properties. Desirable properties lead to continuously growing demand for multilayer films. Multilayer plastic films are typically single-use and, as such, their increased production and disposal have led to waste management problems. Multilayer films are not currently recyclable primarily due to the multiple bound polymers. This work advances delamination as a recycling process to separate and sequester valuable polymers from multilayer films, facilitating the incorporation of these polymers into the circular economy. We effect delamination in a physical process that preserves targeted polymers as solid film, hence retaining their embodied energy. This work documents three different pathways of inducing delamination of multilayer films, with appropriate solvents disrupting adhesion between adjacent layers or dissolving a minor component of the film in less than an hour and at temperatures below 90°C, and where all initial polyethylene is maintained in its solid form throughout the process and is recovered at high purity. Solvent-based delamination is exemplified on commercial multilayer films with majority polyethylene (PE), and polyethylene terephthalate (PET) or ethylene vinyl alcohol copolymer (EVOH) or nylon also present. Solvent-based delamination is an energy-efficient and environmentally friendly recycling process that improves upon dissolution-precipitation recycling, since delamination involves very little dissolution and no precipitation, and is superior to pyrolysis which breaks down the polymers, while delamination keeps polymer chains intact. Furthermore, delamination recycling can contribute to the sustainable use of multilayer films as they continue to protect our food and medicine.

Chemical Recycling↗

Increasing pyrolysis oil yields and decreasing energy consumption via thermal oxo-degradation of polyolefins

Commercialization of pyrolysis of plastics in an inert atmosphere is challenging due to large thermal requirements. This study employs thermal oxo-degradation and demonstrates how oxygen supplied at modest equivalence ratios can both accelerate depolymerization and provide the enthalpy for pyrolysis without dramatically impacting desired product yields. The enthalpies for pyrolysis of high-density polyethylene (HDPE) and polypropylene (PP) are measured to be 2,300 ± 90 J g – -1 and 2,800 ± 60 J g –1 , respectively. Using air as an oxygen source in a fluidized bed reactor, HDPE and PP are rapidly deconstructed while using up to 84% less energy through the energy released by partial oxidation. Characterization of the thermal oxo-degradation product oil shows comparable composition to conventional pyrolysis oil. Thermal oxo-degradation proves to be a promising technology for upcycling of plastics by improving thermal depolymerization of waste plastics and reducing energy requirements while maintaining desirable yields.

42 ENGINEERING↗

Catalytic Upgrading of Pyrolysis Condensables from Postconsumer Polyolefins Using HZSM-5

The conversion of plastic wastes to monomeric olefins is an attractive means for achieving a plastic circular economy. In our study, a fluidized bed reactor converts post-consumer waste high-density polyethylene (HDPE) and polypropylene (PP) to mostly condensed pyrolysis waxes and some oils, preventing carbon loss to gases. The pyrolysis condensables were upgraded to light olefins (C 2 –C 5 ) at carbon yields greater than 76 wt % using the HZSM-5 zeolite catalyst at a post pyrolysis process that employed a micropyrolyzer. These results were comparable to olefin monomer yields from direct ex situ catalytic pyrolysis of the original waste plastics without condensing the vapors, highlighting the potential applicability of this approach in plastic waste recycling. Our results suggest that a centralized catalytic upgrading facility fed by pyrolysis condensables sourced from distributed thermochemical processing plants is a promising pathway to a circular economy. Such an approach enables utilization of available catalytic cracking infrastructure while focusing on setting up distributed thermochemical processing plants close to material recovery facilities. As a result, the energy-dense pyrolysis waxes are more suitable for transportation, contributing to the overall scalability and economic viability of the proposed distributed approach.

10 SYNTHETIC FUELS↗

Effect of Macro- and Microstructures on Catalytic Hydrogenolysis of Polyolefins

Here, polyethylenes of varying molecular weight and branch density, as well as polypropylenes of varying molecular weight and tacticity, were catalytically converted to lower-molecular-weight liquid products to showcase how these various properties in a mixed waste plastic stream could affect the final product. A Pt nanoparticle on a strontium titanate nanocuboid (Pt/STO) catalyst was used under solvent-free conditions in the presence of 170 psi of H 2 at 300 °C for hydrogenolysis. The initial molecular weight of polyethylene was found to have a moderate effect on the yield to the final product (ranging from 55 wt% for M n ~ 7600 Da to 67 wt% for M n ~ 50,950 Da). The microstructure, defined as the length and density of branches in a polymer, of higher-molecular-weight polymers was the dominant factor in determining the yield (ranging from 67 wt% for M n ~ 50,950 Da for linear low-density polyethylene (LLDPE) with C 2 branches to 97 wt% for M n ~ 38,850 Da for LLDPE with C 6 branches). The same products (M n = C 29 –C 46 , Ð = 1.1–1.6) and distribution of undesired light gases (C 1 –C 4 ≈ 90 mol%, C 5 –C 8 ≈ 10 mol%) are obtained from conversions of PE of varying molecular weight. The tacticity of polypropylene at a given molecular weight had a significant effect on the molecular weight of the final product, while not strongly affecting conversion. Hydrogenolysis of isotactic polypropylene (iPP) produced ≈C 18 with a wider polydispersity (Ð ~ 1.4) compared to the narrow ≈C 64 (Ð ~ 1.0) and ≈C 54 (Ð ~ 1.0) products from atactic (aPP) and syndiotactic (sPP) polypropylene, respectively. The stereochemistry of the methyl groups dictates the shape and structure of the polymer in the melt, which in turn affects how the hydrocarbon chain interacts with the catalyst surface, thereby impacting the number of C–C scissions. These results show how various characteristics such as the molecular weight and structure of a waste plastic stream could affect the final product.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Polyhalohydrins: Investigating Vicinal Functionalities by Ring-Opening of Epoxides on Polyolefins

Halohydrins are functional groups that are underexplored in polymer science. This study synthesized and examined structure–property relationships of halohydrin-functionalized polymers derived from polycyclooctene (PCOE), which was obtained via ring-opening metathesis polymerization (ROMP). The polyhalohydrins, including polychlorohydrin, polybromohydrin, and polyiodohydrin, were produced through a two-step process involving epoxidation of PCOE followed by epoxide ring-opening using hydrochloric, hydrobromic, or hydroiodic acid. These stereoirregular and regioirregular polymers are amorphous as measured by differential scanning calorimetry and X-ray scattering. Lap joint shear testing revealed an enhanced adhesive performance in polychlorohydrin and polybromohydrin, with the former demonstrating nearly three times the ultimate shear stress compared to a model polyethylene, hydrogenated PCOE. Additionally, contact angle measurements and surface free energy analysis showed an increase in hydrophilicity and polarity from iodine- to bromine- to chlorine-functionalized polyhalohydrins, aligning with trends in adhesion strength. Furthermore, these results underscore the potential of halohydrin functionalization as a versatile approach for tuning surface properties, offering new opportunities for polymer-to-polymer transformations.

Functional groups↗