Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS CALCULATIONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

A comparison of constant-load and constant-deflection stress-corrosion tests on precracked DCB specimens

A comparison is made between measurements of stress-corrosion crack propagation made by a constant-load procedure and by a constant-deflection procedure. Precracked double cantilever beam specimens from 7075 aluminum alloy plate were used. The specimens were oriented in such a way that cracking would begin in the short-transverse plane and would propagate in the rolling direction. The specimens were subjected to a buffered salt-chromate solution and a 3.6% synthetic sea salt solution. The measurements were made optically with a binocular microscope. Stress intensities and crack lengths were calculated and crack velocities were obtained. Velocity was plotted against the average calculated stress intensity. Good agreement between the two methods was found for the salt-chromate solution, although some descrepancies were noted for the artificial sea salt solution.

Dorward, R. C.↗

Static Indentation Load Capacity of the Superelastic 60NiTi for Rolling Element Bearings

The nickel-rich, binary nickel-titanium alloys, such as 60NiTi (60Ni-40Ti by wt%), are emerging as viable materials for use in mechanical components like rolling element bearings and gears. 60NiTi is a superelastic material that simultaneously exhibits high hardness and a relatively low elastic modulus (approx.100 GPa). These properties result in the potential to endure extremely high indentation loads such as those encountered in bearings, gears and other mechanical components. In such applications, quantifying the load that results in permanent deformation that can affect component performance and life is important. In this paper, the static load capacity is measured by conducting indentation experiments in which 12.7 mm diameter balls made from the ceramic Si3N4 are pressed into highly polished, hardened 60NiTi flat plates. Hertz stress calculations are used to estimate contact stress. The results show that the 60NiTi surface can withstand an approximately 3400 kN load before significant denting (>0.6 microns deep) occurs. This load capacity is approximately twice that of high performance bearing steels suggesting that the potential exists to make highly resilient bearings and components from such materials.

DellaCorte, Christopher↗

The Effect of Pre-Stressing on the Static Indentation Load Capacity of the Superelastic 60NiTi

Superelastic nickel-titanium alloys, such as 60NiTi (60Ni-40Ti by wt.%), are under development for use in mechanical components like rolling element bearings and gears. Compared to traditional bearing steels, these intermetallic alloys, when properly heat-treated, are hard but exhibit much lower elastic modulus (approx.100 GPa) and a much broader elastic deformation range (approx.3 percent or more). These material characteristics lead to high indentation static load capacity, which is important for certain applications especially space mechanisms. To ensure the maximum degree of elastic behavior, superelastic materials must be pre-stressed, a process referred to as "training" in shape memory effect (SME) terminology, at loads and stresses beyond expected use conditions. In this paper, static indentation load capacity tests are employed to assess the effects of pre-stressing on elastic response behavior of 60NiTi. The static load capacity is measured by pressing 12.7 mm diameter ceramic Si3N4 balls into highly polished, hardened 60NiTi flat plates that have previously been exposed to varying levels of pre-stress (up to 2.7 GPa) to determine the load that results in shallow but measurable (0.6 m, 25 in. deep) permanent dents. Hertz stress calculations are used to estimate contact stress. Without exposure to pre-stress, the 60NiTi surface can withstand an approximately 3400 kN load before significant denting (>0.4 m deep) occurs. When pre-stressed to 2.7 GPa, a static load of 4900 kN is required to achieve a comparable dent, a 30 percent increase. These results suggest that stressing contact surfaces prior to use enhances the static indentation load capacity of the superelastic 60NiTi. This approach may be adaptable to the engineering and manufacture of highly resilient mechanical components such as rolling element bearings.

DellaCorte, Christopher↗

Predicting Bone Mechanical Properties of Cancellous Bone from DXA, MRI, and Fractal Dimensional Measurements

This project was aimed at making predictions of bone mechanical properties from non-invasive DXA and MRI measurements. Given the bone mechanical properties, stress calculations can be made to compare normal bone stresses to the stresses developed in exercise countermeasures against bone loss during space flight. These calculations in turn will be used to assess whether mechanical factors can explain bone loss in space. In this study we assessed the use of T2(sup *) MRI imaging, DXA, and fractal dimensional analysis to predict strength and stiffness in cancellous bone.

Harrigan, Timothy P.↗

A weak subducting slab at intermediate depths below northeast Japan

Knowledge of the state of stress in subducting slabs is essential for understanding their mechanical behavior and the physical processes that generate earthquakes. Here, we develop a framework which uses a high-resolution focal mechanism catalog to determine the change in the position of the neutral plane before and after the M9 Tohoku-oki earthquake to determine that the deviatoric stress within the slab at intermediate depths must be very low (~1 MPa). We show that by combining the static stress calculated from coseismic slip distributions with the stress orientations before and after the mainshock, we can determine the full deviatoric stress tensor within the subducting slab at intermediate depths. These results preclude earthquake source mechanisms that require large background driving stresses, favoring a mechanically weak subducting slab, thus providing quantitative constraints on the physical processes that generate intermediate-depth earthquakes.

58 GEOSCIENCES↗

Bellows flow-induced vibrations

Results of theoretical and experimental investigations of bellows typical of those found in space shuttle external tanks are presented. Correlation parameters are identified which generalize the alternating stress calculations cited in an earlier study. Alternating stress amplitudes and mean stress levels form the basis of a fatigue analysis incorporating seven ordinate charts for 347 stainless steel, alloy 21 6-9, and Inco 718. A crack propagation model is included with a program for computing bellows fatigue life. Two phase flow and material hardness properties are discussed.

Johnson, J. E.↗

Tensile and creep rupture behavior of P/M processed Nb-base alloy, WC-3009

Due to its high strength at temperatures up to 1600 K, fabrication of niobium base alloy WC-3009 (Nb30Hf9W) by traditional methods is difficult. Powder metallurgy (P/M) processing offers an attractive fabrication alternative for this high strength alloy. Spherical powders of WC-3009 produced by electron beam atomizing (EBA) process were successfully consolidated into a one inch diameter rod by vacuum hot pressing and swaging techniques. Tensile strength of the fully dense P/M material at 300-1590 K were similar to the arc-melted material. Creep rupture tests in vacuum indicated that WC-3009 exhibits a class 1 solid solution (glide controlled) creep behavior in the 1480 to 1590 K temperature range and stress range of 14 to 70 MPa. The creep behavior was correlated with temperature and stress using a power law relationship. The calculated stress exponent n, was about 3.2 and the apparent activation energy, Q, was about 270 kJ/mol. The large creep ductility exhibited by WC-3009 was attributed to its high strain rate sensitivity.

Hebsur, Mohan G.↗

Reactor Pressure Vessel Fracture Analysis Capabilities in Grizzly

Efforts have been underway to develop fracture mechanics capabilities in the Grizzly code to enable it to be used to perform deterministic fracture assessments of degraded reactor pressure vessels (RPVs). Development in prior years has resulted a capability to calculate -integrals. For this application, these are used to calculate stress intensity factors for cracks to be used in deterministic linear elastic fracture mechanics (LEFM) assessments of fracture in degraded RPVs. The -integral can only be used to evaluate stress intensity factors for axis-aligned flaws because it can only be used to obtain the stress intensity factor for pure Mode I loading. Off-axis flaws will be subjected to mixed-mode loading. For this reason, work has continued to expand the set of fracture mechanics capabilities to permit it to evaluate off-axis flaws. This report documents the following work to enhance Grizzly’s engineering fracture mechanics capabilities for RPVs: • Interaction Integral and -stress: To obtain mixed-mode stress intensity factors, a capability to evaluate interaction integrals for 2D or 3D flaws has been developed. A -stress evaluation capability has been developed to evaluate the constraint at crack tips in 2D or 3D. Initial verification testing of these capabilities is documented here. • Benchmarking for axis-aligned flaws: Grizzly’s capabilities to evaluate stress intensity factors for axis-aligned flaws have been benchmarked against calculations for the same conditions in FAVOR. • Off-axis flaw demonstration: The newly-developed interaction integral capabilities are demon- strated in an application to calculate the mixed-mode stress intensity factors for off-axis flaws. • Other code enhancements: Other enhancements to the thermomechanics capabilities that relate to the solution of the engineering RPV fracture problem are documented here.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

A workflow to assess the efficacy of brine extraction for managing injection-induced seismicity potential using data from a CO 2 injection site near Decatur, Illinois

Injection of CO 2 for storage in a geologic formation increases pore pressure and alters in situ stresses. Depending on the orientation of any existing fault and fracture planes, such as critically stressed planes, this stress alteration will modify normal stresses acting on planes and could result in frictional sliding and release stored energy in the form of seismicity. Brine extraction (BE) is a technique that can be applied prior to, or during, CO 2 injection to reduce pore pressure for increasing storage capacity and, potentially, for reducing the likelihood of frictional sliding. Here a workflow is described to assess the efficacy of BE for mitigating frictional sliding (i.e., seismicity) during injection and entails: site characterization, stress calculations and failure assessment, static and dynamic modeling, and BE operational planning. Site characterization describes the stress field used to calculate the Coulomb Failure Function (CFF) that constrains allowable pore pressure changes and injection rates in the numerical simulation of CO 2 injection scenarios. The inclusion of BE in the workflow allows for determination of the potential need for pressure reduction, and evaluation of the effectiveness of this operation. Example application of the workflow using an injection field dataset near Decatur, IL, provides insight on fracture planes and stresses at the site, formation properties and the impact of variable CO 2 injection-rate targets on whether BE plans are required. The study workflow indicates that BE could enhance CO 2 injection rate by 39% and correspondingly reduce the potential for injection-induced seismicity as indicated by a reduction in CFF.

58 GEOSCIENCES↗

In plane stress analysis

An investigation of the blowing up of UK numerical results for the inplane stress calculations for silicon ribbon is presented. The inplane stress that exists in a thin plate is governed by two general equations of equilibrium and compatibility.

Dillon, O. W., Jr.↗

Projected Seismic Activity at the Tiger Stripe Fractures on Enceladus, Saturn, From an Analog Study of Tidally Modulated Icequakes Within the Ross Ice Shelf, Antarctica

Abstract Dissipation of tidal energy is expected to generate seismicity on icy‐ocean worlds; however, the distribution and timing of this seismic activity throughout an orbital cycle is not known. We used new observations from an icy‐ocean‐world analog environment on Earth to examine the relationship between tidally driven tensile stress and seismic activity within an ice shell. We investigated a pair of rifts within Antarctica's Ross Ice Shelf which are tidally stressed in a manner analogous to the orbital cycle of tidal stress experienced by Enceladus' Tiger Stripe Fractures. We found that seismic activity at the Antarctic rifts is sensitive to both the amplitude and the rate of tensile stress across the rifts. We combined these findings with calculated stress values along Enceladus' Tiger Stripe Fractures to predict seismic‐activity levels expected along the ice‐shell fractures. We predict a peak in seismicity along the four Tiger Stripe Fractures when Enceladus is 90°–120° past pericenter in its orbit around Saturn, at which point tensile stresses would reach ∼2/3 of their maximum value. We also used the magnitude distribution of icequakes along Antarctic rifts to investigate implications for the likely size of stick‐slip rupture patches along icy faults on Enceladus. Our findings predict that the Tiger Stripe Fractures should produce sustained, low‐magnitude seismic events that involve rupture along discrete portions of each fracture's total length. We predict that seismicity would fall to 50% of peak levels when stresses across the Tiger Stripe Fractures are dominantly compressional.

Olsen, Kira G.↗

Predicting failure of specimens with either surface cracks or corner cracks at holes

A previously developed fracture criterion was applied to fracture data for surface-cracked specimens subjected to remote tensile loading and for specimens with a corner crack (or cracks) emanating from a circular hole subjected to either remote tensile loading or pin loading in the hole. The failure stresses calculated from this criterion were consistent with experimental failure stresses for both surface and corner cracks for a wide range of crack shapes and crack sizes in specimens of aluminum alloy, titanium alloy, and steel. Empirical equations for the elastic stress-intensity factors for a surface crack and for a corner crack (or cracks) emanating from a circular hole in a finite-thickness and finite-width specimen were also developed.

Newman, J. C., Jr.↗

Rational approach for assumed stress finite elements

A new method for the formulation of hybrid elements by the Hellinger-Reissner principle is established by expanding the essential terms of the assumed stresses as complete polynomials in the natural coordinates of the element. The equilibrium conditions are imposed in a variational sense through the internal displacements which are also expanded in the natural co-ordinates. The resulting element possesses all the ideal qualities, i.e. it is invariant, it is less sensitive to geometric distortion, it contains a minimum number of stress parameters and it provides accurate stress calculations. For the formulation of a 4-node plane stress element, a small perturbation method is used to determine the equilibrium constraint equations. The element has been proved to be always rank sufficient.

Pian, T. H. H.↗

Evaluation of Increased Peak Temperatures for Spent Fuel Cladding Performance during Dry Storage (Rev.1)

NUREG-2214, “Managing Aging Processes in Storage (MAPS) Report,” (2019) documents the technical basis for age-related degradation mechanisms on spent nuclear fuel assemblies during dry storage operations. The technical bases have been reviewed, and hoop cladding stress calculations were conducted using the Fuel Analysis under Steady-state and Transients (FAST) code at elevated normal condition temperatures of 425°C and 450°C, and at an off-normal and accident conditions temperature of 600°C. The NUREG-2214 conclusions are substantiated by the referenced literature. The calculations demonstrate that the aging mechanisms primarily driven by hoop stress such as hydride reorientation, delayed hydride cracking, thermal and athermal (low-temperature) creep, and localized mechanical overload are either not credible or do not compromise the fuel assembly’s performance for increased peak normal condition temperatures of 425°C or 450°C during the up to 60-year dry storage period. Other aging mechanisms considered are also not credible for compromising the fuel assembly’s performance during 60-year dry storage with a peak temperature of 400ºC as specified in ISG – 11 Rev. 3, and the same is indicated for the increased peak normal condition temperatures of 425°C or 450°C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Modeling fatigue crack growth in cross ply titanium matrix composites

In this study, the fatigue crack growth behavior of fiber bridging matrix cracks in cross-ply SCS-6/Ti-15-3 and SCS-6/Timetal-21S laminates containing center holes was investigated. Experimental observations revealed that matrix cracking was far more extensive and wide spread in the SCS-6/Ti-15-3 laminates compared to that in the SCS-6/Timetal-21S laminates. In addition, the fatigue life of the SCS-6/Ti-15-3 laminates was significantly longer than that of the SCS-6/Timetal-21S laminates. The matrix cracking observed in both material systems was analyzed using a fiber bridging (FB) model which was formulated using the boundary correction factors and weight functions for center hole specimen configurations. A frictional shear stress is assumed in the FB model and was used as a curve fitting parameter to model matrix crack growth data. The higher frictional shear stresses calculated in the SCS-6/Timetal-21S laminates resulted in lower stress intensity factors in the matrix and higher axial stresses in the fibers compared to those in the SCS-6/Ti-15-3 laminates at the same applied stress levels.

Bakuckas, J. G., Jr.↗