Stress intensity factors for deep cracks emanating from the corner formed by a hole intersecting a plate surface

The stress intensity factors (SIFs) at the end points of flaws emanating from the corner formed by the intersection of a plate with a hole were determined using stress freezing photoelasticity and a numerical technique known as the Taylor series correction method to extract the SIF values from the photoelastic data. The geometries studied were crack depth to thickness ratios of about 0.2, 0.5, and 0.75; crack depth to crack length ratios of about 1.0 to 2.0; and crack length to hole radius ratios of about 0.5 to 2.0. The SIFs were determined at the intersection of the flaw border with the plate surface (KS) and with the edge of the hole (KH). It is shown that extension of a crack emanating from a corner of intersection of a hole with a plate under monotonically increasing load is not self-similar and that as the flaw depth increases, KH decreases and KS increases. Existing theories and design criteria significantly overestimate the SIF at both the hole and the surface except for shallow flaws at the hole and deep flaws at the surface.

Mcgowan, J. J.↗

Mixed mode stress-intensity-factors in mode-3 loaded middle crack tension specimen

A three dimensional stress analysis of a middle-crack tension specimen subjected to mode-3 type loading was performed using fracture mechanics based finite element code FRAC3D. Three-dimensional stress intensity factors were calculated for a range of specimen thicknesses that represent the structures used in aerospace and nuclear industries. Calculated SIF for very thick specimen (thickness-to-crack length b/a greater than or equal to 30) agreed very well with the antiplane solution in the literature. The K(sub II) stress field exists near the intersection of the crack front and free surface in a boundary-layer region covers the complete thickness of the plate and K(sub II) dominates all through the thickness. For very thin plates (b/a is less than .1), the average K(sub II) is larger than K(sub III) (about 25% for b/a = 0.1).

Shivakumar, Kunigal N.↗

On the Validity of the Tada Stress Intensity Factor Solution for the Single Edge Notch Tension Specimen With Pinned Ends

The validity of the Tada stress intensity factor (K Tada ) for pinned-ends single edge notch tension [SEN(T)] specimens is assessed via a combined experimental-modeling approach. Analysis of fatigue crack growth rate reductions during constant-∆K Tada loading demonstrates that specific combinations of alloy stiffness, geometry, and loading result in the true K deviating below K Tada . Geometrically non-linear, 3-dimensional finite element calculations confirm mild-to-strong influences of these parameters, which are not captured by K Tada . Most existing pinned SEN(T) data are found to use parameters where KTada is not significantly reduced, but the present results underscore the need for a more broadly applicable K solution.

Non-linear FEA↗

Strain energy release rate determination of stress intensity factors by finite element methods

The stiffness derivative finite element technique is used to determine the Mode I stress intensity factors for three-crack configurations. The geometries examined include the double edge notch, single edge notch, and the center crack. The results indicate that when the specified guidelines of the Stiffness Derivative Method are used, a high degree of accuracy can be achieved with an optimized, relatively coarse finite element mesh composed of standard, four-node, plane strain, quadrilateral elements. The numerically generated solutions, when compared with analytical ones, yield results within 0.001 percent of each other for the double edge crack, 0.858 percent for the single edge crack, and 2.021 percent for the center crack.

Walsh, R. M., Jr.↗

Determination of stress intensity factors for interface cracks under mixed-mode loading

A simple technique was developed using conventional finite element analysis to determine stress intensity factors, K1 and K2, for interface cracks under mixed-mode loading. This technique involves the calculation of crack tip stresses using non-singular finite elements. These stresses are then combined and used in a linear regression procedure to calculate K1 and K2. The technique was demonstrated by calculating three different bimaterial combinations. For the normal loading case, the K's were within 2.6 percent of an exact solution. The normalized K's under shear loading were shown to be related to the normalized K's under normal loading. Based on these relations, a simple equation was derived for calculating K1 and K2 for mixed-mode loading from knowledge of the K's under normal loading. The equation was verified by computing the K's for a mixed-mode case with equal and normal shear loading. The correlation between exact and finite element solutions is within 3.7 percent. This study provides a simple procedure to compute K2/K1 ratio which has been used to characterize the stress state at the crack tip for various combinations of materials and loadings. Tests conducted over a range of K2/K1 ratios could be used to fully characterize interface fracture toughness.

Naik, Rajiv A.↗

Stress intensity factors for deep cracks emanating from the corner formed by a hole intersecting a plate surface

A technique consisting of a marriage between stress freezing photoelasticity and a numerical method was used to obtain stress intensity factors for natural cracks emanating from the corner at which a hole intersects a plate surface. Geometrics studied were: crack depth to thickness ratios of approximately 0.2, 0.5, and 0.75; crack depth to crack length ratios of approximately 1.0 to 2.0. All final crack geometries were grown under monotonic loading and growth was not self similar with most of the growth occurring through the thickness under remote extension. Stress intensity plate surface K sub s factors were determined at the intersection of the flaw border with the plate surface K sub s and with the edge of the hole K sub h. Results showed that for the relatively shallow flaws K sub h approximately equal to 1.5 K sub s, for the moderately deep flaws K sub h approximately equal to K sub s, and for the deep flaws K sub h approximately equal to 0.5 K sub s, revealing a severe sensitivity of K to flaw geometry.

Mcgowan, J. J.↗

Finite elements for determination of crack tip elastic stress intensity factors.

A new type of finite element is introduced which embodies the inverse square root singularity of the stress distribution arising near a crack in an elastic medium. Using this element near the crack tip in two typical cracked configurations, stress intensity factors within 5% of accepted values were obtained, with meshes having as few as 250 degrees of freedom.

Tracey, D. M.↗

Stress-intensity factor calculations using the boundary force method

The Boundary Force Method (BFM) was formulated for the three fundamental problems of elasticity: the stress boundary value problem, the displacement boundary value problem, and the mixed boundary value problem. Because the BFM is a form of an indirect boundary element method, only the boundaries of the region of interest are modeled. The elasticity solution for the stress distribution due to concentrated forces and a moment applied at an arbitrary point in a cracked infinite plate is used as the fundamental solution. Thus, unlike other boundary element methods, here the crack face need not be modeled as part of the boundary. The formulation of the BFM is described and the accuracy of the method is established by analyzing a center-cracked specimen subjected to mixed boundary conditions and a three-hole cracked configuration subjected to traction boundary conditions. The results obtained are in good agreement with accepted numerical solutions. The method is then used to generate stress-intensity solutions for two common cracked configurations: an edge crack emanating from a semi-elliptical notch, and an edge crack emanating from a V-notch. The BFM is a versatile technique that can be used to obtain very accurate stress intensity factors for complex crack configurations subjected to stress, displacement, or mixed boundary conditions. The method requires a minimal amount of modeling effort.

Tan, P. W.↗

Determination of Stress Intensity Factor Distributions for "Interface" Cracks in Incompressible, Dissimilar Materials

The present study was undertaken in order to develop test methods and procedures for measuring the variation of the stress intensity factor through the thickness in bimaterial specimens containing cracks within and parallel to the bond line using the frozen stress photoelastic method. Since stress freezing materials are incompressible above critical temperature, and since thick plates are to be employed which tend to produce a state of plane strain near the crack tip, the interface near tip fracture equations reduce to the classic form for homogeneous materials. Moreover, zero thickness interfaces do not exist when materials are bonded together. It was decided early on that it would be important to insure a uniform straight and accurate crack tip region through the thickness of the body to reduce scatter in the SIF distribution through the thickness. It was also observed that rubberlike materials which were desired to be modeled exhibited significant tip blunting prior to crack extension and that some blunting of the tip would provide a more realistic model. It should be noted that, in normal stress freezing photoelastic work, it is considered good practice to avoid utilizing data near bond lines in photoelastic models due to the bond line stresses which inevitably develop when two parts are bonded together. Thus, the present study involves certain exploratory aspects in deviating from standard practice in stress freezing work. With the above ideas in mind, several different test methods were investigated and are described in the following sections and appendices. The geometry selected for the program was a thick, edge cracked specimen containing a bond line.

Smith, C. W.↗

Stress-intensity factors for cracks emanating from the loaded fastener hole

Using a series approach and the Muskhelishvili formulation in the two-dimensional theory of elasticity, stress-intensity factors K are derived for problems in which cracks emanate radially from the boundary of an arbitrarily loaded internal circular hole in an infinite plate. Numerical values are obtained for K(I) and K(II) for radial cracks from a hole containing a loose-fitted pin or rivet that is pulled perpendicular to the crack direction in the plane of the plate. The method is a general one for determining K for a set of symmetrically emanating radial cracks for a variety of concentrated or distributed tractions on the circular hole.

Shivakumar, V.↗

A virtual crack-closure technique for calculating stress intensity factors for cracked three dimensional bodies

A three-dimensional virtual crack-closure technique is presented which calculates the strain energy release rates and the stress intensity factors using only nodal forces and displacements from a standard finite element analysis. The technique is an extension of the Rybicki-Kanninen (1977) method, and it assumes that any continuous function can be approximated by a finite number of straight line segments. Results obtained by the method for surface cracked plates with and without notches agree favorably with previous results.

Shivakumar, K. N.↗

Dynamic stress intensity factors of brittle materials

A new hybrid experimental-numerical procedure was used to characterize dynamic fracture response of structural ceramics at elevated temperature. The dynamic stress intensity factor (SIF) versus crack velocity relations of glass and reaction bonded silicon nitride (RBSN), are reviewed. The dynamic SIF versus crack velocity relations of alumina, TiB2-particulate/SiC-matrix composite and SiCw/Alumina-matrix composite are also presented. Available data indicated that dynamic arrest SIF was not observed in glass and monolithic ceramics, and suggested that further studies be conducted to resolve the existence or lack of existence of a dynamic arrest SIF in ceramic matrix composites.

Kobayashi, Albert S.↗

Transient analysis of the dynamic stress intensity factors using SGBEM for frequency-domain elastodynamics

In this paper, a two-dimensional symmetric-Galerkin boundary integral formulation for elastodynamic fracture analysis in the frequency domain is described. The numerical implementation is carried out with quadratic elements, allowing the use of an improved quarter-point element for accurately determining frequency responses of the dynamic stress intensity factors (DSIFs). To deal with singular and hypersingular integrals, the formulation is decomposed into two parts: the first part is identical to that for elastostatics while the second part contains at most logarithmic singularities. The treatment of the elastostatic singular and hypersingular singular integrals employs an exterior limit to the boundary, while the weakly singular integrals in the second part are handled by Gauss quadrature. Time histories (transient responses) of the DSIFs can be obtained in a post-processing step by applying the fast Fourier transform (FFT) and inverse FFT to the frequency responses of these DSIFs. Several test examples are presented for the calculation of the DSIFs due to two types of impact loading: Heaviside step loading and blast loading. The results suggest that the combination of symmetric-Galerkin and FFT algorithms in determining transient responses of the DSIFs is robust and effective.

36 MATERIALS SCIENCE↗

Stress intensity factors of eccentric cracks in bi-materials plate under mode I loading

Bi-material plates were generally used to joint electronic devices or mechanical components requiring dissimilar materials to be attached. During services, mechanical failure can be occurred due to the formation of cracks at the interfacial joint or away from the centre. Generally, linear elastic fracture mechanics approach is used to characterize these cracks based on stress intensity factors (SIF). Based on the literature survey, the SIFs for the central cracks were easily available. However, the SIFs for eccentric cracks were difficult to obtain. Therefore, this paper presented the SIFs for eccentric cracks subjected to mode I tension loading. Three important parameters were used such as relative crack depth, a/L, relative offset distance, b/L and elastic mismatch, E{sub 1}/E{sub 2} or α. It was found that such parameters significantly affected the characteristic of SIFs and it was depend on the location of cracks.

42 ENGINEERING↗

Calculation of stress intensity factors in an isotropic multicracked plate. Part 1: Theoretical development

An essential part of describing the damage state and predicting the damage growth in a multicracked plate is the accurate calculation of stress intensity factors (SIF's). Here, a methodology and rigorous solution formulation for SIF's of a multicracked plate, with fully interacting cracks, subjected to a far-field arbitrary stress state is presented. The fundamental perturbation problem is derived, and the steps needed to formulate the system of singular integral equations whose solution gives rise to the evaluation of the SIF's are identified. This analytical derivation and numerical solution are obtained by using intelligent application of symbolic computations and automatic FORTRAN generation capabilities (described in the second part of this paper). As a result, a symbolic/FORTRAN package, named SYMFRAC, that is capable of providing accurate SIF's at each crack tip was developed and validated.

Binienda, W. K.↗