Hydrocarbon-fuel/combustion-chamber-liner materials compatibility

The results of dynamic tests using methane and NASA-Z copper test specimen under conditions that simulate those expected in the cooling channels of a regeneratively cooled LOX/hydrocarbon booster engine operating at chamber pressures up to 3000 psi are presented. Methane with less than 0.5 ppm sulfur contamination has little or no effect on cooling channel performance. At higher sulfur concentrations, severe corrosion of the NASA-Z copper alloy occurs and the cuprous sulfide Cu2S, thus formed impedes mass flow rate and heat transfer efficiency. Therefore, it is recommended that the methane specification for this end use set the allowable sulfur content at 0.5 ppm (max). Bulk high purity liquid methane that meets this low sulfur requirement is currently available from only one producer. Pricing, availability, and quality assurance are discussed in detail. Additionally, it was found that dilute sodium cyanide solutions effectively refurbish sulfur corroded cooling channels in only 2 to 5 minutes by completely dissolving all the Cu2S. Sulfur corroded/sodium cyanide refurbished channels are highly roughened and the increased surface roughness leads to significant improvements in heat transfer efficiency with an attendant loss in mass flow rate. Both the sulfur corrosion and refurbishment effects are discussed in detail.

Homer, G. David↗

Corrosion of 310 stainless steel in H2-H2O-H2S gas mixtures: Studies at constant temperature and fixed oxygen potential

Corrosion of SAE 310 stainless steel in H2-H2O-H2S gas mixtures was studied at a constant temperature of 1150 K. Reactive gas mixtures were chosen to yield a constant oxygen potential of approximately 6 x 10 to the minus 13th power/cu Nm and sulfur potentials ranging from 0.19 x 10 to the minus 2nd power/cu Nm to 33 x 10 to the minus 2nd power/cu Nm. The kinetics of corrosion were determined using a thermobalance, and the scales were analyzed using metallography, scanning electron microscopy, and energy dispersive X-ray analysis. Two corrosion regimes, which were dependent on sulfur potential, were identified. At high sulfur potentials (p sub S sub 2 less than or equal to 2.7 x 10 to the minus 2nd power/cu Nm) the corrosion rates were high, the kinetics obeyed a linear rate equation, and the scales consisted mainly of sulfide phases similar to those observed from pure sulfication. At low sulfur potentials (P sub S sub 2 less than or equal to 0.19 x 10 to the minus 2nd power/cu Nm) the corrosion rates were low, the kinetics obeyed a parabolic rate equation, and scales consisted mainly of oxide phases.

Rao, D. B.↗

Effect of Immersion Time on Corrosion Behavior of Single-Phase Alloy and Nanocomposite Bismuth Telluride-Based Thermoelectrics in NaCl Solution

The corrosiveness of bismuth telluride-based thermoelectric materials (n-type single-phase alloy and a nanocomposite with MoS{sub 2} nanoinclusions), in 0.1 molar solution of sodium chloride (NaCl), was investigated. The electrochemical impedance spectroscopy curves obtained after 1, 24, 48 and 72 h immersion time revealed the enhancement of the corrosion resistance of the nanocomposite specimen in a 0.1 molar NaCl solution in comparison with the single-phase bismuth telluride-based alloys, and the passivity increased by immersion time up to 72 h. The nanocomposite sample with submicron grains provided suitable nucleation sites for passive film nucleation that led to higher protective behavior.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Degradation of Components After Exposure in a Biomass Pyrolysis System

X-ray diffraction, electron probe microanalysis, and scanning transmission electron microscopy with focused ion beam lift-out sample preparation techniques were used to study corrosion products in a 304L (UNS S30403) stainless steel fluidized-bed reactor segment from Iowa State University’s Pyrolysis Process Development Unit Facility. This reactor segment is particularly valuable because a detailed history of operation time, temperature, and biomass feedstock was available. As previously reported for a range of stainless steel pyrolysis-related equipment, external scaling and internal attack along alloy grain boundaries were observed. Here, the scaling was primarily associated with O, although S, Ca, K, Si, Mg, and P were also detected in the outer scale regions. However, unlike those other recent advanced characterization analyses, in this instance the internal alloy grain boundary attack was not directly related to S. Rather, only internal oxidation and localized nanoporosity were observed along the alloy grain boundaries, with associated local nanoscale Cr depletion and Ni enrichment. Mechanistic implications of this finding are discussed.

36 MATERIALS SCIENCE↗

The hot corrosion of Co-25Cr-10Ni-5Ta-3Al-0.5Y alloy /S-57/

A cobalt-base alloy, Co-25Cr-10Ni-5Ta-3Al-0.5Y (S-57), was subjected to hot corrosion in Mach 0.3 burner-rig combustion gases at maximum alloy temperatures of 900 and 1000 C. Various salt concentrations were injected into the burner: 0.5, 2,5, and 10 parts per million synthetic sea salt and 4 parts per million sodium sulfate (Na2SO4). The extent of corrosion was determined by measuring the maximum depth of corrosion in the alloy, and the corrosion process was studied by metallography, X-ray diffraction, scanning electron microscopy, and electron microprobe analysis. While S-57 was found to possess only moderate oxidation resistance at these temperatures, this alloy resisted significant hot corrosion attack under all but the most severe test conditions. The process of hot corrosion attack under the most severe conditions of this study was primarily sulfidation.

Santoro, G. J.↗

Reactions occurring during the sulfation of sodium chloride deposited on alumina substrates

The reaction between solid NaCl and air containing 1 pct SO2 has been studied between 500 and 700 C. The reaction product, Na2SO4, forms not only on the surface of the NaCl but also on surrounding areas of the substrate due to the volatility of the NaCl at these temperatures. At the higher temperatures, the vapor pressure of NaCl is so high that the majority of the reaction product is distributed on the substrate. Above 625 C, the reaction product is a liquid solution of NaCl and Na2SO4 that exists only so long as NaCl is supplied from the original crystal source. Eventually, the liquid solidifies by constitutional solidification as the NaCl is converted to Na2SO4. While it exists, the liquid NaCl-Na2SO4 solution is shown to be highly corrosive to Al2O3 and, on a scale of Al2O3 growing on alloy HOS 875, particularly attacks the grain boundaries of the scale at preferred sites where chromium and iron oxides and sulfides rapidly develop. This is proposed as one mechanism by which NaCl deposition contributes to the initiation of low temperature hot corrosion.

Wu, C. S.↗

Sulfide Generation by Dominant Halanaerobium Microorganisms in Hydraulically Fractured Shales

ABSTRACT Hydraulic fracturing of black shale formations has greatly increased United States oil and natural gas recovery. However, the accumulation of biomass in subsurface reservoirs and pipelines is detrimental because of possible well souring, microbially induced corrosion, and pore clogging. Temporal sampling of produced fluids from a well in the Utica Shale revealed the dominance of Halanaerobium strains within the in situ microbial community and the potential for these microorganisms to catalyze thiosulfate-dependent sulfidogenesis. From these field data, we investigated biogenic sulfide production catalyzed by a Halanaerobium strain isolated from the produced fluids using proteogenomics and laboratory growth experiments. Analysis of Halanaerobium isolate genomes and reconstructed genomes from metagenomic data sets revealed the conserved presence of rhodanese-like proteins and anaerobic sulfite reductase complexes capable of converting thiosulfate to sulfide. Shotgun proteomics measurements using a Halanaerobium isolate verified that these proteins were more abundant when thiosulfate was present in the growth medium, and culture-based assays identified thiosulfate-dependent sulfide production by the same isolate. Increased production of sulfide and organic acids during the stationary growth phase suggests that fermentative Halanaerobium uses thiosulfate to remove excess reductant. These findings emphasize the potential detrimental effects that could arise from thiosulfate-reducing microorganisms in hydraulically fractured shales, which are undetected by current industry-wide corrosion diagnostics. IMPORTANCE Although thousands of wells in deep shale formations across the United States have been hydraulically fractured for oil and gas recovery, the impact of microbial metabolism within these environments is poorly understood. Our research demonstrates that dominant microbial populations in these subsurface ecosystems contain the conserved capacity for the reduction of thiosulfate to sulfide and that this process is likely occurring in the environment. Sulfide generation (also known as “souring”) is considered deleterious in the oil and gas industry because of both toxicity issues and impacts on corrosion of the subsurface infrastructure. Critically, the capacity for sulfide generation via reduction of sulfate was not detected in our data sets. Given that current industry wellhead tests for sulfidogenesis target canonical sulfate-reducing microorganisms, these data suggest that new approaches to the detection of sulfide-producing microorganisms may be necessary.

04 OIL SHALES AND TAR SANDS↗

Effects of CO 2 and H 2 S on Corrosion of Martensitic Steels in Brines at Low Temperature

Corrosion studies were conducted for martensitic carbon steels in 5 wt% NaCl brine solutions at 4°C and 10 MPa (1,450 psi). These studies simulated different subsurface environments relevant to Arctic drilling. Here, two high-strength martensitic carbon steels, S-135 and UD-165, were studied in three different environments: (1) a CO 2 -NaCl-H 2 O solution with a CO 2 :H 2 O molar ratio of 0.312 in the whole system, (2) an H 2 S-NaCl-H 2 O solution with an H 2 S:H 2 O molar ratio of 3.12 × 10 –4 , and (3) a CO 2 -H 2 S-NaCl-H 2 O solution with the same acid gas to water ratios as environments 1 and 2. Results from the CO 2 +H 2 S mixed environment indicated that sour corrosion mechanism was dominant when the CO 2 :H 2 S molar ratio was 1,000. This impact of a small amount of H 2 S on the corrosion mechanism could be attributed to the specific adsorption of H 2 S on the steel surface. Electrochemical and mass loss measurements showed a distinct drop in the corrosion rate (CR) by more than one order of magnitude when transitioning from sweet to sour corrosion. This inhibiting effect on CR was attributed to the formation of a protective sulfide thin film. Tafel analyses of the anodic reaction showed that the Bockris mechanism was unlikely in the conditions tested. As a result, when comparisons were made between modeled and experimental CRs, good agreement was found in the CO 2 -only and H 2 S-only environments, but not in the CO 2 +H 2 S environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Study on the Corrosion Behavior of Carbon Steel Exposed to a H{sub 2}S-Containing NH{sub 4}Cl Medium

NH{sub 4}Cl corrosion failure often occurs in the overhead systems of hydrotreaters, and this failure is always accompanied by the appearance of H{sub 2}S. A combination of electrochemical and surface spectroscopic (SEM/EDS, AFM, XRD) techniques was used to investigate the effect of different factors, including the surface roughness, temperature, dissolved oxygen, pH and H{sub 2}S concentration, on the corrosion behavior of carbon steel in an NH{sub 4}Cl environment with the presence of H{sub 2}S. The effect of H{sub 2}S concentrations (at the ppm level) on the corrosion behavior of carbon steel was systematically revealed. The experimental results clearly indicated that the corrosion rate reached a minimum value at 10 ppm H{sub 2}S. The steel surface was covered by a uniform corrosion product film in a 10 ppm H{sub 2}S environment, and the corrosion product film was tight and protective. The ammonia from NH{sub 4}Cl helped maintaining the protectiveness of the corrosion films in this environment. Dissolved oxygen mainly accelerated the cathodic reaction. The cathodic limiting current density increased with increasing temperature, and the anodic branch polarization curves were similar at different temperatures. The anodic current density decreased as the pH decreased, and the cathodic current density increased as the pH decreased. The absolute surface roughness (R{sub a}) of carbon steel increased from 132.856 nm at 72 h to 153.973 nm at 144 h, and the rougher surface resulted in a higher corrosion rate. The critical innovation in this research was that multiple influential factors were revealed in the NH{sub 4}Cl environment with the presence of H{sub 2}S.

36 MATERIALS SCIENCE↗

Electrodeposition and Characterization of Cr-MoS{sub 2} Composite Coatings

In this study, Cr-MoS{sub 2} composite coatings were electrodeposited from conventional Cr{sup +6} baths containing different amounts of MoS{sub 2} particles and various types of surfactant (cationic and anionic). The effect of bath chemical composition on the coatings properties like their microstructure, morphology, chemical composition, corrosion behavior, surface roughness and microhardness was investigated using x-ray diffraction, scanning electron microscopy (SEM), energy-dispersive x-ray analysis, potentiodynamic polarization, electrochemical impedance spectroscopy, surface profilometry and Vickers microhardness measurement techniques, respectively. The results showed that incorporation of MoS{sub 2} particles into the composite coatings is very limited and Cr matrix with very low crystallinity will be electrodeposited at various experimental conditions. The presence of MoS{sub 2} particles in the bath (up to an optimum value) leads to the formation of the composite coatings with lower surface roughness values than that of conventional chromium coating. Although more MoS{sub 2} particles will be incorporated into the electrodeposits when the solid content of the bath increases, chromium cannot be electrodeposited from baths containing high amounts of MoS{sub 2} particles. Application of cationic surfactant promotes incorporation of particles into the Cr metallic matrix. Moreover, the presence of surfactant in the bath results in the formation of coatings with less microcracks. All the composite coatings have more hardness values than that of conventional chromium coating; maximum hardness is attributed to the coatings that were electrodeposited from baths containing no surfactant. The corrosion test results revealed that the smooth coatings containing more MoS{sub 2} particles and less microcracks exhibit more corrosion resistance than the other ones.

36 MATERIALS SCIENCE↗

Preliminary Compatibility Assessment of Metallic Dispenser Materials for Service in Ethanol Fuel Blends

The compatibility of selected metals representative of those commonly used in dispensing systems was evaluated in an aggressive E20 formulation (CE20a) and in synthetic gasoline (Reference Fuel C) in identical testing to facilitate comparison of results. The testing was performed at modestly elevated temperature (nominally 60 C) and with constant fluid flow in an effort to accelerate potential interactions in the screening test. Based on weight change, the general corrosion of all individual coupons exposed in the vapor phase above Reference Fuel C and CE20a as well as all coupons immersed in Reference Fuel C was essentially nil (<0.3 {micro}m/y), with no evidence of localized corrosion such as pitting/crevice corrosion or selective leaching at any location. Modest discoloration was observed on the copper-based alloys (cartridge brass and phosphor bronze), but the associated corrosion films were quite thin and apparently protective. For coupons immersed in CE20a, four different materials exhibited net weight loss over the entire course of the experiment: cartridge brass, phosphor bronze, galvanized steel, and terne-plated steel. None of these exhibited substantial incompatibility with the test fluid, with the largest general corrosion rate calculated from coupon weight loss to be approximately 4 {micro}m/y for the cartridge brass specimens. Selective leaching of zinc (from brass) and tin (from bronze) was observed, as well as the presence of sulfide surface films rich in these elements, suggesting the importance of the role of sulfuric acid in the CE20a formulation. Analysis of weight loss data for the slightly corroded metals indicated that the corrosivity of the test environment decreased with exposure time for brass and bronze and increased for galvanized and terne-plated steel. Other materials immersed in CE20a - type 1020 mild steel, type 1100 aluminum, type 201 nickel, and type 304 stainless steel - each appeared essentially immune to corrosion at the test conditions.

02 PETROLEUM↗

High performance III-V photoelectrodes for solar water splitting via synergistically tailored structure and stoichiometry

Abstract Catalytic interface of semiconductor photoelectrodes is critical for high-performance photoelectrochemical solar water splitting because of its multiple roles in light absorption, electrocatalysis, and corrosion protection. Nevertheless, simultaneously optimizing each of these processes represents a materials conundrum owing to conflicting requirements of materials attributes at the electrode surface. Here we show an approach that can circumvent these challenges by collaboratively exploiting corrosion-resistant surface stoichiometry and structurally-tailored reactive interface. Nanoporous, density-graded surface of ‘black’ gallium indium phosphide (GaInP 2 ), when combined with ammonium-sulfide-based surface passivation, effectively reduces reflection and surface recombination of photogenerated carriers for high efficiency photocatalysis in the hydrogen evolution half-reaction, but also augments electrochemical durability with lifetime over 124 h via strongly suppressed kinetics of corrosion. Such synergistic control of stoichiometry and structure at the reactive interface provides a practical pathway to concurrently enhance efficiency and durability of semiconductor photoelectrodes without solely relying on the development of new protective materials.

14 SOLAR ENERGY↗

Influence of Rust Permeability on Corrosion of E690 Steel in Industrial and Non-industrial Marine Splash Zones

The corrosion behaviour of E690 steel in industrial and non-industrial marine splash environments was studied by environmental testing, morphology analysis, electrochemical measurements, and scanning Kelvin probe microscopy. Chloride and sulphide anions were found to diffuse across the rust layer following the evaporation of seawater splashed on the steel’s surface. The cation-selective permeability of the rust layer resulted in an anion concentration gradient across the rust layer, which was more significant in the presence of sulphur dioxide. In addition, sulphur dioxide enhanced the formation of α-FeOOH, which led to the formation of distinct anode and cathode areas at the rust/steel interface.

36 MATERIALS SCIENCE↗

Numerical Modeling of High-Temperature Corrosion Processes

Numerical modeling of the diffusional transport associated with high-temperature corrosion processes is reviewed. These corrosion processes include external scale formation and internal subscale formation during oxidation, coating degradation by oxidation and substrate interdiffusion, carburization, sulfidation and nitridation. The studies that are reviewed cover such complexities as concentration-dependent diffusivities, cross-term effects in ternary alloys, and internal precipitation where several compounds of the same element form (e.g., carbides of Cr) or several compounds exist simultaneously (e.g., carbides containing varying amounts of Ni, Cr, Fe or Mo). In addition, the studies involve a variety of boundary conditions that vary with time and temperature. Finite-difference (F-D) techniques have been applied almost exclusively to model either the solute or corrodant transport in each of these studies. Hence, the paper first reviews the use of F-D techniques to develop solutions to the diffusion equations with various boundary conditions appropriate to high-temperature corrosion processes. The bulk of the paper then reviews various F-D modeling studies of diffusional transport associated with high-temperature corrosion.

Nesbitt, James A.↗

Evolution of Non-metallic Inclusions and Precipitates in Oriented Silicon Steel

The evolution of inclusions in oriented silicon steel during the manufacturing process was carried out by chemical composition analysis, non-aqueous electrolytic corrosion, and thermodynamic calculation. The morphology, composition, and size of inclusions were analyzed introducing field emission scanning electron microscope. The oxides were mainly formed during the secondary refining, and the nitrides, sulfides, and compounds were formed during the solidification and cooling of steel in the processes of continuous casting and hot rolling.

36 MATERIALS SCIENCE↗

Evolution of TiS and TiN in Fe-40 MassPctNi Austenitic Alloy During Heating at 1273 K (1000 °C)

Evolution of TiS in composition and morphology as well as the change in size distribution of TiS and TiN in Fe-40 masspctNi austenitic alloy during heating at 1273 K (1000 °C) was investigated using manual/automatic scanning electron microscopy energy-dispersive X-ray spectroscopy (SEM/EDS). Two types of TiS morphologies, spindle and spherical, were maintained during heating. The molar ratio of Ti/S of TiS increased while the aspect ratio of TiS was maintained in both alloys during heating. The number density of TiN inclusions was low compared with TiS in each alloy during heating. The pinning effect of TiS during heating was confirmed, and was stronger in alloy with a larger volume fraction of TiS. The results contribute to the establishment of optimum heat treatment processes for austenitic stainless steel to obtain better pitting corrosion resistance.

36 MATERIALS SCIENCE↗

Study of the effects of gaseous environments on sulfidation attack of superalloys

Studies were conducted to examine the effect of the gaseous corrodents NaCl, HCl, and NaOH on the high temperature oxidation and Na2SO4-induced corrosion behavior of the alumina former NiAl, the chromia former Ni-25 wt.% Cr, elemental Cr, and the superalloy B-1900. Experiments were conducted at 900 and 1050 C in air in the presence and absence of the gaseous corrodents. Effects involving both reaction rates and microstructural changes in oxide morphology were observed due to the presence of these corrodents at levels anticipated to be present in operating industrial and marine gas turbines. The effect of gaseous NaCl, HCl, and possibly NaOH on NiAl in simple oxidation was to remove aluminum from below the protective alumina layer and to simultaneously weaken the adherence of the protective alumina oxide scale to the substrate. The aluminum removed from below the oxide scale was redeposited on its surface as alpha-Al2O3 whiskers. With respect to the chromia formers, gaseous NaCl and HCl promoted breakaway oxidation kinetics and changes in the microstructures of the oxide scales.

Smeggil, J. G.↗

Additive Manufacturing of Isotropic NdFeB PPS Bonded Permanent Magnets

Extrusion based additive manufacturing of polymer composite magnets can increase the solid loading volume fraction with greater mechanical force through the printing nozzle as compared to traditional injection molding process. About 63 vol% of isotropic NdFeB magnet powders were compounded with 37 vol% of polyphenylene sulfide and bonded permanent magnets were fabricated while using Big Area Additive Manufacturing without any degradation in magnetic properties. The polyphenylene sulfide bonded magnets have a tensile stress of 20 MPa, almost double than that of nylon bonded permanent magnets. Additively manufactured and surface-protective-resin coated bonded magnets meet the industrial stability criterion of up to 175 °C with a flux-loss of 2.35% over 1000 h. They also exhibit better corrosion resistance behavior when exposed to acidic (pH = 1.35) solution for 24 h and also annealed at 80 °C over 100 h (at 95% relative humidity) over without coated magnets. Thus, polyphenylene sulfide bonded, additively manufactured, protective resin coated bonded permanent magnets provide better thermal, mechanical, and magnetic properties.

36 MATERIALS SCIENCE↗