Search NASA⌕ Search

SEARCH · Search NASA

Results for “SURFACE FINISH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Investigation of Machinability of Additively Manufactured Ti-6Al-4V

Additively manufactured metals differ from their conventionally produced counterparts due to the inherent material inhomogeneity, porosity, and thermal stress induced by the process. These differences make the machining of additively manufactured metals more difficult and cause premature tool failure or unexpected surface finish at certain conditions. This study takes the first step to investigate and identify the causes of these issues, particularly for Ti-6Al-4V. Printed and wrought samples, as well as heat treatment effect, are compared in a dry cutting condition at a cutting speed of 90 m/min in terms of cutting power, vibration, temperature, and produced surface finish. The results show a lower cutting power and more vibration for as-printed Ti samples, indicating a less ductile microstructure and inclusion of pores. Heat treatment can eliminate these phenomena. There is no significant difference found in the produced surface finish at the current cutting condition.

Raval, Jay↗

Efficient screening of rare large pit anomalies on polished surfaces using a minimalist sampling scheme

Lawrence Livermore National Laboratory (LLNL) has made significant strides in generating clean energy through its inertial confinement fusion (ICF) experiments. These experiments rely on high-density carbon (HDC) coated shells to encapsulate the fusion fuel. The success of these experiments is heavily dependent on the surface quality of these shells, as even minor imperfections, such as deep pits, can negatively impact fusion yield. Ensuring the required smoothness involves an extensive surface-finishing process that spans approximately 20 stages, making it both time-intensive and resource-demanding. A critical challenge in this process is the need for high-resolution scans to detect rare deep pits, which can be costly and impractical if performed on every shell. This highlights the necessity of developing more efficient scanning methods to optimize time and cost without compromising accuracy. To address these challenges, we introduce a novel approach that employs the multivariate Dvoretzky–Kiefer–Wolfowitz (DKW) inequality to provide a probabilistic upper bound on the error in estimating pit distribution characteristics via a Kernel Density Estimator (KDE). This error bound enables efficient and reliable estimation of pit distribution characteristics at a specified statistical confidence level using a minimal number of surface scans. The integrated DKW-KDE approach was validated through surface-finishing experiments across two batches of HDC-coated shells, demonstrating consistent and robust performance across multiple stages of the surface-finishing experiments. The validation studies suggest that the integrated DKW-KDE approach achieves comparable accuracy in estimating the risk of deleterious large pits with six scans, thus conserving time and resources. Further evaluations show that performance remains consistent across batches and over multiple polishing stages. In conclusion, based on these findings, one can leverage the minimal-scan insights to strategically improve the bottleneck inspection process, thus enhancing the productivity and quality of shell polishing and similar challenging manufacturing processes.

Inertial confinement fusion↗

Machinability comparison of additively manufactured and traditionally wrought Ti-6Al-4V alloys using single-point cutting

Post-machining is often needed to provide high dimensional accuracy and fine surface finish for additively manufactured Ti-6Al-4V (Ti64). The material inhomogeneity, such as pores and microstructures, can affect the machining behavior of this already difficult-machine alloy. This study adopts a holistic approach to compare the machinability of additively manufactured and traditionally wrought Ti64 in terms of key machining factors, including forces, temperature, and vibration and the major machining outcomes including tool life, surface finish, and dimensional accuracy. Stress-relief annealing is applied to each of the part conditions as a secondary variable to observe the additional effects. The results show that AM is not particularly more difficult to machine in terms of cutting force and temperature, but it creates high cutting vibrations across a wide range of frequencies (to and over 5 kHz). The high vibrations do not lead to worse surface finish or dimensional accuracy but tend to worsen the tool life by chipping off the cutting edge. The vibration can be attributed to the brittle martensitic microstructure found in additively manufactured Ti64, which is also evidenced by the more serrated chips. Stress-relieving is found to change the microstructure and reduce the level of vibration to that of the wrought counterpart.

36 MATERIALS SCIENCE↗

Mitigating Corrosion in Mg Sheet in Conjunction with a Sheet-Joining Method that Satisfies Structural Requirements within Sub-assemblies

This work was undertaken as a LightMAT project funded by the DOE-Vehicles Technology Office. The goal of this work was to develop corrosion protection strategies that simultaneously mitigate corrosion and achieve Class-A surface finish for Mg components in automotive applications. While automotive metals such as steel and aluminum are protected against corrosion through a variety of coating schemes/packages, the efficacy of these existing coating schemes for Mg and Mg- joints is not clear and needs to be determined. Therefore, five commercially available coating schemes and two joining techniques (riveting and Arplas resistance spot welding) were evaluated. The corresponding individual Mg sheet coupons or Mg/Mg joint test coupons were provided by Magna that were then corrosion tested at PNNL using ASTM B117 procedure. The microstructures and mechanical properties of the coupons were analyzed to determine the effectiveness of the joining and corrosion mitigation strategies. Of the coating schemes evaluated, Henkel Bonderite MgC 2.0 pre-treatment + E-coat showed the best corrosion protection and surface finish for individual Mg coupons and Arplas resistance spot welded coupons. However, the strength of Mg/Mg welded joint was reduced after corrosion testing due to some corrosion at the weld nugget. Mg/Mg rivet joints in conjunction with Chemetall oxisilan pre-treatment + polyurethane coating showed good corrosion resistance and some discoloration on the surface finish. Coating schemes comprising pre-treatment with Alodine 5200 + E-coat or Bonderite 1455 + polyurethane coating, in conjunction with Al rivet joints, showed significant corrosion and extensive discoloration of the surface. We anticipate that the results from this work will provide useful guidance to the automotive industry in selecting the appropriate combinations of corrosion protection coatings and joining techniques to fabricate light-weight Mg-based automotive components.

36 MATERIALS SCIENCE↗

Optical properties of sputtered aluminum on graphite/epoxy composite material

Solar absorptance, emittance, and coating thickness were measured for a range of coating thicknesses from about 400 A to 2500 A. The coatings were sputtered from an aluminum target onto 1-inch-diameter substrates of T300/5209 graphite/epoxy composite material with two different surface textures. Solar absorptance and emittance values for the specimens with the smooth surface finish were lower than those for the specimens with the rough surface finish. The ratio of solar absorptance to emittance was higher for the smooth specimens, increasing from 2 to 4 over the coating thickness range, than for the rough ones, which had a constant ratio of about 1. The solar absorptance and emittance values were dependent on the thickness of the sputtered coating.

Witte, William G., Jr.↗

Lifetime Predictions of a Titanium Silicate Glass with Machined Flaws

A dynamic fatigue study was performed on a Titanium Silicate glass to assess its susceptibility to delayed failure and to compare the results with those of a previous study. Fracture mechanics techniques were used to analyze the results for the purpose of making lifetime predictions. The material strength and lifetime was seen to increase due to the removal of residual stress through grinding and polishing. Influence on time-to-failure is addressed for the case with and without residual stress present. Titanium silicate glass otherwise known as ultra-low expansion (ULE)* glass is a candidate for use in applications requiring low thermal expansion characteristics such as telescope mirrors. The Hubble Space Telescope s primary mirror was manufactured from ULE glass. ULE contains 7.5% titanium dioxide which in combination with silica results in a homogenous glass with a linear expansion coefficient near zero. delayed failure . This previous study was based on a 230/270 grit surface. The grinding and polishing process reduces the surface flaw size and subsurface damage, and relieves residual stress by removing the material with successively smaller grinding media. This results in an increase in strength of the optic during the grinding and polishing sequence. Thus, a second study was undertaken using samples with a surface finish typically achieved for mirror elements, to observe the effects of surface finishing on the time-to-failure predictions. An allowable stress can be calculated for this material based upon modulus of rupture data; however, this does not take into account the problem of delayed failure, most likely due to stress corrosion, which can significantly shorten lifetime. Fortunately, a theory based on fracture mechanics has been developed enabling lifetime predictions to be made for brittle materials susceptible to delayed failure. Knowledge of the factors governing the rate of subcritical flaw growth in a given environment enables the development of relations between lifetime, applied stress and failure probability for the material under study. Dynamic fatigue is one method of obtaining the necessary information to develop these relationships. In this study, the dynamic fatigue method was used to construct a time-to-failure diagram for polished ULE glass.

Tucker, Dennis S.↗

Development of a truss joint for robotic assembly of space structures

This report presents the results of a detailed study of mechanical fasteners which were designed to facilitate robotic assembly of structures. Design requirements for robotic structural assembly were developed, taking into account structural properties and overall system design, and four candidate fasteners were designed to meet them. These fasteners were built and evaluated in the laboratory, and the Hammer-Head joint was chosen as superior overall. It had a high reliability of fastening under misalignments of 2.54 mm (0.1 in) and 3 deg, the highest end fixity (2.18), the simplest end effector, an integral capture guide, good visual verification, and the lightest weight (782 g, 1.72 lb). The study found that a good design should incorporate chamfers sliding on chamfers, cylinders sliding on chamfers, and hard surface finishes on sliding surfaces. The study also comments on robot flexibility, sag, hysteresis, thermal expansion, and friction which were observed during the testing.

Parma, George F.↗

Defect Detectability Improvement for Conventional Friction Stir Welds

This research was conducted to evaluate the effects of defect detectability via phased array ultrasound technology in conventional friction stir welds by comparing conventionally prepped post weld surfaces to a machined surface finish. A machined surface is hypothesized to improve defect detectability and increase material strength.

Hill, Chris↗

Characterizing Performance of Additively Manufacturing Regenerative Cooled Combustion Chambers Through Hot Fire Testing

NASA Marshall Space Flight Center (MSFC) has developed several additive manufactured regenerative cooled combustion chambers from 2014 to present. Chambers have been constructed using the Selective Laser Melting (SLM) powder bed additive manufacturing (AM) technique. The materials used for the chambers has varied from Inconel 718, Inconel 625, GRCop-84, and C18150 metal alloys. The surface finish and build techniques used to successfully manufacture combustion chambers using the SLM AM result in as built surface finish and off nominal geometric features. This paper discusses and reviews the effects of surface roughness, flow area, and hydraulic performance of regenerative cooled combustion chambers. The thrust chambers designs tested ranged from 200 to 1,400 psia producing 1,000 to 35,000 lbf thrust. Empirical data from four test campaigns will be reviewed and related to design modeling parameters such as pressure drop, surface roughness, and actual fluid flow geometry. Correlation results with simple 2-D CFD modeling will also be presented. The goal of the work is to better understand how the finished additive manufactured component characteristics inside internal features can effect regenerative cooling chamber design. Adjustments to design methodology will be discussed and recommended based on the above results.

Garcia, C. P.↗

Effects of surface treatments on ABS mechanical properties from fused filament fabrication

This paper examines the influence of surface treatments on the mechanical properties of acrylonitrile butadiene styrene (ABS) samples printed by fused filament fabrication (FFF). Prior efforts have applied brushing, painting, solvent dipping, infiltration, and vapor smoothing as post-processing surface treatments to improve the mechanical properties of FFF components. Additionally, because FFF can produce components with undesirable surface roughness, mechanical abrasion, epoxy coating, and acetone treatment may increase tensile strength by decreasing stress concentrations. Ridged surface texture may provide desirable tribological or handling properties. Based on these opportunities, this paper investigates abrasive media blasting, epoxy coating, acetone immersion, and ridged texturing surface treatments on the tensile strength and other mechanical properties of FFF ABS samples. ASTM D638-14 Type-I samples were printed, treated on all sample sides, and tested. From tensile tests, the elastic modulus, tensile strength, and fracture strain for both the untreated and treated ABS samples were calculated. For each sample, the surface finish and fracture macromorphology were observed with optical microscopy and the roughness values for the surface finish were calculated from profilometer data. Furthermore, samples were submerged in water and weighed periodically to measure mass changes due to water absorption. From surface profilometry and optical miscopy data, mechanical media blasting, epoxy coating, and immersion in all concentrations of acetone decreased surface roughness. Overall, on average, grit blasting with large beads and epoxy coating led to 2.6% and 1.2% increases in tensile strength, respectively; immersion in 40% acetone led to a 1.9% increase in tensile strength while treatment in 60% and 80% acetone decreased tensile strength by 4.9% and 1.9%, respectively. The study concludes that only grit blasting with large beads, immersion in 60% acetone, and the ridged texture significantly affected the tensile strength.

36 MATERIALS SCIENCE↗

Surface topographical effects on the structural growth of thick sputtered metal and alloy coatings

Thick sputtered S-Monel, silver, and 304 stainless steel coatings were deposited on mica and metal substrates with various surface finishes to investigate the structural growth of the coating by scanning electron microscopy. The geometry and the surface structure of the nodules are characterized. Compositional changes within the coating were analyzed by X-ray dispersion miscroscopy. Defects in the surface finish act as preferential nucleation sites and form isolated and complex nodules and various surface overgrowths in the coating. The nodule boundaries are very vulnerable to chemical etching, and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces.

Spalvins, T.↗

Electropolishing of a Full-Sized U-10Mo Plate

Electropolishing is used to remove material from the surface of a metal using electric potential and current. U-10Mo fuel is produced from a low enriched uranium plate alloyed with 10% molybdenum (U-10Mo). Electropolishing is being considered in two steps of the process of fabricating this U-10Mo fuel. First, it could be used as a means initially improving the surface finish of the cast plate while removing smut from the casting process from the surface prior to homogenization. Second, it could be used again after homogenization to remove oxidation and continue to improve the surface finish prior to hot rolling. The purpose of this work is to demonstrate the process on full-size ingots and optimize the process. A depleted uranium U-10Mo plate was electropolished three times: the first two times were prior to homogenization and the third after a homogenization step. The first two polishes decreased the overall roughness, as measured by laser confocal microscopy. After each polish, a smoother and shinier blue-gold surface was left on the plate. Upon homogenization, the surface had a more matte appearance and the surface roughness increased back to the pre-homogenization values obtained prior to the initial polish. After electropolishing the homogenized pieces, the changes in surface roughness increased, as measured by laser confocal microscopy. The final polishing step was not long enough to return the surface roughness to pre-homogenization conditions, implying less polishing is needed before the homogenization versus afterwards. Heat generation during the polish was addressed by circulating the electrolyte solution through an external heat exchanger; however, solubility and anodization challenges require further study.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Scanning electron microscope investigation of the structural growth in thick sputtered coatings

Sputtered S-Monel, silver, and 304 stainless steel coatings and molybdenum disulfide coatings were deposited on mica and metal substrates with various surface finishes to investigate the structural growth of the coating by scanning electron microscopy. The geometry and the surface morphology of the nodules are characterized. Compositional changes within the coating were analyzed by energy dispersive X-ray analysis. Defects in the surface finish act as preferential nucleation sites and form isolated overlapping and complex nodules and various unusual surface overgrowths on the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces.

Spalvins, T.↗

Surface topographical effects on the structural growth of thick sputtered metal and alloy coatings

Thick sputtered S-Monel, silver, and 304 stainless steel coatings were deposited on mica and metal substrates with various surface finishes to investigate the structural growth of the coating by scanning electron microscopy. The geometry and the surface structure of the nodules are characterized. Compositional changes within the coating were analyzed by X-ray dispersion microscopy. Defects in the surface finish (i.e., scratches, inclusions, etc.) act as preferential nucleation sites and form isolated and complex nodules and various surface overgrowths in the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces. These effects are illustrated by micrographs. Nodular growth within a coating can be minimized or eliminated by reducing the surface roughness.

Spalvins, T.↗

Nodular growth in thick-sputtered metallic coatings

Thick-sputtered S-Monel, silver, and 304 stainless steel coatings were deposited on mica and metal substrates with various surface finishes to investigate the nodular growth in the coating by scanning electron microscopy. The geometry and the surface structure of the nodules are characterized. Compositional changes within the coating were analyzed by energy dispersive X-ray analysis. Defects in the surface finish (i.e., scratches, inclusions, etc.), act as preferential nucleation sites and form isolated and complex nodules and various surface overgrowths in the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces. These effects are illustrated by micrographs. Nodular growth within a coating can be minimized or eliminated by increasing the surface smoothness.

Spalvins, T.↗

Improving fatigue performance of additively manufactured Ti-6Al-4V using sulfur-based self-terminating etching processes

The adoption of Additively Manufactured (AM) Ti-6Al-4V (Ti64) is continually increasing in the industry due to its benefits over the conventional manufacturing techniques. However, AM Ti64 parts are prone to poor surface finish, which significantly affects their fatigue performance. Therefore, AM Ti64 parts need post-processing to enhance surface finish and fatigue performance. Prior work with a sulfur-based self-terminating etching process for AM Ti64 demonstrated support removal and surface roughness reduction. To further this work, this manuscript details the impact of this sulfur-based post-processing technique on the mechanical properties and the fatigue life of AM Ti64 by characterizing the surface roughness, microstructural evolution, and fracture surfaces. Finally, this post-processing technique decreased the surface roughness parameter - S v by 55 % from 84 ± 11 µm to 38 ± 19 µm and increased the average fatigue life by 340 % from about 7000 cycles to 30,000 cycles.

36 MATERIALS SCIENCE↗

Study of dielectric breakdown in liquid xenon with XeBrA: The xenon breakdown apparatus

Maintaining the electric fields necessary for the current generation of noble liquid time projection chambers (TPCs), with drift lengths exceeding 1 m, requires a large negative voltage applied to their cathode. Delivering such high voltage is associated with an elevated risk of electrostatic discharge and electroluminescence, which would be detrimental to the performance of the experiment. The Xenon Breakdown Apparatus (XeBrA) is a 5-l, high voltage test chamber built to investigate the contributing factors to electrical breakdown in noble liquids. Here, in this work, we present the main findings after conducting scans over stressed electrode areas, surface finish, pressure, and high voltage ramp speed in the medium of liquid xenon. Area scaling and surface finish were observed to be the dominant factors affecting breakdown, whereas no significant changes were observed with varying pressure or ramp speed. A general rise in both the anode current and photon rate was observed in the last 30 s, leading up to a breakdown, with a marked increase in the last couple of seconds. In addition, the position of breakdowns was reconstructed with a system of high-speed cameras and a moderate correlation with the Fowler–Nordheim field emission model was found. Tentative evidence for bubble nucleation being the originating mechanism of breakdown in the liquid was also observed. We deem the results presented in this work to be of particular interest for the design of future, large TPCs, and practical recommendations are provided.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Adaptive control for hybrid manufacturing

The primary objective of the technical collaboration is to validate and implement adaptive feed rate control, tool wear monitoring, and anomaly detection for the finish machining of additive components. Most additively manufactured components need finish machining to achieve surface finish and tolerance requirements. Distortions and surface roughness of additively manufactured components can result in high forces and tool breakage or excessive tool wear during post-additive finish machining, which can result in rework or part scrap. In this collaboration, methods, and models for feed rate control, tool wear monitoring, and anomaly detection via a digital twin will be evaluated and validated.

99 GENERAL AND MISCELLANEOUS↗