Enhanced Performance of Silicon Anodes through Hybrid Surface Engineering

Silicon (Si) is a promising anode material for nextgeneration lithium-ion batteries (LIBs) due to its high theoretical capacity. However, Si-containing anodes typically suffer from unacceptably short lives because of the unrestricted growth of the solid electrolyte interphase (SEI). Here, in this study, hybrid surface coatings are developed to stabilize the SEI in high loading pure Si anodes using atomic and molecular layer deposition. The coatings, consisting of LiF paired with lithicone, create an ionically conductive surface that enhances the capacity retention, rate performance, and longevity. Careful binder selection helps demonstrate the full utility of the coatings by enabling high loading electrodes to cycle continuously at current densities of 1200 mA/g Si . Uncoated controls, in comparison, fail within just 10 cycles at lower loadings. X-ray photoelectron spectroscopy and electrochemical impedance spectroscopy are used to provide supporting evidence of the coating composition and efficacy. The data indicate that our lithicone coating is converted to Li 2 CO 3 upon cycling contributing to favorable LiF/Li 2 CO 3 interfaces that enhance the space-charge effect at the active material’s surface. When applied to electrodes made with thermally stable binders and increasingly higher loadings (approaching 5 mAh/cm 2 ), ion transport through the bulk electrode, rather than SEI growth, is shown to be the limiting factor. Furthermore, data suggests a favorable interaction between lithicone precursors and poly(acrylic acid) binders mitigates thermal decomposition at higher temperatures. The work presented here represents the successful realization of composite coatings containing LiF/Li 2 CO 3 components to stabilize high-loading Si anodes. This work helps inform advanced surface engineering strategies to achieve highly reversible, high-capacity Si anodes capable of fast charging for high-performance LIBs.

atomic layer deposition↗

Intrinsic chemical reactivity of solid-electrolyte interphase components in silicon–lithium alloy anode batteries probed by FTIR spectroscopy

Herein we report the solid reaction products from the chemical reaction of aprotic battery electrolyte and three purported components of the Si-based anode SEI : SiO 2 nanoparticles (NPs), lithium silicate (Li x SiO y ) powders, and Si NPs. We use FTIR and classical molecular dynamics/density functional perturbation theory to assess the solid products remaining with these model materials after exposure to electrolyte. The absence of electrochemical bias provides a view of the chemical speciation resulting from early-stage chemical reactivity during battery assembly as well as under open circuit storage conditions. We believe these species represent the initial stages of SEI growth and predict they likely drive subsequent chemical and electrochemical reactions by controlling molecular interactons at the Si active material interface. We find that nominally equivalent materials react differently even before any electrochemistry is performed (e.g., acidic SiO 2 dissolves whereas alkaline SiO 2 is relatively robust), and derive new understanding of the chemical species that could and could not form stable SEI components in Si-based anodes. These results can be used to inform how to passivate Si anode surfaces and potentially generate an artificially engineered SEI that would be stable and enable next-generation battery anodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Organic Solvent Free Process to Fabricate High Performance Silicon/Graphite Composite Anode

Cycling stability is a key challenge for application of silicon (Si)-based composite anodes as the severe volume fluctuation of Si readily leads to fast capacity fading. The binder is a crucial component of the composite electrodes. Although only occupying a small amount of the total composite mass, the binder has major impact on the long-term electrochemical performance of Si-based anodes. In recent years, water-based binders including styrene-butadiene rubber (SBR) and carboxymethyl cellulose (CMC) have attracted wide research interest as eco-friendly and low-cost alternatives for the conventional poly(vinylidene difluoride) (PVDF) binder in Si anodes. In this study, Si-based composite anodes are fabricated by simple solid mixing of the active materials with subsequent addition of SBR and CMC binders. This approach bypasses the use of toxic and expansive organic solvents. The factors of binder, silicon, and graphite materials have been systematically investigated. It is found that the retained capacities of the anodes are more than 440 mAh/g after 400 cycles. These results indicate that organic solvent free process is a facile strategy for producing high performance silicon/graphite composite anodes.

Fang, Chen (ORCID:0000000321011991)↗

Development of Nanosized/Nanostructured Silicon as Advanced Anodes for Lithium-Ion Cells

NASA is developing high energy and high capacity Li-ion cell and battery designs for future exploration missions under the NASA Advanced Space Power System (ASPS) Program. The specific energy goal is 265 Wh/kg at 10 C. center dot Part of effort for NASA advanced Li-ion cells  Anode: Silicon (Si) as an advanced anode.  Electrolyte: advanced electrolyte with flame-retardant additives for enhanced performance and safety (NASA JPL).

silicon↗

Insights into the Crossover Effects in Cells with High‐Nickel Layered Oxide Cathodes and Silicon/Graphite Composite Anodes

Abstract Silicon anodes are regarded as one of the most promising alternatives to graphite (Gr) anodes due to their ultrahigh capacity, abundance, and low cost. Coupling Si‐based anodes with high‐nickel layered oxide cathodes LiNi x Mn y Co 1− x − y O 2 (NMC, x ≥ 0.8) can enhance the driving range for electric vehicles. Transition‐metal (TM) ion dissolution and deposition has been a long‐known failure mode for Gr‐based lithium‐ion batteries. However, the mechanistic insight associated with TM ion deposition on Si‐based anodes has rarely been reported. Herein, the impact of in situ deposited TM ions on SiO x /Gr composite anodes and the individual influences of Ni, Mn, and Co on the structural and electrochemical stability along with the underlying degradation mechanisms are presented. TM ion dissolution causes a greater deleterious impact on Si than on Gr, with different TM ions exhibiting different influences on anode‐electrolyte interphase formation. Specifically, Ni deposit induces more aggressive salt decomposition; Co deposit has negligible effect on salt decomposition, but significantly accelerates solvent decomposition; and Mn deposit aggravates both salt and solvent decompositions, resulting in worse full cell performance. The extent of degradation decreases in the order Mn 2+ > Ni 2+ > Co 2+ . The systematic comparisons presented can guide further development of high energy systems.

Zhang, Xianhui↗

Multi-modal characterization methods of solid-electrolyte interphase in silicon-graphite composite electrodes

Composite silicon-graphite (Si-Gr) anodes can improve battery energy density, due to Si's high gravimetric capacity, while mitigating mechanical degradation of the anode and solid-electrolyte interphase (SEI) caused by Si volumetric expansion. Optimizing these anodes is challenging, in part due to difficulty characterizing the SEI structure and composition. In this work, we present multi-modal characterization of the SEI on composite Si-Gr anodes to relate SEI chemical composition and structure to functional properties. Discrepancies in elemental concentrations from X-ray photoelectron spectroscopy, Auger electron spectroscopy, and energy-dispersive X-ray spectroscopy (EDS) are attributed to varying information depth and lateral resolution of the individual probes. However, by combining quantitative composition information with spatially resolved element mapping from scanning transmission electron microscopy, EDS, and electron energy loss spectroscopy, a holistic picture of the SEI emerges. We observe the bilayer SEI structure and a direct correlation between elemental Li and F, suggesting that most Li in the SEI exists as lithium fluoride (LiF). Further, LiF concentration is directly proportional to the maximum SEI resistivity, as determined by scanning spreading resistance microscopy. Lastly, there is an inverse relationship between lithium carbonate and LiF concentration in the SEI, providing insight into the detailed chemistry of SEI formation and evolution.

25 ENERGY STORAGE↗

Tracking the Oxidation of Silicon Anodes Using Cryo-EELS upon Battery Cycling

Silicon is a high-capacity material for the anode of a rechargeable lithium-ion battery. One of the fundamental challenges for using Si in anodes is capacity fading, which has been revealed to be partially associated with the interfacial instability between the Si and liquid electrolyte due to the large volume swing of Si upon charging and discharging. Smart nanoscale design concepts, either pre-synthesized or formed in-situ, have led to the mitigation of the detrimental factors associated with the volume swing of Si. However, it has never been clear as how the chemical state of Si evolves and contributes to the capacity fading upon battery cycling. Here, we use cryo-electron energy loss spectroscopy (EELS) to directly monitor, at sub-nanometer scale, the chemical evolution of Si upon battery cycling. We discover that during the cycling process, Si particles are progressively oxidized to form SiO 2 , which is initiated from the particle surface and gradually penetrates toward the interior of the particle, directly contributing to the capacity fading. Possible mechanisms of Si oxidation are postulated. We further show how the cycling stability can be improved by an electrolyte additive to form an effective passivation layer, representatively, even a small concentration of fluoroethylene carbonate (FEC) causes the formation of an LiF layer on the Si nanoparticle surface that prevents Si oxidation and improves cycling stability. Furthermore, the present work unveils Si oxidation as a previously unrecognized factor that contributes to capacity fading, therefore providing insight into the design of anodes with Si based materials.

25 ENERGY STORAGE↗

Mitigation of rapid capacity decay in silicon-LiNi 0.6 Mn 0.2 Co 0.2 O 2 full batteries

Silicon (Si)-based materials have been considered as the most promising anode materials for high-energy-density lithium-ion batteries because of their higher storage capacity and similar operating voltage, as compared to the commercial graphite (Gr) anode. But the use of Si anodes including silicon-graphite (Si-Gr) blended anodes often leads to rapid capacity decay in Si-Gr/LiNixMnyCo z O 2 (x+y+z=1) full cells, which has been attributed to surface instability of the Si component. In addition to stabilizing the surface, this work investigates the potential of the Si-Gr blended anodes in a full-cell configuration and its impact on the capacity contribution from active components. Using dQ/dV plots of the full cells, a powerful but simple-to-implement differential potential approach is developed to decouple the capacity contribution and degradation from the graphite and silicon components. Data collected from three-electrode cells confirm the results from the differential potential approach, which suggests a voltage slippage to a higher voltage at the blended anode side. Additionally, the voltage slippage causes a reduced utilization of the Gr component and exacerbates side reactions between the Si-Gr anode and carbonate electrolytes. Furthermore, based on these failure mechanisms, we adopted a mitigation strategy to tune the open circuit voltage of the prelithiated anode while stabilizing the surface. As a result, the full cells with the modified Si-Gr anodes (mass loading, 2.5 mAh/cm 2 ) offer a highly reversible full-cell energy density of 390 Wh/kg (based on the mass of both anode and cathode materials in a full cell) with a cycling CE of 99.9% over 200 cycles.

25 ENERGY STORAGE↗

Size effect on the growth and pulverization behavior of Si nanodomains in SiO anode

Silicon monoxide (SiO) as a promising silicon-based anode electrode of lithium-ion batteries (LIBs) has been the subject of many recent investigations. However, the complex microstructural features of SiO hinder attempts to link the microstructure changes in SiO with its electrochemical performances upon electrochemical cycling. This study employs X-ray pair distribution function (PDF), with a high-resolution transmission electron microscope (HRTEM), to investigate the microstructure of Si nanodomains in SiO and its structural evolution over the electrochemical cycling process. The experiment results reveal the size evolution of Si nanodomains in SiO during the electrochemical cycling and find it highly dependent on the initial Si domain size in SiO. If the initial Si domain size is too large, the average size of Si nanodomains would increase at first and then decrease after a certain number of cycles, which indicates the pulverization of Si domains after the electrochemical-driven growth of Si nanodomains reaches a critical point. Furthermore, these results suggest that an optimal initial Si nanodomain size of 4-6 nm for SiO anode materials is essential to retard the growth and subsequent pulverization process of Si nanodomains and thus to improve the cyclability of SiO during long-term cycling.

25 ENERGY STORAGE↗

Unveiling the Mechanical and Electrochemical Evolution of Nanosilicon Composite Anodes in Sulfide-Based All-Solid-State Batteries

The utilization of silicon anodes in all-solid-state lithium batteries provides good prospects for facilitating high energy density. However, the compatibility of sulfide solid-state electrolytes (SEs) with Si and carbon is often questioned due to potential decomposition. Here, in this paper, operando X-ray absorption near-edge structure (XANES) spectroscopy, ex situ scanning electron microscopy (SEM), and ex situ X-ray nanotomography (XnT) are utilized to investigate the chemistry and structure evolution of nano-Si composite anodes. Results from XANES demonstrate a partial decomposition of SEs during the first lithiation stage, which is intensified by the presence of carbon. Nevertheless, the performances of first three cycles in Si–SE–C are stable, which proves that the generated media is ionically conductive. XnT and SEM results show that the addition of SEs and carbon improves the structural stability of the anode, with fewer pores and voids. A chemo-elasto-plastic model reveals that SEs and carbon buffer the volume expansion of Si, thus enhancing mechanical stability. The balance between the pros and cons of SEs and carbon in enhancing reaction kinetics and structural stability enables the Si composite anode to demonstrate the highest Si utilization with higher specific capacities and a better rate than pure Si and Si composite anodes with only SEs.

36 MATERIALS SCIENCE↗

Solid‐State Prealkylation of Electrode Architectures (SPEAR): Direct Control of Prelithiation Levels in Silicon Anodes and Electrochemical Cycling

The Solid-state Prealkylation of Electrode ARchitectures (SPEAR) is different than traditional electrochemical prealkylation processes. Through SPEAR, alkylation is driven by solid-state diffusion without the simultaneous SEI formation concomitant with polarization. Here, we investigate the prelithiation of 80 wt. % Si-based anodes to varying amounts (up to Li 1.38 Si) to understand the trade-off between improved Li capacity and expansion-induced stress. Through dilatometry, we found that solid-state lithiation led to filling of the electrode pores through silicon expansion. This swelling changed the SEI formation process and accessibility of the silicon compared to an electrochemically lithiated electrode. Indeed, optimal prelithiation to Li 0.82 Si increases the initial C/3 cycling capacity post-SEI formation up to 43%, consistent with deeper Si activation through the electrode bulk. Prelithiation and cycling cells prelithiated beyond Li 0.82 Si results in a state of charge (SOC) close to 100% which facilitates parasitic degradation mechanisms and volume expansion of the Si electrode. The results demonstrate a pathway to modify silicon activation/SEI formation to enable high-energy electrodes.

Musgrove, Amanda L. [Oak Ridge National Laboratory↗

Understanding the Effect of Cathode Composition on the Interface and Crosstalk in NMC/Si Full Cells

Crosstalk between the cathode and the anode in lithium-ion batteries has a great impact on performance, safety, and cycle lifetime. Still, no report exists for a systematic investigation on crosstalk behavior in silicon (Si)-based cells as a function of transition metal composition in cathodes. We studied the effect of crosstalk on degradation of Si-rich anodes in full cells with different cathodes having the same crystal structure but different transition metal compositions, such as LiNi 1/3 Mn 1/3 Co 1/3 O 2 (NM111), LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811). We found that the transition metal composition in cathodes, especially Mn ion concentration, significantly affects electrolyte decomposition reactions, even from very early cycles. This change causes differences in the solid electrolyte interphase (SEI) chemistry of each aged Si sample. As a result, each of the aged Si samples has a different electrochemistry, in terms of initial Coulombic efficiency and the mechanism of capacity fade.

25 ENERGY STORAGE↗

1000 Wh L−1 lithium-ion batteries enabled by crosslink-shrunk tough carbon encapsulated silicon microparticle anodes

Abstract Microparticulate silicon (Si), normally shelled with carbons, features higher tap density and less interfacial side reactions compared to its nanosized counterpart, showing great potential to be applied as high-energy lithium-ion battery anodes. However, localized high stress generated during fabrication and particularly, under operating, could induce cracking of carbon shells and release pulverized nanoparticles, significantly deteriorating its electrochemical performance. Here we design a strong yet ductile carbon cage from an easily processing capillary shrinkage of graphene hydrogel followed by precise tailoring of inner voids. Such a structure, analog to the stable structure of plant cells, presents ‘imperfection-tolerance’ to volume variation of irregular Si microparticles, maintaining the electrode integrity over 1000 cycles with Coulombic efficiency over 99.5%. This design enables the use of a dense and thick (3 mAh cm–2) microparticulate Si anode with an ultra-high volumetric energy density of 1048 Wh L–1 achieved at pouch full-cell level coupled with a LiNi0.8Co0.1Mn0.1O2 cathode.

25 ENERGY STORAGE↗

A04-0491 - Reduced Electrolyte Reactivity of Pitch-Carbon Coated Si Nanoparticles for Li-Ion Battery Anodes

Silicon-based anodes for Li-ion batteries (LIB) have the potential to increase the energy density over graphite-based LIB anodes. However, silicon anodes exhibit poor cycle and calendar lifetimes due to mechanical instabilities and high chemical reactivity with the carbonate-based electrolytes that are typically used in LIBs. In this work, we synthesize a pitch-carbon coated silicon nanoparticle composite active material for LIB anodes that exhibits reduced chemical reactivity with the carbonate electrolyte compared to an uncoated silicon anode. Silicon primary particle sizes <10 nm minimize micro-scale mechanical degradation of the anode composite, while conformal coatings of pitch-carbon minimized the parasitic reactions between the silicon and the electrolyte. When matched with a high voltage NMC622 cathode, the pitch-carbon coated Si anode retains -75% of its initial capacity over 1000 cycles. Efforts to increase the areal loading of the pitch-carbon coated silicon anodes to realize real energy density improvements over graphite anodes results in severe mechanical degradation on the electrode level. Developing procedures to engineer the architecture of the composite silicon anode may be a solution to this mechanical challenge.

DIRECT ENERGY CONVERSION,ENERGY STORAGE↗

Progress of 3D network binders in silicon anodes for lithium ion batteries

Prompted by its overwhelming benefits, silicon (Si) has evolved as one of the most promising anode materials for high-capacity lithium-ion batteries (LIBs). However, some of the intrinsic drawbacks such as low ionic conductivity and inevitable volume change during the alloying/dealloying process seriously hamper the commercialization of Si-based anodes in LIBs. Among the several strategies to overcome the challenges of the Si anode, the development of designed polymeric binders is imperative for enabling stable and satisfactory performance. The improved cell performance due to the designed binders is recognized as an economical and practical approach, especially from the industrial perspective. In addition to their conventional role in integrating electrode components, binders also play a significant role in alleviating the unfavorable phenomenon of volume expansion, and ultimately stabilizing the Si anode and Si-electrolyte interphase. The polymer architecture of the binders significantly influences the binder performance, and three-dimensional (3D) network binders are generally more effective at coping with the stress resulting from the huge volume change of the Si anode. To develop advanced 3D binders, substantial research efforts have been made including various crosslinking strategies in the past decade. In this review, we focus on diverse crosslinking methods including chemical-, physical-, and topological-crosslinking for rationally designing network binders for Si anodes and take a glance at dynamic interactions to construct healable binders for long-term stability.

25 ENERGY STORAGE↗

Evaluating the Effect of Electrolyte Additive Functionalities on NMC622/Si Cell Performance

Unstable electrode/electrolyte interface is the major cause of degradation for silicon (Si)-based anodes for lithium (Li)-ion batteries. Development of functional electrolyte additives can provide a viable path toward stabilizing the dynamic Si/electrolyte interface, which will benefit the development of high energy density Li-ion batteries. Here, we evaluate polymerizable electrolyte additives with varying functional groups (fluorocarbon, thiophosphate, and fluorophosphazene). The additives are examined using LiNi 0.6 Mn 0.2 Co 0.2 O 2 /Si full cells where the cycle performance and impedance are measured. Electrochemical tests show that the fluorine-containing additives provide better passivation at the Si electrode, leading to enhanced full cell performance. Here, among the three additives examined, best electrochemical performance is observed from the fluorocarbon-containing compound, followed by fluorophosphazene- and thiophosphate-containing compounds. Characterization of the solid electrolyte interphase (SEI) on cycled electrodes using Auger electron spectroscopy (AES), X-ray photoelectron spectroscopy (XPS), and attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR) reveal that higher concentration of fluorine and lithium oxide, and lower concentration of carbonate and organic species correlate with enhanced electrochemical performance.

25 ENERGY STORAGE↗

On the dynamics of the fluoroethylene carbonate generated solid electrolyte interphase on silicon anodes during calendar life aging

Here, the widespread use of silicon (Si)-rich anodes in lithium-ion batteries (LIBs) is impeded by an unstable solid electrolyte interphase (SEI) incurring insufficient cell life. Fluoroethylene carbonate (FEC) additive in the electrolyte significantly improves cycle life. However, the gains on calendar life remain unclear; the SEI structure still undergoes detrimental alterations at rest. Thus, elucidating the SEI dynamics during calendar aging is critical to mitigating time-dependent capacity degradation. ATR-FTIR, XPS, and ToF-SIMS are used herein to investigate the SEI structure before and after calendar aging. Si cycled without FEC exhibits no notable SEI chemistry changes Pre- and Post-aging, leaving poor passivation as the main failure pathway. Conversely, the FEC-SEI starts as short oligomeric species from FEC/EC electroreduction prior to aging; after calendar aging, polymerized carbonates become consistently more prominent. Unexpectedly, the deposition of self-polymerized FEC species results from time exposure to the delithiated Si specifically as opposed to the lithiated surface. This unexpected finding is supported by another recent Si calendar-aging research, which albeit not investigating FEC, finds global failure of the SEI upon delithiation resulting in ∼247 fold more reactive surface compared to the lithiated.

Batteries↗