Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Mechanical Properties Degradation of Teflon(Trademark) FEP Returned from the Hubble Space Telescope

After 6.8 years on orbit, degradation has been observed in the mechanical properties of second-surface metalized Teflon(Reg) FEP (fluorinated ethylene propylene) used on the Hubble Space Telescope (HST) on the outer surface of the multi-layer insulation (MLI) blankets and on radiator surfaces. Cracking of FEP surfaces on HST was first observed upon close examination of samples with high solar exposure retrieved during the first servicing mission (SM1) conducted 3.6 years after HST was put into orbit. Astronaut observations and photographs from the second servicing mission (SM2), conducted after 6.8 years on orbit, revealed severe cracks in the FEP surfaces of the MLI on many locations around the telescope. This paper describes results of mechanical properties testing of FEP surfaces exposed for 3.6 years and 6.8 years to the space environment on HST. These tests include tensile testing, surface micro-hardness testing, and bend testing.

Dever, Joyce A.↗

Stiffness reductions during tensile fatigue testing of graphite/epoxy angle-ply laminates

Tensile fatigue data was generated under carefully controlled test conditions. A computerized data acquisition system was used to permit the measurement of dynamic modulus without interrupting the fatigue cycling. Two different 8-ply laminate configurations, viz, + or - 45 (2s) and + or - 67.5 (2s), of a T300/5208 graphite/epoxy composite were tested. The + or - 45 (2s) laminate did exhibit some modulus decay, although there was no well-defined correlation with applied stress level or number of cycles. The + or - 67.5 (2s) laminate did not exhibit any measurable modulus decay. Secondary effects observed included a small but distinct difference between modulus as measured statically and dynamically, a slight recovery of the modulus decay after a test interruption, and a significant viscoelastic (creep) response of the + or - 45 (2s) laminate during fatigue testing.

Odom, E. M.↗

Slow Crack Growth Behavior and Life/Reliability Analysis of 96 wt % Alumina at Ambient Temperature With Various Specimen/Loading Configurations

Extensive constant stress-rate testing for 96 wt % alumina was conducted in room-temperature distilled water using four different specimen/loading configurations: rectangular beam test specimens under four-point uniaxial flexure, square plate test specimens in ring-on-ring biaxial flexure, square plate test specimens in ball-on-ring biaxial flexure, and dog-boned tensile test specimens in pure tension. The slow crack growth (SCG) parameter n was almost independent of specimen/loading configurations, in either four-point uniaxial flexure, ring-on-ring biaxial flexure, ball-on-ring biaxial flexure, or pure tension, ranging from n = 35 to 47 with an average value of n = 41.1 +/- 4.5. The prediction of fatigue strength/reliability based on the four-point uniaxial flexure data by using the CARES/Life design code as well as a simple PIA model was in good agreement with both the ring-on-ring biaxial and the ball-on-ring biaxial flexure data. A poor prediction using the PIA model was observed for the dog-boned tensile test specimens, presumably due to different flaw population involved in the tensile test specimens.

Choi, Sung R.↗

Effects of 50,000 hours of thermal aging on graphite/epoxy and graphite/polyimide composites

Thermal effects on tensile strengths of advanced composite systems have been determined for exposure times of 100 to 50,000 hours (5.7 years). Exposures were conducted at both ambient and reduced pressures at two temperatures for each composite. At the completion of the various aging periods, specimens were removed from the specially constructed aging furnaces, visually examined, and tensile tested at elevated temperature. After tensile testing, many of the thermal aging specimens were examined using a scanning electron microscope. Results of these studies are presented, and the changes in properties and the degradation mechanisms during high-temperature aging are discussed and illustrated using metallographic techniques.

Kerr, J. R.↗

Determination of Material Properties Near the Glass Transition Temperature for an Isogrid Boom

Experiments were performed and results obtained to determine the temperature dependence of the modulus of elasticity for a thermoplastic isogrid tube. The isogrid tube was subjected to axial tensile loads of 0-100 lbf and strain was measured at room and elevated temperatures of 100, 120, 140, 160, 180, 190, and 200 F. These were based on tube manufacturer specifying an incorrect glass transition temperature of 210 F. Two protocols were used. For the first protocol the tube was brought to temperature and a tensile test performed. The tube was allowed to cool between tests. For the second protocol the tube was ramped to the desired test temperature and held. A tensile test was performed and the tube temperature ramped to the next test temperature. The second protocol spanned the entire test range. The strain rate was constant at 0.008 in/min. Room temperature tests resulted in the determination of an average modulus of 2.34 x 106 Psi. The modulus decreased above 100 F. At 140 F the modulus had decreased by 7.26%. The two test protocols showed good agreement below 160 F. At this point the glass transition temperature had been exceeded. The two protocols were not repeated because the tube failed.

Blandino, Joseph R.↗

A comparison of simple shear characterization methods for composite laminates

Various methods for the shear stress/strain characterization of composite laminates are examined and their advantages and limitations are briefly discussed. Experimental results and the necessary accompanying analysis are then presented and compared for three simple shear characterization procedures. These are the off-axis tensile test method, the (+/- 45 deg)s tensile test method and the (0/90 deg)s symmetric rail shear test method. It is shown that the first technique indicates the shear properties of the graphite/epoxy laminates investigated are fundamentally brittle in nature while the latter two methods tend to indicate that these laminates are fundamentally ductile in nature. Finally, predictions of incrementally determined tensile stress/strain curves utilizing the various different shear behaviour methods as input information are presented and discussed.

Yeow, Y. T.↗

A comparison of simple shear characterization methods for composite laminates

Various methods for the shear stress-strain characterization of composite laminates are examined, and their advantages and limitations are briefly discussed. Experimental results and the necessary accompanying analysis are then presented and compared for three simple shear characterization procedures. These are the off-axis tensile test method, the + or - 45 degs tensile test method and the 0 deg/90 degs symmetric rail shear test method. It is shown that the first technique indicates that the shear properties of the G/E laminates investigated are fundamentally brittle in nature while the latter two methods tend to indicate that the G/E laminates are fundamentally ductile in nature. Finally, predictions of incrementally determined tensile stress-strain curves utilizing the various different shear behavior methods as input information are presented and discussed.

Yeow, Y. T.↗

Simultaneous Development and Robust Optimization of a Microstructure Dependent Material

Recent microstructure characterization techniques combined with Symbolic Regression(SR)analysis has been proven to generate white box plasticity models well suited for incorporation into FEA software.The current work builds upon those efforts and demonstrates the applicability of Sequential Monte-Carlo (SMC) methods within SR analysis to condense model development and robust optimization into a single, co-dependent process. In this project, SMC methods provide a mechanism through which the observed microstructure features and associated variability can be incorporated into the discovery phase of model development and simultaneously recover approximate parameter distributions through SR analysis. The demonstration utilized a data set consisting of tensile test results from a limited number of sample specimens with corresponding EBSD data from which microstructure features were characterized.The maximum threshold stress model in the Visco-Plastic Self-Consistent (VPSC) code developed by Los Alamos National Laboratories was calibrated using mechanical test data.Synthetic volume elements with statistically equivalent microstructure were generated with DREAM3Dbased on the observed EBSD data. VPSC was used to simulate the corresponding tensile test response for each of the synthetic volume elements. The simulated microstructure and tensile test data was used astraining datafor SMC-SR algorithm and the resulting model was validated with data from the original empirical data set.

Karl Garbrecht↗

Use of DSC and DMA Techniques to Help Investigate a Material Anomaly for PTFE Used in Processing a Piston Cup for the Urine Processor Assembly (UPA) on International Space Station (ISS)

Human urine and flush water are eventually converted into drinking water with the Urine Processor Assembly (UPA) aboard the International Space Station (ISS). This conversion is made possible through the Distillation Assembly (DA) of the UPA. One component of the DA is a molded circular piston cup made of virgin polytetrafluoroethylene (PTFE). The piston cup is assembled to a titanium component using eight fasteners and washers. Molded PTFE produced for spare piston cups in the first quarter of 2010 was different in appearance and texture, and softer than material molded for previous cups. For the suspect newer PTFE material, cup fasteners were tightened to only one-half the required torque value, yet the washers embedded almost halfway into the material. The molded PTFE used in the DA piston cup should be Type II, based on AMS 3667D and ASTM D4894 specifications. The properties of molded PTFE are considerably different between Type I and II materials. Engineers working with the DA thought that if Type I PTFE was molded by mistake instead of Type II material, that could have resulted in the anomalous material properties. Typically, the vendor molds flat sheet PTFE from the same material lot used to mold the piston cups, and tensile testing as part of quality control should verify that the PTFE is Type II material. However, for this discrepant lot of material, such tensile data was not available. Differential scanning calorimetry (DSC) and dynamic mechanical analysis (DMA) were two of the testing techniques used at the NASA/Marshall Space Flight Center (MSFC) to investigate the anomaly for the PTFE material. Other techniques used on PTFE specimens were: Shore D hardness testing, tensile testing on dog bone specimens and a qualitative estimation of porosity by optical and scanning electron microscopy.

Wingard, Doug↗

Nondestructive Strain Measurement System Used to Determine Surface Strain on Fibers

Small-diameter structural fibers are being considered as reinforcements for high temperature ceramic matrix composite materials, and thus they require characterization. At the NASA Lewis Research Center, a nondestructive optical technique was used to determine surface strain on a structural fiber, in real time, as it was pulled in a tensile test machine. With this technique, interference or speckle patterns from the laser illuminated fiber test specimen are recorded. As the fiber is pulled, its speckle pattern shifts in proportion to the strain, translation, and rotation components of the sample deformation. Shifting speckle patterns are detected in real time by two linear charge-coupled discharge (CCD) camera arrays, and the images are processed by a hardware correlator. Surface strain is selectively detected on fibers with diameters on the order of 100 mm and can be resolved to 19 microstrain. This system was designed to be robust and compact and generally does not require surface preparation of the structural fibers. For strain detection, two laser beams are positioned incident on the structural fiber being tested, as shown in the photograph, where the test specimen is mounted in a tensile test machine via two coupons. As the fiber is pulled, the speckle pattern produced from each laser beam is detected by one of two CCD arrays located inside the tube on the right side of the photograph.

Tuma, Margaret L.↗

Mechanical Properties of Friction Stir Welds in A12195-T8

An extensive study of the mechanical properties of friction stir welded Al-Li 2195 has been conducted by Lockheed Martin Michoud Space Systems under contract to NASA. The study was part of a development program in which weld parameters were defined for using FSW to assemble large-scale aluminum cryogenic tanks. In excess of 300 feet of 0.320 in. gage plate material was welded and tested. The tests include room temperature and cryogenic temperature tensile tests and surface crack tension (SCT) tests, nondestructive evaluation, metallurgical studies, and photostress analysis. The results of the testing demonstrated improved mechanical properties with FSW as compared to typical fusion welding processes. Increases in ultimate tensile strength, cryogenic enhancement and elongation were observed with the tensile test results. Increased fracture toughness was observed with the SCT results. Nondestructive evaluations were conducted on all welded Joints. No volumetric defects were indicated. Surface indications on the root side of the welds did not significantly affect weld strength. The results of the nondestructive evaluations were confirmed via metallurgical studies. Photostress analysis revealed strain concentrations in multi-pass and heat-repaired FSW's. Details of the tests and results are presented.

Kinchen, David G.↗

Effects of Long-Term Thermal Exposure on Commercially Pure Titanium Grade 2 Elevated-Temperature Tensile Properties

Elevated-temperature tensile testing of commercially pure titanium (CP Ti) Grade 2 was conducted for as-received commercially produced sheet and following thermal exposure at 550 and 650 K (531 and 711 F) for times up to 5000 h. The tensile testing revealed some statistical differences between the 11 thermal treatments, but most thermal treatments were statistically equivalent. Previous data from room temperature tensile testing was combined with the new data to allow regression and development of mathematical models relating tensile properties to temperature and thermal exposure. The results indicate that thermal exposure temperature has a very small effect, whereas the thermal exposure duration has no statistically significant effects on the tensile properties. These results indicate that CP Ti Grade 2 will be thermally stable and suitable for long-duration space missions.

Ellis, David L.↗

Evaluation of the Transient Liquid Phase (TLP) Bonding Process for Ti3Al-Based Honeycomb Core Sandwich Structure

The suitability of using transient liquid phase (TLP) bonding to fabricate honeycomb core sandwich panels with Ti-14Al-21Nb (wt%) titanium aluminide (T3Al) face sheets for high-temperature hypersonic vehicle applications was evaluated. Three titanium alloy honeycomb cores and one Ti3Al alloy honeycomb core were investigated. Edgewise compression (EWC) and flatwise tension (FWT) tests on honeycomb core sandwich specimens and tensile tests of the face sheet material were conducted at temperatures ranging from room temperature to 1500 F. EWC tests indicated that the honeycomb cores and diffusion bonded joints were able to stabilize the face sheets up to and beyond the face sheet compressive yield strength for all temperatures investigated. The specimens with the T3Al honeycomb core produced the highest FWT strengths at temperatures above 1000 F. Tensile tests indicated that TLP processing conditions resulted in decreases in ductility of the Ti-14Al-21Nb face sheets. Microstructural examination showed that the side of the face sheets to which the filler metals had been applied was transformed from equiaxed alpha2 grains to coarse plates of alpha2 with intergranular Beta. Fractographic examination of the tensile specimens showed that this transformed region was dominated by brittle fracture.

Bird, R. Keith↗

Exit Presentation

Skills Acquired: Tensile Testing: Prepare materials and setting up the tensile tests; Collect and interpret (messy) data. Outgassing Testing: Understand TML (Total Mass Loss) and CVCM (Collected Volatile Condensable Material); Collaboration with other NASA centers. Z2 (NASA's Prototype Space Suit Development) Support: Hands on building mockups of components; Analyze data; Work with others, understanding what both parties need in order to make a run successful. LCVG (Liquid Cooling and Ventilation Garment) Flush and Purge Console: Both formal design and design review process; How to determine which components to use - flow calculations, pressure ratings, size, etc.; Hazard Analysis; How to make design tradeoffs.

Melone, Kate↗

Mechanical properties of weldments in experimental Fe-12Mn-0.2Ti and Fe-12Mn-1Mo-0.2Ti alloys for cryogenic service

Mechanical properties of weldments in two Fe-12Mn experimental alloys designed for cryogenic service were evaluated. Weldments were made using the GTA welding process. Tests to evaluate the weldments were conducted at -196 C and included: equivalent energy fracture toughness tests; autogenous transverse weld, notched transverse weld, and longitudinal weld tensile tests; and all-weld-metal tensile tests. The Fe-12Mn-0.2Ti and Fe-12Mn-1Mo-0.2Ti alloys proved weldable for cryogenic service, with weld metal and heat-affected zone properties comparable with those of the base metal. Optimum properties were achieved in the base alloys, weld metals, and heat-affected zones after a two-step heat treatment consisting of austenitizing at 900 C followed by tempering at 500 C. The Mo-containing alloy offered a marked improvement in cryogenic properties over those of the Mo-free alloy. Molybdenum increased the amount of retained austenite and reduced the amount of epsilon martensite observed in the microstructure of the two alloys.

Stephens, J. R.↗

Tensile adhesion testing methodology for thermally sprayed coatings

The structure of thermally sprayed coatings consists of lamellae which are oriented parallel to the substrate surface. The lamellae separate and fracture by distinctive mechanisms which are reflected in the failure morphology, and these may be described as adhesive (between the coating and substrate), cohesive (within the coating), or mixed mode. There is a large variability in the failure stress for any nominally identical group of coatings. A lower bound for the fracture toughness of alumina coatings can be calculated as 0.2 MNm exp -3/2. The coating strength values may also be treated as belonging to the statistical distribution of the Weibull function. The Weibull modulus of the coating strength varied from 1.4 to 3.8. This analysis infers that the flaw size within coatings is highly variable and that the flaws are nonuniformly dispersed. The present work focuses on the question of whether tensile adhesion tests are an appropriate testing method for thermally sprayed materials.

Berndt, Christopher C.↗

Creep degradation in oxide-dispersion-strengthened alloys

Oxide dispersion strengthened Ni-base alloys in wrought bar form are studied for creep degradation effects similar to those found in thin gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and three types of advanced ODS-NiCrAl alloys. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, the appearance of dispersoid-free bands, grain boundary cavitation, and internal oxidation in the microstructure were interpreted as creep degradation effects. This work showed that many ODS alloys are subject to creep damage. Degradation of tensile properties occurred after very small amounts of creep strain, ductility being the most sensitive property. All the ODS alloys which were creep damaged possessed a large grain size. Creep damage appears to have been due to diffusional creep which produced dispersoid-free bands around boundaries acting as vacancy sources. Low angle and possibly twin boundaries acted as vacancy sources.

Whittenberger, J. D.↗

Effect of prior creep at 1365 K on the room temperature tensile properties of several oxide dispersion strengthened alloys

An experimental study was conducted to determine whether oxide dispersion-strengthened (ODS) Ni-base alloys in wrought bar form are subject to creep degradation effects similar to those found in thin-gage sheet. The bar products evaluated included ODS-Ni, ODS-NiCr, and advanced ODS-NiCrAl types; the alloys included microstructures ranging from an essentially perfect single crystal to a structure consisting of very small elongated grains. Tensile test specimens were exposed to creep at various stress levels at 1365 K and then tensile tested at room temperature. Low residual tensile properties, change in fracture mode, appearance of dispersoid free bands, grain boundary cavitation, and/or internal oxidation are interpreted as creep degradation effects. The amount of degradation depends on creep strain, and degradation appears to be due to diffusional creep which produces dispersoid free bands around grain boundaries acting as vacancy sources.

Whittenberger, J. D.↗