At least 91 records · Page 5

Thermo-oxidative stability studies of PMR-15 polymer matrix composites reinforced with various fibers

An experimental study was conducted to measure the thermo-oxidative stability of PMR-15 polymer matrix composites reinforced with various fibers and to observe differences in the way they degrade in air. The fibers that were studied included graphite and the thermally stable Nicalon and Nextel ceramic fibers. Weight loss rates for the different composites were assessed as a function of mechanical properties, specimen geometry, fiber sizing, and interfacial bond strength. Differences were observed in rates of weight loss, matrix cracking, geometry dependency, and fiber-sizing effects. It was shown that Celion 6000 fiber-reinforced composites do not exhibit a straight-line Arrhenius relationship at temperatures above 316 C.

Bowles, Kenneth J.↗

Advanced Constituents and Processes for Ceramic Composite Engine Components

The successful replacement of metal alloys by ceramic matrix composites (CMC) in hot-section engine components will depend strongly on optimizing the processes and properties of the CMC microstructural constituents so that they can synergistically provide the total CMC system with improved temperature capability and with the key properties required by the components for long-term structural service. This presentation provides the results of recent activities at NASA aimed at developing advanced silicon carbide (Sic) fiber-reinforced hybrid Sic matrix composite systems that can operate under mechanical loading and oxidizing conditions for hundreds of hours at 2400 and 2600 F, temperatures well above current metal capability. These SiC/SiC composite systems are lightweight (-30% metal density) and, in comparison to monolithic ceramics and carbon fiber-reinforced ceramic composites, are able to reliably retain their structural properties for long times under aggressive engine environments. It is shown that the improved temperature capability of the SiC/SiC systems is related first to the NASA development of the Sylramic-iBN Sic fiber, which displays high thermal stability, creep resistance, rupture resistance, and thermal conductivity, and possesses an in-situ grown BN surface layer for added environmental durability. This fiber is simply derived from Sylramic Sic fiber type that is currently produced at ATK COI Ceramics. Further capability is then derived by using chemical vapor infiltration (CVI) to form the initial portion of the hybrid Sic matrix. Because of its high creep resistance and thermal conductivity, the CVI Sic matrix is a required base constituent for all the high temperature SiC/SiC systems. By subsequently thermo- mechanical-treating the CMC preform, which consists of the S ylramic-iBN fibers and CVI Sic matrix, process-related defects in the matrix are removed, further improving matrix and CMC creep resistance and conductivity.

Yun, H. M.↗

Hafnia-Based Materials Developed for Advanced Thermal/Environmental Barrier Coating Applications

Thermal and environmental barrier coatings (T/EBCs) will play a crucial role in advanced gas turbine engine systems because of their ability to significantly increase engine operating temperatures and reduce cooling requirements, and thus help achieve engine goals of low emissions and high efficiency. Under the NASA Ultra-Efficient Engine Technology (UEET) Project, advanced T/EBCs are being developed for low-emission SiC/SiC ceramic matrix composite (CMC) combustor applications by extending the CMC liner and vane temperature capability to 1650 C (3000 F) in oxidizing and water-vaporcontaining combustion environments. The coating system is required to have increased phase stability, lower lattice and radiation thermal conductivity, and improved sintering and thermal stress resistance under high-heat-flux and thermal-cycling engine conditions. Advanced heat-flux testing approaches (refs. 1 to 4) have been established at the NASA Glenn Research Center for 1650 C coating developments. The simulated combustion water-vapor environment is also being incorporated into the heat-flux test capabilities (ref. 3).

Zhu, Dongming↗

Evaluating Use of Boron- and Hafnium-Modified Polysilazanes for Ceramic Matrix Minicomposites

In this study, the potential of polymer-derived Ceramic Matrix Composites (CMCs) is demonstrated by addition of thin ceramic coatings on Carbon Fiber (CF) bundles. Boron- and hafnium- modified polysilazane liquid precursors were synthesized and used to infiltrate the fiber bundles of CF to fabricate lab-scale Si(B)CN/CF and Si(Hf)CN/CF CMC mini-composites, respectively. The precursor-to-ceramic conversion process was achieved at 800°C with crosslinked precursor to ceramic yield of approx. 90% in Ar environment. The Si(B)CN/CF contained Si-N and B-N bonds, while Si-N and Hf-O-Si bonds were observed for Si(Hf)CN/CF sample with uniform and dense surfaces. Room-temperature tensile tests showed that the Si(Hf)CN/CF sample could reach a tensile strength of ~790 MPa and elastic modulus of 66.88 GPa among the composites. Oxidation study of the Si(Hf)CN/CF mini-composites showed higher stability compared to SiCN/CF and Si(B)CN/CF mini-composites up to 1500°C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Freestanding, heat resistant microporous film for use in energy storage devices

Preferred embodiments of a freestanding, heat resistant microporous polymer film (10) constructed for use in an energy storage device (70, 100) implements one or more of the following approaches to exhibit excellent high temperature mechanical and dimensional stability: incorporation into a porous polyolefin film of sufficiently high loading levels of inorganic or ceramic filler material (16) to maintain porosity (18) and achieve low thermal shrinkage; use of crosslinkable polyethylene to contribute to crosslinking the polymer matrix (14) in a highly inorganic material-filled polyolefin film; and heat treating or annealing of biaxially oriented, highly inorganic material-filled polyolefin film above the melting point temperature of the polymer matrix to reduce residual stress while maintaining high porosity. The freestanding, heat resistant microporous polymer film embodiments exhibit extremely low resistance, as evidenced by MacMullin numbers of less than 4.5.

25 ENERGY STORAGE↗

Wear and Reactivity Studies of Melt infiltrated Ceramic Matrix Composite

As interest grows in the use of ceramic matrix composites (CMCs) for critical gas turbine engine components, the effects of the CMCs interaction with the adjoining structure needs to be understood. A series of CMC/material couples were wear tested in a custom elevated temperature test rig and tested as diffusion couples, to identify interactions. Specifically, melt infiltrated silicon carbide/silicon carbide (MI SiC/SiC) CMC was tested in combination with a nickel-based super alloy, Waspaloy, a thermal barrier coating, Yttria Stabilized Zirconia (YSZ), and a monolithic ceramic, silicon nitride (Si3N4). To make the tests more representative of actual hardware, the surface of the CMC was kept in the as-received state (not machined) with the full surface features/roughness present. Test results include: scanning electron microscope characterization of the surfaces, micro-structural characterization, and microprobe analysis.

Jarmon, David C.↗

Preparation and dielectric properties of Ba{sub 0.95}Ca{sub 0.05}Ti{sub 0.8}Zr{sub 0.2}O{sub 3}-polyethersulfone composites

We report the preparation and dielectric properties of ceramic-polymer composites using Ba{sub 0.95}Ca{sub 0.05}Ti{sub 0.8}Zr{sub 0.2}O{sub 3} (BCTZ) as a ceramic filler and polyethersulfone (PES) as a polymer matrix. The BCTZ powders were synthesized by a sol-gel method to fabricate BCZT-PES composites. The composites with various BCTZ volume fractions were prepared by a solution mixing and hot-pressing method. The composite with 50 vol % BCTZ showed high dielectric constant ({epsilon}=48.80) and low loss (tan {delta}=0.042) at 1 kHz and room temperature. Such excellent dielectric properties of the composites displayed an acceptable stability within a wide range of temperature (from 20 to 150 deg. C) and frequency (from 100 Hz to 100 kHz). The present work indicates that the BCTZ-PES composite can be a candidate for embedded capacitors.

36 MATERIALS SCIENCE↗

Strengthening Aluminum Alloys for High Temperature Applications Using Nanoparticles of Al203 and Al3-X Compounds (X= Ti, V, Zr)

In this paper the effect of nanoparticles A12O3 and A13-X compounds (X= Ti, V, Zr) on the improvement of mechanical properties of aluminum alloys for elevated temperature applications is presented. These nanoparticles were selected based on their chemical stability and low diffusions rates in aluminum matrix at high temperatures. The strengthening mechanism for aluminum alloy is based on the mechanical blocking of dislocation movements by these nanoparticles. Samples were prepared from A12O3 nanoparticle preforms, which were produced using ceramic injection molding process and pressure infiltrated by molten aluminum. A12O3 nanoparticles can also be homogeneously mixed with aluminum powder and consolidated into samples through hot pressing and sintering. On the other hand, the Al3-X nanoparticles are produced as precipitates via in situ reactions with molten aluminum alloys using conventional casting techniques. The degree of alloy strengthening using nanoparticles will depend on the materials, particle size, shape, volume fraction, and mean inter-particle spacing.

Lee, Jonathan A.↗

Method of waste stabilization with dewatered chemically bonded phosphate ceramics

A method of stabilizing a waste in a chemically bonded phosphate ceramic (CBPC). The method consists of preparing a slurry including the waste, water, an oxide binder, and a phosphate binder. The slurry is then allowed to cure to a solid, hydrated CBPC matrix. Next, bound water within the solid, hydrated CBPC matrix is removed. Typically, the bound water is removed by applying heat to the cured CBPC matrix. Preferably, the quantity of heat applied to the cured CBPC matrix is sufficient to drive off water bound within the hydrated CBPC matrix, but not to volatalize other non-water components of the matrix, such as metals and radioactive components. Typically, a temperature range of between 100.degree. C.-200.degree. C. will be sufficient. In another embodiment of the invention wherein the waste and water have been mixed prior to the preparation of the slurry, a select amount of water may be evaporated from the waste and water mixture prior to preparation of the slurry. Another aspect of the invention is a direct anyhydrous CBPC fabrication method wherein water is removed from the slurry by heating and mixing the slurry while allowing the slurry to cure. Additional aspects of the invention are ceramic matrix waste forms prepared by the methods disclosed above.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Unveiling and Mapping Polymorphs in Fluorite Y2TiO5 Using 4D-STEM and Unsupervised Machine Learning

Y2TiO5 belongs to the Ln2TiO5 (Ln = lanthanide or Y) family of ceramic materials and exhibits a range of desirable material properties such as radiation tolerance, frustrated magnetism, and large dielectric constant. However, understanding the complex crystal structure of Y2TiO5 remains elusive, given that Y2TiO5 can adopt multiple polymorphs such as cubic, orthorhombic, and hexagonal phases within the lattice. In this work, we report a detailed structural analysis of Y2TiO5 using four-dimensional scanning transmission electron microscopy coupled with unsupervised machine learning. The pyrochlore nanodomains, characterized by the ordered arrangement of yttrium cations on the A site of their A2BO5 structure, are present within the matrix of a predominantly fluorite-structured Y2TiO5 along with a third polymorph, the hexagonal phase. The pyrochlore phase is found to form 2 nm boundary regions around hexagonal phase stacking faults, highlighting the potential influence of the hexagonal phase on the occurrence and distribution of the pyrochlore phase. Lastly, we identify a unique pyrochlore phase with asymmetric arrangement of cation ordering along a single planar direction. Our findings provide invaluable insights into the possible mechanisms stabilizing pyrochlore nanodomains within the fluorite lattice of Y2TiO5.

36 MATERIALS SCIENCE↗

The Development of Environmental Barrier Coatings for SiCSiC Ceramic Matrix Composites: Challenges and Opportunities

Environmental barrier coatings (EBCs) and SiC/SiC ceramic matrix composites (CMCs) systems will play a crucial role in future turbine engines for hot-section component applications because of their ability to significantly increase engine operating temperatures, reduce engine weight and cooling requirements. The development of prime-reliant environmental barrier coatings is a key to enable the applications of the envisioned CMC components to help achieve next generation engine performance and durability goals. This paper will primarily address the performance requirements and design considerations of environmental barrier coatings for turbine engine applications. The emphasis is placed on current candidate environmental barrier coating systems for SiCSiC CMCs, their performance benefits and design limitations in long-term operation and combustion environments. Major technical barriers in developing advanced environmental barrier coating systems, the coating integrations with next generation CMC turbine components having improved environmental stability, cyclic durability and system performance will be described. The development trends for turbine environmental barrier coating systems by utilizing improved compositions, state-of-the-art processing methods, and simulated environment testing and durability modeling will be discussed.

Environmental Barrier Coatings↗

Advanced Oxide Material Systems For 1650 C Thermal/Environmental Barrier Coating Applications

Advanced thermal/environmental barrier coatings (T/EBCs) are being developed for low emission SiC/SiC ceramic matrix composite (CMC) combustor and vane applications to extend the CMC liner and vane temperature capability to 1650 C (3000 F) in oxidizing and water-vapor containing combustion environments. The 1650 C T/EBC system is required to have better thermal stability, lower thermal conductivity, and improved sintering and thermal stress resistance than current coating systems. In this paper, the thermal conductivity, water vapor stability and cyclic durability of selected candidate zirconia-/hafnia-, pyrochlore- and magnetoplumbite-based T/EBC materials are evaluated. The test results have been used to downselect the T/EBC coating materials, and help demonstrate advanced 1650OC coatings feasibility with long-term cyclic durability.

Zhu, Dongming↗

Integrated High Payoff Rocket Propulsion Technology (IHPRPT) SiC Recession Model

SiC stability and recession rates were modeled in hydrogen/oxygen combustion environments for the Integrated High Payoff Rocket Propulsion Technology (IHPRPT) program. The IHPRPT program is a government and industry program to improve U.S. rocket propulsion systems. Within this program SiC-based ceramic matrix composites are being considered for transpiration cooled injector faceplates or rocket engine thrust chamber liners. Material testing under conditions representative of these environments was conducted at the NASA Glenn Research Center, Cell 22. For the study described herein, SiC degradation was modeled under these Cell 22 test conditions for comparison to actual test results: molar mixture ratio, MR (O2:H2) = 6, material temperatures to 1700 C, combustion gas pressures between 0.34 and 2.10 atm, and gas velocities between 8,000 and 12,000 fps. Recession was calculated assuming rates were controlled by volatility of thermally grown silica limited by gas boundary layer transport. Assumptions for use of this model were explored, including the presence of silica on the SiC surface, laminar gas boundary layer limited volatility, and accuracy of thermochemical data for volatile Si-O-H species. Recession rates were calculated as a function of temperature. It was found that at 1700 C, the highest temperature considered, the calculated recession rates were negligible, about 200 m/h, relative to the expected lifetime of the material. Results compared favorably to testing observations. Other mechanisms contributing to SiC recession are briefly described including consumption of underlying carbon and pitting. A simple expression for liquid flow on the material surface was developed from a one-dimensional treatment of the Navier-Stokes Equation. This relationship is useful to determine under which conditions glassy coatings or thermally grown silica would flow on the material surface, removing protective layers by shear forces. The velocity of liquid flow was found to depend on the gas velocity, the viscosity of gas and liquid, as well as the thickness of the gas boundary layer and the liquid layer. Calculated flow rates of a borosilicate glass coating compared well to flow rates observed for this coating tested on a SiC panel in Cell 22.

Opila, E. J.↗

Lean Premixed Combustion Stabilized by Low Swirl a Promising Concept for Practical Applications

Since its inception, the low-swirl burner (LSB) has shown to be a useful laboratory apparatus for fundamental studies of premixed turbulent flames. The LSB operates under wide ranges of equivalence ratios, flow rates, and turbulence intensities. Its flame is lifted and detached from the burner and allows easy access for laser diagnostics. The flame brush is axisymmetric and propagates normal to the incident reactants. Therefore, the LSB is well suited for investigating detailed flame structures and empirical coefficients such as flame speed, turbulence transport, and flame generated turbulence. Due to its capability to stabilize ultra-lean premixed turbulent flames (phi approx. = 0.55), the LSB has generated interest from the gas appliance industry for use as an economical low-NO(x) burner. Lean premixed combustion emits low levels of NO(x), due primarily to the low flame temperature. Therefore, it is a very effective NO(x) prevention method without involving selective catalytic reduction (SCR), fuel-air staging, or flue gas recirculation (FGR). En the gas turbine industry, substantial research efforts have already been undertaken and engines with lean premixed combustors are already in use. For commercial and residential applications, premixed pulsed combustors and premixed ceramic matrix burners are commercially available. These lean premixed combustion technologies, however, tend to be elaborate but have relatively limited operational flexibility, and higher capital, operating and maintenance costs. Consequently, these industries are continuing the development of lean premixed combustion technologies as well as exploring new concepts. This paper summarizes the research effects we have undertaken in the past few years to demonstrate the feasibility of applying the low-swirl flame stabilization method for a wide range of heating and power generation systems. The principle of flame stabilization by low-swirl is counter to the conventional high-swirl methods that rely on a recirculation zone to anchor the flame. In LSBS, flow recirculation is not promoted to allow the premixed turbulent flames to propagate freely. A LSB with an air-jet swirler is essentially an open tube with the swirler at its mid section. The small air-jets generate swirling motion only in the annular region and leaving the central core of the flow undisturbed, When this flow exits the burner tube, the angular momentum generates radial mean pressure gradient to diverge the non-swirling reactants stream. Consequently, the mean flow velocity decreases linearly. Propagating against this decelerating flow, the flame self-sustains at the position where the local flow velocity equals the flame speed, S(sub f). The LSB operates with a swirl number, S, between 0.02 to 0.1. This is much lower than the minimum S of 0.6 required for the high-swirl burners. We found that the swirl number needed for flame stabilization varies only slightly with fuel type, flow velocity, turbulent conditions and burner dimensions (i.e. throat diameter and swirl injection angle).

Cheng, R. K.↗

Initial Assessment of Environmental Effects on SiC/SiC Composites in Helium-Cooled Nuclear Systems

Ceramic matrix composites, in particular SiC/SiC composites, are currently being evaluated for use at high temperatures and high radiation fields in advanced concept reactors, including high-temperature gas cooled reactors (HTGR), very high temperature reactors (VHTR), gas fast reactors (GFR), sodium fast reactors (SFR) and fluoride-cooled high temperature reactors (FHR). SiC/SiC composites have many desirable properties for high temperature nuclear applications, including excellent thermal and mechanical properties and radiation resistance. However, their behavior in contact with the chemical environment in normal operation conditions and in off-normal accident conditions scenarios still needs to be evaluated. This report summarizes the information available in the literature on the chemical reactivity of SiC/SiC composites and of their components in contact with the helium coolant used in HTGR, VHTR and GFR designs. Under normal operating conditions, ultra-high purity helium will have chemically controlled impurities (water, oxygen, carbon dioxide, carbon monoxide, methane, hydrogen) that will create a slightly oxidizing gas environment. Little is known from direct experiments on the reactivity of third generation (nuclear grade) SiC/SiC composites in contact with low concentrations of water or oxygen in inert gas, at high temperature. However, there is ample information regarding the oxidation behavior of SiC/SiC composites in dry and moist air at high temperatures. This information is reviewed first in the next chapters. The emphasis is placed on the improvement in material oxidation, thermal, and mechanical properties during three stages of development of SiC fibers and at least two stages of development of the fiber/matrix interphase. The chemical stability of SiC/SiC composites in contact with oxygen or steam at temperatures that may develop in off-normal reactor conditions supports the conclusion that most advanced composites (also known as nuclear grade SiC/SiC composites) have the chemical resistance that would allow them maintain mechanical properties at temperatures up to 1200 – 1300 °C in the extreme conditions of an air or water ingress accident scenario. Further research is needed to assess the long-term stability of advanced SiC/SiC composites in inert gas (helium) in presence of very low concentrations (traces) of water and oxygen at the temperatures of normal operation of helium-cooled reactors.

ceramic matrix composites↗

Environmental Barrier Coating Development for SiC/SiC Ceramic Matrix Composites: Recent Advances and Future Directions

This presentation briefly reviews the SiC/SiC major environmental and environment-fatigue degradations encountered in simulated turbine combustion environments, and thus NASA environmental barrier coating system evolution for protecting the SiC/SiC Ceramic Matrix Composites for meeting the engine performance requirements. The presentation will review several generations of NASA EBC materials systems, EBC-CMC component system technologies for SiC/SiC ceramic matrix composite combustors and turbine airfoils, highlighting the temperature capability and durability improvements in simulated engine high heat flux, high pressure, high velocity, and with mechanical creep and fatigue loading conditions. This paper will also focus on the performance requirements and design considerations of environmental barrier coatings for next generation turbine engine applications. The current development emphasis is placed on advanced NASA candidate environmental barrier coating systems for SiC/SiC CMCs, their performance benefits and design limitations in long-term operation and combustion environments. The efforts have been also directed to developing prime-reliant, self-healing 2700F EBC bond coat; and high stability, lower thermal conductivity, and durable EBC top coats. Major technical barriers in developing environmental barrier coating systems, the coating integrations with next generation CMCs having the improved environmental stability, erosion-impact resistance, and long-term fatigue-environment system durability performance will be described. The research and development opportunities for turbine engine environmental barrier coating systems by utilizing improved compositions, state-of-the-art processing methods, and simulated environment testing and durability modeling will be briefly discussed.

Environmental Barrier Coatings↗

FWP FEAA149: “Next Generation Environmental Barrier Coatings”

Environmental barrier coatings (EBCs) are required coatings for utilization of SiC/SiC ceramic matrix composite (CMC) components in gas turbines, where the EBC represents the life-limiting factor for such components. EBC/CMC systems have shown success in aero-engine applications with increased turbine inlet temperatures and improved efficiencies, which are achieved through higher temperature stability, lower density, and decreased reliance on cooling air compared to traditional superalloys. While industrial gas turbines (IGTs) do not currently utilize SiC/SiC CMCs, the current shift towards low-carbon or carbon-free fuel sources for power generation could result in a need for EBC/CMC components with higher temperature capabilities. In this work, three tasks were outlined to improve understanding of EBC lifetimes to encourage use in IGTs with carbon-free fuel such as hydrogen: 1. Define the bond coating oxidation kinetics and EBC failure criteria, 2. Measure thermal expansion coefficients of each layered material, and 3. Perform advanced characterization and modeling to assess EBC lifetimes. Cyclic steam oxidation tests were conducted on various EBC/Si/SiC chemistries and EBC/SiC architectures to define substrate oxidation kinetics and EBC failure modes. An open-source code was developed to quantify the undulating thermally grown oxide thickness with thousands of measurements from specimen cross-section images. Bond coating oxidation kinetics were determined and used to develop a kinetic and thermodynamic model for predicting EBC lifetimes. High-temperature Raman spectroscopy was utilized for determining the SiO 2 thermally grown oxide phase transformation as the life-limiting feature for EBCs. Model efforts supported the claim that the SiO 2 phase transformation causes elevated stress during thermal cycling with associated cracking that decreases the adhesion strength of the EBC, eventually resulting in coating spallation. The finite element model subroutine will be made publicly available upon internal review. Further development of an EBC lifetime model for IGTs involves definition of a critical SiO 2 thickness for EBC spallation and must also consider both environmental (gas velocity, pressure, etc.) and specimen (EBC dopants, layer architectures, etc.) effects into predicted bond coating oxidation kinetics for long-lifetime components.

36 MATERIALS SCIENCE↗

Radioactive waste immobilization of Hanford sludge in magnesium potassium phosphate ceramic forms

Here, this paper evaluates immobilization of Hanford K-Basin tank sludge in magnesium potassium phosphate ceramic forms. The waste forms were produced using two simulated non-radioactive sludge streams, each with distinct characteristics and composition. Ceramicrete with wollastonite as filler was used as the matrix for this purpose. The resulting waste forms were tested for their mechanical properties, radiation stability, and leaching resistance. In another series of tests, the samples were vitrified in borosilicate glass and glass waste forms were produced. The Product Consistency Test, the American Nuclear Society's ANS 16.1 test, and the Toxicity Characteristic Leaching Procedure, which are used to develop waste acceptance criteria in the United States for permanent storage of treated waste, were used for evaluation of the leaching resistance of all waste forms.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗