Electrochemical Impedance Spectroscopy of Alloys in a Simulated Space Shuttle Launch Environment

Corrosion studies began at NASA/Kennedy Space Center in 1966 during the Gemini/Apollo Programs with the evaluation of long-term protective coatings for the atmospheric protection of carbon steel. An outdoor exposure facility on the beach near the launch pad was established for this purpose at that time. The site has provided over 35 years of technical information on the evaluation of the long-term corrosion performance of many materials and coatings as well as on maintenance procedures. Results from these evaluations have helped NASA find new materials and processes that increase the safety and reliability of our flight hardware, launch structures, and ground support equipment. The launch environment at the Kennedy Space Center (KSC) is extremely corrosive due to the combination of ocean salt spray, heat, humidity, and sunlight. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pad were rendered even more severe by the acidic exhaust from the solid rocket boosters. Over the years, many materials have been evaluated for their corrosion performance under conditions similar to those found at the launch pads. These studies have typically included atmospheric exposure and evaluation with conventional electrochemical methods such as open circuit potential (OCP) measurements, polarization techniques, and electrochemical impedance spectroscopy (EIS). The atmosphere at the Space Shuttle launch site is aggressive to most metals and causes severe pitting in many of the common stainless steel alloys such as type 304L stainless steel (304L SS). A study was undertaken to find a more corrosion resistant material to replace the existing 304L SS tubing. This paper presents the results from atmospheric exposure as well as electrochemical measurements on the corrosion resistance of AL-6XN (UNS N08367) and 254-SMO (UNS S32154). Type 304L SS (UNS S30403) was used as a control. Conditions at the Space Shuttle launch pad were simulated by using a hydrochloric acid (HC1) and alumina (Al203) slurry rinse for the atmospheric exposure and an electrolyte consisting of 3.55% sodium chloride (NaC1) with increased concentrations of hydrochloric acid (HC1) for the electrochemical measurements. The results from both types of measurements revealed the superior corrosion performance of the higher-alloyed materials. Unlike 304L SS, 254-SMO and AL-6XN exhibited a significantly improved resistance to corrosion as the concentration of hydrochloric acid in he 3.55% NaCl electrolyte solution was increased.

Calle, L. M.↗

Numerical investigation of micro-galvanic corrosion in Mg alloys: Role of the cathodic intermetallic phase size and spatial distributions

Magnesium alloys are of increasing interest in structural applications due to their low-density, moderate specific strength and stiffness, recyclability, and high damping among other properties. However, the wide-scale applicability of magnesium alloys in structural applications has been limited due to many factors including its poor corrosion resistance. In this work, a numerical investigation to simulate the micro-galvanic corrosion behavior was performed to examine the influence of size and distribution of cathodic intermetallic phase (ß-Mg17Al12) in a Mg matrix. The ratio of cathodic to anodic surface area was kept constant in each simulation condition to understand the effect of size and spacing distributions. In general, fragmentation of a larger intermetallic particle into smaller ones was found to enhance the localized current density. However, the uniform distribution of this small intermetallic phase throughout the matrix was found to reduce the overall dissolution current density and hence, pitting corrosion severity.

Beura, Vikrant↗

Acceleration of Thermochemistry Solves in MOOSE and Pronghorn

This work focuses on the development and implementation of strategies to accelerate thermochemical calculations within MOOSE-based multiphysics simulations, particularly for applications in MSRs. We highlight the inherent complexity of nuclear materials, which require a multiscale approach to accurately model their behavior across various physical domains, including mechanical, chemical, and thermal phenomena. Thermochemical equilibrium calculations are crucial for predicting material properties and enhancing the fidelity of these simulations. The integration of Thermochimica, a Gibbs energy minimizer, into MOOSE allows for the direct minimization of Gibbs energy at every point on the mesh. However, the computational cost of such integration is significant. To address this, we explored acceleration strategies such as multi-threading support and the use of a thermodynamic ValueCache to reduce redundant calculations. Additionally, we investigated modifications to Thermochimica to enable phase constraints and improve its coupling with phase-field models, which are essential for simulating microstructural evolution and corrosion in MSR. These efforts aim to optimize the computational efficiency and accuracy of multiphysics simulations, thereby supporting the development of reliable and efficient nuclear materials for next-generation reactor technologies.

36 - MATERIALS SCIENCE↗

Critical mineral substitutions in IN617: A combined computational and experimental approach to performance evaluation and feasibility

Addressing the escalating demand for critical minerals (CMs) driven by global climate change initiatives, this study explores compositional modifications to Inconel 617 (IN617) by substituting cobalt (Co) with manganese (Mn) across various atomic percentages. Here, we conducted a computational feasibility study employing Molecular Dynamics (MD) simulations to provide strategic guidance for experimental validation. The simulations analyzed tensile strength and corrosion resistance for five modified compositions (M1 to M5) to identify optimal properties. Tensile tests on cubic simulation cells were performed to generate stress-strain curves, revealing the impact of Co replacement with Mn on tensile strength—a metric correlated with hardness. Oxygen penetration simulations were conducted to evaluate corrosion resistance, indicating that reduced oxygen penetration depth corresponds to enhanced resistance. Promising compositions underwent phase diagram calculations for assessing phase stability. The optimal composition (M1), characterized by high tensile strength and minimal oxygen penetration, was chosen for experimental validation using induction melting and friction stir consolidation techniques. The materials were further characterized using SEM-EDS, XRD, and Vickers hardness testing. Our findings suggest that Mn substitution in IN617 can yield mechanical performance at par with high-Co alloys in energy-critical applications.

36 MATERIALS SCIENCE↗

Turbine Airfoil Deposition Models

Gas turbine failures associated with sea-salt ingestion and sulfur-containing fuel impurities have directed attention to alkali sulfate deposition and the associated hot corrosion of gas turbine (GT) blades under some GT operating conditions. These salt deposits form thin, molten films which undermine the protective metal oxide coating normally found on GT blades. The prediction of molten salt deposition, flow and oxide dissolution, and their effects on the lifetime of turbine blades are examined. Goals include rationalizing and helping to predict corrosion patterns on operational GT rotor blades and stators, and ultimately providing some of the tools required to design laboratory simulators and future corrosion-resistant high-performance engines. Necessary background developments are reviewed first, and then recent results and tentative conclusions are presented along with a brief account of the present research plans.

Rosner, D. E.↗

Reduction of Methane Leaks through Corrosion Mitigation Pre-treatments for Pipelines with Field Applied Coatings

Corrosion of buried, coated steel pipelines transporting natural gas is a significant source of methane emissions, from pipeline venting required for maintenance and repairs and from pipeline leaks and incidents. Corrosion of steel under field applied coatings is an important safety concern for the pipeline industry. This project investigates the application of a field applied alloy over girth welds to mitigate external corrosion of buried coated steel pipelines. Various metallic coating options were considered, which were required to meet several criteria: (1) it must resist corrosion under open-circuit or mild cathodic protection conditions, (2) it must protect the substrate steel, and (3) it must not negatively affect the adhesion of the field coating. Finite element models and lab testing were performed of alloy coating compositions to identify promising alloy types underneath disbonded coatings. Polarization curves of coating alloys were generated to provide the boundary conditions for the COMSOL model to compute potential and current distributions around coated areas. Sacrificial and corrosion-resistant metal alloy coatings were evaluated and optimized using corrosion modeling and laboratory electrochemical testing, where aluminum alloy 5356 (5% Mg) and steel alloy B9 (9% Cr) were selected. Corrosion test coupons were designed and fabricated using thermal spray aluminum 5356 and welded B9 steel overlays on API 5L grade X42 line pipe steel. The corrosion test coupons, with simulated pipe coating damage, were tested in a laboratory soil box and a field pipeline site in Texas for 3-months. Corrosion test coupons were then tested for 6-months at field pipeline sites in Texas and Tennessee to quantify corrosion rates and performance of the aluminum and steel alloys under polyethylene tape and 2-part epoxy coatings, various coating holidays, and with and without cathodic protection.

03 NATURAL GAS↗

Wire arc additive manufactured A36 steel performance for marine renewable energy systems

Additive manufacturing has established itself to be advantageous beyond small-scale prototyping, now supporting full-scale production of components for a variety of applications. Despite its integration across industries, marine renewable energy technology is one largely untapped application with potential to bolster clean energy production on the global scale. Wave energy converters (WEC) are one specific facet within this realm that could benefit from AM. As such, wire arc additive manufacturing (WAAM) has been identified as a practical method to produce larger scale marine energy components by leveraging cost-effective and readily available A36 steel feedstock material. The flexibility associated with WAAM can benefit production of WEC by producing more complex structural geometries that are challenging to produce traditionally. Additionally, for large components where fine details are less critical, the high deposition rate of WAAM in comparison to traditional wrought techniques could reduce build times by an order of magnitude. In this context of building and supporting WEC, which experience harsh marine environments, an understanding of performance under large loads and corrosive environments must be understood. Hence, WAAM and wrought A36 steel tensile samples were manufactured, and mechanical properties compared under both dry and corroded conditions. Here, the unique microstructure created via the WAAM process was found to directly correlate to the increased ultimate tensile and yield strength compared to the wrought condition. Static corrosion testing in a simulated saltwater environment in parallel with electrochemical testing highlighted an outperformance of corroded WAAM A36 steel than wrought, despite having a slighter higher corrosion rate. Ultimately, this study shows how marine energy systems may benefit from additive manufacturing components and provides a foundation for future applications of WAAM A36 steel.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Zinc Cold Spray Coatings in a Simulated Natural Gas Environment Containing H2O, CO2, and H2S

The natural gas transmission pipeline network in the U.S. consists of approximately 300,000 miles, is made mainly of carbon steel, and was installed in the 1950s and 1960s. Understanding the pipeline steel behavior in natural gas will inform new pipeline designs and repurposing of existing pipelines. Sulfide stress cracking (SSC) is a problem for steel pipelines transporting natural gas or CO2 containing partial pressures of H2S higher than 0.3 kPa (0.05 psi). Therefore, the objective of this work is to mitigate internal corrosion in steel pipelines transporting natural gas containing H2S using cold spray coatings.

Belarbi, Zineb↗

Pitting Corrosion in 316L Stainless Steel Fabricated by Laser Powder Bed Fusion Additive Manufacturing: A Review and Perspective

Abstract 316L stainless steel (316L SS) is a flagship material for structural applications in corrosive environments, having been extensively studied for decades for its favorable balance between mechanical and corrosion properties. More recently, 316L SS has also proven to have excellent printability when parts are produced with additive manufacturing techniques, notably laser powder bed fusion (LPBF). Because of the harsh thermo-mechanical cycles experienced during rapid solidification and cooling, LPBF processing tends to generate unique microstructures. Strong heterogeneities can be found inside grains, including trapped elements, nano-inclusions, and a high density of dislocations that form the so-called cellular structure. Interestingly, LPBF 316L SS not only exhibits better mechanical properties than its conventionally processed counterpart, but it also usually offers much higher resistance to pitting in chloride solutions. Unfortunately, the complexity of the LPBF microstructures, in addition to process-induced defects, such as porosity and surface roughness, have slowed progress toward linking specific microstructural features to corrosion susceptibility and complicated the development of calibrated simulations of pitting phenomena. The first part of this article is dedicated to an in-depth review of the microstructures found in LPBF 316L SS and their potential effects on the corrosion properties, with an emphasis on pitting resistance. The second part offers a perspective of some relevant modeling techniques available to simulate the corrosion of LPBF 316L SS, including current challenges that should be overcome.

Voisin, T. (ORCID:0000000287462659)↗

Galvanic corrosion of AZ31B joined to dual-phase steel with and without Zn layer by ultrasonic and friction stir welding

Galvanic corrosion of AZ31B joined with bare or Zn-coated DP590 steel by ultrasonic spot welding or linear friction stir welding was quantitatively studied by pre-defining anode and cathode in the lap joint samples. Corrosion volume and depth from Mg anode surfaces exposed to 0.1 M sodium chloride solution was analyzed as functions of cathode surface type and welding method. Characterization of as-welded joints was performed to identify any microstructural feature of the bonding zone that could impact galvanic corrosion behavior. COMSOL modeling with modified user subroutine was conducted to simulate the progression of Mg corrosion in the same joint and electrode configurations used for the corrosion experiments. The experimental results indicated that Zn-coated cathode surface can reduce Mg galvanic corrosion significantly as galvanic polarization and cathodic current on Zn-coated surface remained relatively low for Mg in the weld joints. COMSOL modeling described the growth of Mg galvanic corrosion in a reasonable manner but showed limitation by underestimating the corrosion volume as it did not capture self-corrosion.

36 MATERIALS SCIENCE↗

A comparative study of mechanical and chemical durability of non-wetting superhydrophobic and lubricant-infused surfaces

Fabrication of bioinspired non-wetting superhydrophobic surfaces (SHS) and lubricant-infused surfaces (LIS) has been studied extensively on a variety of materials. In contrast, durability of the surfaces exposed to harsh mechanical and chemical environments has been the subject of little attention. This study considers the mechanical and chemical durability of SHS and LIS copper surfaces fabricated via facile electrodeposition and chemical etching methods. The as-fabricated surfaces demonstrate excellent non-wetting characteristics with water contact angle of 160° and sliding angle below 5°. The surfaces are subject to mechanical wear through scratch test and water jet impingement at 15 psi and 20 psi as well as accelerated corrosion following the ASTM-E407 standard. The performance of the electrodeposited and etched non-wetting surfaces is systematically assessed in terms of contact and sliding angles and corrosion rate in a simulated marine environment. All surfaces are shown to be robust to mechanical wear after scratch test, with excellent stability of contact and sliding angles, and up to two orders of magnitude reduced corrosion rate compared to bare copper surface. SHS retained steadfast non-wetting characteristics under high-pressure water jet tests compared to the other surfaces while LIS, regardless of texturing method, showed one to two orders of magnitude reduced corrosion rate compared to bare copper surface throughout water jet impingement and chemical durability tests. The study presents for the first time a systematic comparison of durability of SHS and LIS through a common set of fabrication and testing protocol and helps identify appropriate non-wetting surfaces and fabrication methods based on the use environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Near-Field Corrosion Interactions between Glass and Corrosion Resistant Alloys

This study explores the corrosion interactions between model nuclear waste glass materials and corrosion resistant alloys, under conditions that simulate the near field of a nuclear waste repository. The interactions between the corrosion of stainless steel (SS) 316, alloy G30, or alloy 625, and international simple glass or soda-lime silica glass are systematically studied. The dissimilar materials were exposed in close proximity to each other in different electrolytes at 90 oC. After exposure, the glass surface exposed near metals showed different regimes of corrosion, with distinct surface morphologies and chemistries that were likely affected by the local environment created by the localized corrosion of metals. Surface and solution analyses showed that the corrosion rate of glass was enhanced by the presence of metals. Infrared spectroscopy data suggested the local build-up of stresses in the contact area of glass, which may lead to the mechanical instability of the glass alteration layer. On the other hand, the effect of glass on metal corrosion is strongly dependent on the leaching solution. In electrolytes containing abundant aggressive anions such as Cl-, glass seems to suppress the localized corrosion of SS by the precipitation of a Si-rich surface film that protects the SS substrate from solutions. However, in less aggressive electrolytes, the corrosion rate of SS was increased by the presence of glass corrosion products. Overall, our study showed that the hidden and localized damage on glass in contact with metals may enhance the release of incorporated radionuclides compared to typical uniform glass corrosion. Therefore, more attention should be paid to the corrosion interactions between metals and glass under repository conditions.

Guo, Xiaolei↗

Advanced neutron absorber Ni-Cr-Mo-Gd alloys seawater corrosion mechanism and susceptibility study

Previous studies demonstrated the corrosion susceptibility of advanced neutron absorber (ANA) Ni-Cr-Mo-Gd in a seawater environment but remained inconclusive. In this paper, scanning electron microscopy was employed to identify the corrosion phase in Ni-Cr-Mo-Gd, and computational thermodynamic simulation was used to study phase corrosion potentials. Results showed that the Ni 5 Gd second phase, distributed along FCC grain boundaries in Ni-Cr-Mo-Gd, has lower corrosion potential than the substrate. Furthermore, heat treatment and alloy chemistry adjustment would not ameliorate the ANA corrosion susceptibility. Finally, isolating the Ni 5 Gd from the corrosion medium through advanced manufacturing is a viable way to improve the ANA corrosion resistance.

36 MATERIALS SCIENCE↗

The origin of passivity in aluminum-manganese solid solutions

In this work, the effects of manganese on the aqueous corrosion of aluminum-manganese alloys were investigated by experiments and atomistic simulations. Electrochemical measurements, x-ray photoelectron spectroscopy, and atom probe tomography analysis indicate that manganese addition enhanced the corrosion resistance of aluminum without participating in the surface oxidation. Furthermore, the selective dissolution of manganese was believed to increase the free volume at the metal/oxide interface to facilitate the formation of a denser, thinner oxide layer with closer to stoichiometry composition. Atomistic simulations showed that the oxide layer compactness increased, and defect density decreased with increasing free volume content in Al, resulting in enhanced barrier characteristics.

36 MATERIALS SCIENCE↗

The Long-term Storage of ILW: Building Stores with the Appropriate Environmental Controls - 20294

In the UK, containers for the storage and disposal of intermediate level radioactive waste (ILW) typically use stainless steel due to its excellent mechanical properties and corrosion resistance. The period of interim storage before a disposal facility is available, however, is longer than available engineering experience with stainless steels in relevant environmental conditions. Additionally, after disposal the ability of ILW containers to withstand further periods of exposure to the environment is expected to provide substantial benefits to the operation of a disposal facility and the safety case underpinning its closure. For these reasons, although there have been no instances of failure of stainless steels in indoor storage conditions, a focused R and D programme has been carried out to identify the environmental envelope over which the material does not significantly degrade. In this study we summarise experimental and modelling studies carried out over the last decade to build a solid mechanistic understanding of the corrosion behaviour of stainless steels in indoor atmospheric conditions. We then identify suitable environmental regimes to minimise the risk of degradation processes and explore approaches to monitoring the storage conditions to gain confidence in the long-term performance of the system. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Patchy particle model of hydrated amorphous silica

Glasses corroded in static aqueous conditions typically reach a slow, residual rate of dissolution as a result of the complex interplay between multiple processes. While intrinsically suited to address this problem, Monte Carlo (MC) models developed to date have relied on lattices to describe the amorphous structure of glass and are thus unable to reproduce the residual rate of glass corrosion. A recently developed MC approach based on amorphous structures derived from molecular dynamics simulations offers a solution [Kerisit and Du J. Non-Cryst. Solids 522 (2019) 119601], but it requires a simple model that can rapidly relax the glass-water interface upon each dissolution/condensation event to retain the ability of MC simulations to reach large spatial and temporal scales. To this end, a patchy particle model of hydrated amorphous silica was developed and evaluated against atomistic simulations in this work. Models of water and amorphous silica were first developed separately, and cross terms were then defined to enable simulations of hydrated amorphous silica structures with varying water content. While the nature of its interaction potential prevents the patchy particle model from reproducing simultaneously the structure and dynamics of the systems of interest with a single set of parameters, it described well the connectivity of hydrated amorphous silica structures and the local coordination geometry of individual species. Therefore, this model opens the door to MC simulations of the residual rate of glass corrosion and offers an alternative to atomistic models to investigate the evolution of silica gels over large spatial and temporal scales.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Toward the performance assessment of advanced nuclear waste forms: temperature dependence of lanthanide borosilicate glass dissolution

Lanthanide borosilicate (LaBS) glasses are among the most promising waste forms for the immobilization of high-level radioactive waste generated from advanced nuclear fuel cycles. However, the temperature dependence of their dissolution kinetics remains poorly understood and constrained, limiting the integration of these materials into established performance assessment models. Here, we investigate the dissolution behavior of the legacy AmCm2-19 LaBS glass and the benchmark alkali aluminoborosilicate ISG-1 in deionized water between 50 °C and 250 °C using ASTM C1285 (Product Consistency Test-B) protocols. For AmCm2-19 LaBS glass, normalized elemental release rates for boron and silicon increase with temperature before plateauing near 150 °C, consistent with solubility-limited behavior. From data obtained at 50 °C and 100 °C, Arrhenius analysis yields activation energies of E a (B) = 24.8 ± 0.3 kJ mol⁻¹ and E a (Si) = 14.4 ± 0.2 kJ mol⁻¹, similar or slightly lower than those previously reported for two other compositions of LaBS glasses. No secondary phases or alteration layers were detected by SEM-EDX or pXRD. These results establish one of the first temperature-dependent kinetic datasets for LaBS glass dissolution, providing quantitative parameters to inform mechanistic corrosion models and predictive simulations of glass degradation in geological disposal environments.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗