Search NASA⌕ Search

SEARCH · Search NASA

Results for “cracking temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Creep fatigue life prediction for engine hot section materials (isotropic)

The Hot Section Technology (HOST) program, creep fatigue life prediction for engine hot section materials (isotropic), is reviewed. The program is aimed at improving the high temperature crack initiation life prediction technology for gas turbine hot section components. Significant results include: (1) cast B1900 and wrought IN 718 selected as the base and alternative materials respectively; (2) fatigue test specimens indicated that measurable surface cracks appear early in the specimen lives, i.e., 15% of total life at 871 C and 50% of life at 538 c; (3) observed crack initiation sites are all surface initiated and are associated with either grain boundary carbides or local porosity, transgrannular cracking is observed at the initiation site for all conditions tested; and (4) an initial evaluation of two life prediction models, representative of macroscopic (Coffin-Mason) and more microscopic (damage rate) approaches, was conducted using limited data generated at 871 C and 538 C. It is found that the microscopic approach provides a more accurate regression of the data used to determine crack initiation model constants, but overpredicts the effect of strain rate on crack initiation life for the conditions tested.

Moreno, V.↗

Reliability Issues with PME and BME Ceramic Capacitors

This work is a review of reliability issues specific for low-voltage precious metal electrode (PME) and base metal electrode (BME) multilayer ceramic capacitors (MLCC). A special attention is given to degradation and failures in capacitors with defects, in particular with cracks. Temperature and voltage reliability acceleration factors have been calculated based on approximation of distributions of degradation rates of leakage currents using a general log-linear Weibull model. Results show a substantial difference in behavior of BME and PME capacitors with defects. Mechanisms of degradation and failures in humid and dry environments and risks of overstressing capacitors during highly accelerated life testing (HALT) are discussed.

Teverovsky, Alexander↗

Separate-Effects Tests for Studying Temperature-Gradient-Driven Cracking in UO 2 Pellets

We report a variety of normal operation and accident scenarios can generate thermal stresses large enough to cause cracking in light-water reactor (LWR) fuel pellets. Cracking of fuel pellets can lead to reduced heat removal, higher centerline temperatures, and localized stress in cladding, all of which impact fuel performance. It is important to experimentally characterize the thermal and mechanical behavior in the pellet before and after cracking to improve cracking models in fuel performance codes. However, in-reactor observation and measurement of cracking is very challenging due to the harsh environment and logistics. Recently, an experimental pellet cracking test stand was developed for separate effects testing of normal operations and accident temperature conditions, using thermal imaging to capture the pellet surface temperature for evaluation of thermal stresses and optical imaging to capture the evolution of cracking in real time. Experiments were performed using depleted uranium dioxide (UO 2 ) pellets, which are useful for collecting data valuable for development and validation of cracking models. A combination of induction and resistance heating was used to create an average temperature gradient of 236°C/cm and 193°C/cm before and after cracking respectively. Characterization of the pellets were done before as well as after cracking. The cracking patterns are somewhat different than those expected in a typical reactor because of the differences in thermal conditions and pellet microstructure. However, if the actual conditions of these experiments are reproduced in computational models, these out-of-pile tests on UO 2 pellets provide relevant data for modeling purposes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Intergranular Stress Corrosion Crack Initiation and Temperature Dependence of Alloy 600 in Pressurized Water Reactor Primary Water

Stress corrosion crack (SCC) initiation of a solution annealed, cold-worked (CW) UNS N06600 (Alloy 600) material was investigated in 360 and 325ºC simulated PWR primary water using constant load tensile instrumented for in-situ detection by the direct current potential drop technique. This CW material with high boron and low carbon bulk concentrations was found to be highly susceptible to SCC. Consistent SCC initiation times were obtained at both temperatures and the thermal activation energy for SCC initiation is estimated at ~116 kJ/mol.

Zhai, Ziqing↗

Experimental Study on Mitigation of Lifetime-Limiting Dielectric Cracking in Extreme Temperature 4H-SiC JFET Integrated Circuits

While NASA Glenn Research Center's "Generation 10" 4H-SiC Junction Field Effect Transistor (JFET) integrated circuits (ICs) have uniquely demonstrated 500 °C electrical operation for durations of over a year, this experimental work has also revealed that physical cracking of chip dielectric passivation layers ultimately limits extreme-environment operating lifetime [1-3]. The prevention of such dielectric passivation cracks should therefore improve IC high temperature durability and yield, leading to more beneficial technology adoption into aerospace, automotive, and energy systems. This report describes Generation 10.2, 11.1, and 11.2 die tested under unbiased and unpackaged accelerated age testing at 500 °C, 600 °C, 720 °C, and 800 °C in air-atmosphere ovens for 100- and 200-hour duration. Additional samples were separately subjected to 10 thermal cycles between the same high temperatures (with 10-hour high-temperature soak each cycle) and 50 °C. It is shown that having two stoichiometric Si3N4 layers in the interconnect dielectric stack substantially decreases the amount of dielectric cracking observed following these oven tests.

Spry, D. J.↗

Fatigue crack growth at elevated temperature 316 stainless steel and H-13 steel

Crack growths were measured at elevated temperatures under four types of loading: pp, pc, cp, and cc. In H-13 steel, all these four types of loading gave nearly the same crack growth rates, and the length of hold time had negligible effects. In AISI 316 stainless steel, the hold time effects on crack growth rate were negligible if the loading was tension-tension type; however, these effects were significant in reversed bending load, and the crack growth rates under these four types of loading varied considerably. Both tensile and compressive hold times caused increased crack growth rate, but the compressive hold period was more deleterious than the tensile one. Metallographic examination showed that all the crack paths under different types of loading were largely transgranular for both CTS tension-tension specimens and SEN reversed cantilever bending specimens. In addition, an electric potential technique was used to monitor crack growth at elevated temperature.

Chen, W. C.↗

A Comparison of Weld-Repaired and Base Metal for Inconel 718 and CRES 321 at Cryogenic and Room Temperatures

Fatigue crack growth tests were conducted to characterize the performance of Inconel 718 and CRES 321 welds, weld heat-affect-zone and parent metal at room temperature laboratory air and liquid nitrogen (-196oC) environments. The results of this study were required to predict the damage tolerance behavior of proposed orbiter main engine hydrogen fuel liner weld repairs. Experimental results show that the room and cryogenic temperature fatigue crack growth characteristics of both alloys are not significantly degraded by the weld repair process. However, both Inconel 718 and CRES 321 exhibited lower apparent toughness within the weld repair region compared to the parent metal.

Newman, John A.↗

High temperature constitutive and crack initiation modeling of coated single crystal superalloys

The purpose of this program is to develop life prediction models for anisotropic materials used in gas turbine airfoils. In the base portion of the program, two coated single crystal alloys are being tested. They are PWA 286 overlay coated and PWA 273 aluminide coated PWA 1480 and PWA 286 overlay coated Alloy 185. Viscoplastic constitutive models for these materials are also being developed to predict the cyclic stress-strain histories required for life prediction of the lab specimens and actual airfoil designs.

Meyer, Thomas G.↗

The influence of temperature on fatigue-crack growth in a mill annealed Ti-6Al-4V alloy

To understand the influence temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude, fatigue crack growth experiments were carried out using a 1/4-inch-thick (6.35 mm) mill annealed Ti-6Al-4V alloy plate as a model material. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C (or, about 550 F/563K) and as a function of the crack tip stress intensity factor in a dehumidified high purity argon environment. Limited correlative experiments indicate that dehumidified oxygen and hydrogen have no effect on the rate of fatigue crack growth in this alloy, while distilled water increased the rate of crack growth slightly in the range tested. Companion fractographic examinations suggest that the mechanisms for fatigue crack growth in the various environments are essentially the same.

Wei, R. P.↗

The influence of temperature on fatigue-crack growth in a mill-annealed Ti-6Al-4V alloy

To understand the influence of temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude fatigue crack growth experiments were carried out using a 1/4 inch thick (6.35 mm) mill-annealed Ti-6Al-4V alloy plate as a model material. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C and as a function of the crack tip, stress intensity factor K, in dehumidified high purity argon environment. The dependence of the rate of fatigue crack growth on K appears to be separable into two regions. The transition correlates with changes in both the microscopic and macroscopic appearances of the fracture surfaces, and suggests a change in the mechanism and the influence of microstructure on fatigue crack growth.

Wei, R. P.↗

Drying Temperature and Capillarity-Driven Crack Formation in Aqueous Processing of Li-Ion Battery Electrodes

Unlike conventional electrode processing for Li-ion batteries, which uses the expensive and highly toxic organic N -methyl-2-pyrrolidone (NMP) solvent, aqueous processing simply employs deionized water as the solvent. Yet, thick aqueous processed cathodes have been found to crack during drying. Here, the influence of electrode drying temperature and thickness on cracking was investigated. LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes prepared with a hydrophilic binder, modified styrene–butadiene rubber (SBR), were coated at various thicknesses and dried at temperatures ranging from 20 to 70 °C. Experiments revealed cracking worsens with increased electrode thickness and elevated drying temperatures. Cracks were formed during the capillarity-driven phase during drying. Strong evaporation and weak diffusion played a critical role in the nonuniform distribution of the inactive phase. Images of electrode surfaces were processed to quantify crack dimensions and crack intensity factor (CIF). The average crack length and width, as well as CIF, increased with drying temperature and electrode thickness. Electrochemical performance revealed a strong and negative correlation between the crack density and performance in terms of specific capacity. Transport limitations associated with the presence of cracks adversely affect the advantage of high volume ratio of active materials in the thick electrodes.

25 ENERGY STORAGE↗

The relationship between low-temperature toughness and secondary crack in low-carbon bainitic weld metals

Highlights: • The crack propagation plane was identified with the decreasing possibility of {110}/{100}, {112} and {123}. • Crack path deviates at some middle-angle misorientation boundaries with high strain concentration. • The most effective barrier to arrest crack in Ni0 and Ni2 is the boundaries of inter-Bain in a CPP packet, while in Ni4 the boundaries of inter-CPP and intra-Bain packets impede crack propagation. - Abstract: This paper aims to reveal the relationship among low-temperature toughness, microstructure and secondary crack from both microstructural and crystallographic perspectives. Instrumented Charpy tests were carried out in the upper platform, transition temperature range, as well as at lower temperatures. Quantitative fractographic analysis, microstructural characterization and secondary crack observation were conducted on half of the impact specimen. Crystallographic features were identified in the secondary crack proximity, e.g. variant selection, orientation relationship, cleavage plane of the corresponding crack matrix. Some results in literature are confirmed. Nickel addition is beneficial to hindering crack propagation as a result of microstructure improvement. The most effective barrier for crack propagation is high-angle misorientation boundaries between Bain packets and the boundaries of ferrite matrix with the microstructure of granular bainite. Additionally, high-angle misorientation boundaries between closed-packed plane packets arrest cracks in the mixed microstructure of fine lath bainite and intricate acicular ferrite. Most preferred crack propagation planes are {110} and {100} in our low carbon bainitic weld metals, with the decreasing possibility of {112} and {123}.

36 MATERIALS SCIENCE↗

A Mechanistic-Based Healing Model for Self-Healing Glass Seals Used in Solid Oxide Fuel Cells

The usage of self-healing glass as hermetic seals is a recent advancement in sealing technology development for the planar solid oxide fuel cells (SOFCs). Because of its capability of restoring the mechanical properties at elevated temperatures, the self-healing glass seal is expected to provide high reliability in maintaining the long-term structural integrity and functionality of SOFCs. In order to accommodate the design and to evaluate the effectiveness of such engineering seals under various thermo-mechanical operating conditions, computational modeling framework needs to be developed to accurately capture and predict the healing behavior of the glass material. In the present work, a mechanistic-based two-stage model was developed to study the stress and temperature-dependent crack healing of the self-healing glass materials. The model was first calibrated by experimental measurements combined with the kinetic Monte Carlo (kMC) simulation results and then implemented into the finite element analysis (FEA). The effects of various factors, i.e. stress, temperature, crack morphology, on the healing behavior of the glass were investigated and discussed.

30 DIRECT ENERGY CONVERSION↗

Applications of elastic-viscoplastic constitutive models in dynamic analyses of crack run-arrest events

Applications of nonlinear techniques to the first series of six HSST wide-plate crack-arrest tests that were performed are described. The experiments include crack initiations at low temperatures and relatively long (20 cm) cleavage propagation phases which are terminated by arrest in high temperature regions. Crack arrest are then followed by ductile tearing events. Consequently, the crack front regions are exposed to wide ranges of strain rates and temperatures.

Bass, B. R.↗

A study on tensile properties of Alloy 709 at various temperatures

In recent years, there have been several advancements in energy production from both fossil fuels and the alternate “clean” sources such as nuclear fission. These advancements are fueled by the need for more efficient systems that will optimize the use of the depleting fossil fuel reserves and shift the focus to cleaner sources of energy. The efficiency of any power generation cycle is dependent on the ability of the structural material to withstand increased peak operating temperatures. Advanced austenitic stainless steels have been in the focus as structural material for the next generation nuclear power plants, due to their strength, corrosion resistance, weldability and the wide range of temperatures at which the austenite phase is stable. Alloy 709, a recently developed advanced austenitic stainless steel, is being investigated in this paper. Here in this study, tensile tests were conducted on dog-bone samples of Alloy 709 in an in-situ scanning electron microscope (SEM) loading and heating stage, equipped with electron backscatter diffraction (EBSD), at various temperatures. The in-situ experiments indicated that the material primarily accommodated deformation by slip at lower temperatures. Void formation and coalescence at grain boundaries preceded slip at higher temperatures. Although crack initiation at all elevated temperatures was intergranular, the crack propagation through the material and the final fracture was transgranular ductile. Additionally, tensile tests were conducted on larger cylindrical samples at 550, 650 and 750 °C in air. The results of tests conducted in air and in-situ were found to be in agreement, at these temperatures.

36 MATERIALS SCIENCE↗