Search NASA⌕ Search

SEARCH · Search NASA

Results for “damage threshold”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Impact of substrate surface scratches on the laser damage resistance of multilayer coatings

Substrate scratches can limit the laser resistance of multilayer mirror coatings on high-peak-power laser systems. To date, the mechanism by which substrate surface defects affect the performance of coating layers under high power laser irradiation is not well defined. In this study, we combine experimental approaches with theoretical simulations to delineate the correlation between laser damage resistance of coating layers and the physical properties of the substrate surface defects including scratches. A focused ion beam technique is used to reveal the morphological evolution of coating layers on surface scratches. Preliminary results show that coating layers initially follow the trench morphology on the substrate surface, and as the thickness increases, gradually overcoat voids and planarize the surface. Simulations of the electrical-field distribution of the defective layers using the finite-difference time-domain (FDTD) method show that field intensification exists mostly near the top surface region of the coating near convex focusing structures. The light intensification could be responsible for the reduced damage threshold. Damage testing under 1064 nm, 3 ns laser irradiation over coating layers on substrates with designed scratches show that damage probability and threshold of the multilayer depend on substrate scratch density and width. Our preliminary results show that damage occurs on the region of the coating where substrate scratches reside and etching of the substrate before coating does not seem to improve the laser damage resistance.

42 ENGINEERING↗

Experimental study correlating damage and permeability in concrete using confined, flattened Brazilian disks

This research experimentally studies coupled hydro-mechanical relationships using flattened Brazilian disks under confinement, with concurrent permeability measurements and acoustic emission monitoring. A series of tests are performed on concrete, as representative samples of brittle geo-materials, under a range of confining stresses between 2.76 and 13.79 MPa. Acoustic emission data is used to quantify damage and identify damage thresholds. Damage is then correlated to pre-peak changes in permeability. The advancement of models that couple transport properties to mechanical responses are of interest in the fields of carbon sequestration, hydrofracking, production of geothermal energy, induced seismicity, and underground nuclear waste storage, and these experiments validate a novel experimental approach towards investigating hydro-mechanical relationships.

Boyce, S.↗

A Survey of Transparent Conducting Films and Optoelectrical Materials for High Optical Power Applications

The lifetime laser damage performance of a wide range of transparent conductive materials is assessed, including ultrathin metal films, doped metal oxides, doped compound semiconductors, and graphene whose carrier densities span five orders of magnitude from 10 18 to 10 23 cm -3 . Lifetime laser damage thresholds are determined by exposing material surfaces to repeated nanosecond laser pulses at near IR wavelengths (1064 nm). Near threshold fluences, two distinct damage modes, i.e., bulk and discrete, emerge depending on carrier density. These bulk and discrete damage modes are attributed to free carrier-induced bulk and localized, defect-driven absorption processes, respectively. For polycrystalline films with free carrier densities greater than ≈10 20 cm -3 , laser damage thresholds are less than 5 J cm -2 . In contrast, bulk absorption is not apparent at thresholds substantially higher than ≈10 J cm-2 in single-crystal films with free carrier concentrations lower than ≈10 19 cm -3 . By increasing thickness, films with lower carrier densities can deliver relevant levels of sheet conductance (<200 Ω sq -1 ) while remaining transparent. These lifetime laser damage threshold measurements offer systematic criteria to select materials aimed at handling high optical powers in optoelectronics devices and emerging plasmonic and metamaterials for lasers.

36 MATERIALS SCIENCE↗

Laser-induced damage-growth threshold at 351 nm in the nanosecond regime in dielectric coatings employing different high-index materials

The laser-damage performance of HfO 2 /SiO 2 and Al 2 O 3 /SiO 2 mirrors was investigated at a laser wavelength of 351 nm with nanosecond pulse durations. A method was developed to quantify the laser-induced damage-growth threshold under conditions relevant to high-repetition-rate, large-aperture laser systems. The results suggest that the damage-growth performance cannot be inferred from the corresponding damage-initiation threshold that is commonly used to evaluate the performance of optical materials. Here, a systematic difference was also observed in the performance between these two groups of high-index materials, with the Al 2 O 3 /SiO 2 mirrors exhibiting about twofold improvement in the damage-growth threshold.

36 MATERIALS SCIENCE↗

Nanosecond-laser-induced damage in potassium titanyl phosphate: pure 532 nm pumping and frequency conversion situations

Nanosecond-laser-induced damage measurements in the bulk of KTiOPO{sub 4} (KTP) crystals are reported using incident 532 nm light or using incident 1064 nm light, which pumps more or less efficient second harmonic generation. No damage threshold fatigue effect is observed with pure 532 nm irradiation. The damage threshold of Z-polarized light is higher than the one for X- or Y-polarized light. During frequency doubling, the damage threshold was found to be lower than for pure 1064 or 532 nm irradiation. More data to quantify the cooperative damage mechanism were generated by performing fluence ramp experiments with varying conditions and monitoring the conversion efficiency. All damage thresholds plotted against the conversion efficiency align close to a characteristic curve.

36 MATERIALS SCIENCE↗

Optical damage performance of conductive widegap semiconductors: spatial, temporal, and lifetime modeling

The optical damage performance of electrically conductive gallium nitride (GaN) and indium tin oxide (ITO) films is addressed using large area, high power laser beam exposures at 1064 nm sub-bandgap wavelength. Analysis of the laser damage process assumes that onset of damage (threshold) is determined by the absorption and heating of a nanoscale region of a characteristic size reaching a critical temperature. We use this model to rationalize semi-quantitatively the pulse width scaling of the damage threshold from picosecond to nanosecond timescales, along with the pulse width dependence of the damage threshold probability derived by fitting large beam damage density data. Multi-shot exposures were used to address lifetime performance degradation described by an empirical expression based on the single exposure damage model. A damage threshold degradation of at least 50% was observed for both materials. Overall, the GaN films tested had 5-10 × higher optical damage thresholds than the ITO films tested for comparable transmission and electrical conductivity. This route to optically robust, large aperture transparent electrodes and power optoelectronics may thus involve use of next generation widegap semiconductors such as GaN.

36 MATERIALS SCIENCE↗

Precision Laser Annealing of Focal Plane Arrays

We present results from laser annealing experiments in Si using a passively Q-switched Nd:YAG microlaser. Exposure with laser at fluence values above the damage threshold of commercially available photodiodes results in electrical damage (as measured by an increase in photodiode dark current). We show that increasing the laser fluence to values in excess of the damage threshold can result in annealing of a damage site and a reduction in detector dark current by as much as 100x in some cases. A still further increase in fluence results in irreparable damage. Thus we demonstrate the presence of a laser annealing window over which performance of damaged detectors can be at least partially reconstituted. Moreover dark current reduction is observed over the entire operating range of the diode indicating that device performance has been improved for all values of reverse bias voltage. Additionally, we will present results of laser annealing in Si waveguides. By exposing a small (<10 um) length of a Si waveguide to an annealing laser pulse, the longitudinal phase of light acquired in propagating through the waveguide can be modified with high precision, <15 milliradian per laser pulse. Phase tuning by 180 degrees is exhibited with multiple exposures to one arm of a Mach-Zehnder interferometer at fluence values below the morphological damage threshold of an etched Si waveguide. No reduction in optical transmission at 1550 nm was found after 220 annealing laser shots. Modeling results for laser annealing in Si are also presented.

42 ENGINEERING↗

Impact damage in small diameter graphite/epoxy composite struts

An investigation was performed to study impact induced damage in small-diameter struts made of a composite material with a brittle matrix system. The major focus is on characterizing the impact behavior associated with the barely visible damage. An experimental procedure including ultrasonic inspection, instrumented impact testing, and delamination buckling and residual strength measurements is presented. From the ultrasonic inspection, it is found that for the strut specimens under investigation, the impact energy level for barely visible damage threshold is above that of the internal damage threshold. A 60- to 65-percent reduction in compressive strength was typical for struts subjected to the barely visible impact damage threshold.

Chen, G.-S.↗

The impact of contamination and aging effects on the long-term laser-damage resistance of SiO 2 /HfO 2 /TiO 2 high-reflection coatings for 1054nm

The laser damage thresholds of optical coatings can degrade over time due to a variety of factors, including contamination and aging. Optical coatings deposited using electron beam evaporation are particularly susceptible to degradation due to their porous structure. In a previous study, the laser damage thresholds of optical coatings were reduced by roughly a factor of two from 2013 to 2017. The coatings in question were high reflectors for 1054 nm that contained SiO 2 and HfO 2 and/or TiO 2 layers, and they were stored in sealed PETG containers in a class 100 cleanroom with temperature control. At the time, it was not certain whether contamination or thin film aging effects were responsible for the reduced laser damage thresholds. Therefore, to better understand the role of contamination, the coatings were recleaned and the laser damage thresholds were measured again in 2018. Here, the results indicate that contamination played the most dominant role in reducing the laser damage thresholds of these optical coatings, even though they were stored in an environment that was presumed to be clean.

42 ENGINEERING↗

Thermal annealing of laser damage precursors on fused silica surfaces

Previous studies have identified two significant precursors of laser damage on fused silica surfaces at fluences <35 J/cm2: photoactive impurities from polishing and surface fractures. We evaluate isothermal heating as a means of remediating the defect structure associated with surface fractures. Vickers indentations are applied to silica surfaces at loads between 0.5 and 10 N, creating fracture networks. The indentations are characterized before and following thermal annealing under various time and temperature conditions using confocal time-resolved photo-luminescence (CTP) imaging, and R/1 damage testing with 3-ns, 355-nm laser pulses. Improvements in the damage thresholds with reductions in CTP intensity are observed at temperatures well below the glass transition temperature (Tg). The damage threshold on 0.5-N indentations improves from <8 to >35 J/cm2 after annealing at approximately 750°C. Larger fracture networks require longer or higher temperature treatment to achieve similar results. At an annealing temperature >1100°C, optical microscopy indicates morphological changes in some of the fractures surrounding the indentations, although remnants of the original fractures are still observed. In conclusion, we demonstrate the potential of using isothermal annealing to improve the laser damage resistance of silica optics, and provide a means of further understanding the physics of optical damage and mitigation.

36 MATERIALS SCIENCE↗

Analysis of the chromaticity of near-field binary beam shapers

The chromatic properties of binary beam shapers inducing a spatially dependent transmission on the near field of an optical source after far-field filtering and imaging are derived. Beam shapers using pixels with two transmission states are highly versatile and have been experimentally realized with distributions of amplitude pixels, phase pixels, or polarization pixels that can be designed using a half-toning algorithm. The amplitude of the shaped beam in an image plane has a precisely controlled continuous profile given by the local density of the two pixel types in the object plane. The wavelength dependence of the field transmission corresponding to the full range of design transmission between 0 and 1 is studied analytically to assess the general performance of the orresponding beam shapers for broadband sources, with an example of a specific 2D transmission profile relevant to laser engineering. Amplitude beam shapers have no significant chromaticity, but have low damage threshold. The high-damage-threshold twisted nematic liquid crystal and phase shapers induce a wavelength-dependent transmission and phase on the shaped beam.

42 ENGINEERING↗

Wide bandgap photoconductor (SiC:V)-based optically addressed light valve for high fluence operation

Optically addressable light valves based on wide bandgap 4H- and 6H-SiC as photoconductors were designed to withstand higher operational laser fluences than the state of-the-art bismuth silicon oxide (BSO; Bi 12 SiO 20 ) based devices. Vanadium-doped SiC was selected as the photoconductors due to their reasonable photoresponsivity while many fold improvement in laser induced damage threshold as compared to BSO. The laser induced damage threshold values of the materials were measured after exposing ~ 200 sites on the samples to increasing levels of fluence of a gaussian pulsed Nd: YAG laser system (1064 nm) with a 5 Hz repetition rate. The measured damage threshold values for BSO, 4H- and 6H-SiC were 0.4 J/cm 2 , 1.75 J/cm 2 and 1.8 J/cm 2 , respectively. Photoconductive switches based on 4H and 6H-SiC samples were characterized at wavelengths of 380 nm, 405 nm, and 447 nm. The peak photoresponsivity values of the 4H- and 6H-SiC materials were measured to be under 380 nm and 405 nm, respectively. The photoconductor was bonded to a BK7 optical window with 5 μm diameter microspheres as spacers. A twisted nematic type E7 liquid crystal (LC) was filled in the 5 μm gap in a vacuum chamber. The desired alignment of the liquid crystal was achieved by mutually orthogonal orientation of LC alignment layers on the two mating faces (SiC and BK7). The fabricated devices were modulated using address beams of wavelengths 380 nm, 405 nm, and 447 nm. In conclusion, required transmission levels of > 90% was achieved for the fabricated OALVs for a sinusoidal voltage waveform that meets the lifetime requirement of the device.

36 MATERIALS SCIENCE↗