Search NASA⌕ Search

SEARCH · Search NASA

Results for “dislocation loops”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Defect formation and transmutation behaviors in irradiated tungsten under thermal-neutron shielded and mixed spectrum conditions

Here, this study investigates the microstructural evolution of pure tungsten irradiated under thermal-neutron shielded and mixed spectrum conditions in the High Flux Isotope Reactor (HFIR). Four samples were irradiated at temperatures from 570 °C to 1130 °C up to 0.73 dpa. Neutron spectrum significantly influenced the accumulation of transmutation products, with Re+Os content estimated at ∼0.3–0.6% under thermal-neutron shielded conditions and ∼5.2% under the mixed spectrum condition. Irradiation temperature strongly influences tungsten’s microstructure, with dislocation loops and fine voids forming at lower temperatures and only larger voids and Re/Os segregation observed at higher temperature. Under thermal-neutron shielded conditions, dislocation loops and voids were observed at 570 °C and 790 °C. At the highest irradiation temperature (1130 °C), dislocation loops were no longer observed, while larger but less dense voids remained. Re and Os segregation to void surfaces was evident at 790 °C and 1130 °C, though no precipitation was observed. In contrast, under the mixed-spectrum condition, both spherical and needle-like Re/Os-rich precipitates were observed, frequently accompanied by large voids. Dislocation loops were not observed, but loop-like contrast within the precipitates suggests they may have nucleated on pre-existing loops. Irradiation-induced hardening was assessed for the shielded samples at 570 °C and 790 °C. Dispersed barrier hardening (DBH) analysis, based on TEM-resolved defects, revealed that voids were the dominant contributors to hardening, consistent with literature results. A schematic model is proposed to describe defect and precipitate evolution in tungsten under fusion-relevant transmutation-to-dpa conditions.

Dislocation loops↗

Helium bubble formation in nickel under in-situ krypton and helium ions dual-beam irradiation

Helium has profound effects on the microstructure and mechanical property of materials used in nuclear power systems. Here to understand the interaction between helium and irradiation-induced defects and its effect on bubble formation, single-beam and dual-beam irradiations on nickel were performed with 16 keV helium ions and 1 MeV krypton ions under in-situ TEM observation. For 1 MeV krypton single-beam irradiation, voids were observed at 600ºC but not at 500ºC and 700ºC. For helium single-beam irradiation at 500ºC, helium moved freely and formed bubble-loop complexes. For dual-beam irradiation at 500ºC, helium was trapped by vacancies and formed bubbles homogeneously. The structure of dislocation loops was also affected by the presence of helium. For krypton single-beam irradiation at 500ºC, the microstructure was {100} periodic wall of faulted and perfect dislocation loops. For dual-beam irradiation at 500ºC, periodic wall was not observed, and dislocation loops were predominantly perfect. For single-beam helium at 500ºC, dislocation loops were produced by athermal process of SIAs ejection or loop punching mechanisms. The interplay between helium and vacancies played an important role on the evolution of helium bubbles and defect microstructures.

36 MATERIALS SCIENCE↗

Radiation response of a Fe–20Cr–25Ni austenitic stainless steel under Fe 2+ irradiation at 500 °C

The radiation response of a Fe–20Cr–25Ni austenitic stainless steel under self-ion irradiation at 500 °C was systematically investigated. The steel was irradiated at 500 °C by 3.5 MeV Fe 2+ ions to 10, 50, and 150 peak dpa, respectively. In the 200–400 nm depth region, radiation-induced Frank loops were relatively stable in both size and number density from 10 to 150 peak dpa. Anisotropic distribution of Frank loops was observed in the 50 and 150 peak dpa specimens, possibly due to interaction of Frank loops and network dislocations with preferred orientations. Coarse voids were found only in the 50 and 150 peak dpa specimens in depths less than 750 nm, suggesting that injected interstitials at deeper regions suppressed the void nucleation. The peak swelling was very low (~0.4%) for both 50 and 150 peak dpa irradiation. Radiation also led to the formation of intragranular plate-like Cr-rich carbides. Radiation-induced segregation of Ni and Si was found at various sinks: dislocation loops, void surfaces, and carbide-matrix interfaces. Finally, irradiation hardening was measured by nanoindentation and the results are consistent with microstructure-based calculations using the dispersed barrier hardening model. The major contributor to irradiation hardening changed from Frank loops at the lowest dose to network dislocations at the highest dose.

dislocation loops↗

Shock response of He bubbles in single crystal Cu

With large-scale molecular dynamics simulations, we investigate shock response of He nanobubbles in single crystal Cu. For sufficient bubble size or internal pressure, a prismatic dislocation loop may form around a bubble in unshocked Cu. The internal He pressure helps to stabilize the bubble against plastic deformation. However, the prismatic dislocation loops may partially heal but facilitate nucleation of new shear and prismatic dislocation loops. For strong shocks, the internal pressure also impedes internal jetting, while a bubble assists local melting; a high speed jet breaks a He bubble into pieces dispersed among Cu. Near-surface He bubbles may burst and form high velocity ejecta containing atoms and small fragments, while the ejecta velocities do not follow the three-dimensional Maxwell-Boltzmann distributions expected for thermal equilibrium. The biggest fragment size deceases with increasing shock strength. With a decrease in ligament thickness or an increase in He bubble size, the critical shock strength required for bubble bursting decreases, while the velocity range, space extension and average velocity component along the shock direction, increase. Small bubbles are more efficient in mass ejecting. Compared to voids and perfect single crystal Cu, He bubbles have pronounced effects on shock response including bubble/void collapse, Hugoniot elastic limit (HEL), deformation mechanisms, and surface jetting. HEL is the highest for perfect single crystal Cu with the same orientations, followed by He bubbles without pre-existing prismatic dislocation loops, and then voids. Complete void collapse and shear dislocations occur for embedded voids, as opposed to partial collapse, and shear and possibly prismatic dislocations for He bubbles. He bubbles lower the threshhold shock strength for ejecta formation, and increase ejecta velocity and ejected mass.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Insights into Prismatic Loop Formation in Irradiated Fe–Cr Alloys from Hypothesis-Driven Active Learning and Causal Analysis

Neutron and electron irradiation experimental studies conducted on body-centered cubic Fe and Fe–Cr alloys have established two prismatic dislocation loop populations, which have Burgers vectors of either a/2$\langle$111$\rangle$ or a$\langle$100$\rangle$. Here, the loop formation depends on factors such as dose (D), dose rate (D rt ), temperature (T), chromium content (Cr%), and other alloying elements. Hence, it is important to understand how irradiation-induced dislocation loops evolve conditional upon the loop characteristics, such as loop density (DD), average loop size d̅, and irradiation parameters (D, D rt , T, and irradiation type), which is still an active area of research. To understand these complex structure–property relationships, machine learning (ML) is employed in a three-step approach. This includes imputing missing data with a k-nearest neighbor, generating functionalized features, and assessing feature importance with random forest classification and regression. Physics-based features are incorporated in a hypothesis-driven active learning scheme to overcome data unavailability challenges. Insights obtained from ML models (i) to categorize dislocation loop types, show the highest correlation with d̅; (ii) Log(DD), obtained through mathematical formulations involving D, Cr%, d̅, and T (e.g., Log(DD) ~ D + exp(-Cr%) + 1/d̅ and log(DD) ~ D + exp(-Cr%) + 1/T). Hypothesis-driven active learning is able to predict Log(DD) in which the experimental date is not known. Causal models verify cause–effect relationships for dislocation loop classification and irradiation factors in FeCr alloys.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Nano-scale microstructure damage by neutron irradiations in a novel Boron-11 enriched TiB 2 ultra-high temperature ceramic

Ultra-high temperature transition-metal ceramics are potential candidates for fusion reactor structural and plasma-facing components. We reveal the irradiation damage microstructural phenomena in Boron-11 enriched titanium diboride (TiB 2 ) using mixed-spectrum neutron irradiations, combined with state-of-art characterization using transmission electron microscopy (TEM) and high resolution TEM. Irradiations were performed using High Flux Isotope Reactor at ~220 and 620 °C up to 2.4 x 10 25 n.m -2 (E > 0.1 MeV). The calculated dose including contribution from residual Boron-10 ( 10 B) transmutation recoils, was ~4.2 displacements per atom. TiB 2 is susceptible to irradiation damage in terms of dislocation loop formation, cavities and anisotropic swelling induced micro-cracking. At both 220 and 620 °C, TEM revealed dislocation loops on basal and prism planes, with nearly two orders of magnitude higher number density of prism-plane loops. HRTEM, electron diffraction and relrod imaging revealed additional defects on {10$ \overline{1}\ $0} planes, identified as faulted prism-plane dislocation loops. High defect cluster density on prism planes will induce a-lattice parameter swelling of TiB 2 , as reported in literature. This anisotropic lattice parameter swelling induced grain boundary micro-cracking, the extent of which decreased with increasing irradiation temperature. The dominance of irradiation defect clusters on prism planes is different than typical hexagonal ceramics where dislocation loops predominantly form on basal planes, causing c-lattice parameter swelling. Helium generation and temperature rise from the transmutation of residual 10 B resulted in matrix and grain boundary cavities for the irradiation at 620 °C. In conclusion, the study additionally signifies isotopic enrichment as a viable approach to produce transition-metal diborides for potential nuclear structural applications.

36 MATERIALS SCIENCE↗

TEM characterization of a simultaneously neutron-irradiated and helium-injected PM2000 ODS alloy

Transmission electron microscopy (TEM) discs of PM2000 were coated on one side with a ~4 µm thick NiAl film and irradiated in HFIR to a neutron displacement damage dose of 21.2 dpa at 500°C. The dpa are primarily produced by fast neutrons, while the in situ He injection (ISHI) to 1230 appm derives from the thermal neutron two-step 59 Ni(n,α) reaction. A uniform He injection profile extends up to about 8 µm below the NiAl coating, hence the remaining material experiences only dpa damage (21.2 dpa at 500°C). This report summarizes analytical TEM analyses to compare the two different regions, i.e., simultaneous He-injection/displacement damage versus displacement damage only, or high and very low He/dpa ratios, respectively. TEM analyses of the He implanted region reveals a high density of small (<2 nm) He bubbles predominantly associated with dislocation loops in the matrix. Because of a very large grain size, no grain or subgrain boundaries were observed in the samples prepared by focused ion beam (FIB) micromachining. The only voids formed were associated with large ODS particles, all of which were amorphous, irrespective of particle size and level of He. The ODS particles range in size from 15-30 nm, and most particles have a single faceted void attached to it that ranges in size from 5 to 15 nm. On the non-implanted side of the sample, no He bubbles could be detected, and faceted voids were found on ~10% of the ODS particles. The He-implanted side contains both <100>{100} and ½<111>{111} dislocation loops and a low density of line dislocations, whereas the un-implanted side possesses predominantly line dislocations with a lower density of dislocation loops. In both regions, nanoscale fcc precipitates exhibiting a cube-on-cube orientation relationship with the bcc matrix were observed. Chemical analysis using energy dispersive x-ray spectroscopy (EDS) indicates this phase is rich in Al and Ti. It was also noted that substantial Cr segregation occurs around the dislocation loops, concurrent with Fe depletion. The clusters of fcc precipitates that do not appear to be associated with the existing loops or line dislocations. The amorphous Y-Al-O particles contain a high Al concentration (>20 at%) and Cr segregation/Fe-depletion at the periphery.

Jung, Hee Joon↗

Neutron irradiation-induced microstructure damage in ultra-high temperature ceramic TiC

Titanium carbide (TiC) is an ultra-high temperature ceramic with potential as a structural material candidate for advanced reactor concepts. However, the irradiation tolerance of TiC is not well understood. Here, we reveal the key irradiation damage microstructure degradation processes in TiC using mixed spectrum neutron irradiations at dose of ~2 displacements per atom (dpa) at temperatures of ~220, 620, and 1115 °C, combined with state-of-art microstructure characterization using transmission electron microscopy (TEM) and high-resolution TEM (HRTEM). The helium injection (~65 atomic parts per million) produced by neutron transmutation also occurred in the sample. TiC was observed to form irradiation-induced interstitial-type dislocation loops and He-stabilized cavities. At 220 and 620 °C, the analysis of the electron diffraction patterns, rel-rod imaging and HRTEM revealed that the dislocation loops were faulted Frank loops with Burgers vector b Frank = 1/3<111> lying on {111} planes. A detailed Burgers vector identification performed by the g.b technique revealed that the dislocation loops forming at 1115 °C were unfaulted, edge-type, with Burgers vectors b = a<100> and a/2<110> with corresponding {100} and {110} habit planes. Using continuum mechanics, we estimated the critical radius at which a faulted dislocation loop transitions to a perfect loop to be 9 nm. Further, no amorphization occurred in TiC under-investigated irradiation conditions while macroscopic swelling under point defect swelling regime was observed. He-stabilized cavities were detected at 1115 °C, but not at lower temperature irradiation. These observations indicate the onset of long-range vacancy migration in TiC occurs between 620 and 1115 °C.

36 MATERIALS SCIENCE↗

Formation of large loop-hydrogen complexes and related effects on mechanical properties of Zirconium investigated with molecular dynamics method

Here, using molecular dynamics (MD) method, interaction between hydrogen (H) atoms and interstitial or vacancy dislocation loops in Zr is extensively studied. The results show that the binding of hydrogen atoms to dislocation loops is anisotropic (attractive or repulsive), depending on the position of the hydrogen atoms with respect to the loop’s core. The anisotropy is governed by excess volume and stress field induced by the loop. For a 1/3[$2\bar1$$\bar1$$0$] interstitial dislocation loop, hydrogen atoms preferentially segregate near the outside of the loop and close to the decomposition knots of the loop. While for a 1/3[$2\bar1$$\bar1$$0$] or 1/6[$20$$\bar2$$3$] vacancy loop, hydrogen atoms prefer to segregate near the inside of the loop. The present work indicates large loop-hydrogen complexes could form in Zr. The binding of hydrogen to loops is stable up to 600 K, while dissociation is observed at 900 K. Formation of loop-hydrogen complexes affect the activation of slip system, resulting in higher yield stress of Zr. The effect increases with the increasing ratio of H to vacancies or interstitials in the vacancy or interstitial loops. The results imply the effects of large loop-hydrogen complexes should be considered to fully understand radiation damage in Zr.

36 MATERIALS SCIENCE↗

In-situ TEM observation of dislocation evolution in Kr-irradiated UO2 single crystal

In-situ transmission electron microscopy (TEM) observation of UO2 single crystal irradiated with Kr ions at high temperatures was conducted to understand the dislocation evolution due to high-energy radiation. The dislocation evolution in UO2 single crystal is shown to occur as nucleation and growth of dislocation loops at low-irradiation doses, followed by transformation to extended dislocation segments and networks at high doses, as well as shrinkage and annihilation of some loops and dislocations due to high temperature annealing. Generally the trends of dislocation evolution in UO2 are similar under Kr irradiation at different ion energies and temperatures (150 keV at 600 degrees C and 1 MeV at 800 degrees C) used in this work, although the specific dislocation loop size and density are quite different. Interstitial-type dislocation loops with Burgers vector along <110> were observed in the Kr-irradiated UO2.The irradiated specimens were denuded of dislocation loops near the surface.

36 MATERIALS SCIENCE↗

Radiation resistance of oxide dispersion strengthened alloys: Perspectives from in situ observations and rate theory calculations

Here, in situ ion irradiation and rate theory calculations were employed to directly compare the radiation resistance of an oxide dispersion strengthened alloy with that of a conventional ferritic/martensitic alloy. Compared to the rapid buildup of dislocation loops, loop growth, and formation of network dislocations in the conventional ferritic/martensitic alloy, the superior radiation resistance of the oxide dispersion strengthened alloy is manifested by its stable dislocation structure under the same irradiation conditions. Thus, the results are consistent with rate theory calculations, which show that high-density nanoparticles can significantly reduce freely migrating defects and suppress the buildup of clustered defects.

36 MATERIALS SCIENCE↗

Effects of neutron irradiation of Ti 3 SiC 2 and Ti 3 AlC 2 in the 121–1085 °C temperature range

Herein we report on the formation of defects in response to neutron irradiation of polycrystalline Ti 3 SiC 2 and Ti 3 AlC 2 samples exposed to doses of 0.14±0.01, 1.6±0.1, and 3.4±0.1 displacements per atom (dpa) at irradiation temperatures of 121±12, 735±6 and 1085±68 °C. After irradiation to 0.14 dpa at 121 °C and 735 °C, black spots are observed in both Ti 3 SiC 2 and Ti 3 AlC 2 . After irradiation to 1.6 and 3.4 dpa at 735 °C, basal dislocation loops, with a Burgers vector of b = ½ [0001] are observed in Ti 3 SiC 2 , with loop diameters of 21±6 and 30±8 nm for 1.6 dpa and 3.4 dpa, respectively. In Ti3AlC2, larger dislocation loops, 75±34 nm in diameter are observed after 3.4 dpa at 735 °C, in addition to stacking faults. Impurity particles of TiC, as well as stacking fault TiC platelets in the MAX phases, are seen to form extensive dislocation loops under all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 °C. Remarkably, denuded zones on the order of 1 µm are observed in Ti 3 SiC 2 after irradiation to 3.4 dpa at 735 °C. Small grains, 3-5 µm in diameter, are damage free after irradiation at 1085 °C at this dose. The presence of the A-layer in the MAX phases is seen to provide enhanced irradiation tolerance. Based on these results, and up to 3.41 dpa, Ti 3 SiC 2 remains a promising candidate for high temperature nuclear applications.

36 MATERIALS SCIENCE↗

Dissolution of Mg-enriched defects in implanted GaN and increased p-type dopant activation

Annealing Mg-implanted homoepitaxial GaN at temperatures above 1400 °C eliminates the formation of inversion domains and leads to improved dopant activation efficiency. Extended defects, in the form of inversion domains, contain electrically inactive Mg after post-implantation annealing at temperatures as high as 1300 °C (one GPa N 2 overpressure), which results in a low dopant activation efficiency. Triple-axis x-ray data reveal that implant-induced strain is fully relieved after annealing at 1300 °C for 10 min, indicating that strain-inducing point defects formed during implantation have reconfigured and inversion domains are formed. However, annealing at temperatures of 1400–1500 °C (one GPa N 2 overpressure) eliminates the presence of the inversion domains. While residual defects, such as dislocation loops, still exist after annealing at and above 1400 °C, chemical analysis at multiple dislocation loops shows no sign of Mg segregation. Meanwhile, an overall decreasing trend in the dislocation loop density is observed after annealing at the higher temperatures and longer times. Additionally, once inversion domains are formed and the samples are cooled to room temperature, they are shown to dissolve with subsequent annealing above 1400 °C. While such defects have been observed before, the important finding that such defects can be dissolved with a short, higher temperature step is key. Earlier work [Breckenridge et al., J. Appl. Phys. Lett. 118, 022101 (2021)] addressing electrical measurements of these types of samples showed that annealing at 1400 °C leads to a dopant activation efficiency that is an order of magnitude higher than that observed at 1300 °C. In conclusion, this work complements earlier work by identifying the inversion domains, which incorporate Mg, and points to the benefits, in terms of defect density and p-type dopant activation, of using higher temperature (>1400 °C) annealing cycles to activate Mg in GaN, even if the Mg-containing inversion domains had been formed during lower temperature annealing.

36 MATERIALS SCIENCE↗

THERMAL ANNEALING OF IRRADIATED PREHYDRIDED ZIRCALOY-4 MATERIALS

Hydrogen-assisted irradiation growth is an important issue for reliability and performance of nuclear materials in nuclear fuel cladding and fuel assembly components. The mechanisms of irradiation growth are not entirely clear and the role of hydrogen and hydrides are less so. There is evidence that breakaway irradiation growth is strongly influenced by the formation and dynamics of dislocation loops that vary with alloy composition, heat treatment and hydrogen content. Thermal annealing of eight Zircaloy-4 specimens irradiated in the Advanced Test Reactor (ATR) at the Idaho National Laboratory as part of the joint EPRI Nuclear Fuels Industry Research (NFIR) and Fuel Reliability Program (FRP) AsTeR irradiation growth study were performed by hot-stage transmission electron microscopy (TEM), differential scanning calorimetry (DSC), and dilatometry via NSUF RTE 17-1093. Two fluence levels (6.7 and 12.3 dpa) and three hydrogen contents (~10, 40, 120 ppm) were investigated. TEM with a hot stage was used for the quantification of "a" and "c" dislocation loop population densities and size distributions at a range of temperatures from 25 to 800oC. DSC and dilatometry were performed by dynamically heating and cooling from 30 to 750ºC at rates of 5, 10, and 20 oC/min to determine the behavior of dislocation loop annealing. Dynamic temperature DSC tests were able to detect the temperature ranges and enthalpies of "a" and "c" loop annihilation, hydride dissolution and precipitation, secondary particle precipitation, and a?a + ß phase transformations upon heating and cooling. Dilatometry tests showed that all of the test showed initial linear expansion followed by a decrease in expansion rate from about 400 to 600 ºC associated with annihilation of "a" and "c" loops and showed evidence for the thermal stabilizing effect of hydrogen on dislocation loops. The results are discussed in the context of the larger AsTeR program that will include higher exposure (~20 dpa) and different alloys when they become available in 2021.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of cold-worked 316 stainless steel flux thimble tubes irradiated up to 100 dpa in a commercial Pressurized Water Reactor

Two flux thimble tubes (FTT) made of 15% cold-worked 316 stainless steel (SS) were harvested from Ringhals Pressurized Water Reactor (PWR) Unit 2, with peak damages of 76 and 100 displacements per atom (dpa) after 29 and 34 years’ service, respectively. Specimens sectioned from parent tubes were comprehensively characterized with nominal damage levels of ~0, ~41, ~74, 76, and 100 dpa at a nominal temperature range of 285-323 °C. Both FTTs contained helium and hydrogen gases as transmutation products. The helium follows a production rate of ~9.8 appm/dpa, while environmental factors complicate hydrogen production obscuring an exact H/dpa ratio. Irradiation-induced dislocation loops, nano-cavities, solute clusters, and microsegregation were all observed. The dislocation loops and nano-cavities indicated saturation at 41 dpa. The solute clusters continued to evolve with Ni-Si clusters formed at 41 dpa, and Ni-Si-Mn-P clusters formed at 74 and 100 dpa, but neither clusters exhibited distinct diffraction patterns at any damage levels. Solute clusters were observed to frequently be co-located with dislocation loops, but fully decorated loops were rarely detected. Significant radiation-induced segregation (RIS) was observed around grain boundaries at all damage levels. The modified inverse Kirkendall (MIK) model captured the RIS behavior of major elements. Large cavities within or around an Mn-S rich region were observed for the first time. Through all the damage levels, void swelling is always below 0.05%, making significant dimensional change unlikely in core internals when used at similar conditions. Meanwhile, the role of overwhelming nanocavities, presumably helium bubbles, should be considered in other potential degradation mechanisms, including irradiation-assisted stress corrosion cracking, embrittlement, and loss of fracture toughness, which remain the concerns for extended operation of nuclear power plants.

Post Irradiation Examination, Isotope Dilution Mas↗

Irradiated Microstructure of Zorita Materials

Reactor baffle plate materials were harvested from the decommissioned Zorita nuclear power reactor after 38 years of service and were characterized with transmission electron microscope. The samples were Type 304 stainless steels and had been irradiated to 0.05, 16.9, ad 48.6 dpa. Faulted dislocation loops, voids, and irradiation-induced precipitates were observed in this material. While dislocation loops were the dominant irradiation defects for all samples, small voids and precipitates were also observed at 16.9 and 48.6 dpa, but not at 0.05 dpa. The size of dislocation loops increased with irradiation dose and saturated below 16.9 dpa. The loop density continued to increase between 16.9 and 48.6 dpa. For voids, both the density and mean size were small, and the volume swelling was negligibly small even at 48.6 dpa. In addition, carbides or G-phase precipitates were detected at 16.9 and 48.6 dpa, and a complex dose dependence was observed. A range of irradiation hardening was estimated at each dose, and the resulting yield strengths were consistent with the previous tensile results measured from the Halden and BOR-60 specimens.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Scanning Transmission Electron Microscopy–Atom Probe Tomography Correlative Analysis for the Characterization of Solute-defect Interactions

Atom probe tomography (APT) and (scanning) transmission electron microscopy ((S)TEM) are complementary techniques that provide spatially resolved chemical and structural information at the atomic scale. Here, in this study, we employ two different STEM/APT correlative analysis methods to investigate Cr segregation at dislocation loops in ultra-high purity Fe–Cr alloys. APT needles for the correlative analysis were extracted either from bulk material or from thinned TEM lamellae. STEM analysis was used to determine the Burgers vectors of ion-irradiation-induced dislocation loops, while APT reconstruction of the same region revealed the Cr segregation to these loops. We extended the g•b = 0 invisibility criterion of dislocation loops from TEM mode in a lamella to STEM mode in a needle-shaped specimen. STEM and APT analysis on the same needle provide straightforward correlative analysis, although it is limited by a small observation volume. In contrast, iterative STEM analysis of TEM lamellae, followed by the selective extraction of specific regions of interest for APT analysis, expands the observation area by up to 100 times but requires additional time-consuming steps for APT needle extraction from the lamellae.

47 OTHER INSTRUMENTATION↗