Investigation of dominant spin wave modes by domain walls collision

Spin wave emission due to field-driven domain wall (DW) collision has been investigated numerically and analytically in permalloy nanowires. The spin wave modes generated are diagonally symmetric with respect to the collision point. The non-propagating mode has the highest amplitude along the middle of the width. The frequency of this mode is strongly correlated to the nanowire geometrical dimensions and is independent of the strength of applied field within the range of 0.1 mT to 1 mT. For nanowire with film thickness below 5 nm, a second spin wave harmonic mode is observed. The decay coefficient of the spin wave power suggests that the DWs in a memory device should be at least 300 nm apart for them to be free of interference from the spin waves.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Imaging of magnetic DW injection processed in patterened Ni80Fe20 structures

Magnetization reversal in patterned ferromagnetic nanowires usually occurs via domain wall (DW) nucleation and propagation from one end (or both ends) of the wire which can be significantly reduced by a large, magnetically soft pad on one of the wire ends. These 'nucleation pads' reverse at lower fields than an isolated nanowire and introduce a DW to the wire from the wire end attached to the pad. Once a critical 'injection' field is reached, the DW sweeps through the wire, reversing its magnetization. Nucleation pads are frequently used as part of nanowire devices and experimental structures. Magnetic-field-driven shift register memory can include an injection pad to write data while those attached to nanowire spiral turn sensors act as both a source and sink of domain walls. Both of these devices use two-dimensional wire circuits and therefore require the use of orthogonal in-plane magnetic fields to drive domain walls through wires of different orientations. These bi-axial fields can significantly alter the fields at which DW injection occurs and control the number of different injection modes. We have used magnetic transmission soft X-ray microscopy (M-TXM) [6] providing 25nm spatial resolution to image the evolution of magnetization configurations in patterned 24nm thick Ni{sub 80}Fe{sub 20} rectangular nucleation pads and attached wires during DW injection. The structures consisted of 2 {micro}m x 3 {micro}m nucleation pads with wires of width 200 nm, 300 nm or 500 nm attached Comparing the magnetic configuration of the injection pads with micromagnetic models, we find that the relative orientation of closure domains in the remanent magnetization configuration of injection pads determines the reversal pathway that follows, although this is further affected by applied transverse fields. Micromagnetic simulations were performed using a hybrid finite element/boundary element code. The magnetic elements were designed with 20 nm thickness and discretized into a mesh of tetrahedral elements with a maximum cell size of 20 nm. Material properties for bulk permalloy were used, i.e. exchange stiffness A = 1.3 x 10{sup -11} J/m, saturation magnetization M{sub S} = 800 kA/m, magneto-crystalline anisotropy K = 0 Jm{sup -3}, damping constant a = 0.01. A linearly increasing magnetic field (1 Oe/ns) was applied parallel to the wire long axis to simulate switching fields. The dimensions of the simulated structures mimicked the essential features of the experimental structures, although edge roughness was neglected from the model. The remanent magnetization state of the pad with no transverse field consists of a uniform magnetization aligned with the wire axis, with closure domains at the edges facing and joining the wire. When H{sub y} = 0 Oe and H{sub x} = 20 Oe, the magnetization state of the pad buckles, forming eight domains, half of which have magnetizations rotated away from the x-axis. As H{sub x} is increased, the rotation of the domains become larger and the non-rotated domains shrink A transverse field applied in addition to the axial field exhibits a more complex modes of magnetization reversal in the pad (Fig. 1). We understand the pathway of pad magnetization more generally by using micromagnetic simulations. Two initial configurations are shown in Fig. 2 with the closure domain on the left-hand edge of the pad either parallel or anti-parallel to both closure domains on the righthand edges of the pad. As H{sub x} is increased to inject a domain wall, the pad magnetization states changed to vortex states, as observed by M-TXM. At higher fields, the magnetization of the modeled pad became single-domain, although closure domains remained at fields up to H{sub x} = 90 Oe. This supports the suggestion that experimentally observed multi-modal injection is due to the magnetization state of the pad. In summary, the relative orientation of closure domains in the pads determines the magnetization reversal pathway under an axial field. However, the addition of transverse fields can alter these and lead to the pads undergoing reversal under lower axial fields. Our observations have wider implications for experiments and devices using patterned magnetic wires.

36 MATERIALS SCIENCE↗

Hard x-ray phase contrast imaging of black lipid membranes

We report hard x-ray phase contrast imaging of black lipid membranes, freely suspended over a micromachined aperture in an aqueous solution. Biomolecular and organic substances can thus be probed in hydrated environments by parallel beam propagation imaging, using coherent multi-kilo-electronvolt x-ray radiation. The width of the thinning film can be resolved from analysis of the intensity fringes in the Fresnel diffraction regime down to about 200 nm. The thinning process, in which solvent is expelled from the space in between two opposing monolayers, is monitored, and the domain walls between coexisting domains of swollen and thinned membrane patches are characterized.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Ferroelastic twin structures in epitaxial WO{sub 3} thin films

Tungsten trioxide is a binary oxide that has potential applications in electrochromic windows, gas sensors, photo-catalysts, and superconductivity. Here, we analyze the crystal structure of atomically flat epitaxial layers on YAlO{sub 3} single crystal substrates and perform nanoscale investigations of the ferroelastic twins revealing a hierarchical structure at multiple length scales. We have found that the finest stripe ferroelastic twin walls along pseudocubic 〈100〉 axes are associated with cooperative mosaic rotations of the monoclinic films and the larger stripe domains along pseudocubic 〈110〉 axes are created to reduce the misfit strain through a commensurate matching of an effective in-plane lattice parameter between film and substrate. The typical widths of the two fine and larger stripe domains increase with film thickness following a power law with scaling exponents of ∼0.6 and ∼0.4, respectively. We have also found that the twin structure can be readily influenced by illumination with an electron beam or a tip-based mechanical compression.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Electron microscopy and computational studies of Ebh, a giant cell-wall-associated protein from Staphylococcus aureus

Ebh, a giant protein found in staphylococci, contains several domains, including a large central region with 52 imperfect repeats of a domain composed of 126 amino acids. We used electron microscopy to observe the rod-like structure of a partial Ebh protein containing 10 repeating units. This is the first report of the direct observation of an Ebh structure containing a large number of repeating units, although structures containing one, two, or four repeating units have been reported. The observed structure of the partial Ebh protein was distorted and had a length of ca. 520 A and a width of ca. 21 A. The observed structures were consistent with those deduced from crystal structure analysis, suggesting that the Ebh domains are connected to form a rod-like structure. The crystal structure data revealed distorted, string-like features in the simulated structure of the whole-length Ebh protein. Superposition of fragments of the simulated whole-length structure of the Ebh protein onto each electron micrograph showed a high level of correlation between the observed and calculated structures. These results suggest that Ebh is composed of highly flexible filate molecules. The highly repetitive structure and the associated unique structural flexibility of Ebh support the proposed function of this protein, i.e. binding to sugars in the cell wall. This binding might result in intra-cell-wall cross-linking that contributes to the rigidity of bacterial cells.

60 APPLIED LIFE SCIENCES↗

Magnetic domain wall contrast under zero domain contrast conditions in spin polarized low energy electron microscopy

Critical applications of spin polarized low energy electron microscopy (SPLEEM) employ this technique's vector imaging capability to resolve domain wall (DW) spin textures. Studying several thin film systems including Co/W(110), Co/Cu(001) and (Co/Ni) n /W(110), we demonstrate that an additional contrast can appear at magnetic DWs. By imaging the magnetization as a function of electron landing energy, electron energies are selected at which the magnetic domain contrast vanishes. Surprisingly, under such conditions of zero contrast between magnetic domains, we observe the appearance of magnetic contrast outlining the DWs. This DW contrast fails to depend on the DW spin texture. Instead, our measurements show that this DW contrast results from a combination of the energy-dependence of the spin reflectivity asymmetry of the magnetic film, the finite energy width of the spin polarized electron source, and the dispersion of the magnetic prism array that separates the illumination and imaging columns of the instrument. Awareness of this DW contrast mechanism is useful to aid correct interpretation of SPLEEM images.

74 ATOMIC AND MOLECULAR PHYSICS↗

Combined effects of vertical and lateral confinement on the magnetic properties of MnAs micro and nano-ribbons

The micromagnetic domain structure of MnAs films gave place to an intense research activity in the last few years due to its potential application in magneto-electronic devices such as domain-wall track memories and logic circuits. These applications require a full knowledge of miniaturization effects on the magnetic properties of the material. In this work, X-ray photoemission electron microscopy has been used for imaging magnetic domains in lithographically fabricated MnAs ribbons, addressing the dependence of the domain configuration on film thickness and ribbon width. Our experiments show a transition from head-on to regular stripe domains below a critical width/thickness ratio w{sub c} ≈ 6. Micromagnetic simulations suggest that this transition is correlated to the magnetic structure of the surface plane. Depending on the ribbon width and thickness, the magnetic configuration is shown to evolve from flux-closure domain structure to a state of almost homogeneous magnetization, observed for narrower ribbons. The evolution of the domain structure, magnetic fraction, and magnetization with temperature has been studied across the ferromagnetic/paramagnetic transition. Our experiments show that the magnetic configuration in ribbons exhibits higher stability to temperature variations than in as-cast films.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Magnetic microstructure and magnetic properties of uniaxial itinerant ferromagnet Fe 3 GeTe 2

Here, magnetic force microscopy was used to observe the magnetic microstructure of Fe 3 GeTe 2 at 4 K on the (001) surface. The surface magnetic structure consists of a two-phase domain branching pattern that is characteristic for highly uniaxial magnets in the plane perpendicular to the magnetic easy axis. The average surface magnetic domain width D s = 1.3 μm determined from this pattern, in combination with intrinsic properties calculated from bulk magnetization data (the saturation magnetization M s = 376 emu/cm 3 and the uniaxial magnetocrystalline anisotropy constant K u = 1.46 × 10 7 erg/cm 3 ), was used to determine the following micromagnetic parameters for Fe 3 GeTe 2 from phenomenological models: the domain wall energy γ w = 4.7 erg/cm 2 , the domain wall thickness δ w = 2.5 nm, the exchange stiffness constant A ex = 0.95 × 10 –7 erg/cm, the exchange length l ex = 2.3 nm, and the critical single domain particle diameter d c = 470 nm.

36 MATERIALS SCIENCE↗

Partnership for Edge Physics Simulation (EPSI)

We propose to develop advanced simulation codes, based upon an extreme parallelism, first principles kinetic approach, to address the challenges associated with the edge region of magnetically confined plasmas. This work is relevant to both existing magnetic fusion facilities and essential for next-generation burning plasma experiments, such as ITER where success is critically dependent upon H-mode operation achieving an edge pedestal of sufficient height for good core plasma performance without producing deleterious large scale edge localized instabilities. The plasma edge presents a well-known set of multi-physics, multi-scale problems involving complex 3D magnetic geometry. Perhaps the greatest computational challenge is the lack of scale separation – temporal scales for drift waves, Alfven waves, ELM dynamics for example have strong overlap. Similar overlap occurs on the spatial scales for the ion poloidal gyro-radius, drift wave and pedestal width. The traditional approach of separating fusion problems into weakly interacting spatial or temporal domains clearly breaks down in the edge. A full kinetic model (full-f model) must be solved to understand and predict the edge physics including non-equilibrium thermodynamic issues arising from the magnetic topology (the open field lines producing a spatially sensitive velocity hole), plasma wall interactions, neutral and atomic physics. The plan here is to model these phenomena within a comprehensive first principles set of equations without the need for the insurmountable multiple-codes coupling issues by building on the XGC1 code developed under the SciDAC Proto-FSP Center for Plasma Edge Simulation (CPES). This proposal includes the critical participants in the XGC1 development. We propose enhancing the capability of XGC1 by including all the important turbulence physics contained in kinetic ion and electron electromagnetic dynamics, by extending the PIC technology to incorporate several positive features found in the Eulerian grid technology, combining the coarse grained XGC0 code into it with a multiscale projective time integration technique to be developed in the project for experimental time scale simulation of the edge multi-physics, and by implementing modern computational technologies to move forward with the extreme scale heterogeneous hardware/software platform development. Ultra-fast edge localized instabilities, involving compressional Alven modes, will be studied using a proper MHD or two-fluid codes employing kinetic closure information from XGC. The proposed research integrates the most important physical processes on overlapping temporal and spatial scales, to study (i) transitions and thresholds for enhanced confinement regimes, (ii) the predictive understanding of the edge pedestal formation, structure and dynamics, (iii) the effect of the edge plasma on the core confinement, (iv) the physics of Edge Localized Modes and their suppression or mitigation via external control techniques, and (v) the heat load on the material wall. Our approach will implement physical models that are valid in their relevant collisionality regimes for current experiments and future burning plasma devices. Comparisons with experimental data will be made at multiple levels including characterization of turbulence dynamics, flux-gradient responses in the energy, particle and momentum channels, and observations of global phenomena such as L-H transitions, momentum generation, ELM dynamics, ELM-free regimes and the tokamak density limit. The proposal team has established strong connections, through joint membership, with other organizations that will be critical for success. These include FASTMath, SUPER and QUEST Institutes respectively for meshing tools and solvers; code performance tuning and uncertainty quantification as well as a proposed Data Management and Visualization Institute.. We will also be teaming with ongoing fusion SciDAC’s: CSWPI for RF-edge plasmas interactions; CEMM for the M3D MHD simulations and with PEPSC for incorporation of energetic particle physics. Finally, the team includes representatives from each of the major U.S. experimental facilities who will coordinate the validation program and the development of synthetic diagnostics.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Declamped Piezoelectric Coefficients in Patterned 70/30 Lead Magnesium Niobate–Lead Titanate Thin Films

Lateral subdivision of blanket piezoelectric thin films increases the functional properties through both increased domain wall mobility and declamping of the intrinsic response. This work presents the local effects of substrate declamping on the piezoelectric coefficient d 33,f of 300 nm thick, rhombohedral, {001}-oriented lead magnesium niobate–lead titanate thin films at the 70/30 composition (70PMN–30PT). Films grown by chemical solution deposition on platinized Si substrates are patterned into strip structures ranging from 0.75 to 9 µm in width. The longitudinal piezoelectric coefficient, d 33,f , is interrogated as a function of position across the patterned structures by three approaches: finite element modeling, piezoresponse force microscopy, and nanoprobe synchrotron X-ray diffraction. It is found that d 33,f increases from the clamped value of 40–50 to ≈160 pm V -1 at the free sidewall under 200 kV cm -1 excitation. The sidewalls partially declamp the piezoelectric response 500–600 nm into the patterned structure, raising the piezoelectric response at the center of features with lateral dimensions less than 1 µm (3:1 width to thickness aspect ratio). The normalized data from all three methods are in excellent agreement, with quantitative differences providing insight to the field dependence of the piezoelectric coefficient and its declamping behavior.

36 MATERIALS SCIENCE↗

On the large eddy simulation of turbulent flows in complex geometry

Application of the method of Large Eddy Simulation (LES) to a turbulent flow consists of three separate steps. First, a filtering operation is performed on the Navier-Stokes equations to remove the small spatial scales. The resulting equations that describe the space time evolution of the 'large eddies' contain the subgrid-scale (sgs) stress tensor that describes the effect of the unresolved small scales on the resolved scales. The second step is the replacement of the sgs stress tensor by some expression involving the large scales - this is the problem of 'subgrid-scale modeling'. The final step is the numerical simulation of the resulting 'closed' equations for the large scale fields on a grid small enough to resolve the smallest of the large eddies, but still much larger than the fine scale structures at the Kolmogorov length. In dividing a turbulent flow field into 'large' and 'small' eddies, one presumes that a cut-off length delta can be sensibly chosen such that all fluctuations on a scale larger than delta are 'large eddies' and the remainder constitute the 'small scale' fluctuations. Typically, delta would be a length scale characterizing the smallest structures of interest in the flow. In an inhomogeneous flow, the 'sensible choice' for delta may vary significantly over the flow domain. For example, in a wall bounded turbulent flow, most statistical averages of interest vary much more rapidly with position near the wall than far away from it. Further, there are dynamically important organized structures near the wall on a scale much smaller than the boundary layer thickness. Therefore, the minimum size of eddies that need to be resolved is smaller near the wall. In general, for the LES of inhomogeneous flows, the width of the filtering kernel delta must be considered to be a function of position. If a filtering operation with a nonuniform filter width is performed on the Navier-Stokes equations, one does not in general get the standard large eddy equations. The complication is caused by the fact that a filtering operation with a nonuniform filter width in general does not commute with the operation of differentiation. This is one of the issues that we have looked at in detail as it is basic to any attempt at applying LES to complex geometry flows. Our principal findings are summarized.

Ghosal, Sandip↗

Evolution of thick domain walls in de Sitter universe

We consider thick domain walls in a de Sitter universe following paper by Basu and Vilenkin. However, we are interested not only in stationary solutions found therein, but also investigate the general case of domain wall evolution with time. When the wall thickness parameter, δ{sub 0}, is smaller than H {sup −1}/√2, where H is the Hubble parameter in de Sitter space-time, then the stationary solutions exist, and initial field configurations tend with time to the stationary ones. However, there are no stationary solutions for δ{sub 0} ≥ H {sup −1}/√2. We have calculated numerically the rate of the wall expansion in this case and have found that the width of the wall grows exponentially fast for δ{sub 0} >> H {sup −1}. An explanation for the critical value δ{sub 0} {sub c} = H {sup −1}/√2 is also proposed.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Charm physics with overlap fermions on 2+1-flavor domain wall fermion configurations*

Decay constants of pseudoscalar mesons D, D s , η c , and vector mesons D*, D$^{*}_{s}$, J/ψ are determined from the N f = 2 + 1 lattice QCD at a lattice spacing a ~ 0.08 fm. For vector mesons, the decay constants defined by tensor currents are given in the $\overline{MS}$ scheme at 2 GeV. The calculation is performed on domain wall fermion configurations generated by the RBC-UKQCD collaborations and the overlap fermion action is used for the valence quarks. Comparing the current results with our previous results at a coarser lattice spacing a ~ 0.11 fm provides a better understanding of the discretization error. We obtain $f$$^{T}_{D^*_s}$($\overline{MS}$, 2 GeV)/f D$^{*}_{s}$ = 0.909(18) with a better precision than our previous result. Combining our f D$^{*}_{s}$ = 277(11) MeV with the total width of D$^{*}_{s}$ determined in a recent study gives a branching fraction 4.26(52) x 10 –5 for D$^{*}_{s}$ leptonic decay.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Magnetic bead detection using domain wall-based nanosensor

We investigate the effect of a single magnetic bead (MB) on the domain wall (DW) pinning/depinning fields of a DW trapped at the corner of an L-shaped magnetic nanodevice. DW propagation across the device is investigated using magnetoresistance measurements. DW pinning/depinning fields are characterized in as-prepared devices and after placement of a 1 μm-sized MB (Dynabeads{sup ®} MyOne{sup ™}) at the corner. The effect of the MB on the DW dynamics is seen as an increase in the depinning field for specific orientations of the device with respect to the external magnetic field. The shift of the depinning field, ΔB{sub dep} = 4.5–27.0 mT, is highly stable and reproducible, being significantly above the stochastic deviation which is about 0.5 mT. The shift in the deppinning field is inversely proportional to the device width and larger for small negative angles between the device and the external magnetic field. Thus, we demonstrate that DW-based devices can be successfully used for detection of single micron size MB.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Multi-region approach to free-boundary three-dimensional tokamak equilibria and resistive wall instabilities

Free-boundary 3D tokamak equilibria and resistive wall instabilities are calculated using a new resistive wall model in the two-fluid M3D-C1 code. In this model, the resistive wall and surrounding vacuum region are included within the computational domain. This implementation contrasts with the method typically used in fluid codes in which the resistive wall is treated as a boundary condition on the computational domain boundary and has the advantage of maintaining purely local coupling of mesh elements. This new capability is used to simulate perturbed, free-boundary non-axisymmetric equilibria; the linear evolution of resistive wall modes; and the linear and nonlinear evolution of axisymmetric vertical displacement events (VDEs). Calculated growth rates for a resistive wall mode with arbitrary wall thickness are shown to agree well with the analytic theory. Equilibrium and VDE calculations are performed in diverted tokamak geometry, at physically realistic values of dissipation, and with resistive walls of finite width. Simulations of a VDE disruption extend into the current-quench phase, in which the plasma becomes limited by the first wall, and strong currents are observed to flow in the wall, in the SOL, and from the plasma to the wall.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Bridging adsorption behavior of confined CH 4 -CO 2 binary mixtures across scales

An accurate understanding of the competitive adsorption of CH 4 -CO 2 binary mixtures in nano-confined systems is critical for engineering CO 2 storage in shale gas reservoirs. Due to difficulties in making reliable experimental observations in nano-scale, atomistic simulations (ASs), such as the Grand Canonical Monte Carlo (GCMC) method, provide a viable approach to studying the adsorption behavior of confined fluids. ASs are, however, limited in the size of the compositional domain due to the high computational cost. This work proposes a framework that combines AS and the lattice Boltzmann (LB) method to bridge the physics of confined fluids across scales. The Peng–Robinson equation of state (PR-EoS) produces fugacity coefficients, which serve as input for conducting multi-component GCMC simulations. These GCMC simulations explore the competitive adsorption behavior of CH 4 -CO 2 in nano-slits at various composition, pressure, and channel-width conditions. Both components generate adsorption layers with high densities near the walls with CO 2 preferentially adsorbing compared to CH 4 on the organic walls of carbon sheets. At the mesoscale, a pseudopotential model represents the intermolecular forces in multi-component, multiple-relaxation-time LB simulations. The LB simulations are in good agreement with the GCMC results, allowing us to obtain values for tunable LB parameters. We then extend the use of LB to simulate adsorption behavior in complex networks with nano-sized channels. The phase behavior and fluid properties in the complex geometries of nano-channels differ from nano-slits and bulk systems. Furthermore, the bridging of physics from GCMC (microscale) to LB (mesoscale) via the macroscale PR-EoS connects the adsorption behavior of binary systems across scales.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In-plane current induced domain wall nucleation and its stochasticity in perpendicular magnetic anisotropy Hall cross structures

Hall cross structures in magnetic nanowires are commonly used for electrical detection of magnetization reversal in which a domain wall (DW) is conventionally nucleated by a local Oersted field. In this letter, we demonstrate DW nucleation in Co/Ni perpendicular magnetic anisotropy nanowire at the magnetic Hall cross junction. The DWs are nucleated by applying an in-plane pulsed current through the nanowire without the need of a local Oersted field. The change in Hall resistance, detected using anomalous Hall effect, is governed by the magnetic volume switched at the Hall junction, which can be tuned by varying the magnitude of the applied current density and pulse width. The nucleated DWs are driven simultaneously under the spin transfer torque effect when the applied current density is above a threshold. The possibility of multiple DW generation and variation in magnetic volume switched makes nucleation process stochastic in nature. The in-plane current induced stochastic nature of DW generation may find applications in random number generation.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗