Effects of Sn addition on precipitation of Al–Zn–Mg alloy at early stage of natural aging

The effect of Sn addition on the natural aging behavior of Al–Zn–Mg alloy was investigated using atom probe tomography (APT) experiments and density functional theory (DFT) calculations. The results demonstrate that Sn retards the natural aging behavior by facilitating the preferential formation of Mg–Sn clusters, which suppress the formation of Guinier-Preston zones (I) during the earliest aging stage. Quantitative solute analysis conducted by APT has suggested increasing amount of Mg–Sn clusters in Sn-contained alloy due to their high binding energy, supported by DFT calculations on the Sn.

36 MATERIALS SCIENCE↗

Early-Stage Shear Viscosity far from Equilibrium via Holography

We report shear viscosity is a crucial property of QCD matter which determines the collective behavior of the the quark-gluon plasma (QGP) in ultrarelativistic heavy-ion collisions. Extending the near-equilibrium, high-precision investigations in theory and experiment, we take into account the fact that, in a collision, the QGP is generated far from equilibrium. We use the AdS/CFT correspondence to study a strongly coupled plasma and find a significant impact on the ratio of shear viscosity to entropy density, η/s. In particular, we investigate the initial heating phase and find a decrease reaching down to below 60% followed by an overshoot to 110% of the near-equilibrium value. This finding might be highly relevant for the extraction of transport coefficients from anisotropic flow measurements at RHIC and LHC.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effect of Salt Concentration on the Interfacial Solvation Structure and Early Stage of Solid–Electrolyte Interphase Formation in Ca(BH 4 ) 2 /THF for Ca Batteries

The Ca 2+ solvation structure at the electrolyte/electrode interface is of central importance to understand electroreduction stability and solid–electrolyte interphase (SEI) formation for the novel multivalent Ca battery systems. Here, using an exemplar electrolyte, the concentration-dependent solvation structure of Ca(BH 4 ) 2 -tetrahydrofuran on a gold model electrode has been investigated with various electrolyte concentrations via electrochemical quartz crystal microbalance with dissipation (EQCM-D) and X-ray photoelectron spectroscopy (XPS). For the first time, in situ EQCM-D results prove that the prevalent species adsorbed at the interface is CaBH 4 + across all concentrations. As the salt concentration increases, the number of BH 4 – anions associated with Ca 2+ increases, and much larger solvated complexes such as CaBH 4 + ·4THF or Ca(BH 4 ) 3 – ·4THF form at the interface at high concentrations prior to Ca plating. Different interfacial chemistries lead to the formation of SEIs with different components demonstrated by XPS. High electrolyte concentrations reduce the solvent decomposition and promote the formation of thick, uniform, and inorganic-rich (i.e., CaO) SEI layers, which contribute to improved Ca plating efficiency and current density in electrochemical measurements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rapid assessment of structural and compositional changes during early stages of zirconium alloy oxidation

A multimodal chemical imaging approach has been developed and applied to detail the dynamic, atomic-scale changes associated with oxidation of a zirconium alloy (Zircaloy-4). Scanning transmission electron microscopy, a gas-phase reactor chamber attached to an atom probe tomography instrument, and synchrotron-based X-ray absorption near-edge spectroscopy were employed to reveal morphology, composition, crystal, and electronic structure changes that occur during initial stages of oxidation at 300 °C. Oxidation was carried out in 10 mbar O 2 gas for short exposure times of 1 and 5 min. A multilayered oxide film with a cubic ZrO adjacent to the oxide/metal interface, a nanoscopic transition region with a graded composition of ZrO 2-x (where 0 < x < 1), and tetragonal ZrO 2 in the outermost oxide were formed. Partitioning of the major alloying element (tin) to the oxide/metal interface and heterogeneously within the oxide accompanied the development of the layered oxide. Our work provides a rapid, high-throughput approach for detailed characterisation of initial stages of zirconium alloy oxidation at an accelerated time scale, with implications for several other alloy systems.

36 MATERIALS SCIENCE↗

Early-stage dynamics of chloride ion–pumping rhodopsin revealed by a femtosecond X-ray laser

Chloride ion–pumping rhodopsin (ClR) in some marine bacteria utilizes light energy to actively transport Cl – into cells. How the ClR initiates the transport is elusive. Here, we show the dynamics of ion transport observed with time-resolved serial femtosecond (fs) crystallography using the Linac Coherent Light Source. X-ray pulses captured structural changes in ClR upon flash illumination with a 550 nm fs-pumping laser. High-resolution structures for five time points (dark to 100 ps after flashing) reveal complex and coordinated dynamics comprising retinal isomerization, water molecule rearrangement, and conformational changes of various residues. Combining data from time-resolved spectroscopy experiments and molecular dynamics simulations, this study reveals that the chloride ion close to the Schiff base undergoes a dissociation–diffusion process upon light-triggered retinal isomerization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Early-Stage Radiation Safety Analysis for the Spallation Neutron Source Second Target Station Bunker Operations

The Second Target Station project at Oak Ridge National Laboratory will develop a cold neutron source to meet growing experimental needs. This paper describes calculations of the residual dose rates associated with the monolith shield plug and the beamline bunker, two key conventional operations and radiation safety features. While neutron production is active, the instrument hall outside the bunker must be generally accessible with dose rates of less than 0.25 mrem/h. When neutron production is halted, the bunker must be accessible for hands-on maintenance operations. Further, these two requirements form the cause for the assessments reported herein of residual dose rates caused by the monolith shield plug and residual dose rates in the bunker. The monolith shield plug was shown to not produce significant dose rates inside the bunker after a 20-year lifetime, and the residual dose rates inside the bunker for the case of an operating beamline were shown to reasonably allow for hands-on maintenance. These calculations are based on preliminary design models of the relevant systems. Additionally, an example showing the significance of considering neutron supermirror physics in transport calculations that track nuclide production and destruction rates to produce gamma sources for residual dose rate calculations is included. The example shows that if neutron supermirror physics is not considered, dose rate fields may be significantly underpredicted.

61 RADIATION PROTECTION AND DOSIMETRY↗