At least 91 records · Page 5

Microhardness and Strain Field Characterization of Self-Reacting Friction Stir and Plug Welds of Dissimilar Aluminum Alloys

Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. Friction plug welding is used to seal the exit hole that remains in a circumferential SR-FSW. This work reports on material properties and strain patterns developed in a SR-FSW with a friction plug weld. Specifically, this study examines the behavior of a SR-FSW formed between an AA 2014-T6 plate on the advancing side and an AA 2219-T87 plate on the retreating side and a SR-FSW (AA 2014-T6 to AA 2219-T87) with a 2219-T87 plug weld. This study presents the results of a characterization of the micro-hardness, joint strength, and strain field characterization of SR-FSW and FPW joints tested at room temperature and cryogenic temperatures.

Horton, Karla Renee↗

Friction-Stir Welding of Aluminum For the Space Program

The Marshall Space Flight Center is developing and characterizing the friction stir welding process for the Space Shuttle and other space programs. This revolutionary process, invented and patented by The Weld Institute in England, offers tremendous advantages for joining aluminum for high performance applications. It is particularly suited for advanced aluminum-lithium alloys, such as 2195, the primary structural alloy used in the External Tank. The friction stir welding process joins metals with minimal heat input, resulting in high-strength joints with high ductility. It is a simple process to demonstrate using a common milling machine for sample parts, but relatively expensive to implement on large-scale hardware, due to the high cost of tooling needed to handle the high forging pressures characteristic of the process. Recent developments at the Marshall Space Flight Center have demonstrated friction stir welding on linear joints up to 5 meters (15 ft.), with material thickness ranging between 2.5 mm and 16.5 mm (0.100" to 0.650"). High efficiency weld joints have been produced in aluminum from the 2000, 5000, and 6000 series alloy systems. A "retractable pin tool" system was patented by MSFC that allows use of friction stir welding for joints with changing material thickness, and with less rigid tooling than previously considered. This presentation will describe the details of alloys welded to-date and technical advances under development at MSFC. These developments could have substantial benefit to industrial applications for welding aluminum.

Jones, Clyde S.↗

Mitigating Abnormal Grain Growth for Friction Stir Welded Al-Li 2195 Spun Formed Domes

Formability and abnormal grain growth (AGG) are the two major issues that have been encountered for Al alloy spun formed dome development using friction stir welded blanks. Material properties that have significant influence on the formability include forming range and strain hardening exponent. In this study, tensile tests were performed for two 2195 friction stir weld parameter sets at 400 F to study the effects of post weld anneal on the forming range and strain hardening exponent. It was found that the formability can be enhanced by applying a newly developed post weld anneal to heat treat the friction stir welded panels. This new post weld anneal leads to a higher forming range and much improved strain hardening exponent. AGG in the weld nugget is known to cause a significant reduction of ductility and fracture toughness. This study also investigated how AGG may be influenced by the heating rate to the solution heat treatment temperature. After post-weld annealing, friction stir welds were strained to 15% and 39% by compression at 400 F before they were subjected to SHT at 950 F for 1 hour. Salt bath SHT is very effective in reducing the grain size as it helps arrest the onset of AGG and promote normal recrystallization and grain growth. However, heat treating a 18 ft dome using a salt bath is not practical. Efforts are continuing at Marshall Space Flight Center to identify the welding parameters and heat treating parameters that can help mitigate the AGG in the friction stir welds.

Chen, Po-Shou↗

Wiping Metal Transfer in Friction Stir Welding

Much evidence suggests that as the friction stir pin-tool moves along a weld seam the displacement of metal takes place by a wiping action at the surface of a plug of metal that rotates with the tool. The wiping model is explained and some consequences for the friction stir welding process are drawn.

Nunes, Arthur C., Jr.↗

Force reduction of friction stir welding and processing of steel

Friction stir welding and processing (FSW&P) is considered as a new fabrication method for canisters and repair of existing dry cask storage system canisters (generally made of austenitic stainless steel). Low heat input compared to fusion joining processes and grain refinement associated with low-temperature FSW&P result in a material with improved mechanical properties and equivalent generalized corrosion performance relative to the base metal. But FSW&P of austenitic stainless steel requires significant tool forge axis force to produce a weld (or a run). Exploratory runs utilizing forge axis force control were conducted to investigate the minimum force required to achieve defect-free runs. The correlation between forge axis force and resultant plunge depth was also investigated. Furthermore, detailed microstructural characterization was conducted to display the microstructural variation within the nugget zone.

36 MATERIALS SCIENCE↗

THE ROLE OF FRACTURE PROPERTIES ON LAP JOINT STRENGTH OF FRICTION STIR WELDED AA7055-T6 SHEETS

Friction stir lap welded (FSLW) joints have weight-saving potential in aluminum-intensive automotive assembly. However, FSLW also modifies the material microstructure close to the joint. Optimizing the FSLW process requires understanding the relationship between the strength and the joint's microstructure. In previous studies, efforts have been dedicated to determining the effects of local softening, the shape of the oxide line, and porosity. However, the impact of changes to the fracture properties on the joint's strength has not been studied. In this work, strength testing, and simulations, aided by material characterization, were used to determine the role of fracture properties on the shear strength of a 3-sheet (aluminum alloys 7055-7055-6022) lap joint. Characterization involved testing for fracture properties in the weld region. This data was then implemented into finite element simulations. As a result, the joint strength was predicted with a deviation of less than 6% from the experimental value. Comparison with strength prediction using only the base metal properties indicates that fracture property in the nugget region determines the strength of AA7055 FSLW.

Finite element analysis, Friction stir welding, ma↗

NDE of Friction Stir Welds in Aerospace Applications

Friction Stir Welding (FSW) is a solid state joining process, which utilizes a cylindrical, shouldered pin tool with a radiused tip that is rotated and plunged into the weld joint. Frictional heating beneath the shoulder, and surrounding the pin tip causes the material to plasticize, intermix and consolidate into a weldment without melting the parent material. FSW in aluminum alloys has many advantages such as low distortion and shrinkage, excellent mechanical properties, and no porosity. However, the propensity of the FSW process to create detrimental defects does exist, and is dependent on FSW parameter limits and controls. Inspection processes for FSW must also be selected and implemented concurrent with the new weld process. This paper describes the efforts by Lockheed Martin and NASA to find proper NDE techniques for detecting and characterizing the anomalies that may be caused by operating outside the envelope of optimized FSW parameters. Potential defects are identified and the results of the exploration of numerous NDE techniques including visual, liquid penetrant, multiple ultrasonic methods, eddy current and conductivity are discussed.

Kinchen, David G.↗

Room temperature corrosion behaviour of plastically deformed AISI 304 stainless steel by friction stir welding in neutral and acidified chloride solutions

Severe plastic deformation of 304L stainless steel plate was carried out by friction stirring under an isothermal tool temperature at 825°C. The friction stirred zone showed extensive grain refinement, high fraction of low angle grain boundaries due to dislocation rearrangement, Σ3 and Σ9 special grain boundaries and discrete Fe–Cr–Mn-rich particles. Electrochemical polarisation measurements were done on the base metal (BM) and friction stir welded (FSW) specimens in the neutral and acidified 3.5% NaCl solutions. The BM showed marginally better pitting resistance in the neutral chloride solution than the FSW because of a larger fraction of special grain boundaries, and larger grain size. Whereas in acidified 3.5% NaCl solution, the FSW showed better corrosion resistance than the BM. Furthermore, the surface film of the FSW had a lower impedance and a lower defect concentration than the BM indicating higher diffusivity of point defects in the FSW.

36 MATERIALS SCIENCE↗

Friction Stir Weld Application and Tooling Design for the Multi-purpose Crew Vehicle Stage Adapter

The Multi-Purpose Crew Vehicle (MPCV), commonly known as the Orion capsule, is planned to be the United States' next manned spacecraft for missions beyond low earth orbit. Following the cancellation of the Constellation program and creation of SLS (Space Launch System), the need arose for the MPCV to utilize the Delta IV Heavy rocket for a test launch scheduled for 2014 instead of the previously planned Ares I rocket. As a result, an adapter (MSA) must be used in conjunction with the MPCV to account for the variation in diameter of the launch vehicles; 5.5 meters down to 5.0 meters. Prior to ight article fabrication, a path nder (test article) will be fabricated to ne tune the associated manufacturing processes. The adapter will be comprised of an aluminum frustum (partial cone) that employs isogrid technology and circumferential rings on each end. The frustum will be fabricated by friction stir welding (FSW) three individual panels together on a Vertical Weld Tool (VWT) at NASA Marshall Space Flight Center. Subsequently, each circumferential ring will be friction stir welded to the frustum using a Robotic Weld Tool (RWT). The irregular geometry and large mass of the MSA require that extensive tooling preparation be put into support structures for the friction stir weld. The tooling on the VWT will be comprised of a set of conveyors mounted on pre-existing stanchions so that the MSA will have the ability to be rotated after each of the three friction stir welds. The tooling requirements to friction stir weld the rings with the RWT are somewhat more demanding. To support the mass of the MSA and resist the load of the weld tool, a system of mandrels will be mounted to stanchions and assembled in a circle. The goal of the paper will be to explain the design, fabrication, and assembly of the tooling, to explain the use of friction stir welding on the MSA path nder, and also to discuss the lessons learned and modi cations made in preparation for ight article fabrication in support of the 2014 launch of the Orion MPCV.

Alcorn, John↗

Heat Treatment of Friction-Stir-Welded 7050 Aluminum Plates

A method of heat treatment has been developed to reverse some of the deleterious effects of friction stir welding of plates of aluminum alloy 7050. This alloy is considered unweldable by arc and high-energy-density beam fusion welding processes. The alloy can be friction stir welded, but as-welded workpieces exhibit low ductility, low tensile and yield strengths, and low resistance to stress corrosion cracking. Heat treatment according to the present method increases tensile and yield strengths, and minimizes or eliminates stress corrosion cracking. It also increases ductility. This method of heat treatment is a superior alternative to a specification-required heat treatment that caused the formation of large columnar grains, which are undesired. Workpieces subjected to the prior heat treatment exhibited elongations <2 percent, and standard three-point bend specimens shattered. The development of the present heat treatment method was guided partly by the principles that (1) by minimizing grain sizes and relieving deformation stresses, one can minimize or eliminate stress corrosion cracking and (2) the key to maximizing strength and eliminating residual stresses is to perform post-weld solution heating for as long a time as possible while incurring little or no development of large columnar grains in friction stir weld nuggets. It is necessary to perform some of the solution heat treatment (to soften the alloy and improve machine welding parameters) before welding. The following is an example of thickness- dependent pre- and post-weld heat treatments according to the present method: For plates 0.270 in. (approx.6.86 mm) thick milled from plates 4.5 in. (114.3 mm) thick, perform pre-weld solution heating at 890 F (477 C) for 1 hour, then cool in air. After friction stir welding, perform solution heating for 10 minutes, quench, hold at room temperature for 96 hours, then age at 250 F (121 C) for 5 hours followed by 325 F (163 C) for 27 hours.

Petter, George E.↗

Low-Temperature Friction-Stir Welding of 2024 Aluminum

Solid state friction-stir welding (FSW) has been demonstrated to involve dynamic recrystallization producing ultra-fine, equiaxed grain structures to facilitate superplastic deformation as the welding or joining mechanism. However, the average residual, equiaxed, grain size in the weld zone has ranged from roughly 0.5 micron to slightly more than 10 micron, and the larger weld zone grain sizes have been characterized as residual or static grain growth as a consequence of the temperatures in the weld zone (where center-line temperatures in the FSW of 6061 Al have been shown to be as high as 480C or -0.8 T(sub M) where T(sub M) is the absolute melting temperature)). In addition, the average residual weld zone grain size has been observed to increase near the top of the weld, and to decrease with distance on either side of the weld-zone centerline, an d this corresponds roughly to temperature variations within the weld zone. The residual grain size also generally decreases with decreasing FSW tool rotation speed. These observations are consistent with the general rules for recrystallization where the recrystallized grain size decreases with increasing strain (or deformation) at constant strain rate, or with increasing strain-rate, or with increasing strain rate at constant strain; especially at lower ambient temperatures, (or annealing temperatures). Since the recrystallization temperature also decreases with increasing strain rate, the FSW process is somewhat complicated because the ambient temperature, the frictional heating fraction, and the adiabatic heating fraction )proportional to the product of strain and strain-rate) will all influence both the recrystallization and growth within the FSW zone. Significantly reducing the ambient temperature of the base metal or work pieces to be welded would be expected to reduce the residual weld-zone grain size. The practical consequences of this temperature reduction would be the achievement of low temperature welding. This study compares the residual grain sizes and microstructures in 2024 Al friction-stir welded at room temperature (about 30C and low temperature (-30C).

Benavides, S.↗

Friction Stir Welding of Curved Plates

Friction stir welding (FSW) is a remarkable technology for making butt and lap joints in aluminum alloys. The process operates by passing a rotating tool between two closely butted plates. This process generates heat and the heated material is stirred from both sides of the plates to generate a high quality weld. Application of this technique has a very broad field for NASA. In particular, NASA is interested in using this welding process to manufacture tanks and curved elements. Therefore, this research has been oriented to the study the FSW of curved plates. The study has covered a number of topics that are important in the model development and to uncover the physical process involve in the welding itself. The materials used for the experimental welds were as close to each other as we could possibly find, aluminum 5454-0 and 5456-0 with properties listed at http://matweb.com. The application of FSW to curved plates needs to consider the behavior that we observed in this study. There is going to be larger force in the normal direction (Fz) as the curvature of the plate increases. A particular model needs to be derived for each material and thickness. A more complete study should also include parameters such as spin rate, tool velocity, and power used. The force in the direction of motion (Fx) needs to be reconsidered to make sure of its variability with respect to other parameters such as velocity, thickness, etc. It seems like the curvature does not play a role in this case. Variations in temperature were found with respect to the curvature. However, these changes seem to be smaller than the effect on Fz. The temperatures were all below the melting point. We understand now that the process of FSW produces a three dimensional flow of material that takes place during the weld. This flow needs to be study in a more detailed way to see in which directions the flow of material is stronger. It could be possible to model the flow using a 2-dimensional model in the particular directions where the flow moves faster. More experimental information is required to enrich the knowledge about FSW, and from this point, derive useful mathematical formulas to optimize the process and the design of the machines that will perform it. More experiments and experimental equipment are required to uncover the mathematics of the process.

Sanchez, Nestor↗

Friction Stir Welding – an Advanced Approach to Repair Nuclear Power Plant Components

Solid phase joining technique friction stir welding (FSW) has been shown to mitigate helium-related issues in fusion welding of irradiated steels. Here, we present detailed characterization results of the first friction stir weld of an irradiated 304L stainless steel (SS) coupon contained 5.2 atomic parts per million (appm) helium. Scanning electron microscopy (SEM) was used to characterize a cross section specimen removed from the friction stir weld. No macro helium induced crack was observed at the analyzed cross-section, and only 1 – 1.5 µm size pores were found in the stir zone (SZ) and the thermal-mechanical affected zone (TMAZ). Moreover, some minor helium aggregations (Maximum ~20 µm in length) appeared along grain boundaries inside the TMAZ. Thereafter, miniature tensile specimens were extracted from the SZ, TMAZ and heat affected zone (HAZ), and base metal (BM) and tested. All welded specimens showed high total elongations (> 60%) and strengths (> 75% BM strengths). Overall, the weld made by FSW showed much better results comparing with traditional fusion welding on irradiated SS.

Tang, Wei↗

Controlling Force and Depth in Friction Stir Welding

Feedback control of the penetration force applied to a pin tool in friction stir welding has been found to be a robust and reliable means for controlling the depth of penetration of the tool. This discovery has made it possible to simplify depth control and to weld with greater repeatability, even on workpieces with long weld joints. Prior to this discovery, depths of penetration in friction stir welding were controlled by hard-tooled roller assemblies or by depth actuators controlled by feedback from such external sensors as linear variable-differential transformers or laser-based devices. These means of control are limited: A hard-tooled roller assembly confines a pin tool to a preset depth that cannot be changed easily during the welding process. A measurement by an external sensor is only an indirect indicative of the depth of penetration, and computations to correlate such a measurement with a depth of penetration are vulnerable to error. The present force-feedback approach exploits the proportionality between the depth and the force of penetration Unlike a depth measurement taken by an external sensor, a force measurement can be direct because it can be taken by a sensor coupled directly to the pin tool. The reading can be processed through a modern electronic servo control system to control an actuator to keep the applied penetration force at the desired level. In comparison with the older depth-control methods described above, this method offers greater sensitivity to plasticizing of the workpiece metal and is less sensitive to process noise, resulting in a more consistent process. In an experiment, a tapered panel was friction stir welded while controlling the force of penetration according to this method. The figure is a plot of measurements taken during the experiment, showing that force was controlled with a variation of 200 lb (890 N), resulting in control of the depth of penetration with a variation of 0.004 in. (0.1 mm).

Adams, Glynn↗

Investigation of Microstructure and Microhardness in Self-Reacting Friction Stir Welded AA2014-T6 and AA2219-T87

Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. This work reports on the microstructure and microhardness of SR-FSW between two dissimilar aluminum alloys. Specifically, the study examines the cross section of the weld joint formed between an AA2014-T6 plate on the advancing side and an AA2219-T87 plate on the retreating side. The microstructural analysis shows an irregularly displaced weld seam from the advancing side past the thermo-mechanical affected zone (TMAZ) into the weld nugget region. There are sharp variations in the microhardness across the weld. These variations are described in the paper and mechanisms for their formation are discussed.

Horton, K. Renee↗

A Micro-Electrochemical Study of Friction Stir Welded Aluminum 6061-T6

The corrosion behavior of friction stir welded Aluminum alloy 606 1-T6 was studied using a micro-electrochemical cell. The micro-electrochemical cell has a measurement area of about 0.25 square mm which allows for measurement of corrosion properties at a very small scale. The corrosion and breakdown potentials were measured at many points inside and outside the weld along lines perpendicular to the weld. The breakdown potential is approximately equal inside and outside the weld; however, it is lower in the narrow border between the weld and base material. The results of electrochemical measurements were correlated to micro-structural analysis. The corrosion behavior of the friction stir welded samples was compared to tungsten inert gas (TIG) welded samples of the same material.

Hintze, Paul E.↗

Tool for Two Types of Friction Stir Welding

A tool that would be useable in both conventional and self-reacting friction stir welding (FSW) has been proposed. The tool would embody both a prior tooling concept for self-reacting FSW and an auto-adjustable pin-tool (APT) capability developed previously as an augmentation for conventional FSW. Some definitions of terms are prerequisite to a meaningful description of the proposed tool. In conventional FSW, depicted in Figure 1, one uses a tool that includes (1) a rotating shoulder on top (or front) of the workpiece and (2) a rotating pin that protrudes from the shoulder into the depth of the workpiece. The main axial force exerted by the tool on the workpiece is reacted through a ridged backing anvil under (behind) the workpiece. When conventional FSW is augmented with an APT capability, the depth of penetration of the pin into the workpiece is varied in real time by a position- or force-control system that extends or retracts the pin as needed to obtain the desired effect. In self-reacting (also known as self-reacted) friction stir welding (SR-FSW), there are two rotating shoulders: one on top (or front) and one on the bottom (or back) of the workpiece. In this case, a threaded shaft protrudes from the tip of the pin to beyond the back surface of the workpiece. The back shoulder is held axially in place against tension by a nut on the threaded shaft. The main axial force exerted on the workpiece by the tool and front shoulder is reacted through the back shoulder and the threaded shaft, back into the FSW machine head, so that a backing anvil is no longer needed. A key transmits torque between the bottom shoulder and the threaded shaft, so that the bottom shoulder rotates with the shaft. A tool for SRFSW embodying this concept was reported in "Mechanism for Self-Reacted Friction Stir Welding" (MFS-31914), NASA Tech Briefs, Vol. 28, No. 10 (October 2004), page 53. In its outward appearance, the proposed tool (see Figure 2) would fit the above description of an SR-FSW tool. In this case, the FSW machine would have an APT capability and the pin would be modified to accept a bottom shoulder. The APT capability could be used to vary the distance between the front and back shoulders in real time to accommodate process and workpiece-thickness variations. The tool could readily be converted to a conventional FSW tool, with or without APT capability, by simply replacing the modified pin with a conventional FSW pin.

Carter, Robert↗

Microstructure and mechanical properties of friction stir weld performed on neutron-irradiated 304L steel with helium

As nuclear power plants (NPPs) approach or exceed 40–60 years of service, it may become necessary to repair damaged neutron-irradiated components to prolong longevity. However, fusion welding repair of irradiated steels and metallic materials is challenging because of helium-induced cracking. This study used friction stir welding (FSW) to address helium-related issues, such as helium bubble formation and grain boundary cracking. The microstructure, helium-induced degradation, and mechanical properties of a friction stir weld produced on neutron-irradiated 304L stainless steel with approximately 5.2 appm of helium were characterized. The analysis focused on variations in grain size, texture, and the morphology of helium-induced damage in the friction stir weld. Mechanical properties were characterized on the irradiated base metal (BM) and metallurgical zones of the friction stir weld: the stir zone (SZ), the thermo-mechanically affected zone (TMAZ), and the heat affected zone (HAZ). Only minor scattered porosity in the SZ and TMAZ and a few short microcracks (below 20 μm in length) in the TMAZ were observed, indicating limited helium-induced degradation. Tensile tests revealed good mechanical properties and fractography analysis demonstrated predominantly ductile fracture. In conclusion, the results highlight the immediate and substantial benefits of the FSW approach for repairing or joining helium-containing irradiated materials in NPPs.

36 MATERIALS SCIENCE↗