Search NASA⌕ Search

SEARCH · Search NASA

Results for “graphite anodes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Understanding the crack formation of graphite particles in cycled commercial lithium-ion batteries by focused ion beam - scanning electron microscopy

Here in this paper, the structure degradation of commercial Lithium-ion battery (LIB) graphite anodes with different cycling numbers and charge rates was investigated by focused ion beam (FIB) and scanning electron microscopy (SEM). The cross-section image of graphite anode by FIB milling shows that cracks, resulted in the volume expansion of graphite electrode during long-term cycling, were formed in parallel with the current collector. The crack occurs in the bulk of graphite particles near the lithium insertion surface, which might derive from the stress induced during lithiation and de-lithiation cycles. Subsequently, crack takes place along grain boundaries of the polycrystalline graphite, but only in the direction parallel with the current collector. Furthermore, fast charge graphite electrodes are more prone to form cracks since the tensile strength of graphite is more likely to be surpassed at higher charge rates. Therefore, for LIBs long-term or high charge rate applications, the tensile strength of graphite anode should be taken into account.

25 ENERGY STORAGE↗

Quarterly update for VTO XFC project

Since the last update, Sandia has performed additional testing on COTS baseline cells, as well as initial testing of University of Michigan baseline graphite anode cells. The COTS cell testing included an extreme stress test using 12C charging, as well as a non-cooled 6C charging test to determine the effectiveness of cooling plates. The Michigan cells were cycled with increasing charge rates to determine rate capability and possible propensity for lithium plating. The COTS cells are 5Ah NMC/Graphite pouches from Kokam with a modest 112 Wh/kg. The University of Michigan cells are NMC ~2.6Ah NMC/Graphite pouches made at the UM Battery Lab, and were designed with a more aggressive energy density. On the horizon, we will be testing additional cells from University of Michigan, including a baseline hard carbon anode cell. We will also disassemble the graphite anode cell, and continue to analyze the dQdV signals obtained during the graphite cell experiment to further understand evidence of possible plating. We also expect to receive cells with improved anodes for eventual testing against baselines.

25 ENERGY STORAGE↗

A stable graphite electrode in superconcentrated LiTFSI-DME/DOL electrolyte and its application in lithium-sulfur full battery

Graphical abstract: In superconcentrated ether-based solutions, the formed SEI film inhibits electrolyte decomposition and graphite exfoliation caused by co-intercalation of solvents. Thus, reversible lithium intercalation and de-intercalation at a graphite electrode has been realized. - Highlights: • Prelithiated graphite anodes are coupled with sulfur composite cathodes to form a Li–S full cell in superconcentrated LiTFSI-DME/DO electrolyte. • The introduced superconcentrated ether-based electrolyte permits reversible lithium intercalation and de-intercalation at a graphite electrode. • The assembled Li–S full battery exhibits better cycle performance and coulombic efficiencies. - Abstract: Herein, prelithiated graphite anodes are coupled with sulfur composite cathodes to form a Li–S full cell in superconcentrated ether electrolyte. This novel system is effective in avoiding sever corrosion of Li-metal anode and significantly improving the safety of present Li–S cell, owing to the replacement of Li-metal anode with graphite. The introduced superconcentrated ether electrolyte has a unique networking structure of Li cations and TFSI anions with Li{sup +}-solvating DME/DOL solvents, which is conducive to form a stable TFSI-derived surface film on the graphite electrode. The stable and dense TFSI-derived film inhibits further electrolyte decomposition and graphite exfoliation caused by co-intercalation of solvents, allowing reversible lithium intercalation and de-intercalation at a graphite electrode. Besides, the severe polysulfides shuttle is also suppressed by the concentrated ether-based solutions. Consequently, the assembled graphite-sulfur full battery retains outstanding capacity of 686 mAh g{sup −1}{sub sulfur} at 0.1C rate after 105 cycles, along with high Coulombic efficiency.

36 MATERIALS SCIENCE↗

Modeling Reversible Volume Change in Automotive Battery Cells with Porous Silicon Oxide-Graphite Composite Anodes

Automotive battery manufacturers are working to improve the individual cell and overall pack design by increasing durability, performance, and range, while reducing cost, and active material volume change is a key aspect that needs to be considered during this design process. Recently, silicon oxide-graphite composite anodes are being explored to increase total anode capacity while maintaining a tolerable amount of cell level reversible volume expansion due to the relatively lower reversible volume change of the silicon oxide compared to pure battery grade or metallurgical grade silicon. To predict the blended anode response and contribution to the overall cell volume change, we integrated the mechanical behavior of the individual active materials with the multi-species, multi-reaction model to predict the state-of-lithiation of the active materials in the cell at a given potential. The resulting simulations illustrate the tradeoff in volume change between the silicon oxide and the graphite during cell operation. This type of modeling approach will allow designers to virtually consider the impact of cell level and pack level design changes on overall system mechanical performance for automotive and grid storage applications, namely that relatively small addition of silicon containing materials can drive a significant increase in the volume change at the cell level, as demonstrated by the 5 wt% addition of silicon oxide accounting for half of the overall volume change in the cell.

Garrick, Taylor R. (ORCID:0000000322518129)↗

Nonflammable Electrolytes for Lithium Ion Batteries Enabled by Ultraconformal Passivation Interphases

Occasional fire accidents and continuous battery safety concerns require advanced lithium ion batteries (LIBs) with high safety as well as great battery performances. The electrolyte plays a critical role in electrochemical and safety properties. Organic phosphate solvents next to the state-of-the-art organic carbonates could formulate nonflammable electrolytes and intrinsically eliminate fire hazards, but their poor compatibility with the graphite anodes remains an obstacle for practical applications. This work reports a promising approach by formulating localized high concentration electrolytes based on a phosphate solvent, ethylene carbonate and a partially fluorinated ether. This electrolyte readily generates robust solid electrolyte interphase on graphite anode and cathode electrolyte interphase on LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode. As a result, this electrolyte shows good compatibility with high voltage cathode and graphite anode, and enables long-term cycling stability in graphite||NMC811 cells. This work sheds a new light in development of nonflammable electrolytes for high energy-density LIBs.

Non-flammable electrolyte, lithium ion battery, lo↗

3D Carbon Coating Enabled High‐capacity and Stable Micro‐sized Silicon Suboxide‐graphite Blended Anodes for Practical Lithium‐ion Batteries

Abstract Silicon oxide (SiO x ) is a promising anode candidate of lithium‐ion batteries (LIBs) owing to its extremely high specific capacity. However, the low initial Coulombic efficiency (ICE) and rapid capacity degradation of SiO x , triggered by the enormous volume variation upon repeated (de)lithiation, gravely hinder its practical use. Herein, two mass‐produced micro‐sized SiO x @C composites with obviously different morphologies for commercial LIBs are reported. Particularly, the SiO x ‐graphite blended anode (SiO x @3D‐G‐Gr) based on SiO x wrapped by three‐dimensional (3D) carbon layers (SiO x @3D‐G) exhibits a capacity of 519 mAh g −1 , an ICE of 90.0 % and a capacity retention of 83.4 % at 0.2 C over 100 cycles. which is far exceeding its counterpart SiO x @C‐H‐Gr (65.7 %). The obtained impressive properties of SiO x @3D‐G originate from the critical contribution of 3D carbon layers, which serves as the effective stress buffer and protective layer as well as the strong networks for electron/Li + transport. Accordingly, the full‐cell based on SiO x @3D‐G‐Gr anode and commercial LiCoO 2 cathode delivers a capacity of 803 mAh and an excellent capacity retention of 95.6 % (616 mAh, 96.6 % for graphite, respectively) at 1 C over 100 cycles with a stabilized CE of nearly 100 %. The micro‐sized SiO x @3D‐G showing a promising prospect in the commercial‐grade anodes in LIBs.

Electrochemistry↗

Achieving SEI preformed graphite in flow cell to mitigate initial lithium loss

The irreversible lithium loss due to the formation of solid electrolyte interphase (SEI) in the initial cycle on the graphite anode greatly reduces the overall cell energy density of lithium ion batteries, that is, the lost Li ions from forming SEI lead to the decrease of Li ions for the intercalation. The method of cathode prelithiation has been widely explored to compensate this lithium loss. However, these cathode additives with high lithium contents inevitably lower the loading of the cathode active materials. In this work, we report a novel approach to solve this challenge, a facile graphite prelithiation method by preforming SEI layers on the surface of graphite powders (Pre-SEI graphite) utilizing a specially designed flow cell. The Li accommodation in the graphite anode can be controlled by the operating time and current density in the flow cell for the electrochemical SEI formation. As a result, we demonstrate a 10% initial Columbic efficiency increase of the LiFePO 4 electrode in a full cell configuration using the Pre-SEI graphite, compared with the pristine graphite anode. The electrochemical preformation of SEI on the graphite powders offers a complete solution to offset initial lithium loss without a sacrifice of active cathode material loading.

25 ENERGY STORAGE↗

Fast charging of Li-ion cells: Effect of separator membranes and mapping of “safe lines” to avoid Li plating

An experimental method is introduced that uses microprobe Li/Cu reference electrodes to map "safe" charging regimes to avoid Li metal plating on graphite anodes at rates to 8C. With this method, a Li-ion cell closely approaches the Li plating condition but avoids descending into this regime. This "safe" approach is used to demonstrate effects of the microporous separator on Li plating in cells consisting of a layered nickel-manganese -cobalt oxide cathode and graphite anode. We argue that most of the difference in behaviors for different separators arises from time delayed Li + ion percolation through the membrane. In conclusion, our study suggests that explicitly treating kinetics of phase transitions in the lithiated graphite anode is essential for electrochemical models predicting "safe" lines for fast charging cells.

25 ENERGY STORAGE↗

High-throughput and high-performance lithium-ion batteries via dry processing

A scalable powder-to-electrode dry processing strategy mainly based on powder dry mixing and rolling/calendering is rationally designed. The dry processed electrodes show lower tortuosity compared to that of conventional slurry-based electrodes. The dry-processed high-loading graphite anodes (6.6 mAh cm -2 ) and LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathodes (6.0 mAh cm -2 ) exhibit promising electrochemical performance in half-cells and full-cells. The full-cells with both electrodes from dry processing demonstrates superb rate performance to their counterpart with conventional slurry-based electrodes and delivers of capacity retentions of 74.1 % and 63.6 % over 400 and 800 cycles, respectively. Notably, the initial Coulombic efficiency of the dry processed graphite anodes is low ascribed to polytetrafluoroethylene binder. Finally, the results suggest that dry processing is promising for future lithium-ion battery manufacturing and also pinpoint the needs of modification for the polytetrafluoroethylene binder in the graphite anodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cycling Performance and Structure Evolution of Co-Free Lithium- and Manganese-Rich Layered Oxides in Lithium-Ion Batteries

Lithium- and manganese-rich (LMR) layered oxides are high-capacity cathode materials that are being considered for electric vehicle (EV) lithium-ion batteries (LIBs). Here, we investigate the electrochemical cycling behavior of cells containing a cobalt-free LMR oxide, 0.3Li 2 MnO 3 ·0.7LiMn 0.5 Ni 0.5 O 2 , paired with either Li or graphite anodes. Two- and three-electrode cells are cycled under varying conditions to examine the effects of oxide activation, upper cutoff voltage, separator type, and electrolyte composition. Post-cycling characterization of harvested electrodes, with electrochemical, X-ray absorption spectroscopy, and solid-state 6 Li nuclear magnetic resonance spectroscopy techniques, are used to correlate cell performance changes with redox state evolution in the oxide and Li inventory shifts in the cell. Our results show that capacity fade and impedance rise primarily originate at the graphite anode and LMR cathode, respectively. Notably, while Ni undergoes reversible redox, Mn shows no evidence of bulk redox activity even in highly-aged electrodes: only relithiated LMR electrodes show some reduction of Mn. Graphite electrodes degrade due to particle isolation and SEI growth, exacerbated by Mn dissolution and deposition on graphite anodes. These findings highlight the coupled structural and electrochemical degradation mechanisms in LMR/graphite cells and underscore lithium inventory retention and electrode interfacial stability as critical factors for enhancing long-term performance.

Badami, Pavan P. [Argonne National Laboratory (ANL↗

Real-time monitoring of subsurface microbial metabolism with graphite electrodes

Monitoring in situ microbial activity in anoxic submerged soils and aquatic sediments can be labor intensive and technically difficult, especially in dynamic environments in which a record of changes in microbial activity over time is desired. Microbial fuel cell concepts have previously been adapted to detect changes in the availability of relatively high concentrations of organic compounds in waste water but, in most soils and sediments, rates of microbial activity are not linked to the concentrations of labile substrates, but rather to the turnover rates of the substrate pools with steady state concentrations in the nM-μ M range. In order to determine whether levels of current produced at a graphite anode would correspond to the rates of microbial metabolism in anoxic sediments, small graphite anodes were inserted in sediment cores and connected to graphite brush cathodes in the overlying water. Currents produced were compared with the rates of [2- 14 C]-acetate metabolism. There was a direct correlation between current production and the rate that [2- 14 C]-acetate was metabolized to 14 CO 2 and 14 CH 4 in sediments in which Fe(III) reduction, sulfate reduction, or methane production was the predominant terminal electron-accepting process. At comparable acetate turnover rates, currents were higher in the sediments in which sulfate-reduction or Fe(III) reduction predominated than in methanogenic sediments. This was attributed to reduced products (Fe(II), sulfide) produced at distance from the anode contributing to current production in addition to the current that was produced from microbial oxidation of organic substrates with electron transfer to the anode surface in all three sediment types. In conclusion, the results demonstrate that inexpensive graphite electrodes may provide a simple strategy for real-time monitoring of microbial activity in a diversity of anoxic soils and sediments.

59 BASIC BIOLOGICAL SCIENCES↗

Tailored Solvent Treatment for Optimized Production of Upcycled Anodes from End-Of-Life Li-Ion Batteries

Recycling processes for lithium-ion batteries typically overlook graphite because of its lower market value relative to that of transition-metal-containing cathode materials. However, graphite recovered from cycled lithium-ion batteries holds additional engineered value associated with the solid-electrolyte interphase (SEI). The SEI contributes critical electronic passivation of the graphite surface but becomes highly resistive with extended cycling, yielding poor cell performance. In this work, we apply tailored solvent treatment to end-of-life (EOL) graphite anodes to selectively remove adverse SEI components while retaining beneficially passivating species. We evaluate a series of polar protic solvents to achieve targeted removal of SEI components and control selectivity through rational variation in solvent properties. The physiochemical properties of treatment solvents correlate with both the retained SEI composition and the corresponding electrochemical performance of solvent-treated “upcycled” graphite anodes. Within the initial set of solvents evaluated, top-performing candidates show capacity and Coulombic efficiency nearly equivalent to those of an analogous pristine anode, as well as promising electrochemical performance enhancement with regard to irreversible capacity-loss metrics. This study establishes critical design principles for an optimized anode upcycling method that enhances the value of recycled graphite by retaining and upgrading the SEI.

25 ENERGY STORAGE↗

Molecular Engineering to Enable High-Voltage Lithium-Ion Battery: From Propylene Carbonate to Trifluoropropylene Carbonate

Molecular engineering of electrolyte structures has led to the successful application of trifluoropropylene carbonate (TFPC), a fluorinated derivative of propylene carbonate (PC), in next-generation high-voltage high-energy lithium-ion cell. Additionally, in contrast to a PC-based electrolyte which cointercalates in the form of Li + -solvated species into the graphene layer and exfoliates a graphite anode, a TFPC-based electrolyte is highly compatible with a graphite anode at low potential. Additionally, it shows exceptional oxidation stability on the charged cathode surface owing to the presence of the -CF 3 group. An all-fluorinated electrolyte, that is, 1.0 M LiPF 6 TFPC/2,2,2-trifluoroethyl carbonate (FEMC) (1/1 volume ratio) + FEC additive, was formulated and demonstrated excellent cycling stability in a high-voltage LiNi 0.5 Mn 0.3 Co 0.2 O 2 /graphite cell cycled between 3.0 and 4.6 V.

25 ENERGY STORAGE↗

Silicon Anodes with Improved Calendar Life Enabled By Multivalent Additives

Silicon is widely recognized as the most promising upgrade for graphite anodes due to its much higher capacity, natural abundance, and ability to be directly applied in the slurry-based, roll-to-roll production lines. However, in addition to the fast capacity decay, silicon anodes also suffer from inferior calendar life in practical applications due to the unstable solid-electrode interface (SEI). Until now, strategies to effectively improve the calendar life by tailored SEIs remain largely unclear, especially in high-Si content, zero-graphite anodes. Here, silicon anodes with superior calendar life are developed by adding small concentrations of multivalent salts into the baseline electrolyte. The Ca additive reacts with the F ions in the electrolyte, forming a layer of nanocrystalline CaF 2 that is closely coated around the silicon particles. The CaF 2 -enabled new SEI is strong and dense, which effectively protects the silicon core from side reactions, leading to lower capacity decay after calendar aging at high voltage. More importantly, the Ca additive is effective universally for all available commercial silicon or SiO sources. This study provides a feasible and low-cost solution for developing silicon anodes with long calendar life, paving the way towards commercially viable silicon anodes.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Improved Capacity Retention of Lithium Ion Batteries under Fast Charge via Metal-Coated Graphite Electrodes

A primary barrier preventing repetitive fast charging of Li-ion batteries is lithium metal plating at the graphite anode. One approach toward mitigating Li metal deposition is the deliberate modification of the graphite anode surface with materials demonstrating high overpotentials unfavorable for Li metal nucleation, such as Ni or Cu nanoscale films. This research explores Ni and Cu surface coatings at different areal loadings (3 or 11 μg cm -2 ) on the electrochemistry of graphite/LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) type Li-ion batteries. Extended galvanostatic cycling of control and metal-coated electrodes in graphite/NMC622 pouch cells are conducted under high rate conditions. Based on the overpotential of Li deposition on metal foil, both Ni and Cu treatments were anticipated to result in reduced lithium deposition. The higher metal film loadings of 11 μg cm -2 Ni- or Cu-coated electrodes exhibit the highest capacity retention after 500 cycles, with mean improvements of 8% and 9%, respectively, over uncoated graphite electrodes. Li plating quantified by X-ray diffraction indicates that the metal films effectively reduce the quantity of plated Li compared to untreated electrodes, with 11 μg cm -2 Cu providing the greatest benefit.

25 ENERGY STORAGE↗

Analysis of the Stable Interphase Responsible for the Excellent Electrochemical Performance of Graphite Electrodes in Sodium-Ion Batteries

Considerable efforts have been exerted to understand the formation and properties of the solid electrolyte interphase (SEI) in sodium ion batteries. However, the puzzling existence and role of SEI behind the huge volume changes of the graphite electrodes need to be answered. Herein, the reason of how ether-derived SEI maintains excellent reversibility despite the huge volume changes during cycling is unraveled. Theoretical simulations and Fourier-transform infrared spectroscopy demonstrate the formation mechanism of an SEI between the graphite anode and electrolyte. Furthermore, the high mechanical tolerance of the ether-derived SEI is confirmed in atomic force microscopy. A depth profile of X-ray photoelectron spectroscopy points to a multilayer structure of the ether-derived SEI. The outer layer comprises organics (sodium alkoxide), while the inorganics (Na 2 CO 3 , NaF) in interior region are mixed with some organics. Notably, the presence of organics ensures the adaptability of the SEI to the volume expansion of graphite during cycling, and the concentrated distribution of inorganics improves the Young's modulus (resistance to deformation). Therefore, the graphite anode exhibits high cycle stability (96.6% capacity retention ratio at 1 A g –1 over 860 cycles) and efficiency (≈99.5%).

25 ENERGY STORAGE↗