At least 91 records · Page 5

Saltstone third quarter calendar year 2019 (3QCY19) toxicity characteristic leaching procedure (TCLP) results

The aqueous waste from Tank 50 (salt solution) is sampled quarterly for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Saltstone Disposal Facility (SDF). Per request of customer, X-TAR-Z-00008, Revision 01, two SDF waste form (saltstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-Area premix material for the third quarter of calendar year 2019 (3QCY19). One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the “Cement-Free grout sample”. Results from this technical report support Task 2: ‘Grout Leaching Analyses’ of the Task Technical Request (TTR) prepared by Savannah River Remediation (SRR). After a 28 day cure, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using the Toxicity Characteristic Leaching Procedure (TCLP). The 3QCY19 saltstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79-268.48 requirements for a non-hazardous waste form with respect to Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development and Characterization of Cementitious Waste Forms for Immobilization of Granular Activated Carbon, Silver Mordenite, and HEPA Filter Media Solid Secondary Waste

Solid secondary waste materials expected to be generated during Hanford Waste Treatment and Immobilization Plant (WTP) operations were characterized (using representative materials) with respect to their ability to retain technetium-99 (Tc), iodine-129 (I), and mercury (Hg) as input to future updates to the Integrated Disposal Facility (IDF) performance assessments (PAs). The waste materials included granular activated carbon (GAC), silver mordenite (AgM), and high-efficiency particulate air (HEPA) filter media; all are used for removal of contaminants and radionuclides from the gaseous effluent treatment systems within the WTP. It is expected that the GAC and AgM will be mixed into a cementitious waste form in which the GAC and AgM particles will be blended/stabilized into the cementitious material. It is also expected that the HEPA filter media will be compacted and placed in a container that is then backfilled with a grout to macroencapsulate the medium. Here we report Kds for all waste materials of interest, examine the physical properties of grout specimens containing the waste materials, and provide solid-state characterization information to further understand the interaction of the waste materials with the encapsulating grout. The Kds are used in PA calculations that estimate contaminant release from the disposal site. Monolithic test specimens were prepared with the GAC and AgM mixed in either a Cast Stone grout formulation (8 weight percent [wt%] ordinary Portland cement [OPC], 45 wt% fly ash [FA], 47 wt% blast furnace slag [BFS]) or a Hanford grout mix 5 (HGM-5) formulation (25 wt% OPC, 75 wt% FA). As the specimens were being prepared, the fluid grout mixes were characterized for processing properties including flowability, set time, and the presence of free liquids during curing. After curing, compressive strengths of the waste forms were measured; the compressive strengths were above 2000 psi, easily exceeding the 500 psi minimum requirement. The cured waste forms were also characterized for their density, porosity, hydraulic conductivity, and water characteristic curve—all properties needed in PA calculations of radionuclide release from the waste forms in the IDF. Finally, EPA Method 1315 leach tests were conducted on the GAC and AgM waste materials encapsulated in the Cast Stone and HGM-5 grouts to determine the rate of release of contaminants from the waste forms. Effective diffusivities are provided, which can be used in future PA analyses of the disposal of these solid secondary waste materials.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Saltstone First Quarter Calendar Year 2021 (1QCY21) Toxicity Characteristic Leaching Procedure (TCLP) Results

The aqueous waste from Tank 50 (salt solution) is sampled quarterly for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Saltstone Disposal Facility (SDF). Per request of customer, X-TTR-Z00023, Revision 0, two SDF waste form (saltstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-Area premix material for the first quarter of calendar year 2021(1QCY21). One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the “Cement-Free grout sample”. Results from this technical report support Task 2: ‘Grout Leaching Analyses’ of the Task Technical Request (TTR) prepared by Savannah River Remediation (SRR). After at least 28 days cured, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using the Toxicity Characteristic Leaching Procedure (TCLP). The 1QCY21 saltstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79-268.48 requirements for a non-hazardous waste form with respect to Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC that was in effect at the time of the tank sampling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Saltstone Third Quarter Calendar Year 2021 (3QCY21) Toxicity Characteristic Leading Procedure (TCLP) Results

The aqueous waste from Tank 50 (salt solution) is sampled quarterly for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Saltstone Disposal Facility (SDF). Per request of customer, X-TTR-Z-00023, Revision 0, two SDF waste form (saltstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-Area premix material for the third quarter of calendar year 2021(3QCY21). One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the “Cement-Free grout sample”. Results from this technical report support Task 2: ‘Grout Leaching Analyses’ of the Task Technical Request (TTR) prepared by Savannah River Remediation (SRR). After at least 28 days cured, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using the Toxicity Characteristic Leaching Procedure (TCLP). The 3QCY21 saltstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79-268.48 requirements for a non-hazardous waste form with respect to Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC that was in effect at the time of the tank sampling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

MEASUREMENT OF SPECIFIC HEAT CAPACITY OF SALTSTONE

One of the goals of the Saltstone variability study is to identify (and quantify the impact of) the operational and compositional variables that control or influence the important processing and performance properties of Saltstone grout mixtures. The heat capacity of the Saltstone waste form is one of the important properties of Saltstone mixes that was last measured at SRNL in 1997. It is therefore important to develop a core competency for rapid and accurate analysis of the specific heat capacity of the Saltstone mixes in order to quantify the impact of compositional and operational variations on this property as part of the variability study. The heat capacity, coupled with the heat of hydration data obtained from isothermal calorimetry for a given Saltstone mix, can be used to predict the maximum temperature increase in the cells within the vaults of the Saltstone Disposal Facility (SDF). The temperature increase controls the processing rate and the pour schedule. The maximum temperature is also important to the performance properties of the Saltstone. For example, in mass pours of concrete or grout of which Saltstone is an example, the maximum temperature increase and the maximum temperature difference (between the surface and the hottest location) are controlled to ensure durability of the product and prevent or limit the cracking caused by the thermal gradients produced during curing. This report details the development and implementation of a method for the measurement of the heat capacities of Saltstone mixes as well as the heat capacities of the cementitious materials of the premix and the simulated salt solutions used to batch the mixes. The developed method utilizes the TAM Air isothermal calorimeter and takes advantage of the sophisticated heat flow measurement capabilities of the instrument. Standards and reference materials were identified and used to validate the procedure and ensure accuracy of testing. Heat capacities of Saltstone mixes were {approx} 55% higher than the previous measurement of specific heat capacity on a reference Saltstone mix in 1997. Values of mixes prepared using Deliquification, Dissolution and Adjustment (DDA), Modular Caustic Side Solvent Extraction Unit (MCU) and Salt Waste Processing Facility (SWPF) simulants and premix at 0.60 w/cm ratio were {approx} 1.95 J/g/{sup o}C and were equivalent within experimental error. The simple law of mixtures was used to predict the heat capacities of the Saltstone and the results were in excellent agreement with experimental data. This simple law of mixtures can therefore be used to predict the heat capacities of Saltstone mixes in those cases where measurements have not been made. The time dependence of the heat capacity is important as an input to the modeling of temperature increase in Saltstone vaults. The heat capacity of a mix of MCU and premix at 0.60 w/cm ratio was measured immediately after initial mixing and then periodically up to times greater than 100 days. Within experimental error, the heat capacity did not change with time. Therefore, the modeling is not complicated by requiring a time dependent function for specific heat capacity. The water to cementitious material (w/cm) ratio plays a key role in determining the value of the heat capacity. Both experimental and predictive values for SWPF mixes as function of the w/cm ratio were obtained and presented in this report. Predictions of the maximum temperatures of the Saltstone mixes were made using the heat of hydration data from previous isothermal measurements and the newly measured heat capacities for DDA, MCU and SWPF mixes. The maximum temperature increase ranged from 37 to 48 C for these mixes. The presence of aluminate at 0.33 M produced a temperature increase of 68 C which is close to the adiabatic temperature rise of 74 C observed by Steimke and Fowler in 1997 for a mix containing 0.35 M aluminate. Aluminum dissolution of the sludge will increase the aluminate in the DSS which in turn will result in a larger temperature increase in the Saltstone vaults during the curing period. The initial temperature of the Saltstone mixes in the Saltstone Production Facility (SPF) can be predicted using the specific heat capacities of Decontaminated Salt Solutions (DSS), the specific heat capacities of cementitious materials, and the initial temperatures of the DSS and the premix. This initial mix temperature is dominated by the DSS temperature due to its high heat capacity relative to the cementitious materials. Therefore, controlling the initial temperature of the DSS to lower temperatures will lead to lower maximum temperatures in the vault for a given batch of Saltstone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

July 2022 Semiannual Saltstone Toxicity Characteristic Leaching Procedure (TCLP) Results

The aqueous waste from Tank 50 (salt solution) is sampled semiannually for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Salstone Disposal Facility (SDF). Per request of customer, X-TTR-Z-00025, Revision 0, two SDF waste form (salstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-Area premix material for the July 2022 Semiannual Toxicity Characteristic Leaching Procedure (TCLP) samples. One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the "Cement-Free grout sample." Results from this technical report support Task 2: 'Grout Leaching Analyses' of the Task Technical Request (TTR) prepared by Savannah River Mission Completion (SRMC). After at least 28 days cured, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using Toxicity Characteristic Leaching Procedure (TCLP). The July 2022 semiannual salstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79-268.48 requirements for the non-hazardous waste form with respect to Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC that was in effect at the time of the tank sampling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Getter Incorporation into Cast Stone and Solid State Characterizations

Washington River Protection Solutions (WRPS) is collecting relevant available data on waste forms for use as a supplemental immobilization technology, to provide the additional capacity needed to treat low-activity waste (LAW) in Hanford Site tanks and complete the tank waste cleanup mission in a timely and cost-effective manner. One candidate supplemental waste form, fabricated using a low-temperature process, is a cementitious grout called Cast Stone. Cast Stone has been under investigation for this application at Pacific Northwest National Laboratory (PNNL) since initial screening tests in FY13. This report is the culmination of work to lower the diffusivities of Tc and I from Cast Stone using getters. Getters are compounds added to a system designed to selectively sequester a species of interest to provide increased stability to the species. The work contained within this report is related to waste form development and testing, and does not directly support the 2017 integrated disposal facility (IDF) performance assessment. However, this work contains valuable information which may be used in performance assessment maintenance past FY17, and in future waste form development. This report on performance characterization of Tc and I getters in Cast Stone fabricated with simulated LAW covers several areas of interest and major findings to WRPS: investigating performance of potassium metal sulfide (KMS-2-SS) and tin (II) apatite (Sn-A) as Tc getters when incorporated into Cast Stone; investigating performance of silver exchanged zeolite (Ag-Z) and argentite (Arg) as I getters when incorporated into Cast Stone; utilizing sequential addition of Tc and I getters to overcome any deleterious interactions between the getters in solution; determining, for the first time, Tc distribution within the cured Cast Stone and its evolution during leaching; and performing solid state characterization of getters and Cast Stone samples to support leach test findings and develop a mechanistic understanding of the processes that control Tc and I release into solution.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

January 2023 Semiannual Saltstone Toxicity Characteristic Leaching Procedure (TCLP) Results

The aqueous waste from Tank 50 (salt solution) is sampled semiannually for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Saltstone Disposal Facility (SDF). Per request of customer, X-TTR-Z-00027, Revision 0, two SDF waste form (saltstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-area premix material for January 2023 semiannual Toxicity Characteristic Leaching Procedure (TCLP) samples. One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag, and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the “Cement-Free grout sample.” Results from the technical report support Task 2: ‘Grout Leaching Analyses’ of the Task Technical Request (TTR) prepared by Savannah River Mission Completion (SRMC). After at least 28 days cured, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using the Toxicity Characteristic Leaching Procedure (TCLP). The January 2023 semiannual saltstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79.268.48 requirements for a non-hazardous waste form with respect to the Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC that was in effect at the time of the tank sampling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Performance of Underground Radioactive Waste Storage Tanks at the Savannah River Site: A 60-Year Historical Perspective

The Savannah River Site produced weapons-grade materials for nearly 35 years between 1953 and 1988. The legacy of this production is nearly 37 million gallons of radioactive waste. Since the 1950s, the liquid waste has been stored in large, underground carbon steel waste tanks. During the past 20 years, the site has begun to process the waste so that it may be stored in vitrified and grout forms, which are more suitable for long-term storage. Over the history of the site, some tanks have experienced leakage of the waste to the secondary containment. This article is a review of the instances of leakage and corrosion degradation that the tanks and associated equipment have experienced since the first tanks were built. Furthermore, the activities that the site has taken to mitigate the degradation and manage the service life of the tank for its anticipated lifetime are reviewed.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

January 2022 Semiannual Saltstone Toxicity Characteristic Leaching Procedure (TCLP) Results

The aqueous waste from Tank 50 (salt solution) is sampled semiannually for transfers to the Saltstone Production Facility (SPF). Salt solution is treated at SPF and disposed of in the Saltstone Disposal Facility (SDF). Per request of customer, X-TTR-Z-00025, Revision 0, two SDF waste form (saltstone) samples were prepared in the Savannah River National Laboratory (SRNL) from the Tank 50 Waste Acceptance Criteria (WAC) sample and Z-Area premix material for the January 2022 semiannual Toxicity Characteristic Leaching Procedure (TCLP) samples. One sample contained a Full Premix which included 10:45:45 (by weight) of cement, slag and fly ash. The second sample contained 60:40 (by weight) of slag and fly ash only referred to as the “Cement-Free grout sample.” Results from this technical report support Task 2: ‘Grout Leaching Analyses’ of the Task Technical Request (TTR) prepared by Savannah River Mission Completion (SRMC). After at least 28 days cured, a sample of each of the SDF waste forms was collected and shipped to a certified laboratory for analysis using the Toxicity Characteristic Leaching Procedure (TCLP). The January 2022 semiannual saltstone (Full Premix) and the Cement-Free grout samples met the South Carolina (SC) Code of Regulations for Hazardous Waste Management Regulations (HWMR) 61-79.261.24 and 61-79-268.48 requirements for a non-hazardous waste form with respect to Resource Conservation and Recovery Act (RCRA) metals and Underlying Hazardous Constituents (UHCs), and also met the SPF WAC that was in effect at the time of the tank sampling.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of Technetium Getters to Improve the Performance of Cast Stone

Cast Stone has been selected as the preferred waste form for solidification of aqueous secondary liquid effluents from the Hanford Tank Waste Treatment and Immobilization Plant (WTP) process condensates and low-activity waste (LAW) melter off-gas caustic scrubber effluents. Cast Stone is also being evaluated as a supplemental immobilization technology to provide the necessary LAW treatment capacity to complete the Hanford tank waste cleanup mission in a timely and cost effective manner. One of the major radionuclides that Cast Stone has the potential to immobilize is technetium (Tc). The mechanism for immobilization is through the reduction of the highly mobile Tc(VII) species to the less mobile Tc(IV) species by the blast furnace slag (BFS) used in the Cast Stone formulation. Technetium immobilization through this method would be beneficial because Tc is one of the most difficult contaminants to address at the U.S. Department of Energy (DOE) Hanford Site due to its complex chemical behavior in tank waste, limited incorporation in mid- to high-temperature immobilization processes (vitrification, steam reformation, etc.), and high mobility in subsurface environments. In fact, the Tank Closure and Waste Management Environmental Impact Statement for the Hanford Site, Richland, Washington (TC&WM EIS) identifies technetium-99 ( 99 Tc) as one of the radioactive tank waste components contributing the most to the environmental impact associated with the cleanup of the Hanford Site. The TC&WM EIS, along with an earlier supplemental waste-form risk assessment, used a diffusion-limited release model to estimate the release of different contaminants from the WTP process waste forms. In both of these predictive modeling exercises, where effective diffusivities based on grout performance data available at the time, groundwater at the 100-m down-gradient well exceeded the allowable maximum permissible concentrations for 99 Tc. (900 pCi/L). Recent relatively short-term (63 day) leach tests conducted on both LAW and secondary waste Cast Stone monoliths indicated that 99 Tc diffusivities were at or near diffusivities where the groundwater at the 100-m down-gradient well would exceed the allowable maximum permissible 99 Tc concentrations. There is, therefore, a need and an opportunity to improve the retention of Tc in the Cast Stone waste form. One method to improve the performance of the Cast Stone waste form is through the addition of “getters” that selectively sequester Tc inside Cast Stone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development of Magnesium Oxysulfate Formulation for SRPPF Aqueous Recovery Liquid Solidification

The liquid effluent from the Savannah River Plutonium Processing Facility (SRPPF) Aqueous Recovery Processes will be solidified into a stable form that is acceptable by Waste Isolation Pilot Plant (WIPP) for disposal. The current Aqueous Recovery flow sheet proposes to solidify the liquid effluent using a grout formula that was developed and tested for the former Waste Solidification Building process. This Portland cement based mixture results in a high pH (~13) leachate from the solidified waste form which is not acceptable to WIPP in the large quantities expected from production at SRPPF. Various cementitious materials were previously evaluated as alternative grout formulations to Portland cement and a MgO-based mix was identified as a promising alternative. A magnesium oxysulfate (MOS) cement formulation comprised of reactive magnesium oxide (MgO), anhydrous magnesium sulfate (MgSO 4 ), and sand, as a non-reactive heat sink provided good mixability, similar density to the original Portland-cement based mix, and a leachate pH of 9.4, within the assumed WIPP brine pH range. However, the MOS formulation exhibited an appreciable amount of heat generation, which resulted in premature setting of a large-scale test.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

A THERMAL MODEL OF THE IMMOBILIZATION OF LOW-LEVEL RADIOACTIVE WASTE AS GROUT IN CONCRETE VAULTS

Salt solution will be mixed with cement and flyash/slag to form a grout which will be immobilized in above ground concrete vaults. The curing process is exothermic, and a transient thermal model of the pouring and curing process is herein described. A peak temperature limit of 85 C for the curing grout restricts the rate at which it can be poured into a vault. The model is used to optimize the pouring.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Concrete Waste Form Properties on Radionuclide Migration

Assessing long-term performance of Category 3 waste cement grouts for radionuclide encasement requires knowledge of the radionuclide-cement interactions and mechanisms of retention (i.e., sorption or precipitation) the mechanism of contaminant release, the significance of contaminant release pathways, how waste form performance is affected by the full range of environmental conditions within the disposal facility, the process of waste form aging under conditions that are representative of processes occurring in response to changing environmental conditions within the disposal facility, the effect of waste form aging on chemical, physical, and radiological properties and the associated impact on contaminant release. This knowledge will enable accurate prediction of radionuclide fate when the waste forms come in contact with groundwater. Numerous sets of tests were initiated in fiscal years (FY) 2006-2009 to evaluate (1) diffusion of iodine (I) and technetium (Tc) from concrete into uncontaminated soil after 1 and 2 years, (2) I and rhenium (Re) diffusion from contaminated soil into fractured concrete, (3) I and Re (set 1) and Tc (set 2) diffusion from fractured concrete into uncontaminated soil, (4) evaluate the moisture distribution profile within the sediment half-cell, (5) the reactivity and speciation of uranium (VI) (U(VI)) compounds in concrete porewaters, (6) the rate of dissolution of concrete monoliths, and (7) the diffusion of simulated tank waste into concrete.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

CHARACTERIZATION OF CORE SAMPLE COLLECTED FROM THE SALTSTONE DISPOSAL FACILITY

During the month of September 2008, grout core samples were collected from the Saltstone Disposal Facility, Vault 4, cell E. This grout was placed during processing campaigns in December 2007 from Deliquification, Dissolution and Adjustment Batch 2 salt solution. The 4QCY07 Waste Acceptance Criteria sample collected on 11/16/07 represents the salt solution in the core samples. Core samples were retrieved to initiate the historical database of properties of emplaced Saltstone and to demonstrate the correlation between field collected and laboratory prepared samples. Three samples were collected from three different locations. Samples were collected using a two-inch diameter concrete coring bit. In April 2009, the core samples were removed from the evacuated sample container, inspected, transferred to PVC containers, and backfilled with nitrogen. Samples furthest from the wall were the most intact cylindrically shaped cored samples. The shade of the core samples darkened as the depth of coring increased. Based on the visual inspection, sample 3-3 was selected for all subsequent analysis. The density and porosity of the Vault 4 core sample, 1.90 g/cm{sup 3} and 59.90% respectively, were comparable to values achieved for laboratory prepared samples. X-ray diffraction analysis identified phases consistent with the expectations for hydrated Saltstone. Microscopic analysis revealed morphology features characteristic of cementitious materials with fly ash and calcium silicate hydrate gel. When taken together, the results of the density, porosity, x-ray diffraction analysis and microscopic analysis support the conclusion that the Vault 4, Cell E core sample is representative of the expected waste form.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Adsorptive Capture of Iodide by Metal-Organic Framework from Off-Gas Condensate Simulate

Millions of gallons of liquid nuclear wastes generated due to nuclear weapon development during the Cold War are in tank storage at several Department of Energy (DOE) sites across the country. DOE is responsible for disposal of the tank nuclear waste and clean-up of the contaminated sites. These efforts are complex and challenging technically and are costly financially, with the predicted overall cost reaching $377 billion over the next few decades [1]. The current practice of nuclear waste treatment and tank closure is to separate high-level waste (HLW) and low-level waste (LLW) [2]. The HLW is then vitrified into a borosilicate-based glass waste form [3], while the LLW is immobilized into cementitious grout or vitrified into glass [4]. However, these treatment processes have met unsolved technical problems

Jiang, Junhua [Savannah River National Laboratory ↗

Dismantling of the Spent Resins Hot Compaction Unit at Tihange NPP, Belgium - 19139

Design, construction and commissioning of the Spent Ion Exchange Resins Hot Compaction Unit at Tihange Nuclear Power Plant took place from 2005 till 2011. In this conditioning process, batches of radioactive resin beads were first dried to less than 4% moisture by a conical vacuum dryer. Resins were then poured in compactable 200-liter drums and super-compacted. Resulting pellets were emplaced in standard 400-liter drums, the packages qualified for final disposal in Belgium, and eventually grouted. The Belgian Waste Management Agency (ONDRAF/NIRAS) was consulted before initiating the project and issued a statement of no objection. The technology turned out to be used for the first time in the particular case of bead shaped resins (unlike powdered resins) and with a grouting requirement. Finally, commissioning tests ended in a safe and reproducible waste form, compliant with prevailing Waste Acceptance Criteria. Volume Reduction Factors of about 2 were recorded after drying and compaction. New tests were carried out to support the Qualification File of the process, which was submitted to ONDRAF/NIRAS. After performing many trials using inactive resins, the Operator dried two batches of radioactive resins and super-compacted four drums: this was a planned qualification step, aiming at the validation of process parameters. In the meantime, ONDRAF/NIRAS made parallel progress in the design of the future Near Surface Repository, where conditioned resins will be disposed of, and found some incompatibility between encapsulated dried resin beads and water intrusion hazards inside the repository. Based on the risk that dried resin beads will swell if they absorb water, causing mechanical stresses likely to compromise the integrity of the disposal site, ONDRAF/NIRAS informed Tihange NPP that the Hot Compaction Unit would not be qualified as spent resins conditioning process. Further to this irrevocable decision, the Operator undertook three actions: - The first one was the qualification and purchase of waste containers to provide additional temporary storage capacity on site for its operational spent resins; - The second one is the selection of a new spent resins conditioning process and the performance of the related qualification tests to demonstrate it meets the updated Waste Acceptance Criteria; - The last one is the dismantling of the Hot Compaction Unit to clear the space and enable the installation of new equipment. This latter task was carried out in 2018, involving decontamination and free release measurements of all the materials, a very limited fraction of it having to be further processed as radioactive waste. Nevertheless, Tihange NPP wishes to keep the super-compactor and its hydraulic unit for a possible resale or reuse for the treatment of mixed waste. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Spectroscopic identification of Ca-bearing uranyl silicates formed in C–S–H systems

Portland cement-based grouts used for radioactive waste immobilisation contain a Ca- and Si-rich binder phase, known as calcium–silicate–hydrate (C–S–H). Depending on the blend of cement used, the Ca/Si ratio can vary considerably. A range of C–S–H minerals with Ca/Si ratios from 0.6 to 1.6 were synthesised and contacted with aqueous U(VI) at 0.5 mM and 10 mM concentrations. Solid-state 29 Si MAS-NMR spectroscopy was applied to probe the Si coordination environment in U(VI)-contacted C–S–H minerals and, in conjunction with U L III -edge X-ray absorption spectroscopy analysis, inferences of the fate of U(VI) in these systems were made. At moderate or high Ca/Si ratios, uranophane-type uranyl silicates or Ca-uranates dominated, while at the lowest Ca/Si ratios, the formation of a Ca-bearing uranyl silicate mineral, similar to haiweeite (Ca[(UO 2 ) 2 Si 5 O 12 (OH) 2 ]·3H 2 O) or Ca-bearing weeksite (Ca 2 (UO 2 ) 2 Si 6 O 15 ·10H 2 O) was identified. This study highlights the influence of Ca/Si ratio on uranyl sequestration, of interest in the development of post-closure safety models for U-bearing radioactive waste disposal.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗