Search NASA⌕ Search

SEARCH · Search NASA

Results for “laser scanning”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

An experimental process parameter study on the identification of defects in additively fabricated Al6061 with laser powder bed fusion

Additively fabricated metal parts using laser powder bed fusion (L-PBF) possess sophisticated morphology due to the recurrent use of laser-induced metal powder melting and solidification. The surface and 3D morphology of these parts often include defects in the form of protrusions, depressions, pores, voids, keyholes, or cracks that are known to be influenced by laser scanning paths and layer-to-layer processing. Such inconsistent part quality hampers the extensive adoption of L-PBF. Pores and cracks are detrimental to the fatigue life of the parts and components. Quantifying and controlling part defects and optimizing processing and scanning strategy parameters adaptively in real-time through in situ monitoring systems are highly desired. This study investigates the optimization of experimental process parameters (power, scan velocity, and hatch spacing) and their effects on the cracking and porosity of Al6061 alloy using machine learning techniques. Multi-objective optimization is formulated and conducted to determine the L-PBF parameters that minimize both porosity and crack densities.

36 MATERIALS SCIENCE↗

Effect of autogenous shrinkage on microcracking and mass transport properties of concrete containing supplementary cementitious materials

It is well-known that supplementary cementitious materials (SCMs) and low water-to-binder (w/b) ratio increase autogenous shrinkage, but the impact on microcracking and long-term transport properties is less understood. This paper examines the effect of microcracking induced by autogenous shrinkage on transport properties of concretes cured up to ~3.6 years. Variables include SCM type (9% SF, 70% GGBS), w/b ratio (0.20–0.45), maximum-aggregate-size (MSA: 5–20 mm) and shrinkage reducing admixture (SRA). Oxygen diffusivity, permeability and water sorptivity were correlated with microcracks characterised using laser scanning confocal microscopy and 3D X-ray microtomography. Results show greater microcracking in mixes containing SCMs, low w/b ratio and large MSA. At the same w/b ratio and binder type, strong positive correlations are observed between transport and microcracking with increasing MSA, confirming the negative impact of autogenous shrinkage. SRA was effective in reducing these effects. The significance is compared with drying shrinkage and implications for durability are discussed.

36 MATERIALS SCIENCE↗

3D imaging techniques for characterising microcracks in cement-based materials

Concrete inherently contains pores and microcracks that can adversely impact its mechanical properties and long-term durability. However, characterising microcracks is difficult due to their complex, multiscale and three-dimensional (3D) nature. This paper presents an evaluation of 3D imaging techniques for characterising microcracks induced by different mechanisms. Seven cement pastes, mortars and concretes subjected to drying shrinkage, autogenous shrinkage and freeze-thaw cycles were investigated using focused ion beam nanotomography (FIB-nt), broad ion beam serial section tomography (BIB-SST), laser scanning confocal microscopy (LSCM) combined with serial sectioning and X-ray microtomography (μCT). The study shows that the characteristics of microcracks vary significantly depending on exposure conditions. Yet there is no single technique that can capture the entire size range of microcracks from sub to tens of μm within a sufficiently representative sampling volume. The achievable image volume and resolution, and the advantages and disadvantages of each technique are compared and discussed.

36 MATERIALS SCIENCE↗

Nanoparticle-enhanced absorptivity of copper during laser powder bed fusion

We report laser powder bed fusion (LPBF) of pure copper for thermal and electrical applications is hampered by its low near-infrared absorptivity and high thermal diffusivity. These material properties make it very difficult to localize the thermal energy needed to produce high density 3D printed parts. Modification of metal powders via nanoparticle additives is a promising approach to increasing absorptivity, but the effect of nanoparticles on absorptivity and melting behavior during LPBF is not well understood. In this study, we developed an in situ calorimetry system to measure effective absorptivity during LPBF on copper substrates. We decorated copper substrates using three nanoparticle systems (CuS, TiB 2 , multilayer graphene flakes) and demonstrated an enhanced absorptivity of the decorated substrates relative to pure copper. Graphene nanoflakes resulted in the highest improved absorption relative to pure copper from 0.09 to 0.48, due to their stability at high laser scanning powers. A thermomechanical model with convective heat transfer provided confidence in the measurements by reproducing the experimental melt pool traces. Full 3D cylindrical prints demonstrated an improvement in relative density of the copper-graphene powder prints (in the range of 0.930–0.992), relative to that of as-purchased copper powder prints (in the range of 0.854–0.972). This work provides a fundamental study of nanoparticle-enabled LPBF of highly reflective metals and demonstrates a viable route for expanding the library of reliably printable metals.

36 MATERIALS SCIENCE↗

Large-Scale Welding Process Simulation by GPU Parallelized Computing

The computational design of industrially relevant welded structures is extremely time consuming due to coupled physics and high nonlinearity. Previously, most welding distortion and residual stress simulations have been limited to small coupons and reduced order (from three-dimensional [3D] to two-dimensional [2D]), or inherent strain approximations were used for large structures. In this current study, an explicit finite element code based on a graphics processing unit was utilized to perform 3D transient thermomechanical simulation of structural components during welding. Laser brazing of aluminum alloy panels as representative of automotive manufacturing scenarios was simulated to predict out-of-plane distortion under different clamping conditions. The predicted deformation pattern and magnitude were validated by laser scanning data of physical assemblies. In addition, the code was used to investigate residual stresses developed during multipass arc welding of a nuclear industry pressurizer surge nozzle and subsequent welding repair where a 3D simulation was necessary. Taking the experimental data as reference, the 3D model predicted better residual stress distribution than a typical 2D asymmetrical model. Stress evolution in welding repair was also presented and discussed in this study. Furthermore, the efficient numerical model made it feasible to use integrated computational welding engineering to simulate welding processes for large-scale structures.

97 MATHEMATICS AND COMPUTING↗

Multiscale investigation of thermomechanical and compositional developments in Ni alloy 718 under laser processing

Laser processing has been widely employed in various applications due to its exceptional spatial resolution. However, the rapid temperature gradients generated in localized areas present significant challenges for experimental characterization using conventional instruments. To characterize Ni alloy 718 during laser processing, we employed in-situ synchrotron X-ray diffraction with a high-speed detector, a method particularly well-suited for probing processes with high temporal and spatial resolution. Through a series of in-situ experiments, we investigated the local variations in the evolution of microstructures and thermomechanical behaviors within a keyhole mode melt pool. The in situ macroscopic thermomechanical behaviors were quantified using an empirical model derived from diffraction patterns, with experimental results showing reasonable agreement with finite element analysis. Various laser parameters were tested to assess their influences on the residual strains in the melt pools. The results revealed that the residual strain in the keyhole mode melt pool is relatively insensitive to variations in the parameters and is smaller than that in the melt pool created under conduction mode laser scanning. Additionally, we analyzed the shapes of individual diffraction spots, providing insights into the plastic behaviors and compositional developments in the resolidified alloy. The analysis confirmed that compositional variations in a dendritic microstructure manifest as asymmetric broadening of the diffraction spots.

Ni alloy 718↗

A Data-Driven Framework for Direct Local Tensile Property Prediction of Laser Powder Bed Fusion Parts

This article proposes a generalizable, data-driven framework for qualifying laser powder bed fusion additively manufactured parts using part-specific in situ data, including powder bed imaging, machine health sensors, and laser scan paths. To achieve part qualification without relying solely on statistical processes or feedstock control, a sequence of machine learning models was trained on 6299 tensile specimens to locally predict the tensile properties of stainless-steel parts based on fused multi-modal in situ sensor data and a priori information. A cyberphysical infrastructure enabled the robust spatial tracking of individual specimens, and computer vision techniques registered the ground truth tensile measurements to the in situ data. The co-registered 230 GB dataset used in this work has been publicly released and is available as a set of HDF5 files. The extensive training data requirements and wide range of size scales were addressed by combining deep learning, machine learning, and feature engineering algorithms in a relay. The trained models demonstrated a 61% error reduction in ultimate tensile strength predictions relative to estimates made without any in situ information. Lessons learned and potential improvements to the sensors and mechanical testing procedure are discussed.

36 MATERIALS SCIENCE↗

A new procedure for implementing the modified inherent strain method with improved accuracy in predicting both residual stress and deformation for laser powder bed fusion

As a metal additive manufacturing (AM) process, laser powder bed fusion (L-PBF) has been widely used to produce parts with complex geometries. The large thermal gradient caused by the fast, intense, and repeated laser scanning induces significant residual deformation and stress to the as-built parts, which increase manufacturing difficulty and geometrical inaccuracy as a result. The modified inherent strain (MIS) method exploiting multiscale process simulations was developed to simulate residual deformation accurately and efficiently. However, the existing procedure of implementing the MIS method is found to give inaccurate residual stress prediction. Here in this work, a new implementation procedure for the MIS method is proposed to improve the simulation accuracy of residual stress without degrading the residual deformation prediction. The new procedure concerns the application of inherent strains to the part-scale layer-by-layer finite element model to obtain residual stress and deformation field. While the existing implementation of the part-scale MIS model involves only mechanical properties at ambient temperature, the new procedure adds one more solution step employing mechanical properties at an elevated temperature determined from the inherent strain extraction step. Both numerical and experimental studies are conducted to validate the proposed new implementation procedure. It shows that by using the new procedure, the MIS-based simulation can predict both residual stress and deformation of as-built L-PBF metal parts with good accuracy.

36 MATERIALS SCIENCE↗

Unravelling Microstructure Selection in an Additively Manufactured Eutectic High‐Entropy Alloy

High-entropy alloys (HEAs) are promising candidates for advanced structural applications due to their excellent mechanical properties. Additive manufacturing (AM), with its rapid solidification conditions, enables the creation of unique nonequilibrium microstructures. To fully leverage the synergy between AM and HEAs, understanding how processing affects structure and properties is essential. Here, how solidification rate influences microstructure evolution and phase transformation pathway in laser additively manufactured AlCrFe2Ni2 eutectic HEAs is investigated. By increasing the laser scan speed and hence the solidification rate, distinct solidification modes evolving from coupled eutectic to anomalous eutectic and eventually to single-phase solidification are revealed. These transitions result in distinct microstructures and a wide range of mechanical properties. Thermodynamic modeling and molecular dynamics simulations reveal that low cooling rates allow for sufficient atomic diffusion and phase separation, facilitating coupled eutectic growth. In contrast, rapid cooling suppresses diffusion and destabilizes the solid–liquid interface, promoting anomalous or single-phase solidification. This integrated experimental and computational approach provides a multiscale understanding of solidification mechanisms in HEAs and underscores how kinetic effects can over-ride thermodynamic predictions under nonequilibrium conditions. Furthermore, these results demonstrate that AM can serve as a powerful tool to design HEAs with tailored microstructures and properties.

36 MATERIALS SCIENCE↗

Utilization of Ultrasonication as a Method of Reducing Organic and Inorganic Contamination in Post‐Consumer Plastic Film Waste

Post-consumer plastic film waste often carries organic and inorganic contaminants that challenge recycling processes and affect the quality of recycled products. An effective contaminant removal procedure through washing such single-used plastic films (SUPFs) can address environmental and waste management concerns. This study compares the efficiency of different washing techniques in reducing SUPF contamination. To evaluate the efficacy of each washing technique, film samples collected from material recovery facilities are individually exposed to friction, ultrasonic-assisted, and a combination of both washes. Thermal analysis indicates that the polymers' melting temperature, crystallization temperature, and crystallinity remain unaffected by the washing methods, demonstrating method aptness. Confocal laser scanning microscope images show that washing results in a cleaner sample surface. 91% ash reduction during the combined wash treatment indicates a high method efficiency compared to the individual friction and ultrasonic wash procedures. This is further validated by reducing characteristic contaminant IR bands (3600–3000, 1750–1600, and 1100–1000 cm −1 ). Elements of concern such as Cd, Cr, Hg, and Pb in SUPFs after each washing technique applied conform with regulations (<100 ppm) for packaging products. This research shows the novel ultrasonic washing reduces more contamination than friction with shorter wash times and no surfactants.

42 ENGINEERING↗

Getting allometry right at the Oak Ridge free‐air CO 2 enrichment experiment: Old problems and new opportunities for global change experiments

Societal Impact Statement Free‐air CO 2 enrichment (FACE) experiments provide essential data on forest responses to increasing atmospheric CO 2 for evaluations of climate change impacts on humanity. Understanding and reducing the uncertainty in the experimental results is critical to ensure scientific and public confidence in the models and policy initiatives that derive therefrom. One source of uncertainty is the estimation of tree biomass using mathematical relationships between biomass and easily obtained and non‐destructive measurements (allometry). We evaluated the robustness of the allometric relationships established at the beginning of a FACE experiment and discuss the challenges and opportunities for the new generation of FACE experiments. Summary Long‐term field experiments to elucidate forest responses to rising atmospheric CO 2 concentration require allometric equations to estimate tree biomass from non‐destructive measurements of tree size. We analyzed whether the allometric equations established at the beginning of a free‐air CO 2 enrichment (FACE) experiment in a Liquidambar styraciflua plantation were still valid at the end of the 12 year experiment. Aboveground woody biomass was initially predicted by an equation that included bole diameter, taper, and height, assuming that including taper and height as predictors would accommodate changes in tree structure that might occur over time and in response to elevated CO 2 . At the conclusion of the FACE experiment, we harvested 23 trees, measured dimensions and dry mass of boles and branches, and extracted and measured the woody root mass of 10 trees. Although 10 of the harvested trees were larger than the trees used to establish the allometric relationship, measured aboveground woody biomass was well predicted by the original allometry. The initial linear equation between bole basal area and woody root biomass underestimated final root biomass by 28%, but root biomass was just 21% of total wood mass, and errors in aboveground and belowground estimates were offsetting. The allometry established at the beginning of the experiment provided valid predictions of tree biomass throughout the experiment. New allometric approaches using terrestrial laser scanning should reduce an important source of uncertainty in decade‐long forest experiments and in assessments of centuries‐long forest biomass accretion used in evaluating carbon offsets and climate mitigation.

59 BASIC BIOLOGICAL SCIENCES↗

The effect of WAAM process parameters on process conditions and production metrics in the fabrication of single-pass multi-layer wall artifacts

The present work seeks to understand the impact of varying dwell time and input deposition power on part quality and overall production time for wire arc additive manufacturing. In this work, multi-layer wall geometries were deposited under different input power conditions without affecting the material deposition rate by setting traverse speed and wire feed speed constant and varying the contact tip-to-workpiece distance and the deposition power settings. Current and voltage data and optical imaging of the deposition zone were captured in situ, and wall geometry was characterized using laser scanning, so to understand the applicability of these methods for determining part height in situ. Furthermore, the present results demonstrate that alternating dwell times with lower input deposition power can result in significantly reduced overall production time and minimal material underbuilding, despite increased deposition geometry width. Furthermore, it is shown that while elimination of process dwell results in severe underbuilding of the deposition, it also yields the highest production rate for a hybrid-finished (e.g., deposited, machined) wall in terms of mm in build direction per minute and the highest buy-to-fly ratio.

36 MATERIALS SCIENCE↗

Effects of weave path parameters on the geometry of wire arc additive manufactured features

Here, the present work investigates the effect of process parameters on the geometry of wire arc additive manufactured parts. The geometric accuracy of features produced with a weaving strategy is compared to what can be accomplished with a typical overlapping bead strategy. In this work, single-layer and multi-layer geometries were deposited under varying process and path parameters. The wavelength, amplitude, and torch speed of the weaving path were varied, while the power, wire feed speed, and contact tip to work distance remained constant. The geometric deposition efficiencies of several samples produced with a weave strategy are directly compared to samples generated with two parallel overlapping beads with torch speeds defined to match the deposition rate of the weave samples. Feature geometries were characterized using optical microscopy and laser scanning data. The results indicate that implementing a weave path strategy can improve the geometric accuracy of wire arc additive features, thus increasing the effective volumetric deposition rate of the process. It is shown that the most consistent improvements resulted from the combination of low wavelength and high amplitude, which correlate to wider and taller printed layers.

GMAW↗

Crystal plasticity model of residual stress in additive manufacturing using the element elimination and reactivation method

Selective laser melting is receiving increasing interest as an additive manufacturing technique. Residual stresses induced by the large temperature gradients and inhomogeneous cooling process can favour the generation of cracks. In this work, a crystal plasticity finite element model is developed to simulate the formation of residual stresses and to understand the correlation between plastic deformation, grain orientation and residual stresses in the additive manufacturing process. The temperature profile and grain structure from thermal-fluid flow and grain growth simulations are implemented into the crystal plasticity model. An element elimination and reactivation method is proposed to model the melting and solidification and to reinitialize state variables, such as the plastic deformation, in the reactivated elements. The accuracy of this method is judged against previous method based on the stiffness degradation of liquid regions by comparing the plastic deformation as a function of time induced by thermal stresses. The method is used to investigate residual stresses parallel and perpendicular to the laser scan direction, and the correlation with the maximum Schmid factor of the grains along those directions. The magnitude of the residual stress can be predicted as a function of the depth, grain orientation and position with respect to the molten pool. The simulation results are directly comparable to X-ray diffraction experiments and stress–strain curves.

316 stainless steel↗

In Situ Observation of Acicular Ferrite Nucleation and Growth at Different Cooling Rate in Ti-Zr Deoxidized Steel

The effects of cooling rate on acicular ferrite (AF) nucleation, growth, and inclusion characteristics in Ti-Zr deoxidation steel were studied by utilizing the high temperature confocal laser scanning microscope (HT-CLSM). The results indicated that with the increase of cooling rate, the ferrite start nucleation temperature decreased, and the difference of first nucleation temperature between AF and ferrite side plate (FSP) reduced. When the cooling rate increased to 10.0 °C/s, AF and FSP simultaneously nucleated at 564.5 °C. In addition, the AF actual growth rate rose with the increase of cooling rate and reached 30.13 µm/s at 10.0 °C/s cooling rate. The AF ratio in microstructure increased first and then decreased with the cooling rate increase and was up to the maximum 45.83 pct at 1.0 °C/s cooling rate. For inclusion characteristics, cooling rates had no obvious effect on inclusion types, but had a great influence on inclusions size distribution. With the cooling rate increase, the inclusion average diameter reduced, and diminished to 1.39 µm at 10.0 °C/s cooling rate. Finally, the AF nucleation on the Ti-Zr-Mn-O-S + TiN inclusion could be explained by the low lattice misfit between ferrite and TiN that precipitated on the Ti-Zr-Mn-O-S inclusion surface.

36 MATERIALS SCIENCE↗

Liquid Inclusion Distortion by Lens Shape Effect: In Situ Observation and Quantification on LCAK Steels Using HT-CSLM

Because of interfacial and surface tension, micron-sized liquid oxide droplets are expected to change from spherical (when fully immersed in liquid steel) to lens shape on top of steel. Inclusion sizes were measured by automated analysis of polished sections of calcium-treated aluminum-killed steel. A sample of the same steel was remelted and observed using confocal scanning laser microscopy. Droplets on the steel surface appear to have approximately twice the diameter of fully immersed spherical inclusions.

36 MATERIALS SCIENCE↗

Agglomeration Mechanism of Complex Ti-Al Oxides in Liquid Ferrous Alloys Considering High-Temperature Interfacial Phenomenon

This work presents the agglomeration mechanism of complex Ti-Al oxides in the liquid ferrous alloy. Cluster characteristics were investigated using Al and Ti/Al-complex deoxidation method in lab scale. The time-dependent size distribution, total number per volume, average size, and circularity of the clusters were quantitatively analyzed. Furthermore, high-temperature confocal laser scanning microscopy was utilized to directly observe the cluster formation of Ti-Al oxides. A capillary force model including wettability parameters was applied to compare the agglomeration capabilities of different types of non-metallic inclusions. When a low Ti is added into melt, the agglomeration of TiO{sub x}·FeO liquid inclusions is one of the key factors to decrease the frequency of cluster formation. When the Al is added into melt, the heterogeneous precipitation on TiO{sub x}·FeO surfaces is the main reaction process. Ti-Al oxides have lower agglomeration ability than that of Al{sub 2}O{sub 3}, which in turn, contribute to a low agglomeration frequency as well.

36 MATERIALS SCIENCE↗

Iron Oxide Reduction Rate Affects Iron Product Morphology

Magnetite concentrates from different parts of the Mesabi Range, exhibiting varying tendencies to encapsulate, were reduced using thermogravimetric analysis (TGA) and a high-temperature confocal scanning laser microscope (CSLM). Gas-phase mass-transfer conditions were intentionally varied by employing two reactors with different geometries: the TGA produced significantly slower reduction, whereas the CSLM setup yielded reduction rates up to 20 times faster under mass-transfer-controlled conditions. A preliminary mechanism is proposed to explain the transition from a porous iron product to a dense encapsulating layer. Encapsulation is interpreted as the outcome of competition between pore creation, driven by the reduction rate, and pore elimination, driven by surface diffusion. When pore formation is insufficient to counteract pore coarsening, a dense iron layer develops and restricts further reduction.

encapsulation↗