At least 91 records · Page 5

A new diffusion-inhibited oxidation-resistant coating for superalloys

A concept for enhanced protection of superalloys consists of adding an oxidation- and diffusion-resistant cermet layer between the superalloy and the outer oxidation-resistant metallic alloy coating. Such a duplex coating was compared with a physical-vapor-deposited (PVD) NiCrAlY coating in cyclic oxidation at 1150 C. The substrate alloy was MA 754 - an oxide-dispersion-strengthened superalloy that is difficult to coat. The duplex coating, applied by plasma spraying, outperformed the PVD coating on the basis of weight change and both macroscopic and metallographic observations.

Gedwill, M. A.↗

Protective aluminum oxide surface coatings and low-temperature forming process for high-temperature applications

A method of both coating a substrate with aluminum oxide and infusing the substrate with elemental aluminum is disclosed. In one example, the method includes providing a metal powder/polymer binder slurry, the slurry having a solvent, an organic binder, metal granules and a seed element, wherein the metal granules include Al; dispersing the slurry upon a Cr-containing surface; after dispersing the slurry, exposing the slurry to air and maintaining the temperature of the slurry and substrate below 110° C. to remove at least a portion of the solvent from the slurry; and, in a combined step, both exposing the binder, metal granules and substrate to air and heating the remaining slurry and substrate at a temperature less than or equal to 1000° C. to both diffuse at least a portion of the metal of the metal granules into the substrate and coat the substrate with aluminum oxide.

36 MATERIALS SCIENCE↗

Oxidation protection coatings for polymers

A polymeric substrate is coated with a metal oxide film to provide oxidation protection in low Earth orbital environments. The film contains about 4 volume percent polymer to provide flexibility. A coil of polymer material moves through an ion beam as it is fed between reels. The ion beam first cleans the polymer material surface and then sputters the film material from a target onto this surface.

Mirtich, M. J.↗

Apparatus for producing oxidation protection coatings for polymers

A polymeric substrate is coated with a metal oxide film to provide oxidation protection in low Earth orbital environments. The film contains about 4 volume percent polymer to provide flexibility. A coil of polymer materials moves through an ion beam as it is fed between reels. The ion beam first cleans the polymer material surface and then sputters the film material from a target onto this surface.

Mirtich, M. J.↗

Oxidation protection coatings for polymers

A polymeric substrate is coated with a metal oxide film to provide oxidation protection in low Earth orbital environments. The film contains about four volume percent polymer to provide flexibility.

Sovey, James S.↗

Thermal barrier coating life prediction model

The objectives of this research were to determine the predominant modes of degradation of a plasma sprayed thermal barrier coating (TBC) system, and then to develop and verify life prediction models accounting for these degradation modes. The TBC system consists of a low pressure plasma sprayed (LPPS) bond coat layer of Ni-22Cr-10Al-O.3Y, an air plasma sprayed (APS) yttria partially stabilized zirconia (ZrO sub 2-8Y sub 2 O sub 3) top coat on a conventionally cast Rene 80 (Ni base) substrate. Thermal cycle testing of TBCs was employed to evaluate the effect of coating edges, bond coat oxidation, bond coat creep, top coat thickness, and bond coat thickness.

Pilsner, B.↗

High-Temperature Air Stability of Electrodeposited Copper Cobalt Oxide and Copper Manganese Oxide Absorber Coatings for Concentrating Solar Power

The solar absorptance of a thermal receiver surface significantly affects the photothermal conversion efficiency of concentrating solar power (CSP) plants. The stability of solar receivers and coatings applied to improve solar absorptance at high temperatures is critical for efficient and long-term operation. This study analyzes the high-temperature air stability of multiscale fractal textured electrodeposited copper manganese oxide and copper cobalt oxide solar receiver coatings over a range of temperatures. The study also investigates the effect of high temperature on phase stability, chemical and morphological evolution, and the optical properties of the two solar absorber materials. A computational model is developed to determine the absorptance of the textured absorbers and is shown to match the experimental measurements closely over a range of heat treatment temperatures from 450 °C to 850 °C and durations up to 100 h. Degradation curves and coating stability maps are developed from the study. Copper manganese oxide and copper cobalt oxide coatings exhibit good thermal stability up to ~815 °C and 630 °C, respectively, with minimal changes in their optical and structural properties with thermal efficiency greater than 90%. Furthermore, the study offers valuable insights into the high-temperature annealing effects on the optical and structural properties of multiscale copper alloyed coatings fabricated by electrodeposition and presents a means of designing the optimal temperature range for maximizing absorber efficiency in practical applications.

14 SOLAR ENERGY↗

Behavior of plasma-sprayed coatings

The microstructural development of plasma sprayed oxide coatings is described with particualr reference to aluminum oxide coatings and thermal barrier coatings of yttria stabilized zirconia (YSZ). The microstructural features of these coatings, observed by optical and electron microscopy, are related to their mechanical behavior. The adhesion of the coatings is also investigated using fracture toughness and tensile tests. It is noted that acoustic emission is valuable in formulating possible fracture mechanisms for YSZ coatings.

Berndt, Christopher C.↗

Functionalized carbon nanotubes for thermionic emission and cooling applications

Barium strontium oxide-coated carbon nanotubes (CNTs) were implemented as a work function lowering and field enhancing functional coating on a coiled tungsten filament to create a new thermionic cathode. This cathode resembles conventional oxide cathodes in structure. It has the same coiled tungsten filament as a conventional oxide cathode but uses barium strontium oxide-coated CNTs instead of the traditional barium strontium calcium oxide powder mixture as an emissive coating. The cathode produces a strong thermionic emission. At 1395 K and 2.5 V/μm, the thermionic emission current of 0.87 A or current density of 2.9 A/cm 2 was obtained from this oxide-coated CNT cathode. This level of emission is about three times as large as a conventional oxide cathode operating at similar temperature and field strength. Strong thermionic emissions from the cathode also lead to a large thermionic cooling effect. Temperature reduction as large as 90° was observed from the cathode surface when it was emitting electrons. Strong thermionic emission and a large cooling effect obtained are the result of the combination of the low work function of barium strontium oxide (1.6 eV) and the large field effect induced by the CNTs. Plasma enhanced chemical vapor deposition was used to grow CNTs, and magnetron sputtering deposition was used to deposit the barium strontium oxide functional coating; details of the cathode fabrication are presented to illustrate both the versatility of the processing techniques and the adaptability of barium strontium oxide-coated CNTs as a functional coating. Finally, measurements on thermionic emission and thermionic cooling of the cathode are also presented.

36 MATERIALS SCIENCE↗

Varying Processing Parameters in the Development of Slurry-Based Oxide Bond Coat for Environmental Barrier Coatings

Silicon carbide (SiC)-based ceramic matrix composites (CMCs) are replacing nickel-base superalloys in some hot-section aircraft engine materials due to their lower density and higher working temperature. CMCs require an environmental barrier coating (EBC) for protection from corrosive combustion species. Current-generation EBCs consist of a rare earth silicate topcoat and a silicon bond coat; however, the relatively low melting point of silicon (1414°C) limits the upper use temperature of these coatings. To extend the capability of next-generation EBCs, an oxide-based bond coat capable of withstanding temperatures of up to 1480°C has been developed at NASA Glenn Research Center. In this study, the oxide-based bond coat was applied to monolithic SiC via a slurry coating process. Parameters including slurry particle size and viscosity were varied, and coating performance was evaluated after steam cycling at 1480°C. The effect of including different rare earth constituents in the bond coat was also explored.

R. I. Webster↗

Start-stop testing of two self-acting air-lubricated spiral groove thrust bearing coatings

Start-stop tests were conducted on air-lubricated spiral-groove thrust bearings. Application of a matrix-bonded molybdenum disulfide (MoS2) coating over a porous chrome oxide coating resulted in significantly lower friction, compared to bearings coated with chrome oxide only. The MoS2 coated bearing sustained 15,000 start-stop cycles at a maximum of 3600 rpm. Each cycle was 15 seconds on, 30 seconds off. The chrome oxide coated bearing failed by local welding after 2030 cycles. Both types of coatings exhibited early failures under higher thrust loads when operating films were insufficient to sustain the load without overheating.

Dunfee, J. D.↗

Effect of bond coat creep and oxidation on TBC integrity

The potential of thermal barrier coatings (TBCs) on high-pressure turbine (HPT) nozzles and blades is limited at present by the inability to quantitatively predict TBC life for these components. The goal is to isolate the major TBC failure mechanisms, which is part of the larger program aimed at developing TBC life prediction models. Based on the results of experiments to isolate TBC failure mechanisms, the effects of bond coat oxidation and bond coat creep on TBC integrity is discussed. In bond coat oxidation experiments, Rene prime 80 specimens coated with a NiCrAlY/ZrO2-8 percent Y2O3 TBC received isothermal pre-exposures at 2000 F in static argon, static air, or received no pre-exposure. The effects of oxidation due to the pre-exposures were determined by thermal cycle tests in both static air and static argon at 2000 F. To study the effect of bond coat creep on TBS behavior, four bond coats with different creep properties were evaluated by thermal cycle tests in air at 2000 F. The test results, the relative importance of these two failure mechanisms, and how their effects may be quantified will also be discussed.

Duderstadt, E. C.↗