At least 91 records · Page 5

Effect of Stitching on Debonding in Composite Structural Elements

Stitched multiaxial warp knit materials have been suggested as viable alternatives to laminated prepreg materials for large aircraft structures such as wing skins. Analyses have been developed to quantify the effectiveness of stitching for reducing strain energy release rates in skin-stiffener debond, lap joint and sandwich debond configurations. Strain energy release rates were computed using the virtual crack closure technique. In all configurations, the stitches were shown to significantly reduce the strain energy release rate.

Raju, I. S.↗

Microfabrication of a High-Throughput Nanochannel Delivery/Filtration System

A microfabrication process is proposed to produce a nanopore membrane for continuous passive drug release to maintain constant drug concentrations in the patient s blood throughout the delivery period. Based on silicon microfabrication technology, the dimensions of the nanochannel area, as well as microchannel area, can be precisely controlled, thus providing a steady, constant drug release rate within an extended time period. The multilayered nanochannel structures extend the limit of release rate range of a single-layer nanochannel system, and allow a wide range of pre-defined porosity to achieve any arbitrary drug release rate using any preferred nanochannel size. This membrane system could also be applied to molecular filtration or isolation. In this case, the nanochannel length can be reduced to the nanofabrication limit, i.e., 10s of nm. The nanochannel delivery system membrane is composed of a sandwich of a thin top layer, the horizontal nanochannels, and a thicker bottom wafer. The thin top layer houses an array of microchannels that offers the inlet port for diffusing molecules. It also works as a lid for the nanochannels by providing the channels a top surface. The nanochannels are fabricated by a sacrificial layer technique that obtains smooth surfaces and precisely controlled dimensions. The structure of this nanopore membrane is optimized to yield high mechanical strength and high throughput.

Ferrari, Mauro↗

A Novel Method for Characterizing Fatigue Delamination Growth Under Mode I Using the Double Cantilever Beam Specimen

A novel method is proposed to obtain Mode I delamination growth rate from a Double Cantilever Beam (DCB) specimen. In the proposed method, Unidirectional (UD) DCB specimens are tested in fatigue at different initial maximum energy release rates levels. The growth rate data obtained in the first increments of crack growth at each maximum energy release rate level are used to generate a Paris Law equation, which characterizes delamination growth rate without fiber-bridging, and can also be used to determine a delamination onset curve. The remaining delamination growth rate data from each test are used to determine a modified Paris law, which characterizes the delamination growth rate in a DCB specimen, explicitly accounting for fiber-bridging. The proposed expression captures well the scatter in experimental data obtained using the DCB specimens, suggesting its adequacy. The Paris Law characterizing delamination growth rate without fiber-bridging predicts higher delamination growth rates for the same maximum energy release rate applied, leading to a conservative estimate for delamination growth. This is particularly relevant, since in generic ply interfaces, fiber-bridging is less predominant than in UD DCB specimens. Failing to account for fiber-bridging in UD DCB specimens may underestimate the delamination growth rate, yielding non-conservative predictions.

Carvalho, Nelson↗

Calculation of Stress Intensity Factors for Interfacial Cracks in Fiber Metal Laminates

Stress intensity factors for interfacial cracks in Fiber Metal Laminates (FML) are computed by using the displacement ratio method recently developed by Sun and Qian (1997, Int. J. Solids. Struct. 34, 2595-2609). Various FML configurations with single and multiple delaminations subjected to different loading conditions are investigated. The displacement ratio method requires the total energy release rate, bimaterial parameters, and relative crack surface displacements as input. Details of generating the energy release rates, defining bimaterial parameters with anisotropic elasticity, and selecting proper crack surface locations for obtaining relative crack surface displacements are discussed in the paper. Even though the individual energy release rates are nonconvergent, mesh-size-independent stress intensity factors can be obtained. This study also finds that the selection of reference length can affect the magnitudes and the mode mixity angles of the stress intensity factors; thus, it is important to report the reference length used with the calculated stress intensity factors.

Wang, John T.↗

Dissolution kinetics of iron-, manganese-, and copper-containing synthetic hydroxyapatites

Micronutrient-substituted synthetic hydroxyapatite (SHA) is being evaluated by the National Aeronautics and Space Administration's (NASA) Advanced Life Support (ALS) Program for crop production on long-duration human missions to the International Space Station or for future Lunar or Martian outposts. The stirred-flow technique was utilized to characterize Ca, P, Fe, Mn, and Cu release characteristics from Fe-, Mn-, and Cu-containing SHA in deionized (DI) water, citric acid, and diethylene-triamine-pentaacetic acid (DTPA). Initially, Ca and P release rates decreased rapidly with time and were controlled by a non-SHA calcium phosphate phase(s) with low Ca/P solution molar ratios (0.91-1.51) relative to solid SHA ratios (1.56-1.64). At later times, Ca/P solution molar ratios (1.47-1.79) were near solid SHA ratios and release rates decreased slowly indicating that SHA controlled Ca and P release. Substituted SHA materials had faster dissolution rates relative to unsubstituted SHA. The initial metal release rate order was Mn >> Cu > Fe which followed metal-oxide/phosphate solubility suggesting that poorly crystalline metal-oxides/phosphates were dominating metal release. Similar metal release rates for all substituted SHA (approximately 0.01 cmol kg-1 min-1) at the end of the DTPA experiment indicated that SHA dissolution was supplying the metals into solution and that poorly crystalline metal-oxide/phosphates were not controlling metal release. Results indicate that non-SHA Ca-phosphate phases and poorly crystalline metal-oxide/phosphates will contribute Ca, P, and metals. After these phases have dissolved, substituted SHA will be the source of Ca, P, and metals for plants.

NASA Discipline Life Support Systems↗

Delamination growth analysis in quasi-isotropic laminates under loads simulating low-velocity impact

A geometrically nonlinear finite-element analysis has been developed to calculate the strain energy released by delaminating plates during impact loading. Only the first mode of deformation, which is equivalent to static deflection, was treated. Both the impact loading and delamination in the plate were assumed to be axisymmetric. The strain energy release rate in peeling, GI, and shear sliding, GII, modes were calculated using the fracture mechanics crack closure technique. Energy release rates for various delamination sizes and locations and for various plate configurations and materials were compared. The analysis indicated that shear sliding was the primary mode of delamination growth. The analysis also indicated that the midplane (maximum transverse shear stress plane) delamination was more critical and would grow first before any other delamination of the same size near the midplane region. The delamination growth rate was higher (neutrally stable) for a low toughness (brittle) matrix and slower (stable) for high toughness matrix. The energy release rate in the peeling mode, GI, for a near-surface delamination can be as high as 0.5GII, and can contribute significantly to the delamination growth.

Shivakumar, K. N.↗

An analytical investigation of delamination front curvature in double cantilever beam specimens

An analytical investigation is conducted to determine the shape of a growing delamination and the distribution of the energy release rate along the delamination front in a laminated composite double cantilever beam specimen. Distributions of the energy release rate for specimens with straight delamination fronts and delamination front contours for delaminations whose growth is governed by the fracture criterion that G = Gc at all points are predicted as a function of material properties and delamination length. The predicted delamination front contours are utilized to ascertain the effect of the changing shape of the delamination front on the value of the critical strain energy release rate as computed from double cantilever beam fracture toughness test data.

Davidson, B. D.↗

Review of Combustion-acoustic Instabilities

Combustion-acoustic instabilities occur when the acoustic energy increase due to the unsteady heat release of the flame is greater than the losses of acoustic energy from the system. The problem of combustion-acoustic instability is a concern in many devices for various reasons, as each device may have a unique mechanism causing unsteady heat release rates and many have unique boundary conditions. To accurately predict and quantify combustion-acoustic stabilities, the unsteady heat release rate and boundary conditions need to be accurately determined. The present review brings together work performed on a variety of practical combustion devices. Many theoretical and experimental investigations of the unsteady heat release rate have been performed, some based on perturbations in the fuel delivery system particularly for rocket instabilities, while others are based on hydrodynamic processes as in ramjet dump combustors. The boundary conditions for rocket engines have been analyzed and measured extensively. However, less work has been done to measure acoustic boundary conditions in many other combustion systems.

Oyediran, Ayo↗

Delamination growth analysis in quasi-isotropic laminates under loads simulating low-velocity impact

A geometrically nonlinear finite-element analysis was developed to calculate the strain energy released by delamination plates during impact loading. Only the first mode of deformation, which is equivalent to static deflection, was treated. Both the impact loading and delamination in the plate were assumed to be axisymmetric. The strain energy release rate in peeling, G sub I, and shear sliding, G sub II, modes were calculated using the fracture mechanics crack closure technique. Energy release rates for various delamination sizes and locations and for various plate configurations and materials were compared. The analysis indicated that shear sliding (G sub II) was the primary mode of delamination growth. The analysis also indicated that the midplane (maximum transverse shear stress plane) delamination was more critical and would grow before any other delamination of the same size near the midplane region. The delamination growth rate was higher (neutrally stable) for a low toughness (brittle) matrix and slower (stable) for high toughness matrix. The energy release rate in the peeling mode, G sub I, for a near-surface delamination can be as high as 0.5G sub II and can contribute significantly to the delamination growth.

Shivakumar, K. N.↗

Influence of 2D Finite Element Modeling Assumptions on Debonding Prediction for Composite Skin-stiffener Specimens Subjected to Tension and Bending

The influence of two-dimensional finite element modeling assumptions on the debonding prediction for skin-stiffener specimens was investigated. Geometrically nonlinear finite element analyses using two-dimensional plane-stress and plane strain elements as well as three different generalized plane strain type approaches were performed. The computed deflections, skin and flange strains, transverse tensile stresses and energy release rates were compared to results obtained from three-dimensional simulations. The study showed that for strains and energy release rate computations the generalized plane strain assumptions yielded results closest to the full three-dimensional analysis. For computed transverse tensile stresses the plane stress assumption gave the best agreement. Based on this study it is recommended that results from plane stress and plane strain models be used as upper and lower bounds. The results from generalized plane strain models fall between the results obtained from plane stress and plane strain models. Two-dimensional models may also be used to qualitatively evaluate the stress distribution in a ply and the variation of energy release rates and mixed mode ratios with lamination length. For more accurate predictions, however, a three-dimensional analysis is required.

Krueger, Ronald↗

Comparison of 2D Finite Element Modeling Assumptions with Results From 3D Analysis for Composite Skin-Stiffener Debonding

The influence of two-dimensional finite element modeling assumptions on the debonding prediction for skin-stiffener specimens was investigated. Geometrically nonlinear finite element analyses using two-dimensional plane-stress and plane-strain elements as well as three different generalized plane strain type approaches were performed. The computed skin and flange strains, transverse tensile stresses and energy release rates were compared to results obtained from three-dimensional simulations. The study showed that for strains and energy release rate computations the generalized plane strain assumptions yielded results closest to the full three-dimensional analysis. For computed transverse tensile stresses the plane stress assumption gave the best agreement. Based on this study it is recommended that results from plane stress and plane strain models be used as upper and lower bounds. The results from generalized plane strain models fall between the results obtained from plane stress and plane strain models. Two-dimensional models may also be used to qualitatively evaluate the stress distribution in a ply and the variation of energy release rates and mixed mode ratios with delamination length. For more accurate predictions, however, a three-dimensional analysis is required.

Krueger, Ronald↗

Interlaminar fracture toughness: Three-dimensional finite element modeling for end-notch and mixed-mode flexure

A computational procedure is described for evaluating End-Notch-Flexure (ENF) and Mixed-Mode-Flexure (MMF) interlaminar fracture toughness in unidirectional fiber composites. The procedure consists of a three-dimensional finite element analysis in conjunction with the strain energy release rate concept and with composite micromechanics. The procedure is used to analyze select cases of ENF and MMF. The strain energy release rate predicted by this procedure is in good agreement with limited experimental data. The procedure is used to identify significant parameters associated with interlaminar fracture toughness. It is also used to determine the critical strain energy release rate and its attendant crack length in ENF and/or MMF. This computational procedure has considerable versatility/generality and provides extensive information about interlaminar fracture toughness in fiber composites.

Murthy, P. L. N.↗

An analytical and experimental investigation of edge delamination in laminates subjected to tension, bending, and torsion

An integrated two-dimensional finite element was developed to calculate interlaminar stresses and strain energy release rates for the study of delamination in composite laminates subjected to uniaxial tension, bending, and torsion loads. Addressed are the formulation, implementation, and verification of the model. Parametric studies were conducted on the effect of Poisson's ratio mismatch between plies and the stacking sequence on interlaminar stress, and on the effect of delamination opening height and delamination length, due to bending, on strain energy release rate for various laminates. A comparison of strain energy release rates in all-graphite and graphite/glass hybrid laminates is included. The preliminary results of laminates subjected to torsion are also included. Fatigue tension tests were conducted on Mode 1 and mixed mode edge-delamination coupons to establish the relationship between fatigue load vs. onset of delamination cycle. The effect on the fatigue delamination onset of different frequencies (1 and 5 Hz) was investigated for glass, graphite,and their hybrid laminates. Although a 20 percent increase in the static onset-of-delamination strength and a 10 percent increase in ultimate strength resulted from hybridizing the all-graphite laminate with a 90 deg glass ply, the fatigue onset is lower in the hybrid laminate than in the all-graphite laminate.

Chan, Wen S.↗

Crack Development in Cross-Ply Laminates Under Uniaxial Tension

This study addresses matrix-dominated failures in carbon fiber/polymer matrix composite laminates in a cross-ply lay-up. The events of interest are interlaminar fracture in the form of transverse cracks in the 90' plies and longitudinal splitting in the 0 deg plies and interlaminar fracture in the form of 0/90 delamination. These events were observed using various nondestructive evaluation (NDE) techniques during static tensile tests. Acoustic emission (AE) x radiography, and edge view microscopy were the principal ones utilized in a real-time environment. A comparison of the NDE results with an analytical model based on the classical linear fracture mechanics concept of strain energy release rate as a criterion for crack growth was performed. The virtual crack closure theory was incorporated with a finite element model to generate strain energy release rate curves for the analytical case. Celion carbon fiber/polyimide matrix (G30-500/PMR-15) was the material tested with cross-ply lay-ups of (0(2)/90(6))s and (0(4)/90(4))s. The test specimens contained thermally induced cracks caused by the high-temperature processing. The analytical model was updated to compensate for the initial damage and to study further accumulation by taking into account the crack interactions. By correlating the experimental and analytical data, the critical energy release rates were found for the observable events of interest.

Gyekenyesi, Andrew L.↗

A study on the thermal and moisture influences on the free-edge delamination of laminated composites

A simple delamination analysis method is presented here. It is based on a shear-type deformation theory and includes hygrothermal effects. These environmental conditions are applied to the strain energy release rate and interlaminar shear stresses. The method is applied to mixed mode edge delamination specimens made of T300/5208 graphite/epoxy material. Residual thermal and moisture stresses significantly influenced the strain energy release rate and interlaminar stresses. Both experienced large increases when thermal conditions were added to the mechanical strains. These effects were alleviated when moisture stresses were included. Thermal effects on the interlaminar shear stress and total energy release rate were totally alleviated for the same specific moisture content. Moreover, the value of the moisture content was not significantly affected by the stacking sequence for the laminates considered.

Mahler, Mary A.↗

An Investigation on the Accuracy of Delamination Analysis Predictions for Unidirectional Laminate Configurations

The state-of-the-art methodologies for predicting delamination growth in composite laminates make use of the concept of mixed-mode fracture mechanics. In mixed-mode fracture approaches the individual Mode I, Mode II and Mode III components of the strain energy release rate (SERR) need to be determined under general loading conditions. Through the use of mixed-mode fracture, the individual components are used in combination with the critical strain energy release rates (interlaminar fracture toughnesses) for each fracture mode in a mixed mode criterion in order to predict delamination extension. These interlaminar fracture toughnesses are traditionally obtained by testing of unidirectional laminate coupons. This work presents an investigation on the accuracy of Double Cantilever Beam (DCB), End Notch Flexure (ENF) and Mixed-Mode Bending (MMB) delamination analysis predictions by comparing measured total strain-energy release rates obtained experimentally to results for structural analysis from closed-form expressions, shell finite element analysis, and continuum two-dimensional (2D) and three-dimensional (3D) (solid) finite element analysis.

Patrick Enjuto↗

Repeatability of mixed-mode adhesive debonding

The repeatability of debond growth rates in adhesively bonded subjected to constant-amplitude cyclic loading was studied. Debond growth rates were compared from two sets of cracked-lap-shear specimens that were fabricated by two different manufacturers and tested in different laboratories. The fabrication method and testing procedures were identical for both sets of specimens. The specimens consisted of aluminum adherends bonded with FM-73 adhesive. Critical values of strain-energy-release rate were also determined from specimens that were monotonically loaded to failure. The test results showed that the debond growth rates for the two sets of specimens were within a scatter band which is similar to that observed in fatigue crack growth in metals. Cyclic debonding occurred at strain-energy-release rates that were more than an order of magnitude less than the critical strain-energy-release rate in static tests.

Everett, R. A., Jr.↗

Repeatability of mixed-mode adhesive debonding

The repeatability of debond growth rates in adhesively bonded subjected to constant-amplitude cyclic loading was studied. Debond growth rates were compared from two sets of cracked-lap-shear specimens that were fabricated by two different manufacturers and tested in different laboratories. The fabrication method and testing procedures were identical or both sets of specimens. The specimens consisted of aluminum adherends bonded with FM-73 adhesive. Critical values of strain-energy-release rate were also determined from specimens that were monotonically loaded to failure. The test results showed that the debond growth rates for the two sets of specimens were within a scatter band which is similar to that observed in fatigue crack growth in metals. Cyclic debonding occurred at strain-energy-release rates that were more than an order of magnitude less than the critical strain-energy-release rate in static tests.

Everett, R. A., Jr.↗