Search NASA⌕ Search

SEARCH · Search NASA

Results for “solution coating”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Synthesis of Porous Tungsten from Tungsten–Cadmium Film Coatings

Solid solutions (alloys) with a Cd concentration of 50.3–76.3 at % were synthesized for the first time in the form of coatings by ion–plasma sputtering and codeposition of ultrafine W and Cd particles. When coatings were formed by tungsten and cadmium nanolayers, the components dissolved mutually to produce solid solutions of one metal in the other. A solid solution of cadmium in tungsten was synthesized at Cd concentrations up to 60.9 at %. At a cadmium concentration of 68.6 at % in the coating, the crystalline structure of cadmium with an admixture of amorphous tungsten was produced. At 800°C, tungsten evaporated from tungsten–cadmium coatings to form porous tungsten. The results of examination of materials fabricated on the basis of porous tungsten are planned to be used in practice.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Effects of Aging on the Luminescence of PEG-Coated Water-Soluble ZnO Nanoparticles Solutions

Water-soluble ZnOnanoparticles coated with polyethylene glycol biscarboxymethyl (PEG(COOH)2)were prepared in ethanol/water solutions. The ZnOnanoparticles have a hexagonal structure with an average size of 10 nm. Three different luminescence bands are observed from the nanoparticle solutions: green emission at 530 nm from surface states or defects, UV emission at 380 nm from the ZnOexcitons, and an emission band at around 338 nm from the PEG(COOH)2. The fresh as-prepared samples have very strong green emission at 530 nm from surface states or defects but very weak excitonic emission at 380 nm. After dilution with ethanol, the green emission decreases in intensity and the excitonic emission increases. In the diluted samples, the excitonic luminescence intensity increases with storage time. This intensity increase is attributed to surface passivation by CH3COO-ligands resulting from precursor reactions in the ethanol solvent.

36 MATERIALS SCIENCE↗

Tuning Organic Semiconductor Packing and Morphology through Non-equilibrium Solution Processing (Final Report)

Organic semiconductors (OSCs) are a promising candidate to produce low-cost, large area, and flexible electronics. There has previously been successful development of organic field effect transistors (OFETs), photovoltaics (OPV), and bioelectronics using OSCs. Solution processing of these materials allows for the fabrication of large-area devices in the kinetic crystallization regime. The charge transport capabilities have been shown to depend on the morphology and molecular packing of the OSC within thin films. Our hypothesis is that solution processing conditions may significantly impact OSC morphology and as a result the charge transport. Therefore, this work has focused on obtaining a fundamental understanding of the morphology and molecular packing of OSCs for optimal device performance. Through our work, we have gained a better understanding of how these structural conditions were influenced by the solution processing conditions. Our studies have led to a more systematic understanding of the various parameters that impact OSC morphology. Solution processing leads to non-equilibrium films, thus allowing for the formation of diverse morphologies that are inaccessible by other fabrication methods. Previously, our group has focused on tuning the morphology of small-molecular OSCs [53, 55-57]. However, little work had been devoted to polymer OSCs. There was a lack of detailed studies characterizing the solution-state of polymer OSCs in terms of their conformation, degree of entanglement, polymer aggregation, and chain relaxation dynamics. The solution state properties are also likely to be influenced by the rigidity and molecular weight of the polymer OSCs investigated. Thus, we have focused our attention on gaining a better insight of polymer OSC films and solution processing methods. Through this proposal, our approach is to investigate the correlation between solution-state properties and the morphology of the resulting polymer OSC films. We worked three specific aims: investigate the effects of 1) polymer OSC solution-state properties on final film morphology; 2) molecular additives on the solution-state and final film properties; 3) controlled pre-aggregation in the solution-state in the final film morphology. More rigid and planar polymer backbones should promote interchain charge transport and more efficient interchain hopping between polymer chains. Through tailoring the polymer backbone, polymer sidechains, and molecular weight, we expected the altered solution-state properties to affect the final film morphology. In addition, reducing the entanglements and promoting chain alignment will likely prevent charge carrier trapping through conformation disorders. We thus studied different mechanisms, such as molecular additives, to reduce entanglements in solution. Devices fabricated from these solutions were expected to have improved charge transport abilities. In addition to tailoring the solution-state characteristics of the polymer OSCs, we investigated the effect of solution processing methods on the molecular packing and morphology of polymer OSC films. Two main solution processing techniques, e.g., spin-coating and solution shearing, were employed to fabricate OFETs. Spin coating was employed to prepare OSC films, which produce isotropic films. This technique creates several parameters to tune such as spin coating speed, acceleration, and time. Additionally, our research group developed the solution shearing method, which consists of the solution initially sandwiched between two plates. By sliding the top plate, the solution front is exposed and drying begins. This technique allows for the creation of aligned large crystalline domains. Solution shearing consists of different processing parameters which can affect the final morphology, such as shearing speed, substrate temperature and temperature gradient, distance between both plates, and the tilt angle of the top plate. Due to the complexity of the polymer systems investigated, numerous techniques were employed to characterize the polymer OSC solution state and films. All the materials were characterized using the DOE supported synchrotron X-ray scattering facilities at the Stanford Synchrotron Radiation Lightsource (SSRL). Using grazing incidence X-ray scattering (GIXS) and Near Edge X-ray Absorption Fine Structure (NEXAFS) techniques, the crystalline structure and molecular orientations of the thin films were measured. Optical absorption (UV-Vis) spectroscopy was employed to determine the aggregation state in solution and films of the polymer systems. Polarized UV-Vis also allowed for the determination of the relative degree of polymer chain alignment for solution sheared films. Additionally, various other techniques were used to investigate other properties within the film, such as atomic force microscopy (AFM) and solution rheology. Finally, the device performance is quantified through the fabrication and characterization of OFETs, which will highlight the effects of morphology on charge transport.

36 MATERIALS SCIENCE↗

The growth of ubiquitous ZnO rods on PMMA-coated substrate by solution-immersion method at different annealing temperatures

In this work, solution-immersion method was used to grow ZnO rods on PMMA-coated substrate. For this purpose, 0.15 M of zinc nitrate hexahydrate (Zn(NO{sub 3}){sub 2}.6H{sub 2}O) and hexamethylenetetramine (C{sub 6}H{sub 12}N{sub 4}) were used to growth of ZnO films at different annealing temperatures (room temperature, 80, 100, 120 and 140 °C). The morphology of the films was investigated by Scanning Electron Microscope (SEM) and optical properties were studied by Ultraviolet (UV-Vis) Spectroscopy. SEM analysis showed ubiquitous growth of ZnO rods that became better aligned and more closely-packed as the annealing temperature increased. As the annealing temperature exceeds 100 °C, the rods tend to merge to adjacent particles and the UV absorption decreased for the sample at higher temperatures (120 °C and 140 °C). Good absorption and better orientation of ZnO was obtained for the sample annealed at 100 °C due to the film possess better distribution and these improved orientation of particles caused the light to be effectively scattered on the sample. Both surface morphology and UV was significantly affected by the change in annealing temperatures thus thermal effect played a dominant role in shaping and improving the orientation of ZnO rods on PMMA-coated and its UV absorption.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Plasma Electrolytic Oxidation Coatings on Pure Ti Substrate: Effects of Na{sub 3}PO{sub 4} Concentration on Morphology and Corrosion Behavior of Coatings in Ringer’s Physiological Solution

Plasma electrolytic oxidation has been used as a relatively new method for applying ceramic coatings having different features. In the present study, commercially pure titanium is used as substrate, and effects of trisodium phosphate electrolyte concentration on the microstructure, as well as corrosion behavior of the coating in Ringer’s physiological solution are investigated. The morphology and phase compositions of coatings were analyzed by using scanning electron microscopy (SEM) and x-ray diffraction patterns. The study on the corrosion behavior of samples in a Ringer’s physiological solution was carried out using open-circuit potential potentiodynamic polarization and electrochemical impedance spectroscopy. The results of electrochemical analysis proved that higher concentration of phosphate electrolyte leads to increase in the corrosion resistance of applied coatings. Accordingly, obtained results revealed that the optimum electrolyte concentration for the best corrosion behavior was 20 g L{sup −1}. Furthermore, SEM images and reduction in the dielectric breakdown potential indicated that increase in the electrolyte concentration leads to morphological improvement and smoothening of the surface.

36 MATERIALS SCIENCE↗

Effect of Time and Deposition Method on Quality of Phosphonic Acid Modifier Self-Assembled Monolayers on Indium Zinc Oxide

Phosphonic acid (PA) self-assembled monolayers (SAMs) are utilized at critical interfaces between transparent conductive oxides (TCO) and organic active layers in organic photovoltaic devices (OPVs). The effects of PA deposition method and time on the formation of close-packed, high-quality monolayers is investigated here for SAMs fabricated by solution deposition, micro-contact printing, and spray coating. The solution deposition isotherm for pentafluorinated benzylphosphonic acid (F5BnPA) on indium-doped zinc oxide (IZO) is studied using polarization modulation-infrared reflection-absorption spectroscopy (PM-IRRAS) at room temperature as a model PA/IZO system. Fast surface adsorption occurs within the first min; however, well-oriented high-quality SAMs are reached only after -48 h, presumably through a continual process of molecular adsorption/desorption and monolayer filling accompanied by molecular reorientation. Two other rapid, soak-free deposition techniques, micro-contact printing and spray coating, are also explored. SAM quality is compared for deposition of phenyl phosphonic acid (PPA), F13-octylphosphonic acid (F13OPA), and pentafluorinated benzyl phosphonic acid (F5BnPA) by solution deposition, micro-contact printing and spray coating using PM-IRRAS. In contrast to micro-contact printing and spray coating techniques, 48-168 h solution deposition at both room temperature and 70 degrees C result in contamination- and surface etch-free close-packed monolayers with good reproducibility. SAMs fabricated by micro-contact printing and spray coating are much less well ordered.

14 SOLAR ENERGY↗

Solar Thermoelectricity via Advanced Latent Heat Storage: A Cost-Effective Small-Scale CSP Application

We are developing a novel concentrating solar electricity-generating technology that is both modular and dispatchable. Solar ThermoElectricity via Advanced Latent heat Storage (STEALS) uses concentrated solar flux to generate high-temperature thermal energy, which directly converts to electricity via thermoelectric generators (TEGs), stored within a phase-change material (PCM) for electricity generation at a later time, or both allowing for simultaneous charging of the PCM and electricity generation. STEALS has inherent features that drive its cost-competitive scale to be much smaller than current commercial concentrating solar power (CSP) plants. Most obvious is modularity of the solid-state TEG, which favors smaller scales in the kilowatt range as compared to CSP steam turbines, which are minimally 50 MWe for commercial power plants. Here, we present techno-economic and market analyses that show STEALS can be a cost-effective electricity-generating technology with particular appeal to small-scale microgrid applications. We evaluated levelized cost of energy (LCOE) for STEALS and for a comparable photovoltaic (PV) system with battery storage. For STEALS, we estimated capital costs and the LCOE as functions of the type of PCM including the use of recycled aluminum alloys, and evaluated the cost tradeoffs between plasma spray coatings and solution-based boron coatings that are applied to the wetted surfaces of the PCM subsystem. We developed a probabilistic cost model that accounts for uncertainties in the cost and performance inputs to the LCOE estimation. Our probabilistic model estimated LCOE for a 100-kWe STEALS system that had 5 hours of thermal storage and 8-10 hours of total daily power generation. For these cases, the solar multiple for the heliostat field varied between 1.12 and 1.5. We identified microgrids as a likely market for the STEALS system. We characterized microgrid markets in terms of nominal power, dispatchability, geographic location, and customer type, and specified additional features for STEALS that are needed to meet the needs of this growing power market.

14 SOLAR ENERGY↗

Method for making nanoporous hydrophobic coatings

A simple coating method is used to form nanoporous hydrophobic films that can be used as optical coatings. The method uses evaporation-induced self-assembly of materials. The coating method starts with a homogeneous solution comprising a hydrophobic polymer and a surfactant polymer in a selective solvent. The solution is coated onto a substrate. The surfactant polymer forms micelles with the hydrophobic polymer residing in the particle core when the coating is dried. The surfactant polymer can be dissolved and selectively removed from the separated phases by washing with a polar solvent to form the nanoporous hydrophobic film.

36 MATERIALS SCIENCE↗

Development of quantum dot materials for infrared cameras (Final CRADA Report)

The aim of this project was to develop scalable methods to produce infrared (IR) mercury telluride (HgTe) colloidal quantum dot (CQD) thin films and demonstrate their utility in a proof-of-concept monolithic SWIR focal plane array (FPA). These objectives were accomplished by scaling up the HgTe CQD synthesis, characterizing physical and electrical properties of HgTe CQDs, evaluating solution-processed coating methods for quality and efficiency, and developing a process flow to integrate HgTe CQDs with commercial-off-the-shelf silicon CMOS readout circuits by solution-processed coating to produce monolithic FPAs. The FPA is the image sensor in an infrared imaging system responsible for detecting and processing reflected or emitted light into an infrared image of the scene under observation. The quality of the image is determined by the sensitivity and resolution of the image sensor in the system. Higher resolution IR FPAs enable higher throughput in manufacturing quality assurance, wider field of view for autonomous navigation, and longer range surveillance for defense.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Manipulation and statistical analysis of the fluid flow of polymer semiconductor solutions during meniscus-guided coating

Recent work in structure–processing relationships of polymer semiconductors have demonstrated the versatility and control of thin-film microstructure offered by meniscusguided coating (MGC) techniques. Here, we analyze the qualitative and quantitative aspects of solution shearing, a model MGC method, using coating blades augmented with arrays of pillars. The pillars induce local regions of high strain rates—both shear and extensional—not otherwise possible with unmodified blades, and we use fluid mechanical simulations to model and study a variety of pillar spacings and densities. We then perform a statistical analysis of 130 simulation variables to find correlations with three dependent variables of interest: thin-film degree of crystallinity and transistor field-effect mobilities for charge-transport parallel (Μ para ) and perpendicular (Μ perp ) to the coating direction. Our study suggests that simple fluid mechanical models can reproduce substantive correlations between the induced fluid flow and important performance metrics, providing a methodology for optimizing blade design.

36 MATERIALS SCIENCE↗

Electrochemical Properties of Commercially Pure Ti with TiB/TiB{sub 2} Coatings in Hanks’ Balanced Salt Solution

In this study, in order to evaluate the electrochemical performance of different titanium boride coatings created on the commercially pure titanium (CP-Ti), distinct electrochemical assays in Hanks’ balanced salt solution at 37 °C were conducted using pack cementation method. The results showed that the boriding at 900 and 1000 °C for 3 h creates the TiB whiskers and TiB whiskers/TiB{sub 2} dense layer on the top of the commercially pure titanium surface, respectively. It was also found that not only borides coating had good adhesion on the substrate, but also that improved the titanium hardness more than five times. Polarization plots clarified the passive behavior of borided specimens. Impedance spectroscopy tests indicated the acceptable corrosion behavior of the borided specimens in Hanks’ balanced salt solution. Mott–Schottky measurements indicated that the passive layers formed on the commercially pure titanium and the borided specimens had doped n-type semiconductor properties. Mott–Schottky measurements displayed that the donor density of the passive layers decreased with the rising time as well. Finally, because of better surface conditions to make a less defective and more protective passive layer, the borided specimen at 900 °C in comparison with the borided specimen at 1000 °C was shown to be the more suitable choice for bioimplant applications.

36 MATERIALS SCIENCE↗

Open-air plasma-assisted deposition of organosilicon coating for corrosion protection of AZ91D Mg alloy

As a corrosion barrier layer, open-air plasma-assisted organosilicon coating was applied on AZ91D Mg alloy. Organosilicon-coated AZ91D samples, prepared from two different plasma coating processes, were used for corrosion evaluation based on multistep electrochemical and H 2 collection measurements in 3.5 wt% sodium chloride (NaCl) solution. Some coated AZ91D samples were characterized with and without corrosion exposure in NaCl solution using electron microscopies and X-ray chemical analysis techniques. Further, the results indicate that the organosilicon coatings from open-air plasma processes are effective to delay the initiation of corrosion attack and also reduce the corrosion rate for AZ91D substrate. The corrosion attack was considered to develop after permeation of NaCl solution through the coating layer.

36 MATERIALS SCIENCE↗

Updated Solution for Stresses and Displacements in TRISO-coated Fuel Particles

A closed-form solution for stresses and displacements in TRISO-coated fuel particles of a high temperature reactor has been updated to enhance its application in fuel particle analysis. The modified solution is applied incrementally through irradiation, which allows the material properties and irradiation temperature to change with time. It also removes the restriction in the original solution that Poisson’s ratio in creep for the pyrocarbon layers be set to 0.5. It is presented in a manner that would enable its application to a system of any number of coating layers, not just the three layers of a TRISO-coated particle. The solution has been implemented in the PARFUME fuel performance code, where it has been demonstrated to perform efficiently in particle failure probability determinations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Understanding the high-temperature behavior and corrosion resistance of Cr-Nb coated cladding for BWRs

While Cr-coated Accident Tolerant Fuel has proven successful in Pressurized Water Reactors, its dissolution in high dissolved oxygen Boiling Water Reactor environments represents a major technological barrier. Here, this study presents a comprehensive evaluation of novel Cr-Nb alloys as a coating breakthrough solution for Accident Tolerant Fuel cladding in Boiling Water Reactors. We systematically investigated Physical Vapor Deposited Cr-Nb coatings with 13% and 24 at% Nb content on commercial Zr-based cladding through rigorous testing under both normal and accident conditions. Our results demonstrate Cr-Nb coatings remained completely intact during extended Boiling Water Reactor autoclave testing, while pure Cr coatings failed catastrophically due to oxide dissolution. Under Loss-of-Coolant Accident conditions at 1100°C, Cr-Nb coatings maintained protective capability for 45 min. At 800°C, the alloy coatings matched pure Cr's excellent corrosion resistance. Despite microstructural changes during prolonged high-temperature exposure, no coating delamination occurred, ensuring continued protection of the underlying Zr substrate. These findings establish Cr-Nb coatings as a viable Accident Tolerant Fuel solution for Boiling Water Reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of Ni Content on Double-Target Co-sputtered CrNiN Coatings

Double-target co-sputtered CrNiN coatings were deposited by DC-pulsed magnetron reactive sputtering. The nickel content increases from 0.7 to 5.0 at.% with the increased Ni target current from 0.10 to 0.40 A. The influence of Ni content on preferred orientation and properties of CrNiN coatings was investigated. The results show that the doped Ni enters CrN to form (Cr,Ni)N solid solution. CrNiN coatings are mainly composed of CrN phase and demonstrate CrN(111) preferred orientation. All the coatings present columnar growth pattern. And the less obvious the preferred orientation, the more intense competitive growth, the less sufficient the columnar growth, the finer the columnar crystal and the denser the microstructure. In spite of the most dense structure with finest grains, the hardness of CrNiN coating containing 0.7 at.% Ni is the lowest. The hardness is affected by multiple effects of preferred orientation, grain size, solid solution strengthening, morphology and stress, especially the intensity degree of preferred orientation.

36 MATERIALS SCIENCE↗