At least 91 records · Page 5

Demonstration of How Manufacturing Innovations Challenge Conventional Structural Design

For almost 100 years, commercial aircraft have been fabricated using riveted aluminum alloy structures. Aside from refining aircraft designs for better aerodynamic efficiency, improving alloy compositions, and automating assembly steps, fuselage construction remains largely unchanged today. The intent of the lightweight metallic fuselage prototype undertaken in NASA’s Advanced Air Transport Technology project was to demonstrate innovative forming and joining processes that advance the design paradigm, i.e. achieve high-rate manufacturing and reduce assembly time/costs. Over the past decade, researchers at NASA Langley Research Center have evaluated the potential to modify the flow forming process to produce near-net shaped cylinders, integrally stiffened along the cylinder axis, for space launch vehicles. The production of integral stiffeners in a formed aluminum cylinder, the size of the Space Shuttle external tank, replaced machined thick plate and welding steps to eliminate > 500,000 pounds of machining chips and ~ 0.5 miles of welds. The flow forming method, called the Integrally Stiffened Cylinder (ISC) process, was successfully demonstrated up to the 10-foot diameter scale, which laid the groundwork for the current investigation of metallic fuselage structures. Using the ISC process as the basis for the re-design of a metallic fuselage eliminates hundreds of thousands of holes and rivets, while significantly reducing assembly time and crack initiation sites in the integral structure. However, the ISC process is not currently configured to fabricate circumferential ring frames for carrying fuselage internal pressure loads. Consequently, a trade study was performed to assess existing and advanced manufacturing processes, including additive manufacturing, forming, and welding. The approach with the lowest barriers to success, while simultaneously improving manufacturing time and cost, was to use formed ring frame segments attached to the ISC via Refill Friction Stir Spot Welding (RFSSW). The RFSSW process is five times faster than drilling, reaming, and riveting and provides similar mechanical performance. Finishing the fuselage structure with conventional windows, floor beams, and floor panels can then be accomplished using incumbent assembly methods, thereby maximizing reuse of existing infrastructure for aircraft construction. Structural analyses were performed to assess and optimize the geometric variables of integrated skin and stiffener configurations. A cost benefit and manufacturing rate analysis was also performed to compare against the current state-of-the-art for single aisle transport class aircraft. The resulting structure offers a weight reduction that rivals current graphite-epoxy composite fuselage structures. The projected manufacturing rate is close to double current metallic fuselages and six times faster than current composite manufacturing practices. The damage tolerance properties of a monocoque fuselage structure have yet to be assessed, but past integral airframe structural work has exploited geometric features to blunt or turn cracks. This concept offers promise that integrated structures can meet stringent aircraft durability specifications. An important benefit is that such aluminum fuselage structures may be inspected and repaired using established practices and existing expertise. Finally, pursuit of advanced manufacturing processes for future aluminum fuselages minimizes waste and the structure is 100% recyclable at the end-of-life for maximum sustainability.

aluminum↗

Power arc welder touch-started with consumable electrode

Power arc welder formed as a hand-held welding gun touch-starts, retracts a consumable electrode to create the desired arc, and then commences feeding of the consumable electrode at the rate required to form the intended bead or spot. This device achieves uniform spot welds repeatedly.

Jeannette, J. C.↗

Making Superconducting Welds between Superconducting Wires

A technique for making superconducting joints between wires made of dissimilar superconducting metals has been devised. The technique is especially suitable for fabrication of superconducting circuits needed to support persistent electric currents in electromagnets in diverse cryogenic applications. Examples of such electromagnets include those in nuclear magnetic resonance (NMR) and magnetic resonance imaging (MRI) systems and in superconducting quantum interference devices (SQUIDs). Sometimes, it is desirable to fabricate different parts of a persistent-current-supporting superconducting loop from different metals. For example, a sensory coil in a SQUID might be made of Pb, a Pb/Sn alloy, or a Cu wire plated with Pb/Sn, while the connections to the sensory coil might be made via Nb or Nb/Ti wires. Conventional wire-bonding techniques, including resistance spot welding and pressed contact, are not workable because of large differences between the hardnesses and melting temperatures of the different metals. The present technique is not subject to this limitation. The present technique involves the use (1) of a cheap, miniature, easy-to-operate, capacitor-discharging welding apparatus that has an Nb or Nb/Ti tip and operates with a continuous local flow of gaseous helium and (2) preparation of a joint in a special spark-discharge welding geometry. In a typical application, a piece of Nb foil about 25 m thick is rolled to form a tube, into which is inserted a wire that one seeks to weld to the tube (see figure). The tube can be slightly crimped for mechanical stability. Then a spark weld is made by use of the aforementioned apparatus with energy and time settings chosen to melt a small section of the niobium foil. The energy setting corresponds to the setting of a voltage to which the capacitor is charged. In an experiment, the technique was used to weld an Nb foil to a copper wire coated with a Pb/Sn soft solder, which is superconducting. The joint was evaluated as part of a persistent-current circuit having an inductance of 1 mH. A current was induced in a loop, and no attenuation of the current after a time interval 1,000 s was discernible in a measurement having a fractional accuracy of 10(exp -4): This observation supports the conclusion that the weld had an electrical resistance <10(exp -10) omega.

Penanen, Konstantin I.↗

DEVELOPMENT OF A LIGHT-WEIGHT REGENERATIVELY COOLED THRUST CHAMBER WITH BRAZED RIBS AND BRAZED OUTER WIRE TRAP

Design and fabrication procedures are discussed of a brazed-ribtype thrust chamber fabricated from stainless steel or inconel for a Sooo-lb thrust 20: 1 expansion-area-ratio regeneratively cooled liquidpropellant rocket engine which is designated as the JPL 6K Engine and operates at a chamber pressure of 150 psia. Hydrazine is used as the fuel and regenerative coolant and nitrogen tetroxide as the oxidizer. The nozzle-throat diameter is 5.42 in. The thrust chamber consists of a sheet-metal gas-side liner with longitudinal ribs spotwelded and brazed to the outer surface. Wire is wrapped over the ribs circumferentially, spot-welded to the ribs, and brazed. The liner, ribs, and wire form the coolant-passage walls. There are three basic advantages to this type of thrust chamber: light weight, ease of fabrication, and comparatively low cost. The total dry weight of a thrust chamber of this type and size made of 347 stainless steel is 46.2 lb, and the wet weight is 56.3 Ib. A total of 87 static engine tests were made on 19 of 23 thrust chambers fabricated by this technique. Four of the chambers tested had an expansion-area ratio of 20:1, and 15, which were shorter but had the same throat diameter, had an expansion-area ratio of 3.5:l. Accumulated test time was 1926 sec, including 558 sec regenerative cooling with hydrazine and 1368 sec cooling with water. One 20:l thrust chamber was subjected to 16 separate engine tests, with an accumulated test time of 399 sec, and was still in very good operating condition after the tests were completed. With water flowing through the coolant passages at 10 lb/sec, the measured nominal pressure drop between coolant manifolds of a 20:l thrust chamber wrapped with flat wire was 17.2 psi.

Thrust Chamber↗

Micromanipulation tool is easily adapted to many uses

A special micromanipulation tool equipped with a plunger mounted in a small tube can be easily adapted to such work operations as cutting, precision clamping, and spot welding of microscopic filaments or other parts. This tool is valuable where extreme steadiness of high magnification is required.

Shlichta, P. J.↗

Development of dispersion-strengthened Ni-Cr-ThOz alloys for the space shuttle thermal protection system

Manufacturing processes were developed for TD-NiCr providing small sheet (45 x 90 cm), and larger sheet (60 x 150 cm) and foil. The alternate alloy, DS-NiCr, was produced by pack-chromizing Ni-ThO2 sheet. Formability criteria are being established for basic sheet forming processes, which are brake forming, corrugation forming, joggling, dimpling, and beading. Resistance spot welding (fusion and solid state), resistance seam welding, solid state diffusion welding, and brazing are included in the joining programs. Major emphasis is centered on an Al-modified Ni-Cr-ThO2 alloy development. These alloys, containing 3 to 5% Al, form the protective Al2O3 scale. This enhances oxidation resistance under reentry conditions. Both TD-NiCrAl and DS-NiCrAl alloys are included. A tentative composition of Ni-16Cr-3.5Al-2ThO2 was selected based on oxidation resistance and fabricability.

Blankenship, C. P.↗

Development of dispersion-strengthened Ni-Cr-ThO2 alloys for the space shuttle thermal protection system.

An improved manufacturing process has been developed for TD-NiCr that provides sheet of improved quality, better gage control, and reproducible properties. A standard manufacturing process has been developed for the alternate alloy, DS-NiCr, produced by pack-chromizing Ni-2ThO2 sheet. Extension of forming and joining technology for TD-NiCr is in process. Formability criteria are being established for basic sheet forming processes related to the manufacture of Shuttle TPS panels. They include brake forming, corrugation forming, joggling, dimpling, and beading. Joining processes applicable to TPS panels are being optimized with emphasis on establishment of joint efficiencies. Resistance spot welding (fusion and solid state), resistance seam welding, solid-state diffusion welding, and brazing are included in the joining programs. Development of improved manufacturing technology for TD-NiCr fasteners is also being accomplished. Mechanical and physical properties of TD-NiCr are being characterized to provide design-allowable data.

Blankenship, C. P.↗

Comparative cut-bar thermal conductivity apparatus.

Construction details, error analysis, and typical data for a rapid comparative device for thermal conductivity measurements are presented. The apparatus consists of a comparative cut-bar arrangement contained in a bell-jar. The cylinder shaped specimen is placed between two ARMCO-iron meter bars of the same diameter. The upper bar is equipped with a heater, while the lower one is terminated in a heat sink. The temperature gradient along the bars is measured with a series of copper/constantan microthermocouples, spot welded to them. The assembly is held together by loading the bars to a desired pressure, via a pneumatic cylinder. Contact resistance at the boundaries between the specimen and the meter bars is minimized by using a Hg/In/Ga alloy film at the interface and sufficient loading force. The gradients determined for the meter bars then may be extrapolated to the boundaries yielding the temperature drop along the specimen. Using two different length specimens, the magnitude of the temperature drop across the interface can be computed, or the true gradient along the specimen can be obtained from the difference in overall temperature drops and lengths.

Gaal, P. S.↗

Flat-band assembly for toroidal transformer cores

Toroidal transformer cores are often banded together by means of strap. Spot welds secure strap. Proper tension is obtained by use of special fixture in conjunction with winding of wire which is placed temporarily on core; winding is excited by dc current to hold core halves together magnetically during alignment.

Mclyman, W. T.↗

Results of aerodynamic heat transfer tests of a 0.0175-scale model of the Rockwell International Space Shuttle Orbiter 139 (model number 22-0) in the NASA/Ames 3.5-foot hypersonic wind tunnel (test OH6)

The results of a hypersonic wind tunnel test program conducted using a 0.0175 scale thin-skin thermocouple model of the Space Shuttle Orbiter to obtain aerodynamic heat transfer data on the Orbiter under simulated reentry conditions were presented. The test program was conducted at a Mach number of 7.3 and a freestream Reynolds number ranging between 1.0 and 6.0 million/foot. The model was tested for angles of attack ranging between 10 deg and 30 deg and a sideslip angle of 0 deg. The model was constructed of 15-5 PH stainless steel with the instrumented areas machined to a nominal skin thickness of 0.030 in. The model instrumentation consisted of 288 iron-constantan thermocouples spot welded to the skin inner surface, but only 75 of these were used in this test program. A high-speed, analog-to-digital data acquisition system was used to record data on magnetic tape.

Dye, W. H.↗

Adding through-bolt holes to pin-fin cold plates

Spot-welding technique is less expensive than secondary-brazing and electron-beam methods. With procedure, standard plates can be modified in quantity for various mounting configurations without need for special tooling.

Ruppe, E. P.↗

Industrial robots in Europe - market, applications and developments

Different companies involving a wide range of products and manufacturing processes were studied to define the requirements for industrial robots. A survey of all such automatic units offered on the world market was made to establish a data base. Principal applications include coating, spot welding, and loading and unloading operations.

Schraft, R. D.↗

Automated space fabrication of structural elements

A description is presented of an automated space fabrication technique for basic structural elements, taking into account as representative the design loads and requirements of the solar power satellite structure. Roll forming for continuous cap and brace members is applicable for all proposed metallic materials. Spot-welding, electron beam welding, ultrasonic welding, laser welding, cold welding, and various mechanical fastening techniques are applicable for the automated fabrication process. Termination of the formed cap and brace members can be accomplished by sawing, shearing, punching, and laser cutting. The most cost effective materials were found to be the aluminum alloys. Selected for further study were AL20224T3 and AL2219-T62. In the area of fiber composites, thermoplastic matrix materials with graphite fibers were selected for future studies.

Engler, E. E.↗

Giant-electrode welder

Welder produces spot-welds in place of rivets and saves time and money. Unit comprised of concical copper electrode base diameter of 11.5 ft is also capable of welding very thin, hard aluminum alloys.

Atkins, B. R.↗

Atlas 5013 tank corrosion test

The type and cause of corrosion in spot welded joints were determined by X-ray and chemical analysis. Fatigue and static tests showed the degree of degradation of mechanical properties. The corrosion inhibiting effectiveness of WD-40 compound and required renewal period by exposing typical joint specimens were examined.

Sutherland, W. M.↗

Adhesive-Bonded Tab Attaches Thermocouples to Titanium

Mechanical strength of titanium-alloy structures that support thermocouples is preserved by first spotwelding thermocouples to titanium tabs and then attaching tabs to titanium with a thermosetting adhesive. In contrast to spot welding, a technique previously used for thermocouples, fatigue strength of the titanium is unaffected by adhesive bonding. Technique is also gentler than soldering or attaching thermocouples with a tap screw.

Cook, C. F.↗