Search NASA⌕ Search

SEARCH · Search NASA

Results for “tungsten”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

The effect of Ni doping on the mechanical behavior of tungsten

The effect of nickel (Ni) on activated sintering of tungsten has been known and investigated for decades. However, there are few reports on the mechanical properties of tungsten when Ni is added as a low alloying additive with less than 1 wt%. In this work, the mechanical behaviors of tungsten doped with 0.2–1.0 wt% nickel from room temperature up to 400 °C were investigated. The results show that the compression ductility of as-sintered Ni doped tungsten is drastically higher than that of as-sintered pure tungsten at all tested temperatures including room temperature, and the fracture toughness at room temperature is increased by 92%. The results suggest that the ductile-to-brittle transition temperature (DBTT) of tungsten can be reduced substantially by doping with Ni.

36 MATERIALS SCIENCE↗

Processing of tungsten through electron beam melting

Additive manufacturing (AM) presents a new design paradigm for the manufacture of engineering materials through the layer-by-layer approach combined with welding theory. In the instance of difficult to process materials such as tungsten and other refractory metals, AM offers an opportunity for radical redesign of critical components for next-generation energy technologies including fusion. In this work, electron beam powder bed fusion (EB-PBF) is applied to process pure tungsten to study the influence of process parameters on the defect density of the material. Here, an in-situ image analysis algorithm is applied to pure tungsten for the first time, and is used to visualize the defect structure in AM tungsten. Finally, a cracking mechanism for AM tungsten is proposed, and suggestions for suppression of cracks in pure tungsten are offered.

36 MATERIALS SCIENCE↗

The effect of metastable atomic levels in neutral tungsten for erosion and impurity transport applications

Long-lived metastable states in neutral tungsten are shown to potentially impact measurements of tungsten erosion from plasma facing components. Time-dependent collisional radiative modeling of neutral tungsten is used to analyze the role of these states in tungsten emission and ionization. The large number of non-quasistatic atomic states in neutral tungsten can take on the order of milliseconds to reach equilibrium, depending on plasma conditions, causing erosion measurements to be affected by the metastable populations. Previous measurements using the 400.88 nm tungsten emission line could be affected by these non-quasistatic metastable effects. Therefore, a scheme for measuring the relative metastable fractions is proposed through simultaneous observation of multiple ultraviolet spectral lines of neutral W. The accuracy of gross erosion measurements could potentially be increased by inclusion of these previously unconsidered metastable effects.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Drift-kinetic effects of tungsten on plasma response to RMP in ITER

Here, effects of high- Z ( Z is the particle charge number) tungsten impurity ions on the plasma response to the resonant magnetic perturbation (RMP) field are numerically investigated for the ITER 15 MA baseline scenario, where the tungsten contribution to the plasma response is computed with a drift-kinetic model while the bulk thermal particle contributions follow the fluid approximation. The study yields three highlights: (i) the drift-kinetic contribution of the tungsten impurity exerts minor influence on the plasma response compared to that computed by the pure fluid model without tungsten; (ii) a new figure of merit, based on the resonant spectrum perturbation at the plasma boundary surface, results in different optimal coil phasing compared to that previously obtained by maximizing the edge-peeling plasma response; (iii) the optimal $n = 3$ RMP (for edge localized mode (ELM) control, $n$ is the toroidal mode number) is found to induce a large tungsten particle influx near the plasma edge associated with the neoclassical toroidal viscosity. The study thus provides useful data on the compatibility of the full tungsten wall with RMP ELM control in ITER.

ITER↗

Helium bubble size effects on the surface morphological response of plasma-facing tungsten

Abstract We report a simulation study on the effects of helium (He) bubble size on the morphological evolution and pattern formation on the surface of tungsten used as a plasma-facing component (PFC) in nuclear fusion devices. We have carried out a systematic investigation based on self-consistent dynamical simulations of surface morphological evolution according to an atomistically-informed, 3D continuum-scale model that captures well the relevant length and time scales of surface nanostructure formation in PFC tungsten. The model accounts for PFC surface diffusion, driven by the biaxial compressive stress originating from the over-pressurized He bubbles in the near-surface region of PFC tungsten as a result of He plasma exposure, combined with the formation of self-interstitial atoms in tungsten that diffuse toward the PFC surface and the flux of surface adatoms generated as a result of surface vacancy-adatom pair formation upon He implantation; this transport of surface adatoms contributes to the anisotropic growth of surface nanostructural features due to the different rates of adatom diffusion along and across step edges of islands on the tungsten surface. Our detailed analysis reveals that varying the average He bubble size plays an important role in the PFC surface growth kinetics as well as the resulting surface topography. Specifically, we find that an increase in the He bubble size leads to a deceleration in the growth rate of the tungsten nanotendrils that emanate from the PFC surface. We also find that the separation distance between the resulting surface features increases with increasing He bubble size, as well as over time. This coarsening effect is a thermally activated process resulting in an accurate description of the temperature dependence of the average surface feature separation by an Arrhenius relation.

36 MATERIALS SCIENCE↗

Effect of Tungsten L-PBF Feedstock Modification on Performance in Bending

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high ductile-to-brittle transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Tungsten-based alloys↗

Bending Performance of Tungsten Printed Via Laser Powder Bed Fusion With Ceramic Dispersion Modified Powder Feedstock

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high brittle-to-ductile transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability and strength. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Additive Manufacturing↗

Survey of tungsten gross erosion from main plasma facing components in WEST during a L-mode high fluence campaign

An initial high fluence campaign was performed in WEST, in 2023, on the newly installed actively cooled tungsten divertor composed of ITER-grade monoblocks. The campaign consisted in the repetition of a 60 s long Deuterium L-mode pulse in attached divertor conditions, cumulating over 10000s of plasma exposure. A maximum deuterium fluence of approximately 5⋅1⁢026 m−2 was reached in the outer strike point region, representative of a few high performance ITER pulses. Gross tungsten erosion inferred from visible spectroscopy shows that the most eroded plasma facing component is the inner divertor target with rates ten times larger than on the outer divertor target. The outer midplane tungsten bumpers, located a few centimeters from the plasma, show gross erosion rates two times lower than at the outer divertor. We conclude that the outer midplane bumpers have a negligible contribution to the long range tungsten migration and deposition onto the lower divertor. The cumulated gross erosion rate on the inner divertor translates in an effective gross erosion thickness of about 20μ⁢m, while it is about 2μ⁢m for the outer divertor. Strikingly, these orderings coincide with the thickness of deposits found locally on the divertor: the exposed surfaces of high field side monoblocks are covered with several tens of μ⁢m tungsten deposits, while on the lower field side, few μ⁢m thin tungsten deposits are only found on the magnetically shadowed parts of monoblocks. The strong impact of those deposits on WEST operation, namely perturbation of surface temperature measurement with infra-red thermography, and the emission of flakes causing radiative perturbation of the confined plasma, calls for anticipating similar issues in ITER. In particular, the start of research operation shall consider the definition of a divertor erosion budget in order to anticipate the formation of deleterious deposits.

Fedorczak, N.↗

Effects of transition metal carbide dispersoids on helium bubble formation in dispersion-strengthened tungsten

Abstract The formation of helium bubbles and subsequent property degradation poses a significant challenge to tungsten as a plasma-facing material in future long-pulse plasma-burning fusion reactors. In this study, we investigated helium bubble formation in dispersion-strengthened tungsten doped with transition metal carbides, including TaC, ZrC, and TiC. Of the three dispersoids, TaC exhibited the highest resistance to helium bubble formation, possibly due to the low vacancy mobility in the Group VB metal carbide and oxide phases. Under identical irradiation conditions, large helium bubbles formed at grain boundaries in tungsten, while no bubbles were observed at the interfaces between the carbide dispersoid and tungsten matrix. Moreover, our results showed the interfaces could suppress helium bubble formation in the nearby tungsten matrix, suggesting that the interfaces are more effective in trapping helium as tiny clusters. Our research provided new insights into optimizing the microstructure of dispersion-strengthened tungsten alloys to enhance their performance.

36 MATERIALS SCIENCE↗

Discovering tungsten-based composites as plasma facing materials for future high-duty cycle nuclear fusion reactors

Abstract Despite of excellent thermal properties and high sputtering resistance, pure tungsten cannot fully satisfy the requirements for plasma facing materials in future high-duty cycle nuclear fusion reactions due to the coupled extreme environments, including the high thermal loads, plasma exposure, and radiation damage. Here, we demonstrated that tungsten-based composite materials fabricated using spark-plasma sintering (SPS) present promising solutions to these challenges. Through the examination of two model systems, i.e., tungsten-zirconium composite for producing porous tungsten near the surface and dispersoid-strengthened tungsten, we discussed both the strengths and limitations of the SPS-fabricated materials. Our findings point towards the need for future studies aimed at optimizing the SPS process to achieve desired microstructures and effective control of oxygen impurities in the tungsten-based composite materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Hole formation effect on surface morphological response of plasma-facing tungsten

We report simulation results on the effect of helium (He) bubble bursting-mediated surface hole formation on the surface morphological response of tungsten plasma-facing components (PFCs) in nuclear fusion devices. Our analysis is based on an atomistically informed, continuum-scale model, which is capable of accessing the spatiotemporal scales relevant to the fuzz nanostructure formation process on the surface of PFC tungsten. Our simulations account, in an empirical fashion, for two types of subsurface bubble dynamical phenomena in the nanobubble region of PFC tungsten during He plasma irradiation, involving bubble bursting and surface crater formation. We demonstrate that the hole formation effect on the PFC tungsten surface accelerates the growth rate of nanotendrils and the onset of fuzz formation. As a result, the predicted incubation time for surface nanotendril growth is shortened, in agreement with experimental data of incubation fluence at comparable plasma exposure conditions. We also explore systematically the dependence of the PFC surface morphological response on the areal density of holes introduced at regular time intervals onto the He-implanted tungsten surface, a parameter in our analysis that serves as a proxy for the rate of He bubble bursting. More importantly, our simulations capture fine surface features in the PFC tungsten surface morphology and predict that the average spacing between nanotendrils is on the order of 100 nm, consistent with the experimental findings.

Chen, Chao-Shou (ORCID:0000000307910042)↗

The effect of ICRH and NBI on tungsten transport in neon edge radiation cooled discharges in TEXTOR

Tungsten is planned to be the plasma-facing material for the main chamber and divertor in future devices like ITER, SPARC, and DTT. To address risks associated with tungsten, R&D is being carried out on various toroidal confinement devices. One particular research question is related to the optimum heating mix for ITER. To investigate the influence of the heating scheme on the release and transport of tungsten, a comparison of neutral beam injection (NBI) and ion cyclotron resonance frequency (ICRF) heating was carried out in TEXTOR tungsten test limiter experiments. The experiments were performed under standard L-mode conditions and in radiative improved-mode operation with neon seeding and boronized walls covering the graphite plasma-facing components. The plasma was heated with hydrogen or deuterium NBI alone or with deuterium NBI in combination with H-minority, ion cyclotron resonance heating. A movable solid tungsten limiter was inserted through a limiter lock system into the edge plasma. The impurity release from this limiter was evaluated from visible spectroscopy. The tungsten concentrations in the plasma core were determined by extreme ultraviolet spectroscopy and bolometry. With deuterium NBI alone, strong central radiation and accumulation of W was observed. This can, however, be avoided by adding ICRF heating.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Weldability, strength, and high temperature stability of chemically vapor deposited tungsten

Three types of CVD tungsten (fluoride-produced, chloride-produced and the combination of the two which is termed duplex) were evaluated to determine their weldability, high temperature strength and structural stability during 5000 hour exposure to temperatures of 1540 C and 1700 C. Each type of CVD tungsten could be successfully electron beam welded but the results for the chloride product were not as satisfactory as those of the other two materials. The high temperature strength behavior of the three materials did not differ greatly. However a large difference was noted for the grain growth behavior of the two basic CVD tungsten materials. Fluoride tungsten was found to be relatively stable while for the most part the grain size of chloride tungsten increased appreciably. The examination of freshly fractured surfaces with a scanning electron microscope revealed numerous bubbles in the fluoride material following its exposure to 1700 C for 5000 hours. Less severe thermal treatments produced relatively few bubbles in this material. Only at certain locations within the chloride material associated with the interruption of tungsten were bubbles noted.

Bryant, W. A.↗

Rapid synthesis of phase-engineered tungsten carbide electrocatalysts via flash joule heating for high-current-density hydrogen evolution

Fabricating durable and high-performance electrocatalysts operating at high current densities for industrial acidic hydrogen evolution remains a daunting challenge. Tailoring the phase composition of electrocatalysts is a promising strategy to harness synergistic effects and improve charge transfer, thereby optimizing their performance. Here, this work presents a fast, green method based on flash joule heating (FJH) to synthesize phase-engineered tungsten carbide electrocatalysts for the acidic hydrogen evolution reaction (HER) at high current densities. Tungsten carbide electrodes with varying FJH treatment durations (3, 10, 30, and 60 s) are fabricated to fine-tune the mixture of tungsten monocarbide (WC) and tungsten semicarbide (W 2 C) phases. Results show that samples with a 30-s treatment (TC-3) exhibit an optimal balance between these phases, leading to a low overpotential of 180.97 and 387 mV at current densities of 10 mA/cm 2 and 4 A/cm 2 , respectively. TC-3 exhibits significantly lower charge transfer resistance compared to the other electrocatalysts, which can be attributed to its optimal phase ratio. Notably, the TC-3 electrocatalyst remains stable for over 9 days at 4 A/cm 2 due to their controlled phases and excellent corrosion-resistant properties. This work highlights a new method to fabricate cost-effective, high-performance tungsten carbide electrocatalysts with well-controlled phase compositions.

Acidic hydrogen evolution reaction↗

Irradiation effects in tungsten—From surface effects to bulk mechanical properties

Advanced materials such as tungsten fibre-reinforced composites allow to overcome severe weaknesses of the baseline materials for plasma-facing components — copper and tungsten. The effect of the fusion environment on the mechanical properties of these materials, e.g. the embrittlement by neutron irradiation, plays a key role for the development of future fusion reactors. To simulate this effect, high-energy ions are used as a substitute for the displacement damage by neutrons. We propose the use of very fine tungsten wire as a possibility of studying the influence of irradiation damage on the mechanical properties. This is possible as they allow full-depth irradiation of almost the entire volume despite the limited penetration depth of ions. Geometrical size effects are mitigated due to the nanoscale microstructure of the wire. In addition, similar wire is used in tungsten fibre-reinforced composites. Thus, the investigation of irradiated wire can directly be used for the prediction of the bulk composite properties. For the proof of this concept tungsten wire with a diameter of 16 μm was electrochemically thinned to 5 μm and irradiated with 20.5 MeV W 6+ ions. The mechanical properties were subsequently determined by macroscopic tensile testing. Irradiation to 0.3, 1 and 9 dpa did not lead to a change of the mechanical behaviour. Both strength and ductility, the latter indicated by the reduction of area, were similar to the as-fabricated state.

36 MATERIALS SCIENCE↗

Activation Analysis in Preparation for a Tungsten Irradiation Experiment at LANSCE

To organize the safe handling of activated material, knowing the residual dose rates is crucial. Here, in this work, we present the pre-experiment activation analysis for an experiment in which tungsten blocks are irradiated by 800-MeV protons. In this analysis, we use the Monte Carlo N-Particle (MCNP) code for radiation transport, Attila4MC for unstructured mesh generation, and Activation in Accelerator Radiation Environments (AARE), including CINDER2008, for activation analysis. If the tungsten blocks must be removed within a day after the experiment, then exposure to personnel entering the room must be reduced. One exposure-reduction strategy is to add carbon steel shielding around the tungsten blocks, efficiently reducing the dose from the activated tungsten. However, the shielding becomes activated itself during irradiation: 56Mn is the dominant contributor for short decay times. The actual schedule at the time of the experiment allowed sufficient cool-off time for the tungsten in the room so that additional shielding was not necessary. A less rigorous comparison of the calculated values with the post-experiment measurements showed reasonable agreement.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Simulations of stand-off runaway electron beam termination by tungsten particulates for tokamak disruption mitigation

Abstract Stand-off runaway electron termination by injected tungsten particulates offers a plausible option in the toolbox of disruption mitigation. Tungsten is an attractive material choice for this application due to large electron stopping power and high melting point. To assess the feasibility of this scheme, we simulate runaway collisions with tungsten particulates using the MCNP program for incident runaway energies ranging from 1 to 10 MeV. We assess runaway termination from energetics and collisional kinematics perspectives. Energetically, the simulations show that 99% of runaway beam energy is removed by tungsten particulates on a timescale of 4–9 µ s. Kinematically, the simulations show that 99% of runaways are terminated by absorption or backscattering on a timescale of 3–4 µ s. By either metric, the runaway beam is effectively terminated before the onset of particulate melting. Furthermore, the simulations show that secondary radiation emission by tungsten particulates does not significantly impact the runaway termination efficacy of this scheme. Secondary radiation is emitted at lower particle energies than the incident runaways and with a broad angular distribution such that the majority of secondary electrons emitted will not experience efficient runaway re-acceleration. Overall, the stand-off runaway termination scheme is a promising concept as a last line of defense against runaway damage in ITER, SPARC, and other future burning-plasma tokamaks.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Operational space for lower hybrid heating scenarios in the full tungsten environment of WEST

In tungsten—W—Environment in Steady-state Tokamak (WEST), the lower hybrid current drive (LHCD) system is key for achieving long pulse operation by providing most of the non-inductive plasma current, as well as a crucial source of electron heating. Therefore, determining the operational space for its application is fundamental. In the present study, the LHCD operational space is deeply analyzed for 0.5 MA pulses. This space is bounded by three limits: (i) the ratio of the LHCD power over density must be above a threshold to compensate tungsten radiation with enough core heating, (ii) the line-averaged density must be high enough to allow good coupling of the hybrid wave with the plasma, and (iii) fast electron ripple losses must be below a limit to avoid reaching a thermal threshold on plasma-facing components. If the tungsten radiation peak or burn-through phase is not safely overcome, a maximum electron temperature of 1.5 keV is obtained, confinement is degraded, and magnetohydrodynamic activity is frequently triggered, potentially causing a disruption. From experimental measurements and interpretative simulations, we highlight the main mechanisms that prevent the plasma from heating up during LHCD power ramp-up. Three parameters play a major role: plasma density, tungsten concentration and LHCD power deposition. A strategy to overcome this limitation is found: a precise density ramp-up performed simultaneously with the increase in LHCD power. Additionally, we show that boronization greatly facilitates the burn-through of tungsten by lowering its content during the heating phase. Finally, taking into account the three constraints given above, the LHCD operational space is determined at power ramp-up and during constant heating phases.

lower hybrid heating and current drive↗