At least 901 records · Page 50

Radiation-induced damage and evolution of defects in Mo

The formation of defects in bcc Mo lattice as a result of 50-keV Xe bombardment is studied via atomistic simulation with an interatomic potential developed using the force-matching ab initio based approach. The defect evolution in the cascade is described. Diffusion and interaction of interstitials and vacancies are analyzed. Only small interstitial atom clusters form directly in the cascade. Larger clusters grow only via aggregation at temperatures up to 2000 K. Stable forms of clusters demonstrate one-dimensional diffusion with a very high diffusion coefficient and escape quickly to the open surface. Point vacancies have much lower diffusivity and do not aggregate. The possibility of a large prismatic vacancy loop formation near the impact surface as a result of fast recrystallization is revealed. The mobility of the vacancy dislocation loop segments is high, however, the motion of the entire loops is strongly hindered by neighbor point defects. This paper explains the existence of the large prismatic vacancy loops and the absence of the interstitial loops in the recent experiments with ion irradiation of Mo foils.

36 MATERIALS SCIENCE↗

Crystallization Dynamics of a Single Layer Complex Plasma

We report a series of complex (dusty) plasma experiments, aimed at the study of the detailed time evolution of the recrystallization process following a rapid quench of a two-dimensional dust liquid. The experiments were accompanied by large-scale (million-particle) molecular dynamics simulations, assuming Yukawa-type interparticle interaction. Both experiment and simulation show a {proportional_to}t{sup {alpha}} (power-law) dependence of the linear crystallite domain size as measured by the bond-order correlation length, translational correlation length, dislocation (defect) density, and a direct size measurement algorithm. The results show two stages of order formation. On short time scales, individual particle motion dominates; this is a fast process characterized by {alpha}=0.93{+-}0.1. At longer time scales, small crystallites undergo collective rearrangement, merging into bigger ones, resulting in a smaller exponent {alpha}=0.38{+-}0.06.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Grain Enhancement in Polycrystalline CuGaSe 2 by AgBr Vapor Treatment

Copper Gallium diselenide (CuGaSe 2 or CGS) thin film were deposited using a three-stage thermal co-evaporation process on molybdenum coated soda lime glass. Recrystallization was carried after the second stage by flashing AgBr for 2 mins. The change in morphology, structure and depth profile were studied after the treatment. SEM and XRD showed an increase in grain size and enhanced crystallinity. Here, a decrease in sodium profile after the treatment was observed through SIMS measurements. Overall, AgBr treatment of CGS seems to be promising for the improvement of film quality, which could help with enhanced device fabrication in the future.

14 SOLAR ENERGY↗

Impact of Indium Chloride Treatment on the Properties of CuInSe 2 Thin Films

Copper Indium diselenide (CIS) semiconductor thin films were deposited by single-stage process. Following the deposition, annealing and recrystallization of CIS was carried out in the presence of InCl 3 at different temperatures. Increase in grain size was observed by SEM in all cases. Increase in peak intensity was observed by XRD after treatment, correlating well with the SEM results. Measurements of the composition by both XRF and EDS indicate significant changes, notably a decrease in copper content. Here, this will likely be an issue for device performance and will need to be addressed.

14 SOLAR ENERGY↗

Effect of Metal Halides Treatment on High Throughput Low Temperature CIGS Solar Cells

Copper indium gallium diselenide (CIGS) semiconductor thin films were deposited at high rate and low temperature using single-stage thermal co-evaporation process on molybdenum back contact. A post deposition treatment was done by flashing AgBr at 350 ºC to induce recrystallization. Changes in morphology were confirmed by SEM, with an observed increase in grain size, as well as by XRD measurements, with a decrease in FWHM. Device results show an improvement of the performance after the AgBr vapor treatment, as all the photovoltaic parameters enhanced. Altogether, AgBr seems to be a suitable transport agent and beneficial for device fabrication.

14 SOLAR ENERGY↗

Post-deposition Metal Halide Treatment of CuGaSe 2 for Photovoltaic Application

Copper gallium diselenide (CGS) semiconductor thin films were deposited by three-stage thermal co-evaporation process. Post-deposition treatments and recrystallization were performed at various AgBr doses of 40 mg, 60 mg, and 80 mg after the 2 nd stage. The changes in surface morphology were confirmed by SEM. The electrical properties were also modified, as the resistivity of the film decreases with increasing doses. Here, the device performance after the treatment did not change as expected, as the overall device performance only slightly increases in the case of 60 mg of AgBr. Substantial changes in the fabrication process will therefore be required for better device results.

14 SOLAR ENERGY↗

Shear-based deformation processing of age-hardened aluminum alloy for single-step sheet production

Shear-based deformation processing by hybrid cutting-extrusion and free machining are used to make continuous strip, of thickness up to one millimeter, from low-workability AA6013-T6 in a single deformation step. The intense shear can impose effective strains as large as 2 in the strip without pre-heating of the workpiece. The creation of strip in a single step is facilitated by three factors inherent to the cutting deformation zone: highly confined shear deformation, in situ plastic deformation-induced heating and high hydrostatic pressure. The hybrid cutting-extrusion, which employs a second die located across from the primary cutting tool to constrain the chip geometry, is found to produce strip with smooth surfaces (S a < 0.4 μm) that is similar to cold-rolled strip. The strips show an elongated grain microstructure that is inclined to the strip surfaces – a shear texture – that is quite different from rolled sheet. Furthermore, this shear texture (inclination) angle is determined by the deformation path. Through control of the deformation parameters such as strain and temperature, a range of microstructures and strengths could be achieved in the strip. When the cutting-based deformation was done at room temperature, without workpiece pre-heating, the starting T6 material was further strengthened by as much as 30% in a single step. In elevated-temperature cutting-extrusion, dynamic recrystallization was observed, resulting in a refined grain size in the strip. Implications for deformation processing of age-hardenable Al alloys into sheet form, and microstructure control therein, are discussed.

36 MATERIALS SCIENCE↗

Control over the Size Effect in the Spectroscopic Properties of Zn{sub x}Cd{sub 1–} {sub x}S Colloidal Quantum Dots

Approaches are developed for controlling the size effect in the absorption and photoluminescence properties of colloidal CdS and Zn{sub 0.5}Cd{sub 0.5}S quantum dots (QDs) in a gelatin matrix and thioglycolic acid. We analyze spectroscopic manifestations of dark Ostwald ripening and size-selective photoetching and demonstrate that the illumination of molten colloidal CdS and Zn{sub 0.5}Cd{sub 0.5}S QD solutions at a wavelength lying at the optical absorption edge in the presence of hydrogen peroxide as a catalyst for photoetching leads to a blue shift of the optical absorption and photoluminescence spectra of the QDs. Analysis of TEM images of QD samples leads us to conclude that photoetching reduces the average QD size as a consequence of the photodissolution of the CdS and Zn{sub 0.5}Cd{sub 0.5}S compounds. We demonstrate that, by contrast, heat treatment of the synthesized CdS and Zn{sub 0.5}Cd{sub 0.5}S QD sols at a temperature between 75 and 90°C leads to an increase in nanocrystal size through recrystallization, which shows up as a redshift of the optical absorption and photoluminescence spectra of the corresponding samples.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Low-temperature dehydration of gypsum single crystals

On the basis of the analysis of the electron spin resonance spectrum of the SO{sub 3}{sup -} radical ion, it is established that the transformation of gypsum (CaSO{sub 4} . 2H{sub 2}O) into bassanite (CaSO{sub 4} . 0.5H{sub 2}O) with partial removal of water molecules occurs through the formation of an anhydrous metastable phase. This phenomenon, reflecting the processes of recrystallization of materials of this class, serves as the scientific basis for the production of binders from sulfate mineral associations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Crystallization, crystal-structure refinement, and IR spectroscopy of a synthetic hexahydroborite analog

The crystal structure of the hexahydroborite analog Ca[B(OH){sub 4}]{sub 2} {center_dot} 2H{sub 2}O (a = 7.9941(3) Angstrom-Sign , b = 6.6321(2) Angstrom-Sign , c = 7.9871(3) Angstrom-Sign , {beta} = 104.166(4) Degree-Sign , V = 410.58(3) Angstrom-Sign {sup 3}, sp. gr. P2/c, Z = 2, {rho}{sub calc} = 1.891 g/cm{sup 3}; Xcalibur S CCD automated diffractometer, 1196 reflections with I > 2{sigma}(I), {lambda}MoK{sub {alpha}}), which was synthesized by the hydrothermal method via the recrystallization of calciborite CaB{sub 2}O{sub 4} (M) in the M - B{sub 2}O{sub 3} - H{sub 2}O system (t = 250 Degree-Sign C and P = 70-80 atm), was refined by the least-squares method with anisotropic displacement parameters (H atoms were located; R{sub 1} = 0.0260). The structure of synthetic hexahydroborite consists of infinite columns running along the c axis. The columns are formed by Ca polyhedra linked together and to [B(OH){sub 4}] orthotetrahedra by sharing edges. Along the two other axes, the translationally equivalent columns are linked only by hydrogen bonds. The presence of a stronger bond between the discrete (Ca-B-O) columns along the shortest (b = 6.6 Angstrom-Sign ) axis accounts for the possibility of the shift of the columns by 1/2T{sub b} and the formation of the second modification of Ca[B(OH){sub 4}]{sub 2} {center_dot} 2H{sub 2}O. The crystals of synthetic hexahydroborite were studied by IR spectroscopy. A crystal-chemical analysis was performed for a series of natural metaborates with the general formula CaB{sub 2}O{sub 4} {center_dot} nH{sub 2}O (CaO: B{sub 2}O{sub 3} = 1: 1, n = 0-6), including calciborite CaB{sub 2}O{sub 4} and hexahydroborite CaB{sub 2}O{sub 4} {center_dot} 6H{sub 2}O as the end members.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of double annealing on the critical parameters of highly textured YBa{sub 2}Cu{sub 3}O{sub 6.9}

The effect of low-temperature treatment (200 Degree-Sign C) and subsequent annealing at 930 Degree-Sign C on the critical parameters of highly textured YBa{sub 2}Cu{sub 3}O{sub 6.9} is studied. The structural defects that are formed during the low-temperature decomposition of this compound into phases with different oxygen contents and during interaction with atmospheric moisture are shown to deteriorate the superconducting properties. After annealing at T = 930 Degree-Sign C and subsequent oxidation, superconductivity is restored and the formed defects are partly retained and serve as effective pinning centers, including the case of high magnetic fields. The stresses induced by the low-temperature treatment lead to primary recrystallization at T = 930 Degree-Sign C, which results in the disappearance of texture and an isotropic state of the material in high fields.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and mechanical properties of V–4Ti–4Cr alloy as a function of the chemical heat treatment regimes

The regularities of the formation of a heterophase structure and mechanical properties of V–4Ti–4Cr alloy as a function of thermomechanical and chemical heat treatments are studied. The regimes of thermomechanical treatment which provide the formation of a heterophase structure with a homogeneous volume distribution of oxycarbonitride nanoparticles with a size of about 10 nm and an increase in the volume content and thermal stability of this phase and which provide an increase in the temperature of alloy recrystallization are developed. The formation of the heterophase structure results in a substantial (up to 70%) increase in the short-term high-temperature strength of the alloy at T = 800°C. The increase in the strength is achieved while keeping a rather high level of plasticity.

36 MATERIALS SCIENCE↗

The effect of thermomechanical treatment regimes on microstructure and mechanical properties of V–Me(Cr, W)–Zr–C alloys

The regularities of the formation of a heterophase structure in dispersion-strengthened vanadium V–Me(Cr, W)–Zr–C alloys are studied as a function of the regimes of their thermomechanical treatment. The regimes of treatment providing a substantial increase in the dispersity and homogeneity of spatial distribution of ZrC particles, temperature of recrystallization, and high-temperature (at T = 800°C) short-time strength are found in comparison to conventional treatment regimes.

36 MATERIALS SCIENCE↗

Results of high heat flux tests of tungsten divertor targets under plasma heat loads expected in ITER and tokamaks (review)

Heat loads on the tungsten divertor targets in the ITER and the tokamak power reactors reach ~10MW m{sup −2} in the steady state of DT discharges, increasing to ~0.6–3.5 GW m{sup −2} under disruptions and ELMs. The results of high heat flux tests (HHFTs) of tungsten under such transient plasma heat loads are reviewed in the paper. The main attention is paid to description of the surface microstructure, recrystallization, and the morphology of the cracks on the target. Effects of melting, cracking of tungsten, drop erosion of the surface, and formation of corrugated and porous layers are observed. Production of submicron-sized tungsten dust and the effects of the inhomogeneous surface of tungsten on the plasma–wall interaction are discussed. In conclusion, the necessity of further HHFTs and investigations of the durability of tungsten under high pulsed plasma loads on the ITER divertor plates, including disruptions and ELMs, is stressed.

36 MATERIALS SCIENCE↗

Influence of Annealing in Freon on the Crystalline Structure of Cadmium-Telluride Layers and the Efficiency of Thin-Film Solar Cells on Their Basis

Solar cells (SCs) based on cadmium-telluride base layers, obtained by thermal evaporation and closed-space sublimation (CSS), are investigated. The base layers are activated via annealing in Freon. Structural and morphological studies are carried out to compare the recrystallization processes occurring during annealing in CdTе layers fabricated by different methods. The output parameters and light diode characteristics of the SCs are investigated, and the possibility of applying Freon annealing in the commercial production technology of thin-film CdS/CdTе SCs with base layers formed by thermal vacuum evaporation is analyzed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Analysis of the Optical Properties of Plastically Deformed ZnS(O) Using Band-Anticrossing Theory

The cathodoluminescence and absorption of plastically deformed ZnS(O) single crystals are investigated in the light of band-anticrossing theory. The difference in the oxygen content in the surface layer and in the sample bulk is found using a scanning electron microscope and according to cathodoluminescence data. This fact explains the specifics of the spectral position of the fundamental absorption edge and exciton spectra. The shift dynamics of the bands of self-activated luminescence on deep A centers (SA luminescence) during deformation recrystallization with an increase in the dissolved oxygen concentration is presented. Restriction of the spectral range of the appearance of self-activated luminescence at shallow levels—“edge” luminescence—is established. The nature of the emission bands in the wavelength ranges of 336–350 and 364–390 nm is established. These results refine the energy model of ZnS(O) crystals and can be useful in the case of the practical use of their structure-sensitive properties.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Effect of Bismuth on the Structural Perfection and the Luminescent Properties of Thin-Film Elastically Stressed Al{sub x}In{sub y}Ga{sub 1–x–y}Bi{sub z}Sb{sub 1–z}/GaSb Heterostructures

The effect of bismuth on the structural perfection and the luminescent properties of Al{sub x}In{sub y}Ga{sub 1–x–y}Bi{sub z}Sb{sub 1–z}/GaSb heterostructures has been studied. The optimal parameters of the process of zone recrystallization with temperature gradient at which epitaxial AlInGaBiSb layers have the minimum roughness and high structural perfection have been revealed: temperature gradient 1 ≤ G ≤ 30 K/cm, the liquid zone thickness 60 ≤ l ≤ 100 μm, the temperature range 773 K ≤ T ≤ 873 K, and bismuth concentration 0.3–0.4 mol fraction.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Influence of Film Thickness on Annealing-Induced Grain Growth in Pt Films

Pt films with thickness h = 20–100 nm deposited on oxidized с-Si(100) substrate have been subjected to vacuum annealing at 500°C for 1 h, which resulted in recrystallization and growth of grains. Simultaneously with the normal growth of grains, abnormal grain growth has been observed, as a result of which the grains have separated in normal and secondary grains. For h = 20–40 nm, the secondary grains become much larger than the normal ones and the grain lateral size distribution therefore becomes bimodal. It has been shown that the abnormal grain growth rate increases with decreasing h, whereas the normal grain growth rate is independent of h. From the Pt(111) and Pt(222) X-ray diffraction peaks analysis it follows that the mean size D of coherently diffracting domains increases as a result of annealing. In the annealed films, D sublinearly grows with h, whereas in the as-prepared films, D grows linearly.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗