Analysis of the Long-Term Performance Degradation of Crystalline Silicon Photovoltaic Modules in Tropical Climates

For this study, the long-term performance degradation of five different types of commercial crystalline silicon (c-Si) photovoltaic (PV) modules (one sample for each type) in the tropics, or more specifically the tropical rainforest climate 'Af' by the Koppen climate classification (Singapore), is investigated over a period of seven years, based on outdoor I-V measurements at 10-s intervals. The degradation rates of these c-Si PV modules, based on the temperature-corrected performance ratio, range from -0.03 to -0.47%/year, which satisfy the products' performance warranty. Further analysis of the short-circuit current (I sc), open-circuit voltage, and fill factor for these modules shows that the performance degradation is mainly attributed to the l sc loss. Lastly, the possible causes of the module performance deterioration are also discussed.

14 SOLAR ENERGY↗

Facet‐dependent Heterogeneous Fenton Reaction Mechanisms on Hematite Nanoparticles for (Photo)catalytic Degradation of Organic Dyes

Although heterogeneous photo‐Fenton reactions on nanoparticulate iron oxides effectively degrade organic pollutants, the underlying surface mechanisms remain debated. Here, we demonstrate how these pathways are modulated by specific hematite crystal facets. To investigate the influence of particle surface structure, methylene blue (MB) adsorption and photodegradation kinetics are examined using facet‐engineered hematite nanoparticles with distinct exposed facets. The results reveal that MB photodegradation strongly depends on both pH and facet orientation. When normalized by surface area, (116) facet shows higher photodegradation activity than those with (104) or (001) facets. This enhanced activity is attributed to favorable electronic structure and surface characteristics, including a smaller optical bandgap, faster charge transfer, and superior H 2 O 2 decomposition. In contrast, the photodegradation capacity follows (104) 〉 (116) 〉 (001), primarily due to the higher density of surface‐active sites on the (104) facet. These sites promote coupled MB adsorption and degradation, enabling removal of a greater overall quantity of MB. Additionally, under high pH conditions, hematite can degrade MB in the dark, with capacities following (001) ≫ (116) 〉 (104). These findings underscore the critical catalytic role of specific hematite surfaces and advance the understanding of facet‐dependent photoinduced redox chemistry at mineral–water interfaces.

(photo)catalytic degradation↗

Oxygen Release Degradation in Li–Ion Battery Cathode Materials: Mechanisms and Mitigating Approaches

Widespread application of Li–ion batteries (LIBs) in large–scale transportation and grid storage systems requires highly stable and safe performance of the batteries in prolonged and diverse service conditions. Oxygen release from oxygen–containing positive electrode materials is one of the major structural degradations resulting in rapid capacity/voltage fading of the battery and triggering the parasitic thermal runaway events. Herein, the authors summarize the recent progress in understanding the mechanisms of the oxygen release phenomena and correlative structural degradations observed in four major groups of cathode materials: layered, spinel, olivine, and Li–rich cathodes. In addition, the engineering and materials design approaches that improve the structural integrity of the cathode materials and minimize the detrimental O 2 evolution reaction are summarized. As a result, the authors believe that this review can guide researchers on developing mitigation strategies for the design of next–generation oxygen–containing cathode materials where the oxygen release is no longer a major degradation issue.

25 ENERGY STORAGE↗

Catalytic Degradation of Polyethylene Terephthalate Using a Phase-Transitional Zirconium-Based Metal–Organic Framework

Polyethylene terephthalate (PET) is utilized as one of the most popular consumer plastics worldwide, but difficulties associated with recycling PET have generated a severe environmental crisis with most PET ending its lifecycle in landfills. We report that zirconium-based metal–organic framework (Zr-MOF) UiO-66 deconstructs waste PET into the building blocks terephthalic acid (TA) and mono-methyl terephthalate (MMT) within 24 hours at 260 °C (total yield of 98 % under 1 atm H 2 and 81 % under 1 atm Ar). Extensive structural characterization studies reveal that during the degradation process, UiO-66 undergoes an intriguing transformation into MIL-140A, which is another Zr-MOF that shows good catalytic activity toward PET degradation under similar reaction conditions. Here these results illustrate the diversity of applications for Zr-MOFs and establish MOFs as a new class of polymer degradation catalysts with the potential to address long-standing challenges associated with plastic waste.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Simultaneous Degradation‐Depolymerization of Bioderived Comb Copolymers

Poly(lactic acid) (PLA) is the most widely explored biodegradable alternative for polystyrene; however, its low toughness and glass transition temperature may limit its wider adoption as a sustainable replacement. To improve its material and thermal properties, PLA can be chemically or physically combined with other polymers, like poly(methyl methacrylate) (PMMA), though the incorporation of vinyl‐based polymer components complicates chemical recycling and reduces the sustainability of the material. Here, in this study, we synthesized polymethacrylate‐PLA comb copolymers designed to be thermally deconstructed. Our design strategically extends current polymer deconstruction methodologies to more complex macromolecular systems. Thermally labile units within the polymethacrylate backbone permitted depolymerization that was concurrent with PLA side chain degradation during heating. This dual degradation‐depolymerization process enhances the overall sustainability of lactide/vinyl‐based copolymers and demonstrates the synergistic potential of integrating multiple deconstruction pathways into a single system. This report elaborates on the design of advanced, degradable copolymers, contributing to the further development of sustainable polymer materials.

PLA↗

Non-isothermal Crystallization and Degradation Kinetics of Fe{sub 3}O{sub 4}–Thymolblue Functionalized Poly(ε-caprolactone)

The Fe{sub 3}O{sub 4}–thymolblue (TB) functionalized or end capped poly(ε-caprolactone) (PCL) was synthesized by ring opening polymerization (ROP) of ε-caprolactone (CL) with Fe{sub 3}O{sub 4}–TB nanohybrid as an effective initiator in the presence of stannous octoate (SO) as a catalyst. The main aim of the present work is to analyze the influence of polymer chain end capping agent or functionalization agent on the structure–property relationship particularly, crystallization and thermal degradation behavior of PCL under non-isothermal condition. The structure of the polymer was analyzed using FTIR and NMR spectra. The particle size of the incorporated Fe{sub 3}O{sub 4}–TB nanohybrid in PCL matrix was found to be less than 20 nm by TEM. The surface morphology, skewness moment and surface roughness were analysed by AFM. The spherulitic growth of the nucleated polymer crystals was confirmed by POM. The spherulitic growth was further verified with various kinetic models. The melting and crystallization behaviors under non-isothermal condition were assessed by DSC. Various kinetic models were employed to comprehend the degradation behavior of Fe{sub 3}O{sub 4}–TB functionalized PCL and its associated kinetic parameters under non-isothermal condition. The energy of activation (E{sub a}) for the crystallization and thermal degradation of PCL were found to be 132 and nearly 140 kJ/mol respectively.

36 MATERIALS SCIENCE↗

Understanding and mitigating degradation in amine-based sorbents for CO 2 direct air capture

The success of direct air capture (DAC) of CO 2 depends on sorbents that combine high capacity, low energy requirements, and long-term durability. Amine-based sorbents-including solid-supported aminopolymers, grafted amines, and amine-functionalized resins-remain the leading candidates, but their limited lifetimes drive up costs and constrain deployment. In this review, we outline the current understanding of amine-based sorbent degradation with an emphasis on clearly identifying what is known about structure-property-performance relationships, as well as important knowledge gaps. More specifically, we discuss how polymer chemistry, sorbent design variables, and environmental and process conditions contribute to performance loss. In parallel, we outline how advances in spectroscopy, modeling, and accelerated testing are beginning to illuminate chemical and physical degradation mechanisms. Looking forward, we identify future research directions that will be critical for gaining a deeper understanding of degradation, as well as opportunities for developing innovative mitigation strategies for improving the lifetime of amine-based sorbents.

organic↗

Parametric analysis of anodic degradation mechanisms for fast charging lithium batteries with graphite anode

In this work, we report the impact of the temperature-driven synergistically-coupled anodic degradation mechanisms on the electrochemical performance of lithium batteries with graphite anode over multiple cycles. Temperature dependence of electrochemical reactions and damage mechanisms, such as solid electrolyte interface (SEI) growth, lithium plating/stripping, dead lithium storage/dissolution, and film cracking are incorporated into the degradation model. Results of a parametric analysis are presented, evaluating the effects of charging rates (1–6 C), operating temperatures (-15 – 45°C) and electrode design parameters, on the relative performance fade in the lithium-ion battery. Thermo-electrochemical process maps are developed to provide insights into the relationship between electrode performance and failure mechanisms. The simulation results predict a severe capacity loss due to lithium plating at low temperatures, which is further aggravated at high charging rates. A common strategy for mitigating lithium plating, through charging at high temperatures, also results in rapid capacity loss due to accelerated SEI formation. Simulation results are used to identify the combination of operating conditions and electrode design parameters that improve the electrochemical performance of the battery. These results demonstrate an opportunity to design safe and high-performance lithium-ion batteries, guided by anodic degradation models.

Battery design↗

Degradation science: Mesoscopic evolution and temporal analytics of photovoltaic energy materials

Based on recent advances in nanoscience, data science and the availability of massive real-world datastreams, the mesoscopic evolution of mesoscopic energy materials can now be more fully studied. The temporal evolution is vastly complex in time and length scales and is fundamentally challenging to scientific understanding of degradation mechanisms and pathways responsible for energy materials evolution over lifetime. We propose a paradigm shift towards mesoscopic evolution modeling, based on physical and statistical models, that would integrate laboratory studies and real-world massive datastreams into a stress/mechanism/response framework with predictive capabilities. These epidemiological studies encompass the variability in properties that affect performance of material ensembles. Mesoscopic evolution modeling is shown to encompass the heterogeneity of these materials and systems, and enables the discrimination of the fast dynamics of their functional use and the slow and/or rare events of their degradation. As a result, we delineate paths forward for degradation science.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pilot testing of a heat integrated 0.7 MWe CO 2 capture system with two-stage air-stripping: Amine degradation and metal accumulation

An advanced 0.7 MWe small pilot coal-fired post-combustion CO 2 capture system with heat integration combined with two-stage stripping was tested here on a slipstream of flue gas by the University of Kentucky Center for Applied Energy Research (UKy-CAER). Evaluation of solvent degradation products was performed to determine the impact of oxygen exposure due to incorporation of the secondary air stripper into the conventional amine absorber/stripper system. The overall degradation rates and products observed during the testing campaign were comparable to previously published reports using 30% monoethanolamine (MEA) as the baseline/commissioning solvent. The rates of heat stable salt accumulation and amine degradation were similar to those from conventional CO 2 capture systems using MEA. Metal accumulation as the result of material corrosion inside the system from an improperly constructed material was observed. Finally, the impact of the secondary air stripper appears negligible relative to other published MEA campaigns tested at similar flue gas conditions and system operating hours.

03 NATURAL GAS↗

Degradation of solid oxide electrolysis cells: Phenomena, mechanisms, and emerging mitigation strategies—A review

Solid oxide electrolysis cell (SOEC) is a promising electrochemical device with high efficiency for energy storage and conversion. However, the degradation of SOEC is a significant barrier to commercial viability. In this review article, the typical degradation phenomena of SOEC are summarized, with great attention into the anodes/oxygen electrodes, including the commonly used and newly developed anode materials. Meanwhile, mechanistic investigations on the electrode/electrolyte interfaces are provided to unveil how the intrinsic factor, oxygen partial pressure , and the electrochemical operation conditions, affect the interfacial stability of SOEC. At last, this paper also presents some emerging mitigation strategies to circumvent long-term degradation, which include novel infiltration method, development of new anode materials and engineering of the microstructure.

36 MATERIALS SCIENCE↗

Evaluation of commercial lithium-ion cells based on composite positive electrode for plug-in hybrid electric vehicle applications. Part II. Degradation mechanism under 2 C cycle aging

Degradation phenomena and inference of their underlying mechanisms during 2 C cycle aging in a cell design comprising {l_brace}LiMn1/3Ni1/3Co1/3O2 + LiMn2O4{r_brace} composite positive electrode are studied and reported in this work. We describe how aging phenomena in the cells were studied and incremental capacity analysis applied to infer cell degradation mechanisms in the cycle aging process. Two stages of degradation were observed in the life cycle under this aging regime. In the first stage, we conclude that loss of lithium inventory was the cause of capacity fade. As a result of such parasitic loss, the cell further suffered from loss of active materials in the second stage, in which the positive electrode kinetics was hampered and the capacity loss accelerated.

33 ADVANCED PROPULSION SYSTEMS↗

Performance degradation due to anodic failure mechanisms in lithium-ion batteries

Here, we report a mechano-chemical model for anodic degradation during fast-charging of nickel-manganese-cobalt (NMC)/graphite (C) cell due to SEI growth, lithium plating/stripping, dead lithium storage, and film fracture of composite SEI and plated lithium film. Degradation of the battery is analyzed for a range of charging rates from 1 to 6 C-rates, and the influence of plating mechanisms – lithium plating and dead lithium deposition and recovery during stripping – on the film resistance of the anode are accounted for in the model. Dynamic evolution of the interfacial properties is modeled using rule-of-mixture approach. Model predictions of plating associated stress fields are used to compute critical energy release rate for film cracking. The results indicate an increased tendency of fracture for thinner SEI film with lithium plating at higher charging rates. The process of reforming the cracked film absorbs a significant portion of the electrode current thereby reducing the cell capacity and plating efficiency. The mechano-chemical model provides an extensive analytical framework for understanding the synergistic coupling of anodic degradation mechanisms, prognosticating conditions of SEI failure, and evaluating the capacity fade and efficiency of lithium-ion battery.

25 ENERGY STORAGE↗

Gaining insight into lithium-ion battery degradation by a calorimetric approach

With the growing demand for lithium-ion batteries (LIBs) in transportation and renewable energy sectors, ensuring reliability and mitigating degradation are crucial challenges for their widespread deployment. Here this study investigates the relationship between thermal characteristics and degradation/reliability by developing an in-situ heat measurement methodology for LIBs operating under grid services. Using adiabatic mode-based calorimetry, we examine the thermal behavior of two commercial cells with different cathode chemistries (Ni-rich layered oxide and olivine) before and after two years of grid service (peak shaving) and demonstrate a strong correlation between thermal characteristics and electrochemical performance and its degradation. By further analyzing the heat sources separation (differentiating between irreversible and reversible heat), we disclose the underlying degradation mechanisms of LIBs. These findings emphasize the critical role of thermal characteristics in determining LIB reliability and deterioration, while the obtained heat data can aid in the development and calibration of LIB state-of-health models for grid applications.

25 ENERGY STORAGE↗

Degradation mechanisms of 1.3 μm C-doped quantum dot lasers grown on native substrate

Here, the aim of this paper is to analyse the degradation modes of 1.3 μm InAs quantum dot laser diodes (QD LDs) grown by using carbon as a p-type dopant, as an alternative to beryllium. The devices were stressed at high current densities, to favor the onset of excited-state (ES) emission, and to study the related degradation phenomena. The study of QD LDs is of fundamental importance for the photonic integrated circuits (PICs). The investigation is based on two types of stress tests: 1) a current step stress and 2) a constant current stress. With these experiments we demonstrate that a) the current is a determining factor for the onset of the ES during the operation of such devices. b) the onset of ES is responsible for a rapid quenching of the ground state (GS) emission. c) stress induces a significant increase in the threshold current of the devices, that is ascribed to the lowering of the injection efficiency, which in turn can be explained by the easier escape of carriers from quantum dots (QDs) from ES energy levels. d) the contribution of defects on the optical and electrical degradation is also discussed.

42 ENGINEERING↗

Root cause analysis and solutions for plastic gamma detector degradation in challenging environments—An overview

Polyvinyl toluene (PVT) plastic is often used to make gamma ray sensitive scintillators and is used in many important applications. For example, PVT is used to scan recycled steel going into a plant to be processed. It is also used in personnel portals to scan employees, and is used at the borders of many countries to scan cargo and cars passing through. In recent years, it was discovered that PVT can become degraded when it absorbs water and then is subjected to daily temperature swings, as is evidence by a reduction in scintillation light. Water absorption by PVT was notionally associated with temporary fogging (i.e., a rapid decrease in opacity which was reversible over time) and permanent fogging (i.e., permanent crack-like defects) and was for some time suspected to be the leading cause of the fogging due to circumstantial evidence. However, definitive proof was not established and in particular the specific mechanisms by which water entered the plastic and ultimately created temporary and permanent point-like defects was not fully understood. This paper is an overview of an effort initiated to reveal the fundamental root cause and also the dynamics of the fogging and degradation processes. This understanding is important not only to solve degradation problems for PVT in fielded systems, but also (1) to provide direction for future procurements for new equipment, and (2) to provide direction for future R&D efforts into advanced plastics with enhanced spectroscopic capabilities or dual particle gamma/neutron capabilities. Unexpected outcomes of this investigation included (1) the capability to predict the onset of fogging based on models using weather data alone, and (2) new modified formulations of PVT and PS which are fog-resistant. This paper provides an overview of the water uptake and associated mechanisms for various compositions, characterization of resulting temporary and permanent defects, predictive modeling of fogging, and possible solutions including encapsulation, heaters and new formulations. While this paper is an overview of the root cause analysis and solution, five accompanying papers (Lance et al., 2018, Myllenbeck and Feng, 2018, Payne et al., 2018, Zaitseva et al. 2018, Kouzes et al., 2018) from the same conference (SORMA 2018) delve further into the details and also expand upon the scope of what will be reported herein.

36 MATERIALS SCIENCE↗

A methodology for customizing implantation profiles of light ions using a single thin foil energy degrader

We report a method was developed to quantify the spatial distribution and implantation depth of energy-degraded light ions with a thin foil rotating energy degrader for use during multiple ion beam irradiation. The methodology covers three physical phenomena: ions passing through the thin foil, ions travelling through the vacuum to the target, and ion implantation into the target, and accounts for the distribution of ions both in depth and in plane. The processes of energy straggling and scattering were calculated using SRIM. The effects of raster-scanning, and the geometry of the system were implemented in scripts handling the SRIM output files. Elastic backscattering (EBS) using 2.38 MeV H+ protons was used to measure the helium depth profiles after implantation with and without thin foil energy degradation. Defect analysis with transmission electron microscopy confirmed the implantation profiles measured with EBS and calculated with SRIM.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Real-time interface investigation on degradation mechanism of organic light-emitting diode by in-operando X-ray spectroscopies

Understanding the chemical evolution at the interface of organic light-emitting diodes (OLEDs) under working conditions is critical for addressing device failure and further improving performance. In this work, an in-operando approach was developed employing synchrotron-based X-ray absorption spectroscopy (XAS) to investigate the electronic structures and chemical degradation mechanisms of a model tris(8-hydroxyquinoline) aluminum (Alq 3 )-based OLED device under working condition. The results identify that Mg atoms from the electrode migrate into the Alq 3 organic layer under a potential bias and replace Al atom sites, forming the unstable Mgq 3 species which lead to device degradation. Here, the findings from the classic and simple model device elucidate the degradation mechanisms occurred at the interface of OLED devices, which may facilitate the development of more efficient and stable OLED devices with complex structures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗