Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 919 records · Page 51

Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing↗

Overcoming Anode Instability in Solid‐State Batteries through Control of the Lithium Metal Microstructure

Abstract Enabling the lithium metal anode (LMA) in solid‐state batteries (SSBs) is the key to developing high energy density battery technologies. However, maintaining a stable electrode–electrolyte interface presents a critical challenge to high cycling rate and prolonged cycle life. One such issue is the interfacial pore formation in LMA during stripping. To overcome this, either higher stack pressure or binary lithium alloy anodes are used. Herein, it is shown that fine‐grained ( d = 20 µm) polycrystalline LMA can avoid pore formation by exploiting the microstructural dependence of the creep rates. In a symmetric cell set‐up, i.e., LiǀLi 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO)ǀLi, fine‐grained LMA achieves > 11.0 mAh cm −2 compared to ≈ 3.6 mAh cm −2 for coarse‐grained LMA ( d = 295 µm) at 0.1 mA cm −2 and at moderate stress of 2.0 MPa. Smaller diffusion lengths (≈ 20 µm) and higher diffusivity pathway along dislocations ( D d ≈ 10 −7 cm 2 s −1 ), generated during cell fabrication, result in enhanced viscoplastic deformation in fine‐grained polycrystalline LMA. The electrochemical performances corroborate well with estimated creep rates. Thus, microstructural control of LMA can significantly reduce the required stack pressure during stripping. These results are particularly relevant for “anode‐free” SSBs wherein both the microstructure and the mechanical state of the lithium are critical parameters.

25 ENERGY STORAGE↗

Reactive Carbide‐Based Synthesis and Microstructure of NASICON Sodium Metal All Solid‐State Electrolyte

Reactive carbide precursor-based synthesis of NASICON-type NZSP (Na 1+x Zr 2 Si x P 3-x O 12 ) solid-state electrolyte (SSE) is demonstrated, in contrast to the established oxide-based approach. Exothermic decomposition of ZrC and SiC in air homogenizes microstructure, yielding 98% compact density after conventional sintering at 1200 °C. Quantitative stereology demonstrates that significant microstructural differences are present. Compacts of carbide-derived Carb-NZSP are 98% dense with a secondary zirconium oxide (ZrO 2 ) volume fraction of 0.2% ± 0.3%, versus 93% dense and 3% ± 1% for oxide-derived baseline. For Carb-NZSP, the secondary glassy phosphate phase is agglomerated, while for baseline, it is dispersed and percolated. Electrochemical testing combined with post-mortem analysis demonstrates how microstructural control of secondary phases is critical for dendrite suppression: Carb-NZSP critical current density (CCD) is 3.1 ± 0.8 mA cm −2 at 0.1 mAh cm −2 , versus 1.0 ± 0.7 mA cm −2 at 0.1 mAh cm −2 . Cryogenic focused ion beam (cryo-FIB) analysis demonstrates that in both materials, the porous 2D sheet-like sodium metal dendrites propagate around and subsume NZSP grains, likely following a path enriched with glassy phase and with porosity. Dendrites also flow around isolated zirconia particles. Phase field simulation reveals deflection of dendrites by mechanically tough zirconia, while brittle glassy phase accelerates dendrite growth, especially when finely distributed.

36 MATERIALS SCIENCE↗

Microstructural Effects on SCC Initiation PWR Primary Water Cold-Worked Alloy 600

SCC initiation behavior of one mill annealed alloy 600 plate heat was investigated in simulated PWR primary water under constant load at yield stress with in-situ direct current potential drop (DCPD) monitoring for crack initiation. Twelve specimens were tested at similar cold work levels among which three showed much shorter SCC initiation times (<400 hrs) than the others (>1200 hrs). Post-test examinations revealed that these three specimens all feature an inhomogeneous microstructure where the primary crack always nucleated along the boundary of large elongated grains protruding normally into the gauge. In contrast, such microstructure was either not observed or did not extend deep enough into the gauge in the other specimens exhibiting ~3-6X longer initiation times. In order to better understand the role of this microstructural inhomogeneity in SCC initiation, high-resolution microscopy was performed to compare carbide morphology and strain distribution between the long grains and normal grains, and their potential effects on SCC initiation are discussed in this paper.

Alloy 600↗

Comparison of the Microstructure and Flux Pinning Properties of Polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} Containing Zn{sub 0.95}Mn{sub 0.05}O or Al{sub 2}O{sub 3} Nanoparticles

Here we compare the microstructure and flux pinning properties of polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} (Y-123 or YBCO) containing either Al{sub 2}O{sub 3} or Zn{sub 0.95}Mn{sub 0.05}O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticles were added up to a concentration of 0.1 wt%. The crystal structure, microstructure, electrical and magnetic properties were analyzed using X-ray diffraction, scanning electron microscopy and transmission electron microscopy (TEM), and electrical resistivity and DC magnetization measurements, respectively. TEM observations showed that the addition of Zn{sub 0.95}Mn{sub 0.05}O resulted in a high density of fine twins and a variety of interacting microstructures, while Al{sub 2}O{sub 3} addition resulted in a high density of Al-rich nanoscale inhomogeneities embedded in the Y-123 matrix. Flux pinning forces were determined, and predominant pinning mechanisms in the prepared samples were proposed. We evaluated the superconducting properties of YBCO considering the effects of adding insulating or magnetic nanoparticles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Rapid Solidification of Sn-Cu-Al Alloys for High-Reliability, Lead-Free Solder: Part I. Microstructural Characterization of Rapidly Solidified Solders

Particles of Cu x Al y in Sn-Cu-Al solders have previously been shown to nucleate the Cu 6 Sn 5 phase during solidification. In this study, the number and size of Cu 6 Sn 5 nucleation sites were controlled through the particle size refinement of Cu x Al y via rapid solidification processing and controlled cooling in a differential scanning calorimeter. Cooling rates spanning eight orders of magnitude were used to refine the average Cu x Al y and Cu 6 Sn 5 particle sizes down to submicron ranges. The average particle sizes, particle size distributions, and morphologies in the microstructures were analyzed as a function of alloy composition and cooling rate. Deep etching of the samples revealed the three-dimensional microstructures and illuminated the epitaxial and morphological relationships between the Cu x Al y and Cu 6 Sn 5 phases. Transitions in the Cu 6 Sn 5 particle morphologies from faceted rods to nonfaceted, equiaxed particles were observed as a function of both cooling rate and composition. Initial solidification cooling rates within the range of 10 3 to 10 4 °C/s were found to be optimal for realizing particle size refinement and maintaining the Cu x Al y /Cu 6 Sn 5 nucleant relationship. In addition, little evidence of the formation or decomposition of the ternary-β phase in the solidified alloys was noted. As a result, solidification pathways omitting the formation of the ternary-β phase agreed well with observed room temperature microstructures.

36 MATERIALS SCIENCE↗

Impact of Defects in Powder Feedstock Materials on Microstructure of 304L and 316L Stainless Steel Produced by Additive Manufacturing

Recent work in both 304L and 316L stainless steel produced by additive manufacturing (AM) has shown that in addition to the unique, characteristic microstructures formed during the process, a fine dispersion of sub-micron particles, with a chemistry different from either the powder feedstock or the expected final material, are evident in the final microstructure. Such fine-scale features can only be resolved using transmission electron microscopy (TEM) or similar techniques. The present paper uses electron microscopy to study both the initial powder feedstock and microstructures in final AM parts. Special attention is paid to the chemistry and origin of these nanoscale particles in several different metal alloys, and their impact on the final build. Finally, comparisons to traditional, wrought material will be made.

36 MATERIALS SCIENCE↗

A Review on Friction Stir Processing of Titanium Alloy: Characterization, Method, Microstructure, Properties

In the past two decades, friction stir processing (FSP) technology has received considerable attention. FSP can be used to adjust and control the microstructure of materials, including eliminating defects, destroying dendrites and controlling fractions in the second stage, and is therefore widely used in titanium and its alloys for biomedical, aerospace and automotive applications. This article comprehensively reviews the methods of studying FSP, the microstructure evolution of materials and the summary of material properties. It begins with the introduction of the FSW system, characterization, structure and elemental analysis, and simulation and performance testing methods, and then introduces the microstructure evolution mechanism of various titanium materials and discusses in detail the material properties of titanium alloy, namely hardness and wear resistance, elasticity and plasticity, corrosion resistance and biocompatibility. Finally, this review presents unresolved issues and outstanding challenges in FSP technology and reveals the direction of this emerging field of research.

36 MATERIALS SCIENCE↗

On the Effects of the Rejuvenation Treatment on Mechanical and Microstructural Properties of IN-738 Superalloy

The main scope of this paper is to show the effects of a specific rejuvenation treatment studied for IN-38 on both the microstructure and the mechanical properties of the creep-damaged superalloy and to compare the tests results with the virgin material and with the recovery obtained through the standard heat treatment. This work will show that this rejuvenation treatment is able to recover the microstructure of creep-damaged specimens and that the creep and tensile properties of the rejuvenated alloy are even better than the virgin material for the tests performed. Moreover, it will be shown that the standard heat treatment provided for IN-738 is not able to fully recover the microstructure and that the creep properties of the superalloy during the tests have been lower than the virgin material.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure and Mechanical Properties of Stellite 12 Fabricated by Laser Additive Manufacturing

Microstructure evolution and wear resistance of Stellite 12 produced by laser additive manufacturing were studied in untreated and heat-treated conditions. In untreated conditions, cobalt matrix dendrites and inter-dendritic eutectic carbides were the primary microstructure, blocky and lamellar eutectic carbides can be found, and M{sub 7}C{sub 3} and M{sub 23}C{sub 6} are the primary carbides. Heat treatment can modify the microstructure of this alloy. Primary carbides were dissolved into the cobalt matrix after solution treatment. Aging treatment resulted in the precipitation of carbides, the transformation of M{sub 7}C{sub 3} into M{sub 23}C{sub 6} carbides, and the increase in microhardness. Solution and aging treatment can also cause the precipitation of carbides, but the morphology and distribution of carbides were absolutely different. The wear resistance of untreated samples at room temperature (RT) and 600 °C is better than that at 200 and 400 °C due to the high hardness at RT and the formation of oxide film at 600 °C. The wear resistance of heat-treated samples was tested at 600 °C; it was dominated by the formation and flake-off of oxide film. The sample that underwent solution plus aging treatment has a superior wear resistance.

36 MATERIALS SCIENCE↗

Effect of Minor Yttrium on Microstructure and Mechanical Properties of Bioimplant Mg-5Zn Alloy

This paper explores cast Mg-5Zn alloy, containing small amounts of yttrium (Y: 0.1-1.5 wt.%), through microstructure evaluation and tensile and hardness tests. The results reveal that addition of Y to the alloy refines microstructure, especially when secondary phases, Mg{sub 3}Zn{sub 6}Y (I) and Mg{sub 3}Zn{sub 3}Y{sub 2} (W), form. I-phase is detected when 0.3 wt.% Y is added to the alloy, while W-phase is only observed in Mg-5Zn-1.5Y alloy. The results also show that the addition of Y improves yield and tensile strength as well as the hardness value of the Mg-5Zn alloy at the expense of its formability. The three effects of the solid solution of Y in α-Mg, grain refinement, and the formation of I- and W-phases are the reasons for such behavior. The improvement is more pronounced when W-phase appears in the microstructure. In other words, Mg-5Zn-1.5Y alloy behaves stronger and harder than other alloys and may be considered as a potential candidate for bioimplant applications if its degradation behavior meets the requirements.

36 MATERIALS SCIENCE↗

Surface Modification by Friction Stir Processing of Low-Carbon Steel: Microstructure Investigation and Wear Performance

A low-carbon steel sheet with a thickness of 5 mm was subjected to friction stir processing (FSP) by one to four different passes. The microstructures of different regions were characterized using the optical microscopy and electron backscatter diffraction. The Vickers micro-harness was measured at the distance of 200 μm below the processed surfaces. The influence of pass numbers (PNs) on wear resistance was studied in terms of coefficients of friction (CoFs), weight losses and wear rates. SEM topographies of the worn surfaces were also studied to evaluate the wear mechanisms. Microstructure observations showed that Widmänstatten ferrite plates were formed in stir zones (SZs) and heat affected zones. As PN increased, these grains were widened due to the increment of the carbon diffusivity and lengthened because of the high heat input and microstructure anisotropy. Besides, increasing the PN causes increasing of the hardness and wear resistance, simultaneously. Specifically, the wear rate in the SZ was reduced from 2.8 × 10{sup −2} mm{sup 3} m{sup −1} in base metal to 0.3 × 10{sup −2} mm{sup 3} m{sup −1} in sample which was subjected to 4 FSP passes. However, variation in PN had no considerable effect on CoFs. Oxidative wear mechanism was observed on the worn surface of the steel and the FSPed samples while more debris was formed by increasing the PNs.

36 MATERIALS SCIENCE↗

Microstructure, Phase Occurrence, and Corrosion Behavior of As-Solidified and As-Annealed Al-Pd Alloys

In the present work, we studied the microstructure, phase constitution, and corrosion performance of Al{sub 88}Pd{sub 12}, Al{sub 77}Pd{sub 23}, Al{sub 72}Pd{sub 28}, and Al{sub 67}Pd{sub 33} alloys (metal concentrations are given in at.%). The alloys were prepared by repeated arc melting of Al and Pd granules in argon atmosphere. The as-solidified samples were further annealed at 700 °C for 500 h. The microstructure and phase constitution of the as-solidified and as-annealed alloys were studied by scanning electron microscopy, energy-dispersive x-ray spectroscopy, and x-ray diffraction. The alloys were found to consist of (Al), ε{sub n} (~ Al{sub 3}Pd), and δ (Al{sub 3}Pd{sub 2}) in various fractions. The corrosion testing of the alloys was performed in aqueous NaCl (0.6 M) using a standard 3-electrode cell monitored by potentiostat. The corrosion current densities and corrosion potentials were determined by Tafel extrapolation. The corrosion potentials of the alloys were found between − 763 and − 841 mV versus Ag/AgCl. An active alloy dissolution has been observed, and it has been found that (Al) was excavated, whereas Al in ε{sub n} was de-alloyed. The effects of bulk chemical composition, phase occurrence and microstructure on the corrosion behavior are evaluated. The local nobilities of ε{sub n} and δ are discussed. Finally, the conclusions about the alloy’s corrosion resistance in saline solutions are provided.

36 MATERIALS SCIENCE↗

Influence of Heat Treatments on Microstructure and Toughness of 9%Ni Steel

The 9%Ni low-carbon steel is applied to utilities and processes at temperatures as low as − 196 °C. However, the microstructural features play an important role on the mechanical properties. Notably, the cryogenic toughness and mechanical strength are strongly dependent on the final heat treatment. In this paper, the microstructure of a 9%Ni low-carbon steel was modified by different heat treatments. The hardness and cryogenic toughness were measured and correlated to microstructural features. The material shows a temper embrittlement with intergranular cracking and minimum cryogenic toughness after tempering around 400 °C. Austempering at 480 °C also produced very low toughness results. On the other hand, excellent cryogenic toughness was obtained with single tempering at 600 °C after quenching or normalizing. Even higher toughness was obtained with the double tempering at 670 °C/2 h plus 600 °C/2 h. The amount of reversed austenite and its morphology in the specimen quenched and tempered at 600 °C were shown in the paper.

36 MATERIALS SCIENCE↗

Effect of Bainitic Microstructure on Ballistic Performance of Armour Steel Weld Metal Using Developed High Ni-Coated Electrode

Welding of armour steel has gained significant importance during the past few years as recent civilian and military requirements demand weld metal properties matching with base metal having good ballistic performance along with high strength and toughness at − 40 °C as per specification. The challenge of armour steel welding therefore lies in controlling the weld metal composition which is strongly dependent on welding electrode/consumables, resulting in desired weld microstructure consisting of lower bainite along with retained austenite. The performance of butt-welded armour steel joints produced by the developed electrodes was evaluated using tensile testing, ballistic testing, impact toughness at room temperature and subzero temperature. Microstructures of weld metals are exclusively characterized by x-ray diffraction technique, scanning electron microscope and transmission electron microscopy with selected area diffraction pattern. Experimental results show that weld metal with relatively lower carbon, higher manganese and lower nickel content was attributed to lower bainite with film type of retained austenite may be considered as a most covetable microstructure for armour steel weld metal.

36 MATERIALS SCIENCE↗

The Prediction of Microstructure Evolution of 6005A Aluminum Alloy in a P-ECAP Extrusion Study

Finite element modeling (FEM) was applied for predicting the recrystallized structure in extruded 6005 aluminum alloy, and simulated results were experimentally validated. First, microstructure evolution of 6005 aluminum alloy during deformation was studied by means of isothermal compression test, where the processing parameters were chosen to reproduce the typical industrial conditions. Second, microstructure evolution was analyzed, and the obtained information was used to fit a dynamic recrystallization model implementing inside the DEFORM-3D FEM code environment. FEM of deformation of 6005 aluminum has been established and validated by microstructure comparison. Finally, the obtained dynamic recrystallization model was applied to tube extrusion by using a portholes-equal channel angular pressing die. The finite element analysis results showed that coarse DRX grains occur in the extruded tube at higher temperature and in the extruded tube at the faster speed of the stem. The test results showed material from the front end of the extruded tube has coarse grains (60 μm) and other extruded tube has finer grains (20 μm).

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Al-Mg-Sc-Zr Alloy Variable Polarity Plasma Arc Welding Joint

Al-Mg-Sc-Zr alloy plates were welded by variable polarity plasma arc welding (VPPAW) with Sc-containing filler wire. The microstructure and mechanical properties were investigated. Results show that the weld zone and heat-affected zone (HAZ) are narrow due to the high concentrated heat input of VPPAW. Primary Al{sub 3}(Sc,Zr) particles are nice nucleating sites for α-Al, which can significantly refine the grains of α-Al, helping the weld zone maintain an outstanding strength. The unmelted Al{sub 3}(Sc,Zr) precipitates of the base metal aggregated near the fusion boundary result in the formation of a fine equiaxed grains zone, which improves the bonding degree between the weld zone and the base metal. The Al{sub 3}(Sc,Zr) precipitates in the HAZ have excellent inhibition effect on recrystallization. According to the observed microhardness distribution and microstructure characteristics, the microstructure model of welded joint is obtained. The fractured position of welded joint locates in the weld zone. The tensile strength of the welded joint without reinforcing rib is 330 MPa. The welding coefficient reaches 74%.

36 MATERIALS SCIENCE↗