Search NASA⌕ Search

SEARCH · Search NASA

Results for “microstructural properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 919 records · Page 51

Microstructures and mechanical properties of compositionally complex Co-free FeNiMnCr 18 FCC solid solution alloy

Recently, a structurally-simple but compositionally-complex FeNiCoMnCr high entropy alloy was found to have excellent mechanical properties (e.g., high strength and ductility). To understand the potential of using high entropy alloys as structural materials for advanced nuclear reactor and power plants, it is necessary to have a thorough understanding of their structural stability and mechanical properties degradation under neutron irradiation. Furthermore, this requires us to develop a similar model alloy without Co because material with Co will make post-neutron-irradiation testing difficult due to the production of the 60 Co radioisotope. In order to achieve this goal, a FCC-structured single-phase alloy with a composition of FeNiMnCr 18 was successfully developed. This near-equiatomic FeNiMnCr 18 alloy has good malleability and its microstructure can be controlled by thermomechanical processing. By rolling and annealing, the as-cast elongated-grained-microstructure is replaced by homogeneous equiaxed grains. The mechanical properties (e.g., strength and ductility) of the FeNiMnCr 18 alloy are comparable to those of the equiatomic FeNiCoMnCr high entropy alloy. Both strength and ductility increase with decreasing deformation temperature, with the largest difference occurring between 293 and 77 K. Extensive twin-bands which are bundles of numerous individual twins are observed when it is tensile-fractured at 77 K. No twin bands are detected by EBSD for materials deformed at 293 K and higher. Ultimately the unusual temperature-dependencies of UTS and uniform elongation could be caused by the development of the dense twin substructure, twin-dislocation interactions and the interactions between primary and secondary twinning systems which result in a microstructure refinement and hence cause enhanced strain hardening and postponed necking.

36 MATERIALS SCIENCE↗

The microstructure and tensile properties of extruded melt-spun ribbons of iron-rich B2 FeAl

The microstructure of extruded rods of iron-rich FeAl(B2-structure), as characterized by TEM, SEM, optical microscopy and x-ray diffractometry, consisted of elongated grains with a 111-line fibre texture containing a high dislocation density. Numerous oxide particles were found, mostly in lines which reflected the matrix flow during extrusion. In addition, some large inclusions were present. Tensile testing of annealed, relatively dislocation-free specimens as a function of increasing temperature found increasing ductility up to 900K, above which a ductility drop occurred accompanied by a change in fracture mode, from transgranular cleavage to intergranular fracture. The yield strength, which was independent of temperature up to 800K (at about 500MPa), also decreased rapidly as diffusion became more important. The predominant slip vector changed from 111-line to 100-line around 700K.

Baker, I.↗

Microstructure and magnetic properties of MFe{sub 2}O{sub 4} (M = Co, Ni, and Mn) ferrite nanocrystals prepared using colloid mill and hydrothermal method

Three kinds of spinel ferrite nanocrystals, MFe{sub 2}O{sub 4} (M = Co, Ni, and Mn), are synthesized using colloid mill and hydrothermal method. During the synthesis process, a rapid mixing and reduction of cations with sodium borohydride (NaBH{sub 4}) take place in a colloid mill then through a hydrothermal reaction, a slow oxidation and structural transformation of the spinel ferrite nanocrystals occur. The phase purity and crystal lattice parameters are estimated by X-ray diffraction studies. Scanning electron microscopy and transmission electron microscopy images show the morphology and particle size of the as-synthesized ferrite nanocrystals. Raman spectrum reveals active phonon modes at room temperature, and a shifting of the modes implies cation redistribution in the tetrahedral and octahedral sites. Magnetic measurements show that all the obtained samples exhibit higher saturation magnetization (M{sub s}). Meanwhile, experiments demonstrate that the hydrothermal reaction time has significant effects on microstructure, morphologies, and magnetic properties of the as-synthesized ferrite nanocrystals.

36 MATERIALS SCIENCE↗

Effect of non-axisymmetric arc on microstructure, texture and properties of variable polarity plasma arc welded 5A06 Al alloy

Highlights: • Variable polarity plasma arc welding of 5A06 Al alloy was carried out under the condition of non-axisymmetric arc. • Deformation bands formed in the weld joint were due to microstructural inhomogeneities. • Tensile fracture occurred along the deformation bands in the TZ/HAZ fusion boundary on the side of “lower arc”. • The weld zones are harder than the BM due to dislocation sub-structure, deformation bands and ultrafine subgrain. - Abstract: Microstructure, texture and mechanical properties in the weld joint of variable polarity plasma arc welding of 5A06 Al alloy under the condition of non-axisymmetric arc have been investigated. The weld joint are characterized by elongated structure in the base material (BM), the heat affected zone (HAZ) and the transition zone (TZ) and equiaxed structure in the fusion zone (FZ). Microstructure of the weld joint is asymmetrical and inhomogeneous leading to deformation bands. Deformation texture and recrystallization texture were developed in the weld zones. The FZ center was dynamic recrystallized due to severe deformation. Materials in the TZ have undergone dynamic recovery. The weld zones are harder than the BM due to dislocation sub-structure, deformation bands and ultrafine subgrains. Microhardness distribution was homogeneous in the regions without deformation bands. Tensile fracture occurred along the deformation bands on the side of “lower arc” exhibiting ductile fracture, while the BM is less ductile.

36 MATERIALS SCIENCE↗

Effect of temperature on microstructure and mechanical properties of ECAPed (TiB + La2O3)/Ti-6Al-4V composites

Highlights: • Dynamic recrystallization resulted in ultrafine grains near TiB interface region. • Tensile strength of ECAPed composites increased by up to 18%. • The average aspect ratio of TiB reduced with increasing ECAP temperature. • Interface debonding of TiB led to crack propagation and low ductility. TiB short fibers and La{sub 2}O{sub 3} particles reinforced titanium matrix composites (TMCs) were successfully equal-channel angular pressed (ECAPed) at 600 °C–900 °C. The effect of ECAP temperature on the microstructure and mechanical properties of the TMCs was investigated. The results indicated that dislocation tangling formed cell structures in matrix at lower ECAP temperature. In contrast, continuous dynamic recrystallization occurred at higher ECAP temperature, and promoted the formation of numerous new ultrafine grains. The average aspect ratio of TiB short fibers decreased with increasing ECAP temperature, which induced interfacial debonding. The tensile strength of TMCs ECAPed at 800 °C was up to 1128 MPa, which was 18% higher than the as-received composites. Interfacial debonding led TiB short fibers in low aspect ratios disabled to bear load, while the formation of ultrafine grains increased the strength of TMCs. The coupling of these two factors resulted in little effect of ECAP temperature on the tensile strength. However, the elongation of ECAPed TMCs generally decreased due to the loss of strain hardening capacity. Stress concentration tended to occur around the tips of TiB short fibers due to the interfacial debonding and cause crack propagation. It led to the premature fracture and low ductility.

36 MATERIALS SCIENCE↗

Uranium-Titanium Alloys: The Effect of Ti Content on Phase Transformations, Microstructures, and Mechanical Properties

This report documents the findings of collaborative research done at Sandia National Laboratory and the Y-12 Development Division during the 1980s. Ongoing progress reports were presented at various U. S. Department of Energy (DOE) meetings throughout the 1980s, but the findings were never integrated into an inclusive final report. This report provides a summary of the key findings and implications of this research. This work was supported by the DOE National Nuclear Security Administration. The effect of titanium content on phase transformations, microstructures, and mechanical properties of uranium-titanium alloys has been investigated in alloys containing 0.3 wt.% to 2.0 wt.% Ti.

36 MATERIALS SCIENCE↗

Microstructure and tribological properties of Ti-contained amorphous carbon film deposited by DC magnetron sputtering

Pure amorphous carbon (a-C) film and that with a small amount of Ti were deposited on high speed steel (W18Cr4V) substrates by means of dc closed field unbalanced magnetron sputtering. The chemical composition and microstructure of the a-C films were performed using x-ray photoelectron spectroscopy, x-ray diffraction, Raman spectra, and transmission electron microscopy. The mechanical and tribological properties were evaluated using a nanoindentor, Rockwell and scratch tests, and a conventional ball-on-disk tribometer, respectively. The pure a-C film showed the high hardness (53 GPa), elastic modulus (289 GPa), but the poor adhesive strength. When adding a small amount of Ti to the a-C film, both the adhesive strength and the tribological properties were improved. The Ti contained a-C film had the low wear rate (1.9x10{sup -17} m{sup 3} N{sup -1} m{sup -1}) and friction coefficient in humid air.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of quenched and tempered 300M steel

Type 300M steel, which is being used for the landing gear on the space shuttle orbiter, was subjected to a wide range of quenched and tempered heat treatments. The plane-strain fracture toughness and the tensile ultimate and yield strengths were evaluated. Cryogenic mechanical properties were obtained for conventionally heat-treated steel. The microstructure of all heat-treated test coupons was studied both optically and by transmission electron microscopy. Fracture surfaces were studied by means of scanning electron microscopy. Results indicate that substantial improvement in toughness with no loss in strength can be accomplished in quenched and tempered steel by austenitizing at 1255 K or higher. Low fracture toughness in conventionally austenitized 300M steel (1144 K) appears to be caused by undissolved precipitates, seen both in the submicrostructure and on the fracture surface, which promote failure by quasi-cleavage. The precipitates appeared to dissolve in the range 1200 to 1255 K.

Youngblood, J. L.↗

Influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy

Highlights: • The grain size was continuously reduced with the increasing Sc content. • No evidence for the formation of the Cu-rich and Sc-containing W phase was observed. • Sc addition could promote the precipitation of S′ in the absence of pre-age stretch. • Sc addition would reduce the growth rate of δ′ and δ′-PFZs. • The highest combinations of strength and ductility were obtained in cast Al-Li alloys. - Abstract: In this work, the influence of Sc content on the microstructure and mechanical properties of cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was investigated. It was found that the grain size of As-cast alloy was significantly reduced in steps with the increase of Sc addition, accompanied by the arising and increasing of cubic primary Al{sub 3}(Sc, Zr) phases. No evidence for the presence of the ternary W (Al{sub 8−x}Cu{sub 4+x}Sc) phase was obtained. The volume fraction of nanoscale Al{sub 3}(Sc, Zr) dispersoids was improved with the increase of Sc content, and the presence of Sc was observed to refine the S′ (Al{sub 2}CuMg) morphology during ageing. The addition of Sc lowered the growth rates of δ′ (Al{sub 3}Li) particles and δ′-Precipitate-free zones (δ′-PFZs) of the base alloy. The tensile property results showed that, with the increasing Sc content and ageing times, the yield strength (YS) and ultimate tensile strength (UTS) were continuously increased, and the highest elongation of 6.0% was obtained in the 0.2Sc-containing alloy aged for 32 h at 175 °C. The results indicated that the optimal Sc addition in cast Al-2Li-2Cu-0.5Mg-0.2Zr alloy was 0.2 wt%.

36 MATERIALS SCIENCE↗

Effect of Hot Isostatic Pressing on the Microstructure and Mechanical Properties of Additively Manufactured Ti Alloys

A previous SAND report, SAND2020-11353 described the basic metallurgical and surface roughness properties of additively manufactured Ti-64 material made using a powder bed fusion process. As part of that work, material was post-processed using a hot isostatic press (HIP) to densify and heat treat the material. This report is meant as an addendum to the original report and to provide specific data on material processed with HIP. The main focus of this report is to show the effects of HIP on the microstructure and mechanical properties of AM Ti-64 and Ti-5553.

36 MATERIALS SCIENCE↗

Effect of Yb Substitution on Microstructure and Superconducting Properties of Y{sub 1−x}Yb{sub x}Ba{sub 2}Cu{sub 3}O{sub 7−δ} Films

The purpose of this study was to improve the critical current density (J{sub c}) of YBa{sub 2}Cu{sub 3}O{sub 7−δ} (YBCO) superconducting films at high magnetic fields. Thin Y{sub 1−x}Yb{sub x}Ba{sub 2}Cu{sub 3}O{sub 7−δ} (Y{sub 1−x}Yb{sub x}BCO) superconducting films on LaAlO{sub 3} substrates were prepared by modified low-fluorine metal organic deposition method (LF-MOD) in order to investigate the effect of Yb substitution on the microstructure and superconducting properties of a YBCO-coated conductor. In this study, single-phased, c-axial-aligned Y{sub 1−x}Yb{sub x}BCO films were obtained. Yb doping had a little effect on the critical temperature (T{sub c}) and transition width (ΔT) values of Y{sub 1−x}Yb{sub x}BCO films. An abnormal phenomenon was observed that the J{sub c} of Y{sub 1−x}Yb{sub x}BCO films at low field was smaller than that of the pure YBCO film, but the J{sub c} of Y{sub 1−x}Yb{sub x}BCO films at high field was much greater than that of the undoped YBCO film. Compared to pure YBCO film, the J{sub c} values of Y{sub 0.75}Yb{sub 0.25}BCO and Y{sub 0.25}Yb{sub 0.75}BCO films were enhanced by a factor of 8 at 8 T, 65 K, which meant that chemical substitution of Yb into the Y site could improve flux pinning significantly under the high magnetic field in Y{sub 1−x}Yb{sub x}BCO coated conductors.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

An integrated study of thermal treatment effects on the microstructure and magnetic properties of Zn-ferrite nanoparticles

The evolution of the magnetic state, crystal structure and microstructure parameters of nanocrystalline zinc–ferrite, tuned by thermal annealing of ~4 nm nanoparticles, was systematically studied by complementary characterization methods. Structural analysis of neutron and synchrotron x-ray radiation data revealed a mixed cation distribution in the nanoparticle samples, with the degree of inversion systematically decreasing from 0.25 in an as-prepared nanocrystalline sample to a non-inverted spinel structure with a normal cation distribution in the bulk counterpart. The results of DC magnetization and Mossbauer spectroscopy experiments indicated a superparamagnetic relaxation in ~4 nm nanoparticles, albeit with different freezing temperatures T f of 27.5 K and 46 K, respectively. The quadrupole splitting parameter decreases with the annealing temperature due to cation redistribution between the tetrahedral and octahedral sites of the spinel structure and the associated defects. DC magnetization measurements indicated the existence of significant interparticle interactions among nanoparticles (‘superspins’). Additional confirmation for the presence of interparticle interactions was found from the fit of the T f (H) dependence to the AT line, from which a value of the anisotropy constant of K eff = 5.6 × 10 5 erg cm -3 was deduced. Further evidence for strong interparticle interactions was found from AC susceptibility measurements, where the frequency dependence of the freezing temperature T f (ƒ) was satisfactory described by both Vogel–Fulcher and dynamic scaling theory, both applicable for interacting systems. The parameters obtained from these fits suggest collective freezing of magnetic moments at T f .

Antic, Bratislav↗

Impact of initial temper of base metal on microstructure and mechanical properties of friction stir welded AA 7055 alloy

Highlights: • Friction stir welded 7055-T4 alloy exhibits higher tensile properties than T6 alloy. • Friction stir welded 7055-T4 alloy exhibits more uniform hardness distribution. • Some regions in heat affected zone have higher hardness than base metal in T4-joint. • Effect of initial temper on precipitate evolution in different zones is discussed. AA 7055-T6 and AA 7055-T4 aluminium alloy sheets were friction stir welded to investigate the impact of initial base metal temper on microstructure, hardness and tensile properties of the joints. In the joint of alloy in T6 temper (T6-joint), the hardness of the weld zone is lower than that of base metal; in the joint of alloy in T4 temper (T4-joint), however, some regions in the heat affected zone exhibit higher hardness than base metal. The weld nugget zone in T6-joint exhibits slightly lower hardness compared with that in T4-joint. The hardness minima is slightly higher in T4-joint than in T6-joint. T4-joint exhibits higher yield strength, ultimate tensile strength and elongation compared with T6-joint. Based on microstructure examination by transmission electron microscopy, the impact of initial precipitate state on precipitation behavior in the weld nugget zone, thermo-mechanically affected zone and heat affected zone during friction stir welding and mechanical properties of the joints is discussed.

36 MATERIALS SCIENCE↗

Microstructure, texture and mechanical properties of 6061 aluminum laser beam welded joints

Highlights: • Strong cube texture ({001}<100>) is observed in columnar dendrites. • The ratio of equiaxed dendrites shows proportional relationship with the strength. • The relations between process-microstructure-property are accurately established. - Abstract: In the present study, laser beam welding was carried out with 6061 Al alloy plate to study the microstructural evolution under various welding heat input (ηP/v = 30 J/mm, 38 J/mm, 46 J/mm, and 58 J/mm). The width of the weld metals increased continuously with the heat input values. Quantitatively correlation of the microstructure distribution with welding parameters was developed based on the EBSD results. The weld metals mainly consisted of coarse columnar dendrites and equiaxed dendrites. The ratio of equiaxed dendrites which were controlled by constitutional supercooling and heterogeneous nuclei showed directly proportional relationship with the weld strength. Strong cube texture ({001}<100>) was observed in columnar dendrites, which showed harmful effect on the weld strength. Slight softening in heat affected zone due to recrystallization was identified by nanoindentation tests. All specimens failed in weld metal and the fracture surfaces showed the characteristics of ductile fracture.

36 MATERIALS SCIENCE↗

Microstructure and dielectric properties of BaTiO{sub 3} ceramic doped with yttrium, magnesium, gallium and silicon for AC capacitor application

Graphical abstract: Core–shell structure can be obtained in BaTiO{sub 3} ceramics co-doped with Y–Mg-Ga-Si. Y-Mg-Ga-Si co-dopant can obviously reduce dielectric loss, improve AC breakdown voltage and flatten temperature dependence of capacitance curve. - Highlights: • Y-Mg-Ga-Si co-doped BaTiO{sub 3} ceramics with core-shell structure were prepared. • Y{sup 3+}, Mg{sup 2+}, and Ga{sup 3+} dissolved in the lattice BaTiO{sub 3} replacing Ba{sup 2+} site or Ti{sup 4+} site. • Y{sup 3+} and Ga{sup 3+} tended to remain close to the grain boundaries as a shell maker. • Y-Mg-Ga-Si co-doped BaTiO{sub 3} ceramics show high AC breakdown voltage and low tanδ. - Abstract: The microstructures and dielectric properties of Y-Mg-Ga-Si co-doped barium titanate ceramics were investigated. Y{sup 3+} dissolved in the lattice of BaTiO{sub 3} replacing both Ba{sup 2+} site and Ti{sup 4+} site, and Mg{sup 2+} replaced Ti{sup 4+} site. The replacements of Y{sup 3+} and Mg{sup 2+} inhibit the grain growth, cause tetragonal-to-pseudocubic phase transition, reduce the dielectric loss, and flatten the temperature dependence of capacitance curve. The incorporation of Ga{sup 3+} can improve sintering and increase permittivity. Y{sup 3+} and Ga{sup 3+} tended to remain close to the grain boundaries, and play an important role as a shell maker in the formation of the core–shell structure in the co-doped BaTiO{sub 3} ceramics. Excellent dielectric properties: ϵ{sub r} = ∼2487, tanδ = ∼0.7% (at 1 kHz), ΔC/C{sub 25} < ∼6.56% (from −55 °C to 125 °C) and alternating current breakdown voltage E < ∼4.02 kV/mm can be achieved in the BaTiO{sub 3}–0.02Y{sub 2}O{sub 3}–0.03MgO–0.01Ga{sub 2}O{sub 3}–0.005SiO{sub 2} ceramics sintered at 1380 °C. This material has a potential application in alternating current multilayer ceramic capacitor.

36 MATERIALS SCIENCE↗

Effect of pre-cold rolling on the evolution of microstructure, microtexture, and mechanical properties of the mushy state rolled in-situ Al-4.5Cu-5TiB2 composite

Highlights: • Microstructure-Microtexture evolution study of the mushy state rolled composite (MRC) and MRC with pre-cold rolling (PCMRC). • The Microstructure and microtexture were characterized using SEM, EBSD, and TEM. • Exactly opposite trends in micro-hardness variation across the thickness of MRC and PCMRC were discussed. • The PCMRC exhibited the best combination of hardness, strength, and ductility. • A proper microstructure-microtexture-property correlation was established with experimental evidence. The mushy state rolling has been found as a promising technique for near-net forming of the cast Al-4.5 wt% Cu-5 wt% TiB{sub 2} in-situ composite to obtain microstructural refinement and moderate mechanical properties. Cold rolling with 30% reduction in thickness was carried out before mushy state rolling, for achieving a relatively more homogeneous distribution of CuAl{sub 2}-TiB{sub 2} particles as well as an appropriate microstructure to enhance the mechanical properties. A comparative investigation on the microstructural and microtextural evolution, along with mechanical properties of both the mushy state rolled composite (MRC) and pre-cold rolled mushy-state rolled composite (PCMRC) was performed, and the microstructure-property correlation was established. The PCMRC exhibited the lowest homogenized lengthscale parameter (L{sub H} 29 μm) indicating the maximum uniformity of particle distribution, computed with the help of multi-scalar analysis of area fractions (MSAAF) technique. Electron back-scattered diffraction (EBSD) and transmission electron microscopy (TEM) studies revealed the presence of fine sub-grains within centrally located deformed Al grains due to dynamic recovery, as well as the particle stimulated nucleation of equiaxed fine Al grains by dynamic recrystallization or rapid solidification of liquid near edges for both the investigated composites. The PCMRC displayed a superior combination of hardness (96.82 ± 4.5 HV{sub 5kgf}), 40% higher ultimate tensile strength (301.4 ± 1.8 MPa), and 68% more uniform elongation (30.8% ± 0.5%), compared to the MRC. The improvement in mechanical properties is attributed to the uniform particle distribution and presence of both higher density of low angle boundaries and recrystallized grains adjacent to the particles, obtained from prior cold rolling.

36 MATERIALS SCIENCE↗

Microstructural Characteristics, Mechanical Properties, and Corrosion Behavior of Field-Assisted Diffusion Welded Alloy 617

This study investigated the microstructural characteristics, mechanical response, and corrosion resistance of Alloy 617 diffusion welded by electric field-assisted sintering (EFAS). The microstructure exhibited good grain boundary (GB) migration across the interface and flat interface in the samples bonded at different conditions. Graded grain size was observed, with grain coarsening being more significant near sample surface due to EFAS-induced temperature gradient. Tensile testing revealed that the specimens fractured in the matrix away from the interface. The peak strength of 807 MPa was obtained in the samples welded at 1000°C. The materials obtained at 1100°C exhibited reduced tensile strength but improved ductility. Strain maps revealed by digital image correlation showed the flat interfaces were less ductile compared to the matrix. The hardness reduced near sample surfaces due to enlarged grains induced by temperature gradient. The interfaces with GB migration exhibited improved corrosion resistance in molten salt compared to the flat interfaces.

36 - MATERIALS SCIENCE↗

The Effects of Heat Treatment on Microstructure and Mechanical Properties of Tribaloy 400 Coatings Deposited by Laser Cladding

The effects of heat treatment on the microstructure, microhardness, nanohardness and wear resistance of Tribaloy 400 coatings prepared by laser cladding on 304 stainless steel were studied in this paper. The results show that the microstructures of Tribaloy 400 laser cladding layer are cobalt matrix dendrites and eutectic structure. After the heat treatment at 1250 °C for 1 h, the eutectic structure disappears and the strip-like Laves phase is formed on the Co matrix. Meanwhile, the hardness is obviously improved. After the heat treatment at 1250 °C for 1 h and then 900 °C for 4 h, a small amount of ε-Co appears, the strip-like Laves phases become coarser and blunter, and some of the strip structures combine together to form blocky structures, and the hardness is decreased. The wear resistance of the samples at 600 °C is better than that at RT since the hardness of the Laves phase increases with the rise in temperature.

36 MATERIALS SCIENCE↗