Field cooling dependence of the anisotropy in exchange biased FeF{sub 2}/Co films.

The magnetization reversal in exchange biased FeF{sub 2}/Co films was studied using polarized neutron reflectometry and magneto-optical imaging (MOI). After field cooling in a field H perpendicular to the c axis (the easy axis of FeF{sub 2}) through the FeF{sub 2} Neel temperature, the magnetization curve measured with H parallel to the c axis showed a double loop, one with a positive exchange bias field (H{sub E}) and one with a negative H{sub E}. This behavior suggests that the antiferromagnet (AFM) is split into two types of domains with H{sub E} in opposite directions along the c axis. However, the observation of spin-flip reflectivity in the field region separating the two loops indicates that some rotation of the Co magnetization also occurred during reversal. Concurrently, small inhomogeneous domains with sizes much less than 30 {micro}m were observed using MOI. This implies that small AFM domains with opposing H{sub E} created during cooling and the resulting frustration of the interface exchange interaction with the ferromagnet are responsible for the perpendicular magnetization during reversal.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Magnetocapacitance of polycrystalline Bi{sub 5}Ti{sub 3}FeO{sub 15} prepared by sol-gel method

Bi{sub 5}Ti{sub 3}FeO{sub 15} bulk ceramic and thin film samples are prepared using the sol-gel method. The dielectric, ferroelectric, and magnetic behaviors of these samples are measured in order to investigate the possible multiferroic effect. The superparamagnetic behavior with dominant antiferromagnetic (AFM) interaction background for the as-prepared Bi{sub 5}Ti{sub 3}FeO{sub 15} samples is revealed. The clearly identified magnetocapacitance effect at low temperature is argued to originate from the suppression of the AFM interaction by external magnetic field.

36 MATERIALS SCIENCE↗

Kinetic mechanism of the thermal-induced self-organization of Au/Si nanodroplets on Si(100): Size and roughness evolution

Very thin Au layer was deposited on Si(100) using the sputtering technique. By annealing at 873 K Au/Si nanodroplets were formed and their self-organization was induced changing the annealing time. The evolution of droplet size distribution, center-to-center distance distribution, and droplet density as a function of the annealing time at 873 K was investigated by Rutherford backscattering spectrometry, atomic force microscopy (AFM), and scanning electron microscopy. As a consequence of such study, the droplet clustering is shown to be a ripening process of hemispherical three-dimensional structures limited by the Au surface diffusion. The application of the ripening theory allowed us to calculate the surface diffusion coefficient and all other parameters needed to describe the entire process. Furthermore, the AFM measurements allowed us to study the roughness evolution of the sputtered Au thin film and compare the experimental data with the dynamic scaling theories of growing interfaces.

36 MATERIALS SCIENCE↗

On PbTiO{sub 3}-(111)-Pt interfacial layers and their x-ray photoelectron spectroscopy signature

In this work emphasis is placed on the investigation of interfacial layers between sol-gel processed PbTiO{sub 3} (PTO) thin films and (111)Pt terminated silicon substrates. The methods used are x-ray diffraction, x-ray photoelectron spectroscopy (XPS) combined with depth profiling, and atomic force microscopy (AFM). In order to avoid artifacts related to ion bombardment, e.g., reduction of Pb ions and preferential sputtering, gentle argon ion bombardment conditions were first derived. AFM investigations of native and ion bombarded films at different stages of depth profiling show that the films are homogenously sputtered, whereby the film roughness remains practically unchanged in the course of sputtering. An annealing treatment at 550 deg. C under reducing atmosphere was used to provoke the formation of an interfacial intermetallic (111)Pt{sub x}Pb phase, which is shown to coexist with an amorphous oxide film. This could allow us to establish the XPS signature of the intermetallic phase. A negative shift of the Pt (4f) binding energy and a large full width at half maximum of the Pb (4f) peak are the attributes of this signature. PTO-film annealing in air at temperatures between 350 and 600 deg. C leads to the formation of the perovskite phase, starting at 500 deg. C, directly from the amorphous phase. Based on its derived XPS signature it is shown that the intermetallic phase still exists at the interface with variable thickness depending on the annealing temperature. The pronounced (111) texture of the PTO-crystallized films is thought to be the direct consequence of this intermetallic template layer. It is also shown that the outermost surface of the PTO film is enriched with PbO as a result of segregation phenomena.

36 MATERIALS SCIENCE↗

Real-time studies of surface roughness development and reticulation mechanism of advanced photoresist materials during plasma processing

Surface roughness development of photoresist (PR) films during low pressure plasma etching has been studied using real-time laser light scattering from photoresist materials along with ellipsometric and atomic force microscopy (AFM) characterization. We show that evolution of the intensity of light scattered from a film surface can be used to study the development of surface roughness for a wide range of roughness starting from subnanometer to few hundred nanometers. Laser light scattering in combination with ellipsometry and AFM is also used to study the reticulation mechanism of 193 and 248 nm PRs during argon plasma processing. We employ a three-layer model (modified layer, rough layer, and bulk film) of the modified PR surface (193 and 248 nm PRs) to simulate and understand the behavior of ellipsometric {psi}-{delta} trajectories. Bruggeman's effective medium approximation is employed to study the roughness that develops on the surface after reticulation. When the glass transition temperature of the organic materials is reached during Ar plasma processing, the PR films reticulate and roughness develops rapidly. Roughness development is more pronounced for 248 nm PR than for 193 nm PR. Simulation of {psi}-{delta} shows that the growth of roughness is accompanied by strong expansion in the materials, which is stronger for 248 nm PR than 193 nm PR. The leading factors responsible for reticulation are found to be compressive stress that develops in the modified surface layer as it is created along with strong molecular chain motion and expansion of the material when the temperature is increased past the glass transition temperature. Reticulation leads to a significantly different surface morphology for 248 nm PR as compared to 193 nm PR and can be related to differences in molecular structure and composition leading to different responses when a modified surface layer is formed by ion bombardment accompanying plasma etching.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of thermal processing on silver thin films of varying thickness deposited on zinc oxide and indium tin oxide

Silver films of varying thicknesses (25, 45, and 60 nm) were deposited on indium tin oxide (ITO) on silicon and zinc oxide (ZnO) on silicon. The films were annealed in vacuum for 1 h at different temperatures (300-650 deg. C). Four-point-probe measurements were used to determine the resistivity of the films. All films showed an abrupt change in resistivity beyond an onset temperature that varied with thickness. Rutherford backscattering spectrometry measurements revealed agglomeration of the Ag films upon annealing as being responsible for the resistivity change. X-ray pole figure analysis determined that the annealed films took on a preferential <111> texturing; however, the degree of texturing was significantly higher in Ag/ZnO/Si than in Ag/ITO/Si samples. This observation was accounted for by interface energy minimization. Atomic force microscopy (AFM) measurements revealed an increasing surface roughness of the annealed films with temperature. The resistivity behavior was explained by the counterbalancing effects of increasing crystallinity and surface roughness. Average surface roughness obtained from the AFM measurements were also used to model the agglomeration of Ag based on Ostwald ripening theory.

36 MATERIALS SCIENCE↗

A direct micropipette-based calibration method for atomic force microscope cantilevers

In this report, we describe a direct method for calibrating atomic force microscope (AFM) cantilevers with the micropipette aspiration technique (MAT). A closely fitting polystyrene bead inside a micropipette is driven by precisely controlled hydrostatic pressures to apply known loads on the sharp tip of AFM cantilevers, thus providing a calibration at the most functionally relevant position. The new method is capable of calibrating cantilevers with spring constants ranging from 0.01 to hundreds of newtons per meter. Under appropriate loading conditions, this new method yields measurement accuracy and precision both within 10%, with higher performance for softer cantilevers. Furthermore, this method may greatly enhance the accuracy and precision of calibration for colloidal probes.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Influence of Hydrogen Plasma Treatment Time to Si:H Layer Deposition Time Ratio on the Properties of Layer-by-Layer Deposited Hydrogenated Silicon (Si:H) Thin Films

Hydrogenated silicon (Si-H) thin films were deposited from a mixture of pure silane (SiH{sub 4}) and hydrogen (H{sub 2}) gases in a home-built plasma enhanced chemical vapour deposition (PECVD) system using the layer-by-layer (LBL) deposition technique. In the LBL process, the deposition was performed by periodically alternating the deposition of Si:H layer with the hydrogen treatment process of the growth surface. In this work, the effects of the H plasma treatment time to Si-H layer growth time ratio on the film properties were studied. The LBL deposited Si-H films studied in this work were deposited using different Si-H layer growth times ranging from 2 minutes to 7 minutes with the hydrogen plasma treatment time on the growth surface fixed at 3 minutes. Optical transmission spectroscopy, X-ray diffraction (XRD), micro-Raman scattering spectroscopy, Fourier transform infrared (FTIR) spectroscopy and atomic force microscopy (AFM) measurements were done on these films to investigate the optical, structural and morphological properties of the films. The films deposited by this technique produced the highest deposition rate of 6.3 A ring /s when the growth time of the Si-H layer was fixed at 5 minutes. These films were amorphous in structure and had large optical energy gaps irrespective of the Si-H layer deposition time. High concentration of cone-like structures was observed in the AFM images for the films deposited using the higher Si-H layer deposition times.

36 MATERIALS SCIENCE↗

Surface modification of magnetic recording media by filtered cathodic vacuum arc

Surface modification of a magnetic recording medium was accomplished by filtered cathodic vacuum arc (FCVA). The carbon overcoat of thin-film disks was removed by Ar{sup +} ion sputter etching in vacuum to prevent oxidation of the exposed magnetic medium, which was then modified by FCVA carbon plasma under conditions of zero and -100 V pulsed substrate bias. Monte Carlo simulations performed with the T-DYN code, x-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM), and surface force microscopy (SFM) provided insight into carbon implantation profiles, surface chemical composition, roughness, and nanomechanical properties of the surface-treated magnetic medium. The dependence of surface modification on the FCVA treatment conditions is discussed in the context of T-DYN, XPS, AFM, and SFM results. The findings of this study demonstrate the potential of FCVA to provide overcoat-free magnetic recording media exhibiting oxidation resistance and enhanced nanomechanical properties.

36 MATERIALS SCIENCE↗

On eigenmodes, stiffness, and sensitivity of atomic force microscope cantilevers in air versus liquids

The effect of hydrodynamic loading on the eigenmode shapes, modal stiffnesses, and optical lever sensitivities of atomic force microscope (AFM) microcantilevers is investigated by measuring the vibrations of such microcantilevers in air and water using a scanning laser Doppler vibrometer. It is found that for rectangular tipless microcantilevers, the measured fundamental and higher eigenmodes and their equivalent stiffnesses are nearly identical in air and in water. However, for microcantilevers with a tip mass or for picket shaped cantilevers, there is a marked difference in the second (and higher) eigenmode shapes between air and water that leads to a large decrease in their modal stiffness in water as compared to air as well as a decrease in their optical lever sensitivity. These results are explained in terms of hydrodynamic interactions of microcantilevers with nonuniform mass distribution. The results clearly demonstrate that tip mass and hydrodynamic loading must be taken into account in stiffness calibration and optical lever sensitivity calibration while using higher-order eigenmodes in dynamic AFM.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electronic properties of ultrananocrystalline diamond surfaces.

We have characterized ultrananocrystalline diamond films with different surface terminations by x-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM), scanning tunneling microscopy (STM) and scanning tunneling spectroscopy (STS). The surface terminations were performed by plasma functionalization in atmospheres of hydrogen, fluorine, and oxygen. XPS proves the dense monolayer coverage of the surface functionalization. AFM and STM show low impact of the plasma treatment on the surface morphology. STS has been used to investigate the surface electronic properties, for H-terminated surfaces the electronic structure is dominated by the sp{sup 3} carbon phase of the grain surfaces; for O- and F-terminated surfaces, however, sp{sup 2} carbon from the grain boundaries seems to determine the surface band gap.

08 HYDROGEN↗

Magnetic properties of iron nanoparticle

Magnetic properties of Fe nanoparticles with different sizes synthesized by a physical deposition technique have been investigated experimentally. We have used a high pressure sputtering technique to deposit iron nanoparticles on a silicon substrate. The nanoparticles are then analyzed using atomic force microscopy (AFM), transmission electron microscopy (TEM), and superconducting quantum interference device techniques. TEM and AFM data show that the particle size could be tuned by adjusting the deposition conditions. The magnetic properties have been investigated from temperature dependent magnetization M(T) and field dependent magnetization M(H) measurements. The results show that two phases including both ferromagnetic and superparamagnetic particles are present in our system. From these data we extracted the superparamagnetic critical size to be 9 nm for our samples. Ferromagnetic particles are single magnetic domain particles and the magnetic properties can be explained by the Stoner and Wohlfarth model. For the superparamagnetic phase, the effective anisotropy constant, K{sub eff}, decreases as the particle size increases.

36 MATERIALS SCIENCE↗

Integration of an Atomic Force Microscope in a Beamline Sample Environment

We developed and optimised an optics-free Atomic Force Microscope (AFM) that can be directly installed on most of the synchrotron radiation end-stations. The combination of Scanning Probe Microscopies with X-ray microbeams adds new possibilities to the variety of synchrotron radiation techniques. The instrument can be used for atomic force imaging of the investigated sample or to locally measure the X-ray absorption or diffraction, or it can also be used to mechanically interact with the sample while simultaneously taking spectroscopy or diffraction measurements. The local character of these measurements is intrinsically linked with the use of the Atomic Force Microscope tip. It is the sharpness of the tip that gives the opportunity to measure the photons flux impinging on it giving beam position monitor features, or allows to locally measure the absorption coefficient or the shape of the diffraction pattern. As an example of the possibilities opened by the instrument we will show diffraction measurements performed on a Ge/Si island while being indented with the AFM tip providing local measure of the Young coefficient. Three ESRF beamlines are going to be equipped with this new instrument.

43 PARTICLE ACCELERATORS↗

Improved in situ spring constant calibration for colloidal probe atomic force microscopy

In colloidal probe atomic force microscopy (AFM) surface forces cannot be measured without an accurate determination of the cantilever spring constant. The effective spring constant k depends upon the cantilever geometry and therefore should be measured in situ; additionally, k may be coupled to other measurement parameters. For example, colloidal probe AFM is frequently used to measure the slip length b at solid/liquid boundaries by comparing the measured hydrodynamic force with Vinogradova slip theory (V-theory). However, in this measurement k and b are coupled, hence, b cannot be accurately determined without knowing k to high precision. In this paper, a new in situ spring constant calibration method based upon the residuals, namely, the difference between experimental force-distance data and V-theory is presented and contrasted with two other popular spring constant determination methods. In this residuals calibration method, V-theory is fitted to the experimental force-distance data for a range of systematically varied spring constants where the only adjustable parameter in V-theory is the slip length b. The optimal spring constant k is that value where the residuals are symmetrically displaced about zero for all colloidal probe separations. This residual spring constant calibration method is demonstrated by studying three different liquids (n-decanol, n-hexadecane, and n-octane) and two different silane coated colloidal probe-silicon wafer systems (n-hexadecyltrichlorosilane and n-dodecyltrichlorosilane).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrical characterization of HgTe nanowires using conductive atomic force microscopy

Self-organized HgTe nanowires grown by molecular beam epitaxy (MBE) have been characterized using conductive atomic force microscopy. As HgTe will degrade or evaporate at normal baking temperatures for electron beam lithography (EBL) resists, an alternative method was developed. Using low temperature optical lithography processes, large Au contacts were deposited on a sample covered with randomly oriented, lateral HgTe nanowires. Nanowires partly covered by the large electrodes were identified with a scanning electron microscope and then localized in the atomic force microscope (AFM). The conductive tip of the AFM was then used as a movable electrode to measure current-voltage curves at several locations on HgTe nanowires. The measurements revealed that polycrystalline nanowires had diffusive electron transport, with resistivities two orders of magnitude larger than that of an MBE-grown HgTe film. The difference can be explained by scattering at the rough surface walls and at the grain boundaries in the wires. The method can be a solution when EBL is not available or requires too high temperature, or when measurements at several positions along a wire are required.

36 MATERIALS SCIENCE↗

Effect of tip shape on line edge roughness measurement based on atomic force microscopy

Atomic force microscopy (AFM) is an important tool in line edge roughness (LER) measurements, where accuracy for line edge identification is influenced by the shape of the tip. In this article, the effect of tip shape on LER measurement based on AFM is studied theoretically. The formulas for calculating the distance between the measured and actual line edge of the sample are presented. The effects of the three kinds of tips with different shapes are experimentally compared for validation. Suggestions on how to reduce measuring error caused by tip shape are also given.

36 MATERIALS SCIENCE↗

Switching surface polarization of atomic force microscopy probe utilizing photoisomerization of photochromic molecules

An attempt to develop an atomic force microscopy (AFM) probe with optically switchable polarization is described. Modification with a single molecular layer of photochromic molecules was attempted onto a Si substrate that is a prototype for a probe surface. Polarization switching caused by alternate irradiation of UV and visible lights were detected using the electrostatic force?>spectroscopy (EFS) technique. Si substrates modified with spiropyran and azobenzene exhibited reversible polarization switching that caused changes in CPD of about 100 and 50 mV, respectively. Modification with spiropyran was also attempted onto a Si probe and resulted in a CPD change of about 100 mV. It was confirmed that modification of an AFM probe or substrate with a single molecular layer of photochromic molecules can generate surface polarization switching of a mechanically detectable level.

74 ATOMIC AND MOLECULAR PHYSICS↗

UV nanoimprint lithography for the realization of large-area ordered SiGe/Si(001) island arrays

We use UV nanoimprint lithography for the pit-patterning of silicon substrates. Ordered silicon-germanium islands are grown inside these pits by molecular-beam epitaxy on arrays of 3x3 mm{sup 2} and characterized by atomic force microscopy (AFM) and photoluminescence (PL) measurements. AFM-based statistics reveals an extremely uniform size distribution of the islands in the patterned areas. These results are confirmed by very narrow and uniform PL peaks recorded at various positions across the patterned arrays.

36 MATERIALS SCIENCE↗