At least 937 records · Page 52

Understanding Pore Formation in ALD Alumina Overcoats

AlO X thin films deposited by atomic layer deposition (ALD) have previously been used to increase both stability and selectivity of supported palladium catalysts and are known to develop nanoscale porosity upon heating. Furthermore, understanding the factors that affect ALD thin film porosity would enable future design of layered catalytic structures with tunable nanoscale features on industrially relevant high surface area materials. In this study, porous and nonporous aluminum oxide supports with and without palladium nanoparticles were overcoated with thin films of 2 - 7 nm AlO X by ALD deposited at temperatures of 100 °C, 200 °C and 300 °C. Hydroxyl loss and changes in surface chemistry were observed upon heating the films, and changes in surface area and pore volume of the annealed films were correlated to AlO x deposition temperature and presence of Pd. Crystallization of the overcoat to γ-Al 2 O 3 is shown to occur separately from hydroxyl loss and pore formation. A mechanistic understanding of pore formation in AlO X ALD films is obtained by reference to studies of the structural transformations accompanying the formation of transition aluminas from hydroxide precursors. Additionally, a direct and tunable correlation is established between pore development and the overall hydroxyl content of AlO X ALD coatings.

36 MATERIALS SCIENCE↗

Robust Fe divalent state in one-unit-cell $\mathrm{FeSe/SrTiO_3}$ thin films

The orbital occupancy, as the origin of Hund's rule coupling, provides critical information in understanding the multiorbital iron-based superconductors. The one-unit-cell (1UC) FeSe thin film on a SrTiO 3 substrate with superconductive T c above 60 K has been reported with unique electronic structures as well as orbital occupancy. In this paper, we present the x-ray absorption spectroscopy and resonant inelastic x-ray scattering (RIXS) study of the FeSe/STO thin films of different thicknesses. Together with the atomic multiplet simulation analysis, the FeSe/STO thin films (from 1UC to 10UC) are shown with the pure 3d6 electronic configuration which is identical to the bulk FeSe. Moreover, 1UC FeSe/STO is found to be distinctively more persistent in hosting the 3d6 configuration other than the thicker films under the oxidization process. The robustness of the 3d6 in 1UC FeSe/STO is discussed as a result of charge transfer from the substrate, as well as a mechanism to maintain the high-T c superconductivity. Additionally our research calls for a further high-resolution RIXS study of the pristine superconductive 1UC FeSe/STO thin film.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

On the reliability of nanoindentation hardness of Al{sub 2}O{sub 3} films grown on Si-wafer by atomic layer deposition

The interest in applying thin films on Si-wafer substrate for microelectromechanical systems devices by using atomic layer deposition (ALD) has raised the demand on reliable mechanical property data of the films. This study aims to find a quick method for obtaining nanoindentation hardness of thin films on silicon with improved reliability. This is achieved by ensuring that the film hardness is determined under the condition that no plastic deformation occurs in the substrate. In the study, ALD Al{sub 2}O{sub 3} films having thickness varying from 10 to 600 nm were deposited on a single-side polished silicon wafer at 300 °C. A sharp cube-corner indenter was used for the nanoindentation measurements. A thorough study on the Si-wafer reference revealed that at a specific contact depth of about 8 nm the wafer deformation in loading transferred from elastic to elastic–plastic state. Furthermore, the occurrence of this transition was associated with a sharp increase of the power-law exponent, m, when the unloading data were fitted to a power-law relation. Since m is only slightly material dependent and should fall between 1.2 and 1.6 for different indenter geometry having elastic contact to common materials, it is proposed that the high m values are the results from the inelastic events during unloading. This inelasticity is linked to phase transformations during pressure releasing, a unique phenomenon widely observed in single crystal silicon. Therefore, it is concluded that m could be used to monitor the mechanical state of the Si substrate when the whole coating system is loaded. A suggested indentation depth range can then be assigned to each film thickness to provide guidelines for obtaining reliable property data. The results show good consistence for films thicker than 20 nm and the nanoindentation hardness is about 11 GPa independent of film thickness.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Atomic-Scale Behavior of Radiation-Resistant ZnO under High-Energy Electron Bombardment

Understanding the atomic structure and defect characteristics of ZnO thin films is crucial for optimizing their electronic properties and performance in advanced applications. Here, we investigate the atomic structure and defect characteristics of atomic layer deposition (ALD)-grown ZnO thin films by using aberration-corrected scanning transmission electron microscopy (STEM). Atomic-resolution imaging identifies prevalent stacking faults, dipole disorder, and various grain boundary types, which are believed to influence the electronic properties of ZnO. Additionally, real-time electron beam exposure experiments demonstrate structural transformations, including crystal growth and surface rearrangements. These findings provide insights into the growth mechanisms of ALD ZnO under high-energy electron irradiation conditions, an important finding for the use of polycrystalline ZnO wide bandgap semiconductors in space-like conditions. In conclusion, our results underscore the capability of STEM in directly visualizing and quantifying atomic-scale defects and beam-induced transformations in radiation-resistant ZnO.

Defects↗

The Piezoresponse in WO3 Thin Films Due to N2-Filled Nanovoids Enrichment by Atom Probe Tomography

Tungsten trioxide (WO3) is a versatile n-type semiconductor with outstanding chromogenic properties highly used to fabricate sensors and electrochromic devices. We present a comprehensive experimental study related to piezoresponse with piezoelectric coefficient d33 = 35 pmV−1 on WO3 thin films ~200 nm deposited using RF-sputtering onto alumina (Al2O3) substrate with post-deposit annealing treatment of 400 °C in a 3% H2/N2-forming gas environment. X-ray diffraction (XRD) confirms a mixture of orthorhombic and tetragonal phases of WO3 with domains with different polarization orientations and hysteresis behavior as observed by piezoresponse force microscopy (PFM). Furthermore, using atom probe tomography (APT), the microstructure reveals the formation of N2-filled nanovoids that acts as strain centers producing a local deformation of the WO3 lattice into a non-centrosymmetric structure, which is related to piezoresponse observations.

36 MATERIALS SCIENCE↗

High sensitive formaldehyde graphene gas sensor modified by atomic layer deposition zinc oxide films

Zinc oxide (ZnO) thin films with various thicknesses were fabricated by Atomic Layer Deposition on Chemical Vapor Deposition grown graphene films and their response to formaldehyde has been investigated. It was found that 0.5 nm ZnO films modified graphene sensors showed high response to formaldehyde with the resistance change up to 52% at the concentration of 9 parts-per-million (ppm) at room temperature. Meanwhile, the detection limit could reach 180 parts-per-billion (ppb) and fast response of 36 s was also obtained. The high sensitivity could be attributed to the combining effect from the highly reactive, top mounted ZnO thin films, and high conductive graphene base network. The dependence of ZnO films surface morphology and its sensitivity on the ZnO films thickness was also investigated.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Growth study of ion assisted evaporated molybdenum thin films

We reported optimization of ion-to-atom ratios and ion energy for growth of molybdenum thin film on oxidized silicon substrate using ion assisted electron beam evaporation system. The ion-to-atom ratio is varied by independently adjusting the ion current density and deposition rate. The structural characterization of the films is carried out by hard X-ray reflectivity. We observed improvement in film density from 85.5% to 98.2% and film roughness from {approx}2 nm to 0.84nm on {approx}26 nm thick Mo film by optimizing ion parameters. The observed results are discussed considering the effect of kinetic of adatoms during growth of film.

36 MATERIALS SCIENCE↗

Atomic layer deposition of titanium nitride for quantum circuits

Superconducting thin films with high intrinsic kinetic inductance are of great importance for photon detectors, achieving strong coupling in hybrid systems, and protected qubits. We report on the performance of titanium nitride resonators, patterned on thin films (9–110 nm) grown by atomic layer deposition, with sheet inductances of up to 234 pH/. For films thicker than 14 nm, quality factors measured in the quantum regime range from 0.2 to 1.0 × 10 6 and are likely limited by dielectric two-level systems. Additionally, we show characteristic impedances up to 28 kΩ, with no significant degradation of the internal quality factor as the impedance increases. In conclusion, these high impedances correspond to an increased single photon coupling strength of 24 times compared to a 50 Ω resonator, transformative for hybrid quantum systems and quantum sensing.

36 MATERIALS SCIENCE↗

Dynamics of Emergent Crystallinity in Photonic Quantum Materials

This proposal will employ a revolutionary cold atom/photon hybrid material that combines the advantages of cold atom and semiconductor approaches: By confining a thin layer of Rydberg-EIT dressed atoms in the waist of a confocal optical resonator, a new synthetic material will emerge, akin to an exciton-polariton gas, but with stronger interactions and exquisite control: In the resonator, photons and Rydbergs hybridize, producing quasi-particles whose low mass is inherited from photons, and strong interactions from the Rydbergs. These particles have adjustable mass, interactions, and confinement, allowing tuning from a BEC to an unexplored regime expected to exhibit crystallinity. By studying non-equilibrium evolution near this transition, it will be possible to investigate quantum dynamics in a non-classical crystal, where quantum zero-point motion is substantial. Such a regime offers a unique opportunity to probe the universality of quantum dynamics, and also to study, for the first time, a form of quantum “soft-matter”, where the lattice structure is emergent, and competes with quantum fluctuations through the introduction of strongly interacting topological defects.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Optical and morphological characterizations of pyronin dye-poly (vinyl alcohol) thin films formed on glass substrates

Thin films of pyronin dye mixed with poly(vinyl alcohol) (PVA) on glass substrate were prepared by using spin-coating technique. The optical and morphological properties of the thin films were studied by UV-Vis., steady-state fluorescence spectroscopies and atomic force microscopy (AFM). The thin films on glass substrate were fabricated at various [PVA]/[dye] (P/D) ratios. Hence, the monomeric and H-aggregates thin films of pyronin dye mixed with PVA were formed as a function of the dye and PVA concentration. It was determined that while the monomeric thin films showed strong fluorescence, the formation of H-aggregates in the thin film caused to decreasing the fluorescence intensity. AFM studies demonstrated that the morphology of the thin film was drastically varied with changing the optical property of the thin film such as monomeric and H-aggregates thin films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Optical characteristics of nanocrystalline Al{sub x}Ga{sub 1−x}N thin films deposited by hollow cathode plasma-assisted atomic layer deposition

Gallium nitride (GaN), aluminum nitride (AlN), and Al{sub x}Ga{sub 1−x}N films have been deposited by hollow cathode plasma-assisted atomic layer deposition at 200 °C on c-plane sapphire and Si substrates. The dependence of film structure, absorption edge, and refractive index on postdeposition annealing were examined by x-ray diffraction, spectrophotometry, and spectroscopic ellipsometry measurements, respectively. Well-adhered, uniform, and polycrystalline wurtzite (hexagonal) GaN, AlN, and Al{sub x}Ga{sub 1−x}N films were prepared at low deposition temperature. As revealed by the x-ray diffraction analyses, crystallite sizes of the films were between 11.7 and 25.2 nm. The crystallite size of as-deposited GaN film increased from 11.7 to 12.1 and 14.4 nm when the annealing duration increased from 30 min to 2 h (800 °C). For all films, the average optical transmission was ∼85% in the visible (VIS) and near infrared spectrum. The refractive indices of AlN and Al{sub x}Ga{sub 1−x}N were lower compared to GaN thin films. The refractive index of as-deposited films decreased from 2.33 to 2.02 (λ = 550 nm) with the increased Al content x (0 ≤ x ≤ 1), while the extinction coefficients (k) were approximately zero in the VIS spectrum (>400 nm). Postdeposition annealing at 900 °C for 2 h considerably lowered the refractive index value of GaN films (2.33–1.92), indicating a significant phase change. The optical bandgap of as-deposited GaN film was found to be 3.95 eV, and it decreased to 3.90 eV for films annealed at 800 °C for 30 min and 2 h. On the other hand, this value increased to 4.1 eV for GaN films annealed at 900 °C for 2 h. This might be caused by Ga{sub 2}O{sub 3} formation and following phase change. The optical bandgap value of as-deposited Al{sub x}Ga{sub 1−x}N films decreased from 5.75 to 5.25 eV when the x values decreased from 1 to 0.68. Furthermore, postdeposition annealing did not affect the bandgap of Al-rich films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Growth of crystalline Al{sub 2}O{sub 3} via thermal atomic layer deposition: Nanomaterial phase stabilization

We report the growth of crystalline Al{sub 2}O{sub 3} thin films deposited by thermal Atomic Layer Deposition (ALD) at 200 °C, which up to now has always resulted in the amorphous phase. The 5 nm thick films were deposited on Ga{sub 2}O{sub 3}, ZnO, and Si nanowire substrates 100 nm or less in diameter. The crystalline nature of the Al{sub 2}O{sub 3} thin film coating was confirmed using Transmission Electron Microscopy (TEM), including high-resolution TEM lattice imaging, selected area diffraction, and energy filtered TEM. Al{sub 2}O{sub 3} coatings on nanowires with diameters of 10 nm or less formed a fully crystalline phase, while those with diameters in the 20–25 nm range resulted in a partially crystalline coating, and those with diameters in excess of 50 nm were fully amorphous. We suggest that the amorphous Al{sub 2}O{sub 3} phase becomes metastable with respect to a crystalline alumina polymorph, due to the nanometer size scale of the film/substrate combination. Since ALD Al{sub 2}O{sub 3} films are widely used as protective barriers, dielectric layers, as well as potential coatings in energy materials, these findings may have important implications.

36 MATERIALS SCIENCE↗

Many routes to ferroelectric HfO 2 : A review of current deposition methods

Although 10 years have passed since the initial report of ferroelectricity in hafnia (HfO 2 ), researchers are still intensely fascinated by this material system and the promise it holds for future applications. A wide variety of deposition methods have been deployed to create ferroelectric HfO 2 thin films such as atomic layer deposition, chemical solution deposition, and physical vapor deposition methods such as sputtering and pulsed laser deposition. Process and design parameters such as deposition temperature, precursor choice, target source, vacuum level, reactive gases, substrate strain, and many others are often integral in stabilizing the polar orthorhombic phase and ferroelectricity. We examine processing parameters across four main different deposition methods and their effect on film microstructure, phase evolution, defect concentration, and resultant electrical properties. The goal of this review is to integrate the process knowledge collected over the past 10 years in the field of ferroelectric HfO 2 into a single comprehensive guide for the design of future HfO 2 -based ferroelectric materials and devices.

36 MATERIALS SCIENCE↗

Atomic Oxygen Durability Evaluation of a UV Curable Ceramer Protective Coating

The exposure of most silicones to atomic oxygen in low Earth orbit (LEO) results in the oxidative loss of methyl groups with a gradual conversion to oxides of silicon. Typically there is surface shrinkage of oxidized silicone protective coatings which leads to cracking of the partially oxidized brittle surface. Such cracks widen and branch crack with continued atomic oxygen exposure ultimately allowing atomic oxygen to reach any hydrocarbon polymers under the silicone coating. A need exists for a paintable silicone coating that is free from such surface cracking and can be effectively used for protection of polymers and composites in LEO. A new type of silicone based protective coating holding such potential was evaluated for atomic oxygen durability in an RF atomic oxygen plasma exposure facility. The coating consisted of a UV curable inorganic/organic hybrid coating, known as a ceramer, which was fabricated using a methyl substituted polysiloxane binder and nanophase silicon-oxo-clusters derived from sol-gel precursors. The polysiloxane was functionalized with a cycloaliphatic epoxide in order to be cured at ambient temperature via a cationic UV induced curing mechanism. Alkoxy silane groups were also grafted onto the polysiloxane chain, through hydrosilation, in order to form a network with the incorporated silicon-oxo-clusters. The prepared polymer was characterized by H-1 and Si-29 NMR, FT-IR, and electrospray ionization mass spectroscopy. The paper will present the results of atomic oxygen protection ability of thin ceramer coatings on Kapton H as evaluated over a range of atomic oxygen fluence levels.

Banks, Bruce A.↗

Exquisite growth control and magnetic properties of yttrium iron garnet thin films

A layer-by-layer epitaxial growth up to 227 atomic layers of ferrimagnetic insulator yttrium iron garnet (YIG) thin films is achieved on (110)-oriented gadolinium gallium garnet substrates using pulsed laser deposition. Atomically smooth terraces are observed on YIG films up to 100 nm in thickness. The root-mean-square roughness is as low as 0.067 nm. The easy-axis lies in the film plane, indicating the dominance of shape anisotropy. For (110)-YIG films, there is well-defined two-fold in-plane anisotropy, with the easiest axis directed along [001]. The Gilbert damping constant is determined to be 1.0 × 10{sup −4} for 100 nm thick films.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

PEALD grown high-k ZrO{sub 2} thin films on SiC group IV compound semiconductor

The study of ZrO{sub 2} thin films on SiC group IV compound semiconductor has been studied as a high mobility substrates. The ZrO{sub 2} thin films were deposited using the Plasma Enhanced Atomic Layer Deposition System. The thickness of the thin films were measured using ellipsometer and found to be 5.47 nm. The deposited ZrO{sub 2} thin films were post deposition annealed in rapid thermal annealing chamber at temperature of 400°Ð¡. The atomic force microscopy and X-гау photoelectron spectroscopy has been carried out to study the surface topography, roughness and chemical composition of thin film, respectively.

36 MATERIALS SCIENCE↗

Local atomic structure and lattice defect analysis in heavily Co-doped ZnS thin films using X-ray absorption fine structure spectroscopy

Iin this work, X-ray absorption fine structure (XAFS) spectroscopy was used to address both the local atomic structure and the local electronic structure around Zn, Co, and S in Co-doped ZnS thin films. X-ray absorption near-edge spectroscopy (XANES) revealed changes in the strong pre-edge feature of the S K-edge spectra that depend on the Co concentration and are related to atomic bound-state transitions through hybridization between $3d$ transition metal and $sp$ host semiconductor electronic states. These changes reveal intrinsic effects, such as S vacancies and dopant effects. From the Co K-edge XANES spectra, substitution of Co 2+ into ZnS is observed. The local atomic structure around the dopant, obtained by XAFS spectroscopy, indicates a reduction of the Co–S bond length. Optical analysis shows deep absorption centers or intermediate states in the bandgap, ascribed to $d$-$d$ transitions in the Co atoms that modify the electronic band structure and cause a decrease in the bandgap as a function of Co concentration. This work provides direct evidence of dopant effects in heavily Co-doped ZnS, including bond distances and Debye-Waller factors, providing key elements to generate a realistic atomic structural model, which is crucial to understand the observed electronic properties of this material.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Atomic Layer Deposition for Lithium-Based Batteries

With the increasing demand for energy at a low cost and minimal environmental impact, the development of next-generation high-performance batteries has drawn considerable attention. Owing to the capability of forming conformal coatings of thin films and nanoparticles, atomic layer deposition (ALD) has shown great potential in deposition and surface modification of electrode materials with various nanostructures, deposition of solid-state electrolyte, and fabrication of electrochemical catalysts. This paper reviews the recent development and applications of ALD in Li-based batteries, especially beyond Li-ion systems, and provides suggestions for further development of ALD techniques for these batteries.

25 ENERGY STORAGE↗