SEARCH · Search NASA
Results for “Accelerated testing”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Experimental demonstration of energy-chirp compensation by a tunable dielectric-based structure
N/A
Spectral modification of shock accelerated ions using a hydrodynamically shaped gas target
We report on reproducible shock acceleration from irradiation of a λ=10 μm CO2 laser on optically shaped H2 and He gas targets. A low energy laser prepulse (I≲10 14 W cm –2 ) is used to drive a blast wave inside the gas target, creating a steepened, variable density gradient. This is followed, after 25 ns, by a high intensity laser pulse (I>10 16 W cm –2 ) that produces an electrostatic collisionless shock. Upstream ions are accelerated for a narrow range of prepulse energies. For long density gradients (≳40 μm), broadband beams of He + and H + were routinely produced, whilst for shorter gradients (≲20 μm), quasimonoenergetic acceleration of protons is observed. These measurements indicate that the properties of the accelerating shock and the resultant ion energy distribution, in particular the production of narrow energy spread beams, is highly dependent on the plasma density profile. These findings are corroborated by 2D particle-in-cell simulations.
Understanding and controlling chromaticity shift in LED devices
Chromaticity shift in light-emitting diode (LED) devices arises from multiple mechanisms, and at least five different chromaticity shift modes (CSMs) have been identified to date. This paper focuses on the impacts of irreversible phosphor degradation as a cause of chromaticity shifts in LED devices. The nitride phosphors used to produce warm white LEDs are especially vulnerable to degradation due to thermal and chemical effects such as reactions with oxygen and water. As a result, LED devices utilizing these phosphors were found to undergo either a green shift or, less commonly, a red shift depending on the phosphor mix in the LED devices. These types of chromaticity shifts are classified as CSM-2 (green shift) and CSM-5 (red shift). This paper provides an overview of the kinetic processes responsible for green and red chromaticity shifts along with examples from accelerated stress testing of 6” downlights. Both CSMs appear to proceed through analogous mechanisms that are initiated at the surface of the phosphor. A green shift is produced by the surface oxidation of the nitride phosphor that changes the emission profile to lower wavelengths. As the surface oxidation reaction proceeds, reactant limitations slow the rate and bulk oxidation processes become more prevalent. We found that a red chromaticity shift arises from quenching of the green phosphor, also possibly due to surface reactions of oxygen, which shift the emission chromaticity in the red direction. In conclusion, we discuss the implications of these findings on projecting chromaticity.
Progress Towards Prognostic Health Management of Passive Components in Advanced Reactors – Model Selection and Evaluation
This paper presents recent progress towards developing a prognostic health management framework for passive components of advanced reactors (AR). The focus of this paper is on lifecycle prognostics for passive components using a Bayesian prognostic algorithm that provides a natural framework for incorporating different sources of variability, and uncertainties inherent in the operations of AR. High-temperature creep damage, a prototypic failure mechanism in AR materials, is used as the context for this research. A Bayesian model selection approach is implemented to select the appropriate creep degradation model at any given time, using relevant sensor measurements reflecting the material degradation state. The model selection approach, based on reversible jump Markov chain Monte Carlo methods, is integrated with Bayesian particle filter-based prognostic framework. The proposed approach is evaluated using strain measurements obtained from accelerated creep testing of stainless steel specimens. Results indicate feasibility of the proposed approach in accurately identifying the creep degradation stage from the available measurements at a given time. Effect of uncertainties in material degradation model and measurement noise on the performance of the prognostic algorithm is also investigated.
Nondestructive Characterization of Antireflective Coatings on PV Modules
Antireflective coatings (ARCs) are used on the vast majority of solar photovoltaic (PV) modules to increase power production. However, ARC longevity can vary from less than 1 to over 15 years depending on coating quality and deployment conditions. A technique that can quantify ARC degradation nondestructively on commercial modules would be useful both for in-field diagnostics and accelerated aging tests. In this article, we demonstrate that accurate measurements of ARC spectral reflectance can be performed using a modified commercially available integrating-sphere probe. The measurement is fast, accurate, nondestructive, and can be performed outdoors in full-sun conditions. We develop an interferometric model that estimates coating porosity, thickness, and fractional area coverage from the measured reflectance spectrum for a uniform single-layer coating. We demonstrate the measurement outdoors on an active PV installation, identify the presence of an ARC, and estimate the properties of the coating.
Solder Bond Fatigue is Insensitive to Module Size
In this article, we explore the influence of module size on the rate of interconnecting solder bond thermomechanical fatigue (TMF) damage. Structural mechanics models of crystalline silicon PV models are created to solve with the finite-element method. Results conclusively demonstrate that the rate of solder bond TMF damage is independent of module size, interconnect location across the cell and cell location across the module.
Multiscale Characterization of Photovoltaic Modules—Case Studies of Contact and Interconnect Degradation
The current popularity of photovoltaic (PV) systems is due in large part to their exceptional reliability and significantly lower cost than other energy sources. Studying cell and module degradation is key to promote further development in the state of the art. Fielded or accelerated aged modules exhibit different failure modes, of which metallization degradation (contacts and interconnections) is prevalent. In this work, we discuss how multiscale characterization methods can be applied to a variety of module technologies that have been field exposed and have undergone accelerated age testing. These methods include performing characterization on the module level, cell level, and finally the materials level. The observed performance losses from the module- and cell-level characterization can be correlated with materials properties to find out the root cause of degradation. We recommend an initial nondestructive characterization suite, including module- and cell-level current-voltage ( I--V ), Suns-V OC , photoluminescence and electroluminescence imaging, quantum efficiency, ultraviolet fluorescence imaging, and thermal infrared imaging. Samples are then extracted from particularly degraded regions of the module and prepared for materials characterization techniques, such as top-down and cross-sectional scanning electron microscopy, energy-dispersive X-ray spectroscopy, X-ray photoelectron spectroscopy, secondary ion mass spectrometry, Raman spectroscopy, and transmission electron microscopy, allowing a deeper look into the mechanism behind the metallization degradation. This article serves as an instructional review to introduce the different multiscale characterization methods and how they can be effectively applied to perform PV degradation studies. Furthermore, we also share some of our examples and discuss the strengths, limitations, and best practices for each of the characterization techniques.
Development of Fixtures and Methods to Assess the Durability of Balance of Systems Components
The degradation of photovoltaic (PV) balance of systems (BoS) components is not well studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were, therefore, examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using a benchtop prototype fixture to identify the most influential environmental stressors on BoS components as well as the effect of external mechanical perturbation. The prototype fixture was used to develop a perturbation capability for future use in the combined-accelerated stress testing chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 °C from ~40 °C) and a different failure mode (arcing at the metal pins rather than overheating of the fuse filament) were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (measured for static specimens, with failure occurring in the fuses) to 15 A (for tests with mechanical perturbation, with failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy). Chemical composition analysis included energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.
Failure Mode and Effects Analysis (FMEA) for Photovoltaic Inverter
Photovoltaic (PV) inverters are critical yet vulnerable components in modern energy systems, often acting as reliability bottlenecks that increase the levelized cost of energy (LCOE). To address this, this paper presents a comprehensive Failure Mode and Effects Analysis (FMEA) tailored for PV inverters. Leveraging field data and literature, we identify failure-prone components, such as capacitors,, and relays, and prioritize their risks based on quantitative Risk Priority Numbers (RPNs). The analysis reveals that surge-induced MOV short circuits, capacitor degradation, and environmental cooling fan failures dominate the risk profile. These findings provide a targeted framework for reliability improvement, guiding future efforts in predictive diagnostics, design optimization, and accelerated life testing strategies.
Near-Busbar Degradation of Screen-Printed Metallization in Silicon Photovoltaic Modules
We study photovoltaic (PV) module degradation after extended accelerated stress testing including 2000 hours of damp heat followed by a current-injection procedure meant to stabilize defects linked to light-induced degradation. In addition to de-stabilization/recovery of light-induced defects, we observe severe series resistance due to loss of contact between the Si cell and near-busbar screen-printed metallization (i.e. grid finger delamination). Using scanning electron microscopy and energy dispersive x-ray spectroscopy on cell fragments cored from the module, we show poor contact is caused by a gap between the screen-printed Ag metallization and Si due to missing glass frit.
In-Situ Luminescence Imaging of Perovskite Solar Cells Demonstrates Increasing Spatial Nonuniformity Upon Light-Soaking Degradation
In this work we investigate degradation rates of triplecation mixed-halide perovskite p-i-n solar cells. We present an accelerated stress testing procedure using periodic blue light-soaking at elevated temperatures until devices reach ~80% of their initial efficiency. We track light-induced degradation via in-situ: photoluminescence (PL), current-voltage (I-V) curves, and transient photovoltage. Devices underwent 165 hours of light bias at 65degrees C. Results suggest that spatial uniformity in PL intensity decreases as device degradation increases. This investigation lays the groundwork to address the current gap in understanding the interplay between device performance and the evolution of macroscopic features in perovskite solar cells. Thus, we believe spatial characterization techniques will play a crucial role in the commercialization of perovskite solar cells.
Increasing Multilayer Ceramic Capacitor Lifetime With Bipolar Voltage Cycling
Enhancing the lifetime of multilayer ceramic capacitors (MLCCs) is critical in many aerospace, naval, or electrical grid applications, where device failure could lead to catastrophic consequences. The migration of oxygen vacancies from the ceramic to the electrode interface under constant bias is known to reduce the lifetime of oxide-based MLCCs. Bias cycling presents an opportunity to enhance MLCC lifetime by reducing oxygen vacancy migration. The ideal frequency range is expected to lie between frequencies low enough to avoid self-heating but high enough to avoid interfacial defect formation. However, the impact of low-frequency bipolar voltage cycling (BVC) on MLCC degradation mechanisms has not been well studied. This work investigates the impact of periodic BVC on the degradation of MLCCs through highly accelerated lifetime testing (HALT) on X7R capacitors. HALT tests were conducted at 255 °C and 60 V using different switching frequencies: 0 (dc), 0.1, 2.5, and 10 Hz. BVC was found to improve the lifetime of MLCCs compared to dc test conditions. MLCCs tested at 10-Hz BVC showed a 311% increase in average time to failure compared to the dc case. Impedance spectroscopy shows that BVC decreases the rate of resistance degradation within MLCCs, indicating that oxygen vacancy migration to the electrodes is mitigated. The impedance spectra taken on BVC samples highlight how grain boundaries play a vital role in trapping oxygen vacancies. Periodic cycling causes oxygen vacancies to become trapped at grain boundaries, resulting in oxygen vacancies taking longer to reach the electrode interface and thus increasing MLCC lifetime. This work highlights not only how BVC can be used to increase MLCC lifetime but also how periodically cycling MLCCs could increase lifetime in extreme environments, such as at elevated temperatures and electric fields.
Thermo-Oxidation Analysis of Structural Adhesives: An Experimental Study
Abstract Cross-linked polymers play an important role in structural applications as adhesives. In this article, we performed an experimental study to understand the effects of high temperature i.e. thermo-oxidative aging on the mechanical behavior of polymers. Subsequently, the constitutive behavior, i.e. stress-strain relation of these adhesives before and after the accelerated aging tests were studied on samples aged at different temperature and different time durations at zero humidity. The aging conditions and periods selected for the tests have been specifically designed to simulate the effects of aging under the working conditions that the materials will be subjected to in their standard applications. The focus of this study is on the investigation of the effects of aging on the polymeric adhesives used in automotive applications. Consequently, four different polymeric adhesives (one silicone-based, two polyurethane-based, and one acrylic type), which are being used extensively in these applications, have been chosen. The quasi-static tensile loading was used on these four adhesives and the changes in the constitutive behavior were measured. The failure tensile tests as well as the cyclic tensile tests were performed in our lab using a Test-Resources tensile testing machine. The temperatures that were used in this work are 60, 80 and 95°C for varying aging periods of 24hrs, 240hrs, and 720hrs. Then, all the data was collected and consequently analyzed, and the resulting behavior was compared to that of the unaged material, showing varying results depending on the material, temperature, and aging period. Different behaviors have been observed after aging. The polymers’ behavior was expanding from no effect to significant damage caused by aging conditions. This work provides the core understanding required for modeling the material behavior during aging and lays down the groundwork for further data-infused model-free approaches.
La- and Mn-doped cobalt spinel oxygen evolution catalyst for proton exchange membrane electrolysis
Discovery of earth-abundant electrocatalysts to replace iridium for the oxygen evolution reaction (OER) in a proton exchange membrane water electrolyzer (PEMWE) represents a critical step in reducing the cost for green hydrogen production. Here we report a nanofibrous cobalt spinel catalyst codoped with lanthanum (La) and manganese (Mn) prepared from a zeolitic imidazolate framework embedded in electrospun polymer fiber. The catalyst demonstrated a low overpotential of 353 millivolts at 10 milliamperes per square centimeter and a low degradation for OER over 360 hours in acidic electrolyte. A PEMWE containing this catalyst at the anode demonstrated a current density of 2000 milliamperes per square centimeter at 2.47 volts (Nafion 115 membrane) or 4000 milliamperes per square centimeter at 3.00 volts (Nafion 212 membrane) and low degradation in an accelerated stress test.
Impact of Carbon Support Structure on the Durability of PtCo Electrocatalysts
High performing, low-Pt content fuel cell membrane electrode assemblies (MEAs) are critical to the economic viability of proton exchange membrane fuel cells (PEMFCs) for the transportation industry. Considerable research has been conducted to reduce the Pt content in fuel cells, leading to the development of transition metal alloys, such as Platinum-Cobalt (PtCo). The degree of degradation of PtCo catalysts can be impacted by the catalyst metal itself and its interactions with the carbon support. Several low-loaded PtCo MEAs were fabricated, with various combinations of porous and solid carbon cathode catalyst supports. The MEAs were subjected to an accelerated stress test (AST), and the catalyst degradation characterized using electrochemical, X-ray scattering, and electron microscopy techniques. Porous supports retain more of their electrochemically-active surface area (ECSA) and demonstrate higher performance after the AST. Overall, this is believed to be due to the ability of the porous supports to trap the metal particles within the pores, slowing their dissolution/precipitation, and agglomeration.