Microstructure Evolution and Stress Corrosion Cracking Susceptibility of 12Cr Martensitic Steel Upon Long-Term Service in Power Plants

After 230,000-h long-term service at 550 °C/13.7 MPa, the microstructure of a kind of 12Cr martensitic steel was investigated using scanning electron microscopy, backscattering electron microscope and x-ray diffraction analysis. The results show that the precipitation and coarsening of carbides at grain/lath boundaries are the main cause of microstructure degradation. The static immersion tests and the slow strain rate test coupled with electrochemical impedance spectroscopy were conducted on the served steel in 1.0% NaCl solution, and it turns out that the pitting corrosion resistance and repassivation ability of the steel are significantly reduced as a result of microstructure degradation. The stress corrosion cracking susceptibility of the steel was also studied. Fracture morphology analysis shows that the secondary crack in conjunction with slip lines is a result of the coalescence of micro-cracks nucleated from the pits.

36 MATERIALS SCIENCE↗

Multi stage and illumination dependent segregation in MAPb(I,Br)3

© COPYRIGHT SPIE. Downloading of the abstract is permitted for personal use only. An unsolved problem of mixed halide perovskites is the light induced compositional instability. Under illumination microscopic clusters with a higher iodide content form which act as efficient recombination centers reducing device performance. In photoluminescence measurements this leads to the development of a secondary peak at low energies that increases in intensity and shifts towards lower energies. Different theories for about the origin have been developed but the underlying key mechanisms are still under debate. In the presented study the photoluminescence evolution of MAPb(I1.5Br1.5) perovskites with varying microstructure is investigated at various excitation densities and temperatures. We find a more evolved segregation mechanism with an intermediate stage between the commonly reported mixed phase and the appearance of the I-rich clusters (Br content < 50%). In this intermediate stage perovskite domains with nearly pure iodide content form (Br content < 25%). Using low excitation densities, the interplay between the I-rich domains and the I-rich clusters leads to a blue shift of the conjunct I-rich luminescence peak. At high excitation densities the I-rich domains and the I-rich clusters are clearly distinguishable, due to a stronger PL response of the I-rich domains. With continuous illumination more I-rich cluster form acting as carrier traps and recombination centers. Due to this, the influence of the few I-rich domains on the PL signature decreases leaving only the commonly reported red shift of the I-rich clusters at later stages of the segregation. The formation of the I-rich domains is fully reversible in the dark and occurs also at elevated temperatures. Measurements on sample with varying grain size further indicate an enhanced formation of those I-rich domains on samples with high grain boundary density possibly by a faster halide mobility along them.

Babbe, F↗

Microstructural refinement in ultrasonically modified A356 aluminum castings

Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.

36 MATERIALS SCIENCE↗

Bubble evolution in Kr-irradiated UO 2 during annealing

Transmission electron microscopy observation of Kr bubble evolution in polycrystalline UO 2 annealed at high temperature was conducted in order to understand the inert gas behavior in oxide nuclear fuel. The average size of intragranular bubbles increased gradually from 0.8 nm in as-irradiated sample at room temperature to 2.6 nm at 1600 °C and the bubble size distribution changed from a uniform distribution to a bimodal distribution above 1300 °C. The size of intergranular bubbles increased more rapidly than intragranular ones and bubble denude zones near grain boundaries formed in all the annealed samples. It was found that high-angle grain boundaries held bigger bubbles than low angle grain boundaries. Complementary atomistic modeling was conducted to interpret the effects of grain boundary character on the Kr segregation. Lastly, the area density of strong segregation sites in the high-angle grain boundaries is much higher than that in the low angle grain boundaries.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Electron Backscatter Diffraction (EBSD) Characterization of Uranium and Uranium Alloys

Electron backscatter diffraction (EBSD) was used to examine the microstructures of unalloyed uranium, U-6Nb, U-10Mo, and U-0.75Ti. For unalloyed uranium, we used EBSD to examine the effects of various processes on microstructures including casting, rolling and forming, recrystallization, welding, and quasi-static and shock deformation. For U-6Nb we used EBSD to examine the microstructural evolution during shape memory loading. EBSD was used to study chemical homogenization in U-10Mo, and for U-0.75Ti, we used EBSD to study the microstructure and texture evolution during thermal cycling and deformation. The studied uranium alloys have significant microstructural and chemical differences and each of these alloys presents unique preparation challenges. Each of the alloys is prepared by a sequence of mechanical grinding and polishing followed by electropolishing with subtle differences between the alloys. U-6Nb and U-0.75Ti both have martensitic microstructures and both require special care in order to avoid mechanical polishing artifacts. Unalloyed uranium has a tendency to rapidly oxidize when exposed to air and a two-step electropolish is employed, the first step to remove the damaged surface layer resulting from the mechanical preparation and the second step to passivate the surface. All of the alloying additions provide a level of surface passivation and different one and two step electropolishes are employed to create good EBSD surfaces. Because of its low symmetry crystal structure, uranium exhibits complex deformation behavior including operation of multiple deformation twinning modes. EBSD was used to observe and quantify twinning contributions to deformation and to examine the fracture behavior. Figure 1 shows a cross section of two mating fracture surfaces in cast uranium showing the propensity of deformation twinning and intergranular fracture largely between dissimilarly oriented grains. Deformation of U-6Nb in the shape memory regime occurs by the motion of twin boundaries formed during the martensitic transformation. Deformation actually results in a coarsening of the microstructure making EBSD more practical following a limited amount of strain. Figure 2 shows the microstructure resulting from 6% compression. Casting of U-10Mo results in considerable chemical segregation as is apparent in Figure 2a. The segregation subsists through rolling and heat treatment processes as shown in Figure 2b. EBSD was used to study the effects of homogenization time and temperature on chemical heterogeneity. It was found that times and temperatures that result in a chemically homogeneous microstructure also result in a significant increase in grain size. U-0.75Ti forms an acicular martinsite as shown in Figure 4. This microstructure prevails through cycling into the higher temperature solid uranium phases.

36 MATERIALS SCIENCE↗

Microstructure evolution of Al-doped zinc oxide and Sn-doped indium oxide deposited by radio-frequency magnetron sputtering: A comparison

The microstructure and morphology evolution of Al-doped zinc oxide (AZO) and Sn-doped indium oxide (ITO) thin films on borosilicate glass substrates deposited by radio-frequency magnetron sputtering at room temperature (RT) and 300 °C were investigated by X-ray diffraction and atomic force microscopy (AFM). One-dimensional power spectral density (1DPSD) functions derived from the AFM profiles, which can be used to distinguish different growth mechanisms, were used to compare the microstructure scaling behavior of the thin films. The rms roughness R{sub q} evolves with film thickness as a power law, R{sub q} ∼ d{sub f}{sup β}, and different growth exponents β were found for AZO and ITO films. For AZO films, β of 1.47 and 0.56 are obtained for RT and 300 °C depositions, respectively, which are caused by the high compressive stress in the film at RT and relaxation of the stress at 300 °C. While for ITO films, β{sub 1} = 0.14 and β{sub 2} = 0.64 for RT, and β{sub 1} = 0.89 and β{sub 2} = 0.3 for 300 °C deposition are obtained, respectively, which is related to the strong competition between the surface diffusion and shadowing effect and/or grain growth. Electrical properties of both materials as a function of film thickness were also compared. By the modified Fuchs-Sondheimer model fitting of the electrical transport in both materials, different nucleation states are pointed out for both types of films.

36 MATERIALS SCIENCE↗

Experiments and simulations on solidification microstructure for Inconel 718 in powder bed fusion electron beam additive manufacturing

Previous research on the powder bed fusion electron beam additive manufacturing of Inconel 718 has established a definite correlation between the processing conditions and the solidification microstructure of components. However, the direct role of physical phenomena such as fluid flow and vaporization on determining the solidification morphology have not been investigated quantitatively. In this work, we investigate the transient and spatial evolution of the fusion zone geometry, temperature gradients, and solidification growth rates during pulsed electron beam melting of the powder bed with a focus on the role of key physical phenomena. The effect of spot density during pulsing, which relates to the amount of heating of the build area during processing, on the columnar-to-equiaxed transition of the solidification structure was studied both experimentally and theoretically. Predictions and the evaluation of the role of heat transfer and fluid flow were established using existing solidification theories combined with transient, three-dimensional numerical heat transfer and fluid flow modeling. Metallurgical characteristics of the alloy’s solidification are extracted from the transient temperature fields, and microstructure is predicted and validated using optical images and electron backscattered diffraction data from the experimental results. Simulations show that the pure liquid region solidified quickly, creating a large two-phase, mushy region that exists during the majority of solidification. While conductive heat transfer dominates in the mushy region, both the pool geometry and the solidification parameters are affected by convective heat transfer. Lastly, increased spot density during processing is shown to increase the time of solidification, lowering temperature gradients and increasing the probability of equiaxed grain formation.

36 MATERIALS SCIENCE↗

Magnetic Processing – A Pervasive Energy Efficient Technology for Next Generation Materials for Aerospace and Specialty Steel Markets

Thermomagnetic Magnetic Processing is an exceptionally fertile, pervasive and cross-cutting technology that is just now being recognized by several major industry leaders for its significant potential to increase energy efficiency and materials performance for a myriad of energy intensive industries in a variety of areas and applications. ORNL has pioneered the use and development of large magnetic fields in thermomagnetically processing (T-MP) materials for altering materials phase equilibria and transformation kinetics. ORNL has discovered that using magnetic fields, we can produce unique materials responses. T-MP can produce unique phase stabilities & microstructures with improved materials performance for structural and functional applications not achieved with traditional processing techniques. These results suggest that there are unprecedented opportunities to produce significantly enhanced materials properties via atomistic level (nano-) microstructural control and manipulation. ORNL (in addition to others) have shown that grain boundary chemistry and precipitation kinetics are also affected by large magnetic fields. This CRADA has taken advantage of ORNL’s unique, custom-designed thermo-magnetic, 9 Tesla superconducting magnet facility that enables rapid heating and cooling of metallic components within the magnet bore; as well as ORNL’s expertise in high magnetic field (HMF) research. Carpenter Technologies, Corp., is a a US-based industrial company, that provides enhanced performance alloys for the Aerospace and Specialty Steel products. In this CRADA, Carpenter Technologies, Corp., is focusing on applying ORNL’s Thermomagnetic Magnetic Processing (TMP) technology to improve their current and future proprietary materials’ product performance and open up new markets for their Aerospace and Specialty Steel products. Unprecedented mechanical property performance improvements have been demonstrated for a high strength bainitic alloy industrial/commercial alloy that is envisioned to provide the potential for new markets for this alloy. These thermomechanical processing results provide these alloys with a major breakthrough demonstrating that simultaneous improvements in yield strength and ductility are achieved: 12 %, 10%, 13%, and 22% increases in yield strength, elongation, reduction-in-area, and impact energy respectively. In addition, TMP appears to overcome detrimental chemical homogeneity impacts on uniform microstructure evolution.

36 MATERIALS SCIENCE↗

Report on use of Inoculants in Missile Application Alloys

This report documents the status of current inoculant research relevant to missile application alloys and MTCR control language. The information is intended to provide data on current inoculants for us determining the current state of development and identifying potential research directions. Although there has been significant scientific research into the development and synthesis of inoculants, their current availability is limited is traditional powder inoculants employed during casting processes. However, research continues the development of complex oxides, ribbon materials, high entropy alloys, and other inoculant product forms, including the use of inoculants in the melt pools produced during additive manufacturing. Research to date has focused primarily on aluminum and steel alloys with emphasis on refining grain structures and evolving equiaxed morphologies while increasing strength and castability. The primary inoculants in steel and cast irons include TiN, SiC, FeSi75, and Ce which have increased strength properties. Chief inoculants for Al alloys often include TiC, SiC, Al3Sc(x) and TiB2 to aid in precipitation and refinement. Ti and Ni alloys have fewer research activities involving inoculants, although TiN, TiB, ZrN and LaB6 (for Ti alloys) and WC, Co3FeNb2, and CrFeNb (for Ni alloys) have been used. Sic, Al2O3, Mg and Ti are key inoculants for Mg alloys. Multiple cast alloys from each of the material classes demonstrated increased strength and performance properties using inoculants, with several approaching requirements applicable to missile service environments. The continued evolution of advanced manufacturing capabilities is making it easier to produce high temperature near net shape structural materials using inoculant powders. These shapes may include the geometric shapes addressed within the MTCR (tubes and limited wall thicknesses). The use of inoculants may enable further development of high temperature alloys into near net shapes traditionally produced via casting processes due to limited ductility. This may decrease material and manufacturing costs. In addition, inoculation provides controlled kinetics and achievable chemical segregation that enables potential for far-from equilibrium thermodynamic microstructures and chemistries that could provide new metastable alloy states and subsequent properties to address co-design engineering constraints, including needs for increased strength and ductility. It is recommended that specific material combinations within these alloy classes be carefully watched as the materials evolve, with controls aimed at those having material properties above current MTCR levels. This specifically includes the use of refractory inoculants in alloys, and the application of inoculants in high strength and high temperature alloys via additive manufacturing processes, with care to link capabilities to product forms similar to the current requirements on tube geometries and material feed stocks. The continued development of nanoparticle inoculants will increase strength and ductility of high strength castings and additive manufactured metallic components. For example, adding inoculants into the casting of maraging steels and other precipitation strengthened alloys may drastically elevate mechanical properties above the control limit of current regulations.

36 MATERIALS SCIENCE↗

Microstructure, phase transition, and interfacial chemistry of Gd{sub 2}O{sub 3}/Si(111) grown by electron-beam physical vapor deposition

The effects of growth temperature, film thickness, and oxygen flux on the microstructure, phase transition, and interfacial chemistry of gadolinium oxide (Gd{sub 2}O{sub 3}) films grown on Si(111) substrates by electron-beam physical vapor deposition were investigated using a combination of transmission electron microscopy (TEM), electron diffraction, scanning TEM, x-ray energy dispersive spectrometry, and electron energy loss spectrometry. The authors find that a low growth temperature (250 Degree-Sign C) and a high oxygen flux (200 sccm) led to a small grain size and a high porosity of the Gd{sub 2}O{sub 3} film. Lowering the oxygen flux to 50 sccm led to reduced film porosity, presumably due to the increased diffusion length of the Gd atoms on the surface. Increasing the growth temperature to 650 Degree-Sign C resulted in a film with large columnar grains and elongated pores at the grain boundaries. Thin films grown at 250 Degree-Sign C consisted of cubic Gd{sub 2}O{sub 3}, but thermodynamically less stable monoclinic phase formed as the film thickness increased. Lowering the oxygen flux apparently further promoted the formation of the monoclinic phase. Furthermore, monoclinic phase dominated in the films grown at 650 Degree-Sign C. Such phase transitions may be related to the stress evolution of the films at different temperatures, thicknesses, and oxygen fluxes. Enhanced Gd{sub 2}O{sub 3}/Si interfacial reaction was observed as the growth temperature, film thickness, and oxygen flux increased. Moreover, oxygen was found to play a crucial role in the Gd{sub 2}O{sub 3}/Si interfacial reaction and the formation of Gd-Si-O interface layers, which proceeded by the reaction of excess oxygen with Si followed by the intermixing of SiO{sub x} and Gd{sub 2}O{sub 3}.

36 MATERIALS SCIENCE↗

Strengthening mechanisms, hardening/softening behavior, and microstructure evolution in an LPSO magnesium alloy at elevated temperatures

Here, rapid degradation of the mechanical properties of conventional Mg alloys with temperature precludes their wide application in industry. The LPSO (long period stacking ordered) Mg alloys, on the other hand, show considerable potential to achieve excellent high-temperature mechanical performance. In this study, a Mg-5.1Y-2.4Zn (wt.%) extrusion alloy with the microstructure comprising of α-Mg matrix and LPSO phase was prepared. It is shown that the yield strength of the alloy at 200 °C retained ~83% of the yield strength of 198 MPa at room temperature (RT). Importantly, the ductility also improved, owing to the increased non-basal slip activities at elevated temperatures. In contrast to RT and 200 °C, the alloy exhibited softening tensile behavior with an apparent loss of yield strength at 300 °C. In-situ lattice strain analysis revealed that load transfer from α-Mg to LPSO remains effective at temperatures up to 200 °C, governing the high yield strength of the alloy. The post-mortem analysis by means of electron microscopy confirmed that the LPSO phase is structurally stable at 200 °C. In particular, the high strain hardenability is rationalized by the sandwiched LPSO structures together with stacking faults serving as effective obstacles to the motion of non-basal dislocations. The load transfer effect disappears at the temperature of 300 °C, resulting in the fast deterioration of strength of the alloy. The cracking of the LPSO phase along with the recrystallizing of α-Mg grains were found to be the main causes for the softening behavior of the alloy at 300 °C.

36 MATERIALS SCIENCE↗

Evolution of texture and internal stresses within polycrystalline rock salt using in situ 3D synchrotron computed tomography and 3D X-ray diffraction

Over time rock salt caverns have been extensively used as reliable repositories for hazardous waste such as nuclear waste, oil or compressed gases. Undisturbed rock salt deposits in nature are usually impermeable and have very low porosity. However, rock salt formations under excavation stresses can develop crack networks, which increase their porosities; and in the case of a connected crack network within the media, rock salt may become permeable. Although the relationship between the permeability of rock salt and the applied stresses has been reported in the literature, a microscopic study that investigates the properties influencing this relationship, such as the evolution of texture and internal stresses, has yet to be conducted. This study employs in situ 3D synchrotron micro-computed tomography and 3D X-ray diffraction (3DXRD) on two small-scale polycrystalline rock salt specimens to investigate the evolution of the texture and internal stresses within the specimens. The 3DXRD technique measures the 3D crystal structure and lattice strains within rock salt grains. The specimens were prepared under 1D compression conditions and have shown an initial {111} preferred texture, a dominant {110}$\langle1\bar{1}0\rangle$ slip system and no fully connected crack network. The {111} preferred texture under the unconfined compression experiment became stronger, while the {111}$\langle1\bar{1}0\rangle$ slip system became more prominent. The specimens did not have a fully connected crack network until applied axial stresses reached about 30 MPa, at a point where the impermeability of the material becomes compromised due to the development of multiple major cracks.

36 MATERIALS SCIENCE↗

Microstructure characterization of LAE442 magnesium alloy processed by extrusion and ECAP

The magnesium alloy LAE442 was processed by extrusion and equal channel angular pressing (ECAP) to achieve ultrafine grained microstructure. Detailed characterization of the microstructure was performed by scanning electron microscope, electron back scattered diffraction (EBSD) and transmission electron microscope. The initial, as-cast, microstructure consisted of large grains of ~ 1 mm. The grain refinement due to the processing by severe plastic deformation led to a decrease of the average grain size to ~ 1.7 μm after the final step of ECAP. A detailed characterization of secondary phases showed the precipitation of Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. X-ray diffraction measurements proved that Li is dissolved within the magnesium matrix in the as-cast condition. Newly formed Al{sub 3}Li phase was observed after ECAP. The texture formation due to the extrusion and ECAP was different from that in the other magnesium alloys due to the activation of non-basal slip systems as a result of the decrease of the c/a ratio. - Highlights: • Combined extrusion and equal channel angular pressing results in significant grain refinement by factor 1000 approximately. • Al{sub 11}RE{sub 3}, Al{sub 2}Ca and Al{sub 10}RE{sub 2}Mn{sub 7} secondary phases are present in the as-cast material while Li was dissolved in the Mg matrix. • Extrusion and ECAP have no effect on the composition of the secondary phases but they influence strongly their distribution. • Texture evolution is affected by decrease of c/a ratio due to the presence of Li and resulting activation of non-basal slip.

36 MATERIALS SCIENCE↗

Direct observation of C 3 S particle dissolution using fast nano X-ray computed tomography

Tricalcium silicate (C 3 S) occupies 50 % to 70 % of ordinary portland cement (OPC) by mass and it is an important component affecting the hydration of OPC [1], [2], [3], [4], [5], [6], [7]. Generally, the hydration of C 3 S is described by two processes: the dissolution of C 3 S particles and the precipitation of hydration products. While it is understood that the dissolution rates of C 3 S vary with time, more precise measurements are needed to understand this process. Many mechanisms have been proposed to explain the time-evolving dissolution rates of C 3 S [2]. The metastable barrier hypothesis suggests that a thin metastable layer of hydrates forms around the C 3 S particle surface and prohibits the access of grains to the aqueous solution [8], [9], [10], [11], [12]. The slow dissolution step hypothesis suggests that the increased ion concentration from the initial reaction delays the C 3 S dissolution [2], [13], [14], [15], [16], [17]. More recent publications suggest that C 3 S may react differently depending on the existence of crystallographic defects [18], [19], [20]. Etch pits are thought to open on the particle surface during the initial reaction and this contributes to the C 3 S dissolution [21], [22]. As hydrates precipitate and cover these highly reactive surfaces, hydration slows down and the induction period starts [18], [23], [24], [25], [26]. Many experiments have been conducted to test the aforementioned mechanisms. Some hydration studies utilize bulk measurements, such as isothermal calorimetry [27], [28], [29], pore solution analysis [30], quasi-elastic neutron scattering [31], and nuclear magnetic resonance spectroscopy [32], [33]. One limitation of these measurements is that they do not provide direct and detailed information on the individual C 3 S particles. Some other studies utilize imaging techniques, such as scanning electron microscopy (SEM) [34], [35], [36] and transmission electron microscopy (TEM) [37]. However, SEM/TEM cannot track the evolution of individual particles throughout hydration [34], [35], [38], [39], [40] and they do not give insights into the microstructure of materials before hydration [34], [35], [39]. This makes it challenging to draw strong conclusions from only SEM or TEM observations. Synchrotron X-ray tomography techniques have been used more broadly in recent years to study cement hydration. They are not only non-destructive but also able to image a sample in full 3D with resolutions that can reach from micron to nanoscale. Nano computed tomography (nCT) is one technique that has been applied to study cement hydration at the nanoscale [26], [41]. A typical nCT can reach a pixel size from 15 to 65 nm, providing enough detail for observing features <1 μm. However, nCT often takes >0.5 h to finish one scan. This makes the application of this technique on continuous scans for in-situ observations challenging. Fast X-ray computerized tomography (fCT) is another technique that has shown success in studying the time-evolving cement microstructures [20], [42], [43], [44], [45], [46], [47], [48], [49]. Due to the high flux of the X-ray beam from the synchrotron ring, fCT allows a scan to be captured within 1 min at a pixel size of 1 μm. This allows a paste sample to be continuously scanned during the hydration process. However, the micron-sized resolutions limit does not provide detailed insights for particles <5 μm [20], [49]. Fortunately, the combination of nCT and fCT has allowed the development of fast nano X-ray computed tomography (fnCT). fnCT can capture a 3D data set in <2 min at a pixel size of 50 nm. This makes this procedure an exciting method to evaluate hydrating pastes. fnCT collects multiple X-ray radiographs at various rotation angles and generates a 3D model of the scanned sample, which is also referred to as a 3D tomography [50], [51]. In one tomography, the X-ray absorptions of different components (e.g., C 3 S and hydrates) differ as functions of density and chemistry [52], [53]. These X-ray absorption contrasts can be used to extract detailed information about the 3D microstructure [26], [54], [55]. In this paper, fnCT is used to collect time-lapse tomographs of hydrating C 3 S paste from 18 min after mixing to 7 h of hydration. The bulk measurements of anhydrous C 3 S, as well as the microstructural changes of individual C 3 S particles, are directly observed, quantified, and discussed. The dissolution behavior of C 3 S particles at various size scales is systematically analyzed and compared. This work aims to find the relationship between the size of C 3 S particle sizes and their dissolution rates. This provides significant insights into the early-age hydration of C 3 S on length and time scales not previously possible. Because of the magnitude of the data and the substantial amount of observations, this work will solely focus on the change in the anhydrous particles. Changes in the hydration products will be reported in future work.

42 ENGINEERING↗

The evolution and growth of Al2O3 scales on beta-NiAl

The formation and growth of Al2O3 scales on (beta)-NiAl were studied using electron microscopy and other analytical techniques to gain an understanding of the oxidation properties of (beta)-NiAl and of alumina-forming alloys, in general. The transient and mature stages of oxidation were studied as well as the transformation stage during which the oxide scale transforms from metastable Al2O3 phases to the thermodynamically stable alpha-Al2O3 phase. The transient oxidation stages were studied at 800 deg C and for short times at 1100C. At 800C, the scales consist predominantly of delta-Al2O3 which forms by cation vacancy ordering in the defective spinel lattice of gamma-Al2O3. At 1100C, a fast-growth morphology of theta-Al2O3 forms as a surface layer over delta-Al2O3. For both oxidation temperatures, the scales are often epitaxially oriented with respect to the metal. The transient scales grow by outward cation diffusion as evidenced by surface growth morphologies. The transformation to alpha-Al2O3 occurs within 1 hour at 1100C by a nucleation and radial growth process. The large volume decrease associated with the transformation results in a highly strained alpha-Al2O3 microstructure. A change in scale growth mechanism from outward cation to inward anion diffusion allows transient surface morphologies to be smoothed by surface diffusion. The mature stage of oxidation involves the growth of an alpha-Al2O3 scale having the lacey morphology formed as a result of the gamma yields alpha transformation. Growth of the scale occurs by counterdiffusion along grain boundaries resulting in ridges formed by impingement of alpha-Al2O3 nuclei during the transformation stage. Also scale growth occurs by inward oxygen diffusion through healed cracks; the cracks result from transformation stresses. The measured growth rates of scales having the lacey morphology are an order of magnitude less than fine-grained alpha-Al2O3 scales. Metal orientations were found to have a large effect on oxide morpholoies during all stages of oxidation.

Doychak, J. K.↗

Modeling and Simulation of Microstructure Evolution and Deformation in an Irradiated Environment

The ability to predict the behavior of structural components in a nuclear power plant is critical to the nuclear industry. Structural metals in the primary loop of nuclear power plants must endure challenges such as irradiation and mechanical and thermal loading, and these structural metal components must continue to function in potential transient and accident conditions throughout the operational lifetime of the power plant. This extreme operational environment changes the metal microstructure by creating additional defects. The physical interactions of dislocations with these defects govern how the metal will respond to future conditions. Therefore predicting the mechanical response of these metals requires a set of physically based and reliable models of dislocation and defect interactions. These microstructure elements include glide mobile and immobile dislocations, geometrically necessary dislocations, twinning dislocations, irradiation defects, and thermal aging defects. We present here a continuum dislocation dynamics crystal plasticity framework to capture the interaction mechanisms of these dislocations and defects, verified with a combination of benchmark problems and comparisons with experimental data for two different types of structural metals: alpha iron and nickel-based alloys. In our simulations of $\alpha$ iron we highlight the advantages of applying a Monte Carlo stochastic model of cross slip dislocation motion and show the importance of capturing the 3D nature of glide dislocation and self-interstitial atom loop radiation defect interactions. We demonstrate coupling of glide dislocations with geometrically necessary dislocations to capture the influence of lattice bending, including the sensitivity of the geometrically necessary dislocations to changes in the grain boundary angle. We further examine the interaction of glide dislocations with the twin dislocations and thermally aged defects which have been observed in a nickel-based alloy with additional models. Finally we assess the reliability of this crystal plasticity framework by comparing two dislocation glide velocity models across the range of normal operation temperatures. In successfully applying our crystal plasticity framework to multiple metals, we provide further evidence of the reliability of our approach. The results of this mechanism-based continuum dislocation dynamics crystal plasticity framework can be used to inform engineering scale models throughout the nuclear industry.

36 MATERIALS SCIENCE↗

Effect of High-Density Nanoparticles on Recrystallization and Texture Evolution in Ferritic Alloys

Ferritic alloys are important for nuclear reactor applications due to their microstructural stability, corrosion resistance, and favorable mechanical properties. Nanostructured ferritic alloys having a high density of Y-Ti-O rich nano-oxides (NOs < 5 nm) are found to be extremely stable at high temperatures up to ~1100 °C. This study serves to understand the effect of a high density of nano-particles on texture evolution and recrystallization mechanisms in ferritic alloys of 14YWT (14Cr-3W-0.4Ti-0.21Y-Fe wt %) having a high density of nano-particles and dispersion-free FeCrAl (13Cr-5.2Al-0.05Y-2Mo-0.2Si-1Nb wt %). In order to investigate the recrystallization mechanisms in these alloys, neutron diffraction, electron backscattered diffraction, and in situ and ex situ transmission electron microscopy have been utilized. It has been observed that even though the deformation textures of both the 14YWT and FeCrAl alloys evolved similarly, resulting in either the formation (in FeCrAl alloy) or increase (in 14YWT) in γ-fiber texture, the texture evolution during recrystallization is different. While FeCrAl alloy keeps its γ-fiber texture after recrystallization, 14YWT samples develop a ε-fiber as a result of annealing at 1100 °C, which can be attributed to the existence of NOs. In situ transmission electron microscopy annealing experiments on 14YWT show the combination and growth of the lamellar grains rather than nucleation; however, the recrystallization and growth kinetics are slower due to NOs compared to FeCrAl.

36 MATERIALS SCIENCE↗

Salt-Mediated Coarsening in Conversion-Reaction-Synthesized Nanoporous Metals and Nanocomposites Resolved through In Situ Synchrotron Diffraction Studies

High-energy synchrotron X-rays were used to probe the structural and microstructural evolution in Fe, Co, and Cu nanoporous metals (NPMs) and metal/salt nanocomposites (NCs) produced by recently developed conversion reaction synthesis (CRS) methods. Microstructure analysis of as-synthesized samples via whole pattern fitting showed that the NPMs exhibit domain sizes that increase as Co < Fe < Cu, with both Fe and Co having crystallite sizes below 3.0 nm. The as-synthesized metal/salt NCs had similar metal sizes, and additionally, the salt in the composite had unusually large lattice microstrain whose origin is attributed to chemical substitution of metal ions into the salt (e.g., Li $1–3x$ Fe $x$ Cl for Fe 3+ ). When thermal annealing is used to modify crystallite size, pore collapse often occurs in NPMs but NCs can be effectively tuned without this problem. While the NC coarsening occurs slowly at low temperatures, it was found that there is a drastic acceleration of the reaction rate at a specific onset temperature that results in the crystallite size increasing by an order of magnitude in about a minute. Curiously, there was no evidence in the diffraction data for salt melting at this onset temperature. However, there was a sharp reduction in the salt chemical lattice strain at the onset temperature, indicating that rapid metal coarsening is facilitated by the salt. Importantly, this behavior indicates an unexpectedly coupled reaction mechanism by which the metal ions needed for grain growth are supplied by the salt in a rate-limiting fashion.

77 NANOSCIENCE AND NANOTECHNOLOGY↗