Search NASA⌕ Search

SEARCH · Search NASA

Results for “Interphases”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 955 records · Page 53

High-Voltage and High-Safety Practical Lithium Batteries with Ethylene Carbonate-Free Electrolyte

Serious safety issues are impeding the widespread adoption of high-energy lithium-ion batteries for transportation electrification and large-scale grid storage. Herein, a triple-salt ethylene carbonate (EC) free electrolyte for high-safety and high-energy pouch-type LiNi 0.8 Mn 0.1 Co 0.1 O 2 |graphite (NMC811|Gr) cells is reported. This EC-free electrolyte can effectively stabilize the NMC811 surface under high potential (up to 4.5 V), as well as generate a stable interphase to achieve a superior compatibility with the Gr anode. The electrolyte strategy enables significantly enhanced intrinsic safety (trigger temperature of thermal runaway (TR) increased by 67.0 °C), excellent electrochemical properties (4.2V, ≈100% after 200 cycles), and superior high voltage stability (4.5 V, 82.1% after 200 cycles). Furthermore, the work opens up a new avenue for developing novel electrolyte systems to build safer high-energy batteries for practical applications.

25 ENERGY STORAGE↗

Insights into the Crossover Effects in Cells with High‐Nickel Layered Oxide Cathodes and Silicon/Graphite Composite Anodes

Abstract Silicon anodes are regarded as one of the most promising alternatives to graphite (Gr) anodes due to their ultrahigh capacity, abundance, and low cost. Coupling Si‐based anodes with high‐nickel layered oxide cathodes LiNi x Mn y Co 1− x − y O 2 (NMC, x ≥ 0.8) can enhance the driving range for electric vehicles. Transition‐metal (TM) ion dissolution and deposition has been a long‐known failure mode for Gr‐based lithium‐ion batteries. However, the mechanistic insight associated with TM ion deposition on Si‐based anodes has rarely been reported. Herein, the impact of in situ deposited TM ions on SiO x /Gr composite anodes and the individual influences of Ni, Mn, and Co on the structural and electrochemical stability along with the underlying degradation mechanisms are presented. TM ion dissolution causes a greater deleterious impact on Si than on Gr, with different TM ions exhibiting different influences on anode‐electrolyte interphase formation. Specifically, Ni deposit induces more aggressive salt decomposition; Co deposit has negligible effect on salt decomposition, but significantly accelerates solvent decomposition; and Mn deposit aggravates both salt and solvent decompositions, resulting in worse full cell performance. The extent of degradation decreases in the order Mn 2+ > Ni 2+ > Co 2+ . The systematic comparisons presented can guide further development of high energy systems.

Zhang, Xianhui↗

Uncovering the Solvation Structure of LiPF 6 –Based Localized Saturated Electrolytes and Their Effect on LiNiO 2 –Based Lithium–Metal Batteries

Electrolytes play a critical role in stabilizing highly reactive lithium-metal anodes (LMAs) and high-voltage cathodes for rechargeable lithium-metal batteries (LMBs). Localized high concentration electrolytes (LHCEs) have achieved remarkable success in the context of LMBs. However, the state-of-the-art LHCEs are based on LiFSI salt, which is prohibitively expensive. Here, the utility of low-cost LiPF 6 salt in localized saturated electrolytes (LSEs) with a series of solvents and diluents in LMBs with cobalt-free LiNiO 2 cathode is systematically explored. Experimental and theoretical analyses reveal that the unique solvation structure formed not only changes the distribution of solvents and anions but also alters the atom–atom distances within them, leading to different reduction and oxidation stabilities compared to low-concentration electrolytes. In addition, LSEs help form LiF-rich interphase layers on the LMA and LiNiO 2 cathode, protecting the electrodes from degradation during cycling. Different LSEs also lead to differences in lithium plating morphology and impedance buildup during cycling, impacting the performance of LMBs. Finally, the solvent and diluent must be carefully selected for compatibility with a lithium salt when developing LHCEs and LSEs for LMBs.

25 ENERGY STORAGE↗

Enhanced Electrolyte Transport and Kinetics Mitigate Graphite Exfoliation and Li Plating in Fast–Charging Li–Ion Batteries

Despite significant progress in energy retention, lithium-ion batteries (LIBs) face untenable reductions in cycle life under extreme fast-charging (XFC) conditions, which primarily originate from a variety of kinetic limitations between the graphite anode and the electrolyte. Through quantitative Li + loss accounting and comprehensive materials analyses, it is directly observed that the operation of LIB pouch cells at 4 C||C/3 (charging||discharging) results in Li plating, disadvantageous solid-electrolyte-interphase formation, and solvent co-intercalation leading to interstitial decomposition within graphite layers. It is found that these failure modes originate from the insufficient properties of conventional electrolytes, where employing a designed ester-based electrolyte improved the capacity retention of these cells from 55.9% to 88.2% after 500 cycles when operated at the aforementioned conditions. These metrics are the result of effective mitigation of the aforementioned failure modes due to superior Li + transport and desolvation characteristics demonstrated through both experimental and computational characterization. Finally, this work reveals the vital nature of electrolyte design to XFC performance.

25 ENERGY STORAGE↗

Conjugated Imine Polymer Synthesized via Step‐Growth Metathesis for Highly Stable Silicon Nanoparticle Anodes in Lithium‐Ion Batteries

Abstract This work reports a new method to synthesize polyphenylmethanimine (polyPMI) as a linear or a hyperbranched, conjugated polymer using an aldehyde‐imine metathesis reaction. This work details the reaction mechanisms of this polymerization by characterizing a red‐shift in its absorption spectrum as polymer conjugation length increases and verifies that this optical shift results from extended π‐condensation using density functional theory. This new synthetic approach provides a polymer that can potentially be depolymerized for facile recyclability and is compatible with air‐ and water‐sensitive chemistries. As an example of the utility of this new approach, this work demonstrates that this polymer can be directly grown on silicon nanoparticles to create silicon anodes for lithium‐ion batteries with a high degree of electrochemical interfacial passivation. These silicon anodes exhibit Coulombic efficiencies above 99.9% and can accommodate silicon nanoparticle expansion and contraction during lithiation and delithiation as demonstrated by stable reversible capacities for 500 cycles. Finally, this work demonstrates that polyPMI facilitates the formation of a lithium fluoride rich solid electrolyte interphase that remains chemically and mechanically stable after long term cycling.

25 ENERGY STORAGE↗

Intermetallics Based on Sodium Chalcogenides Promote Stable Electrodeposition–Electrodissolution of Sodium Metal Anodes

Sodiophilic micro-composite films of sodium-chalcogenide intermetallics (Na 2 Te and Na 2 S) and Cu particles are fabricated onto commercial copper foam current collectors (Na 2 Te@CF and Na 2 S@CF). For the first time a controllable capacity thermal infusion process is demonstrated. Enhanced wetting by the metal electrodeposition leads to state-of-the-art electrochemical performance. For example, Na 2 Te@CF-based half-cells demonstrate stable cycling at 6 mA cm -2 and 6 mAh cm -2 , corresponding to 54 µm of Na electrodeposited/electrodissolved by geometric area. Sodium metal batteries with Na 3 V 2 (PO 4 ) 3 cathodes are stable at 30C (7 mA cm -2 ) and for 10 000 cycles at 5C and 10C. Cross-sectional cryogenic focused ion beam (cryo-FIB) microscopy details deposited and remnant dissolved microstructures. Sodium metal electrodeposition onto Na 2 Te@CF is dense, smooth, and free of dendrites or pores. On unmodified copper foam, sodium grows in a filament-like manner, not requiring cycling to achieve this geometry. Substrate–metal interaction critically affects the metal–electrolyte interface, namely the thickness and morphology of the solid electrolyte interphase. Density functional theory and mesoscale simulations provide insight into support-adatom energetics, nucleation response, and early-stage morphological evolution. On Na 2 Te sodium atomic dispersion is thermodynamically more stable than isolated clusters, leading to conformal adatom coverage of the surface.

36 MATERIALS SCIENCE↗

A High Energy–Density, Cobalt–Free, Low–Nickel LiNi 0.7 Mn 0.25 Al 0.05 O 2 Cathode with a High–Voltage Electrolyte for Lithium–Metal Batteries

Cobalt-free cathode materials have garnered increased attention for applications in next-generation batteries for electric vehicles, as cobalt is considered to have at a high supply chain risk. Here, the use of a localized saturated electrolyte (LSE) to enable stable cycling of a cobalt-free, low-nickel layered-oxide cathode LiNi 0.7 Mn 0.25 Al 0.05 O 2 (NMA-70) to higher voltages (4.6 V) in a lithium-metal battery is demonstrated. Compared to the baseline LP57 electrolyte, the LSE extends the cycle life from ≈100 cycles to ≈400 cycles before reaching 80% capacity retention. Visual indicators of cell degradation, such as product deposition, are observed on electrodes cycled in LP57. It is shown that cycling NMA-70 in LSE reduces the overall active material loss and overpotential growth during extended cycling. This is attributed to the formation of a beneficial fluorinated interphase layer, a lower degree of rock-salt phase formation, and a reduction in the gas evolution from the cathode surface. The decrease in gas evolution from the cathode cycled in LSE reflects a lower degree of electrolyte reactivity and an overall improvement in the safety characteristics of the cell. Furthermore, this study highlights the importance of a stable electrolyte to enable the high-voltage cycling of alternative, lower nickel, and cobalt-free cathodes.

25 ENERGY STORAGE↗

Crack‐Free Single‐Crystalline LiNiO 2 for High Energy Density All‐Solid‐State Batteries

Abstract Single‐crystalline layered oxide (LiNi 1‐ x ‐ y Mn x Co y O 2 ) cathodes have been found to exhibit exceptional electrochemical properties when coupled with various inorganic solid electrolytes (ISEs) in all‐solid‐state batteries (ASSBs). Their advantages stem from the robust morphological integrity with the absence of grain boundaries and the high electrochemical oxidative stability. Here, ASSBs featuring single‐crystalline LiNiO 2 (LNO) with the highest Ni content are reported, offering a high theoretical specific capacity of 275 mAh g ‐1 alongside a high average discharge voltage (3.7 V vs Li + /Li). Through a careful investigation, it is demonstrated that micron‐sized single‐crystalline LNO (µSC‐LNO) composite cathodes with a halide ISE exhibit a high initial discharge capacity of 205 mAh g ‐1 with an outstanding cycle performance over 200 cycles in room‐temperature ASSBs. The significance of engineering parameters is emphasized, such as particle size and specific density, in promoting a homogeneous and fast Li + transport within the composite cathodes. Furthermore, the formation of undesirable interphase between the halide ISE in the cathode and sulfide ISE separator is elucidated, which may be a critical factor impeding long‐term cyclability of ASSBs. This work provides insights into the design of composite cathodes for high‐energy‐density ASSBs.

Chemistry↗

Mechanical Milling – Induced Microstructure Changes in Argyrodite LPSCl Solid-State Electrolyte Critically Affect Electrochemical Stability

Microstructure of argyrodite solid-state electrolyte (SSE) critically affects lithium metal electrodeposition/dissolution. While the stability of unmodified SSE is mediocre, once optimized state-of-the-art electrochemical performance is achieved (symmetric cells, full cells with NMC811) without secondary interlayers or functionalized current collectors. Planetary mechanical milling in wet media (m-xylene) is employed to alter commercial Li 6 PS 5 Cl (LPSCl) powder. Quantitative stereology demonstrates how milling progressively refines grain and pore size/distribution in the SSE compact, increases its density, and geometrically smoothens the SSE-Li interface. Mechanical indentation demonstrates that these changes lead to reduced site-to-site variation in the compact's hardness. Milled microstructures promote uniform early-stage electrodeposition on foil collectors and stabilize solid electrolyte interphase (SEI) reactivity. Analysis of half-cells with bilayer electrolytes demonstrates the importance of microstructure directly contacting current collector, with interface roughness due to pore and grain size distribution being key. For the first time, short-circuiting Li metal dendrite is directly identified, employing 1.5 mm diameter “mini” symmetrical cell and cryogenic focused ion beam (cryo-FIB) electron microscopy. The branching sheet-like dendrite traverses intergranularly, filling the interparticle voids and forming an SEI around it. Importantly, mesoscale modeling reveals the relationship between Li-SSE interface morphology and the onset of electrochemical instability, based on underlying reaction current distribution.

25 ENERGY STORAGE↗

A Sulfide‐Based Solid Electrolyte With High Humid Air Tolerance for Long Lifespan All‐Solid‐State Sodium Batteries

Abstract Sulfide‐based superionic conductors present great promise to achieve high energy density and safety for all‐solid‐state sodium batteries (ASSSBs). However, the poor electrolyte/electrode interface compatibility and humid air stability seriously hinder their deployment in ASSSBs. Herein, a series of high‐performance Na 3‐□ Sb 1‐4x (SnWCaTi) x S 4 sulfide‐based solid electrolytes (SSEs) are reported by coupling the vacancy effect with configurational entropy, which displays an excellent interface stability against sodium metal and an extraordinary tolerance toward the moist atmosphere, even for water. The optimized electrolyte effectively inhibits the detrimental mixed ion‐electron conducting interphase formation, achieving the ultra‐stable operation of Na–Na symmetric cell up to 1000 h. Furthermore, the Na + diffusion kinetics is obviously enhanced by increasing the Na sites local anisotropy and Na vacancies. Eventually, the assembled TiS 2 //Na 5 Sn ASSSBs deliver a remarkable reversible capacity of 211.6 mAh g −1 at 0.5C with a long‐term cycling performance of 450 cycles at room temperature. More importantly, it achieves a steady running up to 100 cycles at 1C even if this electrolyte is placed in the air with a dew temperature of 13.8 °C for 30 min, the highest values in the state‐of‐the‐art sulfide‐based ASSSBs. The well‐designed SSEs open a new avenue for realizing the advanced and powerful ASSSBs.

Guo, Yayu↗

Effect of Propagating Dopant Reactivity on Lattice Oxygen Loss in LLZO Solid Electrolyte Contacted with Lithium Metal

Lithium lanthanum zirconium oxide (LLZO) is widely known as the most stable solid electrolyte against lithium metal electrodes. This thermodynamic stability can be lost by the presence of dopants which are required to stabilize the cubic phase of LLZO and can be reduced by lithium metal. However, the role of oxygen in such reactions is taken for granted. In this work, the reduction of Nb-substituted LLZO (Nb-LLZO) is explored by Li metal and shows that interfacial reactions propagate and lead to the decomposition with substantial Nb 5+ reduction deep into the bulk electrolyte. Scanning Transmission Electron Microscopy with Energy Dispersive X-ray Spectroscopy and thermogravimetric analyses show much of the reduction is due to oxygen vacancies formed, leading to increased electronic conductivity mapped with conductive Atomic Force Microscopy. Density functional theory calculations indicate oxygen release is favored by increased excess lithiation of Nb-LLZO. Electrochemical impedance of polycrystalline Nb-LLZO shows the continuous evolution of ionically resistive interphases near the lithium metal interface with Nb-LLZO while single crystals show little reactivity at room temperature and self-limiting reduction at 60°C. This work underlines the role of grain boundaries in propagating destructive solid electrolyte reactions and highlights previously unseen mechanisms involving lattice oxygen in LLZO.

Li metal, solid-state electrolytes↗

The Origin of Improved Performance in Boron‐Alloyed Silicon Nanoparticle‐Based Anodes for Lithium‐Ion Batteries

Stabilizing the solid electrolyte interphase (SEI) remains a key challenge for silicon‐based lithium‐ion battery anodes. Alloying silicon with secondary elements like boron has emerged as a promising strategy to improve the cycle life of silicon anodes, yet the underlying mechanism remains unclear. To address this knowledge gap, how boron concentration influences battery performance is systematically investigated. These results show a near‐monotonic increase in cycle lifetime with higher boron content, with boron‐rich electrodes significantly outperforming pure silicon. Additionally, silicon‐boron alloy anodes exhibit nearly three times longer calendar life than pure silicon. Through detailed mechanistic analysis, alternative contributing factors are systematically ruled out, and it is proposed that improved passivation arises from a strong permanent dipole at the nanoparticle surface. This dipole, formed by undercoordinated and highly Lewis acidic boron, creates a static, ion‐dense layer that stabilizes the electrochemical interface, reducing parasitic electrolyte decomposition and enhancing long‐term stability. These findings suggest that, within the SEI framework, the electric double layer is an important consideration in surface passivation. This insight provides an underexplored parameter space for optimizing silicon anodes in next‐generation lithium‐ion batteries.

25 ENERGY STORAGE↗

Decoding Gas Evolution Pathways and Interfacial Chemistry in Layered Oxide Cathodes for Safer Sodium‐Ion Batteries

Sodium-ion batteries (SIBs) are attractive for the low cost and abundance of sodium. Yet, gas evolution—a critical challenge in SIBs—remains underexplored. Here, online electrochemical mass spectrometry is used to probe gas evolution in layered oxide cathodes with various compositions, cutoff voltages, dopants, and particle morphologies. Compared to LiNiO 2 (LNO), NaNiO 2 releases more gas, even at lower states of charge, due to the higher covalency of Ni─O bond caused by the more ionic Na─O bond through the inductive effect. Among Co, Mn, Al, and Mg, Mn and Mg doping suppress gas release most effectively by enhancing the metal-oxygen bond strength. NaNi 1/3 Fe 1/3 Mn 1/3 O 2 (NFM) cathodes synthesized via coprecipitation (CP-NFM) and solid-state routes exhibit distinct particle morphologies; CP-NFM exhibits more gas evolution, yet secondary particle morphology helps reduce it through differential cathode-electrolyte reactivity between inner and outer primary particles. Among Li, Ti, Mg, and Cu doping in NFM, Li has the largest effect, reducing gas levels comparable to LNO. Nuclear magnetic resonance and X-ray photoelectron spectroscopies reveal that electrolyte solvent decomposition mainly produces organic-rich cathode-electrolyte interphase (CEI) rather than soluble species. NaPF 6 salt further exacerbates cathode-electrolyte reactions, forming surface Na 2 O species. The findings provide actionable guidance for designing safer, durable SIBs.

25 ENERGY STORAGE↗

An Artificial SEI Enables the Use of A LiNi0.5Mn1.5O4 5 V Cathode with Conventional Electrolytes

LiNi0.5Mn1.5O4 spinel is considered one of the most promising cathodes for advanced lithium ion batteries. However, the operation potential of LiNi0.5Mn1.5O4, ~4.75 V, is beyond the high voltage limit of the state-of-art electrolyte, ~4.3 V. Here, using thin films of LiNi0.5Mn1.5O4 as a model material, we show evidence that an artificial solid electrolyte interphase (SEI) enables the use of this 5 V cathode with conventional carbonate electrolytes. A thin coating of Lipon (lithium phosphorus oxynitride) as an artificial SEI on LiNi0.5Mn1.5O4 could remedy the decomposition of the electrolyte. The thickness of the Lipon artificial SEI is optimized by balancing the protection and additional resistance. The strategy of artificial SEI on cathodes is expected to enable the wide application of other high voltage cathodes for lithium ion batteries.

artificial SEI↗

A mechanistic modeling framework for gas-phase adsorption kinetics and fixed-bed transport

Adsorption is a complex physicochemical process involving interparticle transport, interphase mass-transfer, intraparticle diffusion, and surface reactions. Although the exact description of the adsorption process will inevitably vary from system to system, it will always be governed by those primary mechanisms. Thus, by devising a model framework that can inherently include those mechanisms, it would be possible to create a modeling platform on which many different adsorption problems could be solved numerically. In order to accomplish this task, a generalized 1-D conservation law model was created to include the necessary mechanisms of adsorption on several different geometrical domains. Specific model applications for adsorption were developed under that framework and validated using experimental data available in literature or obtained in this work. This modeling platform makes it easier to model various adsorption problems and develop new adsorption models because of the common treatment of the mathematics governing the physical processes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A High‐Energy‐Density Potassium Battery with a Polymer‐Gel Electrolyte and a Polyaniline Cathode

Abstract A safe, rechargeable potassium battery of high energy density and excellent cycling stability has been developed. The anion component of the electrolyte salt is inserted into a polyaniline cathode upon charging and extracted from it during discharging while the K + ion of the KPF 6 salt is plated/stripped on the potassium‐metal anode. The use of a p‐type polymer cathode increases the cell voltage. By replacing the organic‐liquid electrolyte in a glass‐fiber separator with a polymer‐gel electrolyte of cross‐linked poly(methyl methacrylate), a dendrite‐free potassium anode can be plated/stripped, and the electrode/electrolyte interface is stabilized. The potassium anode wets the polymer, and the cross‐linked architecture provides small pores of adjustable sizes to stabilize a solid‐electrolyte interphase formed at the anode/electrolyte interface. This alternative electrolyte/cathode strategy offers a promising new approach to low‐cost potassium batteries for the stationary storage of electric power.

Gao, Hongcai↗

Salt‐Based Organic–Inorganic Nanocomposites: Towards A Stable Lithium Metal/Li 10 GeP 2 S 12 Solid Electrolyte Interface

Abstract Solid‐state Li metal battery technology is attractive, owing to the high energy density, long lifespans, and better safety. A key obstacle in this technology is the unstable Li/solid‐state electrolyte (SSE) interface involving electrolyte reduction by Li. Herein we report a novel approach based on the use of a nanocomposite consisting of organic elastomeric salts (LiO‐(CH 2 O) n ‐Li) and inorganic nanoparticle salts (LiF, ‐NSO 2 ‐Li, Li 2 O), which serve as an interphase to protect Li 10 GeP 2 S 12 (LGPS), a highly conductive but reducible SSE. The nanocomposite is formed in situ on Li via the electrochemical decomposition of a liquid electrolyte, thus having excellent chemical and electrochemical stability, affinity for Li and LGPS, and limited interfacial resistance. XPS depth profiling and SEM show that the nanocomposite effectively restrained the reduction of LGPS. Stable Li electrodeposition over 3000 h and a 200 cycle life for a full cell were achieved.

Gao, Yue↗

Synergy of Epoxy Chemical Tethers and Defect‐Free Graphene in Enabling Stable Lithium Cycling of Silicon Nanoparticles

Abstract We report a new approach for nanosilicon–graphene hybrids with uniquely stable solid electrolyte interphase. Expanded graphite is gently exfoliated creating “defect‐free” graphene that is non‐catalytic towards electrolyte decomposition, simultaneously introducing high mass loading (48 wt. %) Si nanoparticles. Silane surface treatment creates epoxy chemical tethers, mechanically binding nano‐Si to CMC binder through epoxy ring‐opening reaction while stabilizing the Si surface chemistry. Epoxy‐tethered silicon pristine–graphene hybrid “E‐Si‐pG” exhibits state‐of‐the‐art performance in full battery opposing commercial mass loading (12 mg cm −2 ) LiCoO 2 (LCO) cathode. At 0.4 C, with areal capacity of 1.62 mAh cm −2 and energy of 437 Wh kg −1 , achieving 1.32 mAh cm −2 , 340.4 Wh kg −1 at 1 C. After 150 cycles, it retains 1.25 mAh cm −2 , 306.5 Wh kg −1 . Sputter‐down XPS demonstrates survival of surface C‐Si‐O‐Si groups in E‐Si‐pG after repeated cycling. The discovered synergy between support defects, chemical‐mechanical stabilization of Si surfaces, and SEI‐related failure may become key LIB anode design rule.

Liu, Wei↗