Search NASA⌕ Search

SEARCH · Search NASA

Results for “Sputtering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 955 records · Page 53

Mechanical and chemical effects of ion-texturing biomedical polymers

To determine whether sputter etching may provide substantial polymer surface texturing with insignificant changes in chemical and mechanical properties, an 8 cm beam diameter, electron bombardment, argon ion source was used to sputter etch (ion-texture process) nine biomedical polymers. The materials included silicone rubber, 32% carbon impregnated polyolefin, polyoxymethylene, polytetrafluoroethylene, ultrahigh molecular weight (UHMW) polyethylene, UHMW polyethylene with carbon fibers (10%), and several polyurethanes (bioelectric, segmented, and cross linked). Ion textured microtensile specimens of each material except UHMW polyethylene and UHMW polyethylene with 10% carbon fibers were used to determine the effect of ion texturing on tensile properties. Scanning electron microscopy was used to determine surface morphology changes, and electron spectroscopy for chemical analysis was used to analyze the near surface chemical changes that result from ion texturing. Ion energies of 500 eV with beam current densities ranging from 0.08 to 0.19 mA/sq cm were used to ion texture the various materials. Standard microtensile specimens of seven polymers were exposed to a saline environment for 24 hours prior to and during the tensile testing. The surface chemical changes resulting from sputter etching are minimal in spite of the often significant changes in the surface morphology.

Weigand, A. J.↗

The stability of water on Io

Various processes have been examined to determine their impact on water loss from Io and the formation of an anhydrous surface. Thermal escape, photolysis, and gas-phase charged particle interactions are shown to be unimportant. Recent laboratory experiments have shown that charged-particle sputtering is likely to be an effective mechanism for the removal of water ice from Io's surface. Vaporization of ice by meteoroid impacts may also be significant. The overall sputtering rate appears to be sufficiently high that the formation of a substantial regolith due to meteoroid bombardment will be prevented. However, meteoroid bombardment is probably capable of maintaining a thin (about 500 microns) overturned surface layer from which all free water has been removed by sputtering. Alternatively, a thick anhydrous surface layer may have formed on Io as the result of primordial heating. The survival of such a layer to the present implies the absence of subsequent water evolution onto the surface of the satellite.

Pilcher, C. B.↗

Static evaluation of surface coatings for compliant gas bearings in an oxidizing atmosphere to 650 C

Hard wear-resistant coatings and soft low shear strength coatings were developed for an air-lubricated compliant journal bearing for a future automotive gas turbine engine. The coatings were expected to function in either 540 or 650 C ambient. Soft lubricant coatings were generally limited in temperature. Therefore emphasis was on the hard wear-resistant coatings. The coating materials covered were TiC, B4C, Cr3C2, WC, SiC, CrB2, TiB2, Cr2O3, Al2O3, Si3N4, Tribaloy 800, CaF2, CaF2-BaF2 eutectic, Ni-Co, silver, CdO-graphite and proprietary compounds. The coatings on test coupons were subjected to static oven screening tests. The test consisted of exposure of material samples in an oven for 300 h at the maximum temperature (540 or 650 C) and ten temperature cycles from room temperature to the maximum service temperature. On the basis of the specimen examinations the following coatings were recommended for future wear tests: TiC (sputtered), Cr2O3 (sputtered), Si3N4 (sputtered), CdO and graphite (fused), Kaman DES (a proprietary coating), CrB2 (plasma sprayed), Cr3C2 (detonation gun) and NASA PS-106 (plasma sprayed).

Bhushan, B.↗

Ion beam texturing of surfaces

Textured surfaces, typically with conical structures, have been produced previously by simultaneously etching a surface and seeding that surface with another material. A theory based on surface diffusion predicts a variation in cone spacing with surface temperature, as well as a critical temperature below which cones will not form. Substantial agreement with theory has been found for several combinations of seed and surface materials, including one with a high sputter yield seed on a low sputter yield surface (gold on aluminum). Coning with this last combination was predicted by the theory for a sufficiently mobile seed material. The existence of a minimum temperature for the formation of cones should also be important to those interested in ion-beam machining smooth surfaces. Elements contained in the environmental contaminants or in the sputtered alloys or compounds may serve as seed material.

Kaufman, H. R.↗

The erosion of planetary and satellite atmospheres by energetic atomic particles

Analytic expressions are presented which may be used to compute the sputter-erosion yield from any unimolecular gravitationally bound gas by any atomic charged particle of any energy. A calculation of solar wind proton and alpha particle induced erosion of the CO2 atmosphere of Mars predicts molecular sputtering yields. An expression for the emission yield of energetic molecular fragments produced in primary knock-on events is given in closed form; such fragment emission is of secondary importance for mass loss compared to the molecular yield itself. Erosion by radiation belt protons of a hypothetical thin O2 atmosphere associated with the Jovian satellite Ganymede is considered, and molecular sputtering yields for proton energies are determined.

Haff, P. K.↗

Improved refractory coatings

The adhesion, friction and wear properties of sputtered refractory coatings on substrates of materials that form stable nitrides are enhanced by placing each substrate directly below a titanium carbide target of a commercial radiofrequency diode apparatus in a vacuum chamber. Nitrogen is bled into the system through a nozzle resulting in a small partial pressure of about 0.5% to 2.5% during the first two minutes of deposition. The flow of nitrogen is then stopped, and the sputtering ambient is reduced to pure argon through a nozzle without interrupting the sputtering process. When nitrogen is deliberately introduced during the crucial interface formation, some of the titanium at the interface reacts to form titanium nitride while the metal of the substrate also forms the nitride. These two nitrides atomically mixed together in the interfacial region act to more strongly bond the growing titanium carbide coating as it forms on the substrate.

Brainard, W. A.↗

Prototype Ge:Ga detectors for the NASA-Ames cooled grating spectrometer

The detectors were fabricated from a Ge:Ga wafer from Eagle-Pitcher with a room temperature resistivity of approx. 12ohms cm. The wafer is approximately 2 inches in diameter and 0.061 inches thick. The contact material was ion implanted with Boron using 10 to the 14th power ions/sq cm at 25 Kev and 2 x10 to the 14th power ions/sq cm at 50 Kev. The crystal was then sputter-cleaned and metallized first with sputtered Ti and then sputter Au. In addition to the usual infrared measurements of responsivity and noise, measurements were made of the detectors' response to ionizing radiation.

Houck, J. R.↗

Ion beam deposited protective films

Sputter deposition of adherent thin films on complex geometric surfaces by ion beam sources is examined in order to evaluate three different types of protective coatings for die materials. In the first experiment, a 30 cm diameter argon ion source was used to sputter deposit adherent metallic films up to eight microns thick on H-13 steel, and a thermal fatigue test specimen sputter deposited with metallic coatings one micron thick was immersed in liquid aluminum and cooled by water for 15,000 cycles to simulate operational environments. Results show that these materials do protect the steel by reducing thermal fatigue and thereby increasing die lifetime. The second experiment generated diamond-like carbon films using a dual beam ion source system that directed an eight cm argon ion source beam at the substrates. These films are still in the process of being evaluated for crystallinity, hardness and infrared absorption. The third experiment coated a fiber glass beam shield incorporated in the eight-cm diameter mercury ion thruster with molybdenum to ensure proper electrical and thermal properties. The coating maintained its integrity even under acceleration tests.

Mirtich, M. J.↗

Ion beam surface modification

The essential details of a study on the practical applications and mechanisms of polymer sputtering via Argon ion impact are summarized. The potential to modify the properties of polymer surfaces to improve their adherence, durability, biocompatibility, or other desirable properties by ion beam sputtering was emphasized. Ion beam milling can be of benefit as an analytical tool to obtain composition versus depth information. Ion impact from a directed ion gun source specifically etches polymer structures according to their morphologies, therefore this technique may be useful to study unknown or new morphological features. Factors addressed were related to: (1) the texture that arises on a polymer target after ion impact; (2) the chemistry of the top surface after ion impact; (3) the chemistry of sputtered films of polymeric material deposited on substrates placed adjacent to targets during ion impact; and (4) practical properties of textured polymer targets, specifically the wettability and adhesive bonding properties.

Dwight, D. W.↗

Development of an 1100 deg F capacitor

The feasibility of developing a high temperature capacitor for 1100 F operation which is as small and light as conventional capacitors for normal operating temperatures is discussed. Pyrolyic boron nitride (PBN) was selected for the dielectric. The PBN capacitors were made by slicing and lapping material from thick blocks and then sputtering thin film electrodes. These capacitors had breakdown strengths of 7,000 volts per mil and a dissipation factor of less than 0.001 at 1100 F. Additional processing improvements were made after testing a multi-layer or stacked PBN capacitor for 1,000 hours at 1100 F. Sputter etching the wafers before depositing electrodes resulted in a reduction in dissipation factor. A sputtered boron nitride film applied to the outer electrode surfaces produced a more stable capacitor. A design for a 0.1 mu F capacitor and a summary of PBN wafer fabrication costs are given.

Stapleton, R. E.↗

Refractory coatings and method of producing the same

The adhesion, friction, and wear properties of sputtered refractory coatings on substrates of materials that form stable nitrides is improved by placing each substrate directly below a titanium carbide target of a commercial radiofrequency diode apparatus in a vacuum chamber. Nitrogen is bled into the system through a nozzle resulting in a small partial pressure of about 0.5% to 2.5% during the first two minutes of deposition. The flow of nitrogen is then stopped, and the sputtering ambient is reduced to pure argon through a nozzle without interrupting the sputtering process. When nitrogen is deliberately introduced during the crucial interface formation, some of the titanium at the interface reacts to form titanium nitride while the metal of the substrate also forms the nitride. These two nitrides atomically mixed together in the interfacial region act to more strongly bond the growing titanium carbide coating as it forms on the substrate.

Brainard, W. A.↗

Refractory coatings

A thin sputtered film is discussed which exhibits improved adherence to a substrate and has improved friction and wear characteristics. Each substrate is placed directly below a titanium carbide target of a commercial radiofrequency diode apparatus in a vacuum chamber. Nitrogen is bled into the system through a nozzle resulting in a small partial pressure of about 0.5% to 2.5% during the first two minutes of deposition. The flow of nitrogen is then stopped, and the sputtering ambient is reduced to pure argon through a nozzle without interrupting the sputtering process.

Brainard, W. A.↗

Endurance test of a 30-CM-diameter engineering model ion thruster. Task 12: Investigation of thin-film erosion monitors for ion thrusters

An investigation of short term measurement techniques for predicting the wearout of ion thrusters resulting from sputter erosion damage is described. The previously established laminar thin film techniques to provide high precision erosion rate data. However, the erosion rates obtained using this technique are generally substantially higher than those obtained during long term endurance tests (by virtue of the as deposited nature of the thin films), so that the results must be interpreted in a relative sense. Absolute measurements can be performed using a new masked substrate arrangement which was developed during this study. This new technique provides a means for estimating the lifetimes of critical discharge chamber components based on direct measurements of sputter erosion depths obtained during short duration (10 hour) tests. The method enables the effects on lifetime of thruster design and operating parameters to be inferred without the investment of the time and capital required to conduct long term (1000 hour) endurance tests. Results obtained using the direct measurement technique are shown to agree with sputter erosion depths calculated for the plasma conditions of the test and also with lifetest results. The direct measurement approach is shown to be applicable to both mercury and argon discharge plasma environments and should be useful in estimating the lifetimes of inert gas and extended performance mercury ion thrusters presently under development.

Beattie, J. R.↗

A direct-measurement technique for estimating discharge-chamber lifetime

The use of short-term measurement techniques for predicting the wearout of ion thrusters resulting from sputter-erosion damage is investigated. The laminar-thin-film technique is found to provide high precision erosion-rate data, although the erosion rates are generally substantially higher than those found during long-term erosion tests, so that the results must be interpreted in a relative sense. A technique for obtaining absolute measurements is developed using a masked-substrate arrangement. This new technique provides a means for estimating the lifetimes of critical discharge-chamber components based on direct measurements of sputter-erosion depths obtained during short-duration (approximately 1 hr) tests. Results obtained using the direct-measurement technique are shown to agree with sputter-erosion depths calculated for the plasma conditions of the test. The direct-measurement approach is found to be applicable to both mercury and argon discharge-plasma environments and will be useful for estimating the lifetimes of inert gas and extended performance mercury ion thrusters currently under development.

Beattie, J. R.↗

Ion-beam-textured and coated surfaces experiment (S1003)

The objective of this LDEF experiment is to measure the effects of exposure to the shuttle launch and near Earth space environments on the optical properties of ion beam textured high absorptance solar thermal control surfaces, the optical and electrical properties of ion beam sputtered conductive solar thermal control surfaces, and the weight loss of ion beam deposited oxide polymer films. The various types of surfaces to be tested include six major categories: (1) ion beam textured surfaces suitable for space solar thermal (solar concentration) application; (2) painted and/or state of the art solar thermal surfaces; (3) ion beam sputtered conductive coatings for thermal and space charge control (e.g., indium-oxide coated metalized FEP Teflon); (4) ion beam sputtered conductive coated solar sail materials for space charge control and cooling through emittance; (5) micrometeoroid sensitive samples whose optical properties change only as a result of micrometeoroid impact; and (6) Kapton coated with oxide polymer films to minimize oxygen degradation at near Earth orbit altitudes.

Mirtich, M. J., Jr.↗

Escape of sulfur and oxygen from Io

Charged particle sputtering is reexamined as a mechanism for escape of sulfur and oxygen from Io. Corotating ions and energetic ions are considered, using the best available determinations of ion fluxes and sputtering yields. It is unclear whether molecular SO2 is the dominant escaping neutral from Io or whether atomic O and S are dominant, but the Voyager detection of SO2(+) in the cold torus implies the presence of molecular SO2 there. Thin atmosphere models encounter serious difficulty in achieving adequate sulfur and oxygen escape rates, but they are not yet ruled out. Ionization and dissociation of SO2 in a sputter corona can dominate direct escape. In thick atmosphere models the neutral escape rates can be much higher, but the oxygen escape rate tends to be too high relative to the sulfur escape rate unless diffusive separation in the atmosphere is limited, perhaps by rapid mixing.

Cheng, A. F.↗

Do the Satellites of Uranus Control Its Magnetosphere?

The importance of the satellites of Uranus as sources of magnetospheric plasma were investigated. It is found that neither an Io like plasma source nor a Titan like source is likely at Uranus. The likely presence of a heavy ion plasma torus maintained by charged particle sputtering of the icy satellites is examined. Sputtering of Saturn's icy satellites is considered an important source of heavy ion (oxygen) plasma in Saturn's inner magnetosphere. A major unresolved question is whether this sputtering process does depend on the preexistence of magnetospheric heavy ions derived from another source, Titian.

Cheng, A. F.↗

Plasma Production by Meteoroid Impact

Material ejected from the surfaces of satellites in the outer solar system plays an important role in the magnetospheres of the outer planets, and may dominate the mass loading, as in the vicinity of the Jovian satellite Io. At least four potential ejection mechanisms can be identified - intrinsic geologic activity, thermal sublimation, sputtering, and micrometeoroid impact vaporization. On all the icy satellites, except possibly Enceladus, sputtering and impact vaporization are the only two potentially important sources of magnetospheric plasma. Sputtering was shown to be an important mass source at both Jupiter and Saturn. The impact mechanism as a plasma source is assessed.

Haff, P. K.↗