Investigation of Mixed-Type Craters and the Role of Bifluoride Additives to Produce Zirconia-Toughened Alumina-Based PEO Coating
Al{sub 2}O{sub 3}-ZrO{sub 2} composite ceramic coatings were prepared on Al6061 aluminum alloy by plasma electrolytic oxidation in Na{sub 3}PO{sub 4}-K{sub 2}ZrF{sub 6}-Na{sub 2}SiF{sub 6}-based alkaline electrolyte. Optimum processing time for the coating formation was found to be ~ 50 min. Cross section and surface morphology of the coatings were analyzed using scanning electron microscope. From the phase and elemental composition analysis, the presence of m-ZrO{sub 2} and t-ZrO{sub 2} phases was confirmed. It was further observed that the peak intensities of t-ZrO{sub 2} and α-Al{sub 2}O{sub 3} phases increased with processing time, which was attributed to the enhanced crystallinity caused by the efficient sintering conditions. Corrosion properties were investigated by potentiodynamic polarization test in 3.5 wt.% NaCl solution. The results showed high improvement in corrosion rate with minimum recorded value ~ 0.25 mmy (mm/year) and corrosion current ~ 0.15 × 10{sup −6} A/cm{sup 2}.