Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscattered diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 973 records · Page 54

Effect of Nd:YAG laser welding on microstructure and hardness of an Al-Li based alloy

Butt joints of 3.0 mm thick sheets of an Al-Li based alloy have been produced using Nd:YAG laser welding without filler metals. The hardness distribution and microstructure of the alloy and welded joints were investigated. The changes in the grain shapes, grain orientations, microtexture, and precipitates of the fusion zone were analyzed using optical microscope, electron back scattered diffraction (EBSD) and transmission electron microscopy (TEM). The results show that Nd:YAG laser welding leads to a change of the microhardness, grain shape, grain orientations, and a disappearance of the microtexture and precipitates. A narrow band of EQZ along the fusion boundary and a predominantly equiaxed dendritic structure are developed in the fusion zone. The formation of the predominately equiaxed dendritic grains is due to a heterogeneous nucleation mechanism aided by equilibrium A1{sub 3}Zr phases as well as the growth of pre-existing nuclei created by dendrite fragmentation, or by grain detachment resulted from Nd:YAG laser welding processes. In addition, Nd:YAG laser welding produces lower Vickers hardness than that of the base metal due to the decrease in the in quantity of {delta} Prime precipitates in the fusion zone. - Graphical Abstract: The grain shapes, grain orientations, microtexture, and precipitates of the solidified fusion zone were investigated and compared with the base metal using optical microscope, electron back scattered diffraction (EBSD) and transmission electron microscope (TEM). EBSD orientation map of laser welded joint in 5A90 alloys is presented in Fig. 3. It clearly shows that a narrow band EQZ along the fusion boundary and the predominantly equiaxed grains have been developed in the fusion zone of 5A90 alloys. Also, it is clear that the microstructure of the base metal is characterized by laminated grains with preferred orientations, whereas the fusion zone is predominately equiaxed grains in different colors having random orientations. Highlights: Black-Right-Pointing-Pointer The predominantly equiaxed dendritic structure is developed in the fusion zone. Black-Right-Pointing-Pointer The fusion zone with equiaxed grains shows random orientations and microtexture. Black-Right-Pointing-Pointer The loss in hardness in the fusion zone is due to the decrease in {delta} Prime precipitates. Black-Right-Pointing-Pointer The non-epitaxial growth occurs at fusion boundary. Black-Right-Pointing-Pointer The equilibrium A1{sub 3}Zr phases maybe the nuclei of new grains in the fusion zone.

36 MATERIALS SCIENCE↗

Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers

This paper investigates the microstructural characterization of the fracture propagation edge during laser beam welding of Ti6Al4V and 304 stainless steel using Cu, V, and Ni interlayers as a single Cu interlayer and composite interlayer structures with different Cu interlayer thicknesses. This study attempts to increase the Ti-SS joint strength through the use of the composite interlayers. X-ray diffraction characterization based on a 0.5-mm-thick Cu interlayer showed that the SS/Cu/Ti joint contained considerable brittle IMCs; however, the fracture surface of the SS/Cu-V/Ti composite interlayer sample did not contain any Fe-Ti IMCs or Cr{sub 2}Ti. EBSD observation indicated that the crack propagated transgranularly from solidified CuTi in the interdendritic regions of the FeTi compounds in the composite interlayer sample; however, the crack propagated intergranularly along Fe{sub 2}Ti grain boundaries in the single interlayer sample. The investigation based on a 1-mm-thick Cu interlayer showed that the SS/Ni-Cu1/Ti sample was stronger than the SS/Cu1/Ti sample due to a lack of CuTi at 3.5 kW. The tensile strength of the SS/Cu1-V/Ti joint was greater than that of the SS/Ni-Cu1/Ti joint due to the formation of ductile NiTi instead of brittle NiTi{sub 2}. The microstructures of the fracture edges after tensile testing illustrated that the eutectic CuTi + CuTi{sub 2} fractured at the SS/Cu1/Ti joint after tensile testing, while CuTi{sub 2} and eutectoid αTi + CuTi{sub 2} compounds fractured during the tensile experiment at the SS/Ni-Cu1/Ti and SS/Cu1-V/Ti joints, respectively. Investigations based on both the 0.5- and 1-mm-thick Cu interlayers showed that the tensile strength and elongation of the composite interlayer joints at a laser power of 3.5 kW were greater than those of the single interlayer joints.

36 MATERIALS SCIENCE↗

A New Grain Refiner for Ferritic Steels

A new grain refiner, LaB{sub 6}, was identified for ferritic steels based on the crystallographic calculation using the edge-to-edge matching model. Addition of 0.5 wt pct LaB{sub 6} led to a reduction of the average grain size from 765 to 92 μm and the proportion of the columnar structure from 35 to 8 pct in an as-cast Fe-4Si ferritic alloy. Although LaB{sub 6} was supposed to act as an active inoculant for δ-ferrite, thermodynamic calculation indicated that LaB{sub 6} is not thermodynamically stable in the melt of the Fe-4Si alloy. It was subject to decompose into La and B solutes. Consequently, both La and B reacted with Fe, O and S, forming different compounds. Microstructural examination at room temperature observed La{sub 2}SO{sub 2} and La{sub 2}O{sub 3} particles within the ferrite grains and Fe{sub 2}B along the grain boundaries in the samples. Through EBSD analysis, a reproducible orientation relationship between ferrite and La{sub 2}SO{sub 2} was identified. In addition, the edge-to-edge matching calculation also predicted the high potency for La{sub 2}SO{sub 2} to be an effective nucleant for δ-ferrite. It was considered that the grain refinement of LaB{sub 6} was attributed to the enhanced heterogeneous nucleation of δ-ferrite by La{sub 2}SO{sub 2}, and the solute effect of B due to the high Q-value in ferrite.

36 MATERIALS SCIENCE↗

High-Temperature Properties and Microstructural Stability of the AISI H13 Hot-Work Tool Steel Processed by Selective Laser Melting

The microstructural stabilities, softening resistance, and high-temperature tensile properties of the H13 hot-work tool steel by selective laser melting (SLM) were systematically studied. A series of tempering procedures were performed on the as-SLMed specimens. Afterwards, the mechanism of softening resistance behavior was discussed based on the XRD, SEM, EBSD observations, hardness measurements, and high-temperature tensile tests. It was found that the as-SLMed H13 consisted of α-iron and γ-iron. The carbide-stabilizing elements aggregated as the cell-like substructures for the rapid solidification of the SLM process. After the softening resistance treatment, the retained austenite transformed to ferrite and carbide mixtures. The cell-like substructures dissolved slowly into the matrix when the temperature was below 550 °C. These factors increased the hardness and retarded the softening of the material. When the temperature was 600 °C, the microstructural constituents transformed to soft ferrite and globular carbides, which lead to a considerable decrease of the hardness. Due to the grain refinement, solid solution strengthening, and residual stress, the as-SLMed H13 exhibited better mechanical properties than that of the wrought counterparts.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructure Evolution During Bending–Unbending Deformation of Pure Titanium Sheet

In this study, the pure titanium sheets with thickness of 1 mm are deformed 1-5 times in the form of bending–unbending cyclic deformation. The bending angles before and after unbending are 120° and 180°, respectively. Mechanical properties of samples during cyclic deformation, including M/(BH){sup 2}-surface strain curve and spring back in each bending cycle, have been investigated. Moreover, the twinning/detwinning behavior and texture evolution in three typical bending layers (i.e., the tensile layer, neutral layer and compressive layer) in cyclic deformation have been tested by EBSD and TEM, and analyzed systematically. The results indicate that the most intensive twins, consist of similar proportion of tensile and compressive ones, distribute in the inner layer after 1st bending. While they disappear almost entirely after 1st unbending. The twins in outer layer could also be detwinned, and the new twins could be activated during 1st unbending. Besides, the twin density increases obviously and the residual twins could not be detwinned clearly after multiple passes of cyclic deformation. Moreover, the Schmid factor along the σ{sub 2} direction functions in the activation of twin variants regardless of the three-direction stress states.

36 MATERIALS SCIENCE↗

Corrosion Behavior of 316L Stainless Steel Fabricated by Selective Laser Melting Under Different Scanning Speeds

This work discussed the effects of different scanning speeds (800, 1083, 1200 and 1400 mm/s) on the microstructure of 316L stainless steel manufactured by selective laser melting (SLM) and the related corrosion behavior. Results showed that there were more voids with faster scanning speeds, and there were oxide powder and non-melt silicon inside the defects. The SLM 316L exhibited a full gamma austenite phase filled with sub-grains, and the average grain size of SLM-1083 mm/s 316L was approximately 42 μm, three times larger than that of the quenched 316L. The pitting potentials for the SLM 316L were all approximately 300 mV higher than that of the quenched due to the modification of inclusions in SLM, but the corrosion rate for the SLM 316L was faster, which was attributed to the voids and unstable passive film. The number of pitting sites increased with the scanning speed, and the pits occurred preferentially at the voids in SLM 316L.

36 MATERIALS SCIENCE↗

EBSD Study on Processing Domain Parameters of Oxide Dispersion Strengthened 18Cr Ferritic Steel

This paper presents the results of an experimental study aimed to identify hot working domains in oxide dispersion strengthened (ODS) 18Cr ferritic steel over a wide range of temperatures (1323-1473 K) and strain rates (0.01-10 s{sup −1}). The experimental data were obtained by uniaxial compression test using the Gleeble-1500D simulator in this range of temperature and strain rate. An inverse relationship with temperature and positive strain rate sensitivity associated with dynamic recovery and recrystallization, which is influenced by temperature and strain rate, was derived from the flow stress. Based on the processing map generated at 0.5 true strain, using rate dynamic material model (DMM) approach and the calculated instability parameter (ξ(ϵ́))>0, the optimum processing domain has been determined for this steel. The most favorable processing parameters are found in the temperature ranges of 1350-1450 K with a strain rate of 0.01 s{sup −1} and 1473 K with a strain rate 0.1 s{sup −1} with peak efficiency of 30 and 35%, respectively. The material flow behavior was studied using scanning electron microscopy (SEM)-based EBSD microstructural characterization. The steel subjected to 1323 K at high strain rate 10 s{sup −1} in the low-efficiency workability region showed low aspect ratio as compared to the elongated bamboo-like initial microstructure; however, minimum strain rate (0.01 s{sup −1}) showing that localized slip/shearing is the key mechanism and fiber texture studied from the intensity distribution of inverse pole figure showed the presence of significant amount of θ-fibers. In contrast, dynamic recrystallization dominated at higher efficiency region in the safe domain of processing map and γ-fiber texture was evident in the specimen deformed at 1373 and 1473 K with strain rate of 0.01 and 0.1 s{sup −1}, respectively, which is responsible for the change in the initial 〈1 1 0〉//ED α-fiber texture.

36 MATERIALS SCIENCE↗

Superior Corrosion Resistance Properties of TiN-Based Coatings on Zircaloy Tubes in Supercritical Water

Thin films of TiN and Ti0.35Al0.65N nanocomposite were deposited on polished Zircaloy-4 tubes. After exposure to supercritical water for 48 h, the coated tubes are remarkably intact, while the bare uncoated tube shows severe oxidation and breakaway corrosion. X-ray diffraction patterns, secondary electron images, backscattered electron images, and energy dispersive X-ray spectroscopy data from the tube surfaces and cross-sections show that a protective oxide, formed on the film surface, effectively prevents further oxidation and corrosion to the Zircaloy-4 tubes. This result demonstrates the effectiveness of thin film ceramics as protective coatings under extreme environments.

36 MATERIALS SCIENCE↗

Microstructure and nanohardness distribution in a polycrystalline Zn deformed by high strain rate impact

Polycrystalline Zn with an average grain size of about 300 {mu}m was deformed by direct impact Hopkinson pressure bar at a velocity of 29 m/s. An inhomogeneous grain structure was found consisting of a center region having large average grain size of 20 {mu}m surrounded by a fine-grained rim with an average grain size of 6 {mu}m. Transmission electron microscopy investigations showed a significant dislocation density in the large-grained area while in the fine-grained rim the dislocation density was negligible. Most probably, the higher strain yielded recrystallization in the outer ring while in the center only recovery occurred. The hardening effect of dislocations overwhelms the smaller grain size strengthening in the center part resulting in higher nanohardness in this region than in the outer ring. - Graphical Abstract: (a): EBSD micrograph showing the initial microstructure of polycrystalline Zn that was subsequently submitted to high strain rate impact. (b): an inhomogeneous grain size refinement was obtained which consists of a central coarse-grained area, surrounded by a fine-grained recrystallized rim. The black arrow points to the disc center. Research Highlights: {yields} A polycrystalline Zn specimen was submitted to high strain rate impact loading. {yields} Inhomogeneous grain refinement occurred due to strain gradient in impacted sample. {yields} A fine-grained recrystallized rim surrounded the coarse-grained center of specimen. {yields} The coarse-grained center exhibited higher hardness than the fine-grained rim. {yields} The higher hardness of the center was caused by the higher dislocation density.

36 MATERIALS SCIENCE↗

Microstructure characterization of recycled IN718 powder and resulting laser clad material

Highlights: • A simple and efficient recycling procedure of IN718 powder has been defined for the laser cladding process. • Characterization of wasted and cleaned powder and comparison with new IN718 powder pointed out a slight diameter increase. • Microstructure characterization of clad builds showed differences between builds with new and recycled powders. • Clad microstructure and porosity increase remain constant static properties but decrease rupture strain after 3 reuses. • Without special precautions for cladding, the recycled powder can be reused twice without modifying the properties of IN718. - Abstract: The possibility to reuse the metal powder wasted in Laser Material Deposition (LMD) process has been evaluated and a simple procedure developed. LMD uses metal powder which is fed through a nozzle into the focal point of a laser, where it melts the powder and the substrate material. During the process, a high ratio of particles hits against an unmelted area and directly bounces off the deposited area. The efficiency ratio of deposition can drop to 40% depending on the configuration and spot size. This work deals with the design of a procedure to recollect and reuse the wasted powder of a nickel based superalloy IN718. After usage, powder is recollected, undesired fractions are magnetically segregated and aggregates are removed by sieving. The particles are mixed again and ready for reuse. In order to study the effectiveness of the process, no new powder has been added to the recovered fraction, and this procedure has been repeated five times. Experimental tests show that deposited material present similar properties than those obtained with new powder grains. But, after 3 reuses, the porosity content increases consequently and the rupture strain decreases strongly. The implementation of this process allows the improvement of the final efficiency, reducing costs and decreasing the hazardous powder amount.

36 MATERIALS SCIENCE↗

Effect of Ni content on the microstructure and mechanical properties of weld metal with both-side submerged arc welding technique

Highlights: • This manuscript primarily studied the effects of Ni content on the K65 weld metals; • Increase Ni content could significantly improve the strength and low temperature impact toughness of the weld metal. • The beneficial effect of Ni is attributed to its positive effect on phase transformation. • GBF keeps K-S or N-W relations only with one austenite and the variants belong to the same bain group are two reasons. • The M/A islands are considered to be another reason for the reduced toughness. - Abstract: The effects of nickel (Ni) content on the mechanical properties and microstructure evolution in the weld metals of commercial K65 oil and gas pipeline steel were studied. Increase Ni content could significantly improve the strength and low temperature impact toughness (−40 °C and −60 °C) of the weld metal. The above influences of Ni were attributed to the formation of predominant acicular ferrite (AF), at the expense of grain boundary ferrite (GBF), ferrite side plates (FSP) and martensite/austenite (M/A) constituent in weld metal. EBSD results indicated that GBF keeps K-S or N-W relations only with the prior austensite grain that belongs to one side of the grain boundary and the variants belong to the same bain group which always forms low angle boundary. Moreover, the retained austenite as one part of M/A constituent was mainly found in the weld metal with lower Ni content. It indicated that the transformation process could be promoted more completely by the increase of Ni content. The mechanism of the toughness improvement brought by Ni increasing was ascribed to the relatively uniform transformation to final microstructure, which reduces the appearance of GBF and M/A constituents.

36 MATERIALS SCIENCE↗

Effect of strain level on the evolution of microstructure in a recently developed AD730 nickel based superalloy during hot forging

Highlights: • Hot forging of AD730 led to formation of large non-recrystallized grains. • Similarity in chemical compositions of the non-recrystallized zones and the matrix. • Increase in strain level promoted recrystallization. - Abstract: Design and control of microstructure of engineering parts made from nickel based superalloys with superior mechanical properties for high temperature applications, require the parts to be subjected to certain thermo-mechanical processing during forging. This often includes sequential straining and annealing at elevated temperatures followed by subsequent aging heat treatments at lower temperatures. In this study, the effect of strain magnitude on the evolution of microstructure during hot forging of a recently developed AD730 nickel based superalloy has been investigated. Microstructural heterogeneity was observed in a forged material manifested in a form of large non-recrystallized grains within the recrystallized matrix that is observed to be dependent on the level of deformation (i.e. strain magnitude). Analyses of microstructure indicated significant reduction in the fraction of low-angle grain boundaries and sub-structures with an increase in the applied strain, suggesting higher fraction of recrystallization with higher levels of strains. It was concluded that the lower strain levels were insufficient to provide enough driving force for complete recrystallization throughout the entire microstructure of the forged material.

36 MATERIALS SCIENCE↗

Development of microstructure and texture during single and multiple pass friction stir processing of a strain hardenable aluminium alloy

Highlights: • Development of microstructure and texture during single and multiple pass FSP of a strain hardenable aluminium alloy • Strain induced boundary migration (SIBM) is the dominant nucleation mechanism for recrystallization • Weak crystallographic texture development influenced by SIBM with the relative dominance of shear texture components • Stable microstructure and texture development after multiple pass FSP • FSP is a promising method for the secondary processing of strain hardenable aluminium alloys - Abstract: In the present study, microstructure and texture development during single and multiple pass friction stir processing (FSP) of a strain hardenable wrought AlMg alloy (AA5086) was investigated. Subtle differences were observed while comparing with heat treatable alloys in the nucleation mechanism of the recrystallized microstructure observed in the nugget zone. Strain induced boundary migration was the dominant mechanism of microstructure evolution in the alloy, which influenced the crystallographic texture development by weakening it. Micro-texture measurements reveal variations in the crystallographic texture along the thickness of the sample. Recrystallization texture components were observed in the nugget zone indicative of a pronounced static recrystallization in the alloy as compared to the heat treatable alloys. Bulk texture measurements within the nugget zone of the optimally processed sample reveal a relatively dominant C component of shear texture. Average grain size in the nugget zone remained the same and the bulk crystallographic texture components were retained during multiple-pass FSP. The lower strain energies involved and the enhanced recovery processes due to the high temperature materials processing of the alloy during FSP resulted in a stable microstructure and texture. In summary, FSP could be promoted as a competent and suitable secondary processing technique for the bulk production of ultra-fine-grained materials in strain hardenable aluminium alloys.

36 MATERIALS SCIENCE↗

Effect of build geometry on the microstructural development of 316L parts produced by additive manufacturing

Highlights: • Stainless steel ribs were created via direct metal laser sintering to investigate microstructural effect of part design. • EBSD confirmed the presence of large elongated grains in the center of the part, with preferred orientation. • Small grains at the rib surface were found to grow towards the center of the rib with random orientation. • By changing rib thickness and build angle varying texture was observed in the final products. • Large intragranular misorientations were observed in all samples. - Abstract: Additive manufacturing (AM) technology has shown great potential in manufacturing complex products, such as lattice structures without extensive tooling. The focus of this study was to understand the effect of the part geometry on the resulting microstructure. Direct metal laser sintering was used for fabrication of ribs with thicknesses varying between 0.2 and 3.0 mm as well as inclined ribs the with build angles of 30° and 45°. The investigation showed that grains were growing in an epitaxial manner parallel to the building direction. The large elongated grains had a preferential orientation, resulting from the temperature gradient. Additionally, it was found that small grains had formed close to the part surface which were inclined towards the center of the rib. In contrast to the elongated grains, they had a random orientations. The results also indicated that at build angles below 45°, the formed microstructure consisted of the large grains elongated in the building direction. For the used process parameters, the critical part thickness to avoid large elongated grains was found to be about 0.4 mm. These findings allowed us to establish the basics for design rules when it comes to thin wall structures.

36 MATERIALS SCIENCE↗

Effect of filling materials on the microstructure and properties of hybrid laser welded Al-Mg-Si alloys joints

Highlights: • A serious comparison was made on the hybrid laser welded AA6061-T6 joint with different filling materials. • The microstructure of the welded joint was characterized using EBSD and SEM. • A strength model was successfully built to predict the strength of the hybrid laser welded AA6061-t6 joint. • The study shed new insights on how to select appropriate filling materials when using hybrid laser welding. - Abstract: A serious investigation was conducted to examine the influence of filling materials on the microstructure and properties of hybrid laser welded AA6061-T6 joints. The results of the tensile tests showed that the welded joint with ER4043 filling materials had higher tensile strength than that with ER5356 filling material. Based on the results obtained a strength model was built to predict and explain the enhancement of the yield strength of the hybrid laser welded AA6061-T6 joint with different welding wires. In contrast to the tensile strength, the ER4043 joint showed lower fatigue strength than that of the ER5356 joint due to extensive presence of micropores in fusion zone. Further, the corrosion experiment illustrated that the ER4043 joint had poorer resistance to the corrosive attack under 3.5% NaCl solution. A summary was made on the performance of both welded joints to shed new insights on selecting appropriate filling materials when welding AA6061-T6 by hybrid laser welding method.

36 MATERIALS SCIENCE↗

Densification, microstructure and properties of TiB2 ceramics fabricated by spark plasma sintering

Highlights: • Nearly full densification of in-house processed TiB{sub 2} ceramic powders at 1500 °C. • Microstructures revealing the size and shape of TiB{sub 2} grains after SPS. • The effect of sub-micron particles on the densification during SPS. • The effect of sintering pressure on the microstructure. • Microhardness and nano-indentation measurements along with oxidation studies. - Abstract: This study reports the fabrication of high-density TiB{sub 2} ceramics at reduced temperatures (1500 °C) by using field assisted sintering technology/spark plasma sintering (FAST/SPS) technique. In-house processed TiB{sub 2} powders with high purity were employed as starting materials. The effects of SPS conditions on the sintering behavior and microstructure of TiB{sub 2} were investigated. Sub-micron character of TiB{sub 2} particles has a strong influence on the densification during SPS. Microstructural analyses revealed that the high pressure affected both the grain size and the shape of TiB{sub 2} crystallites. Elongated grains with average size of 6 μm were perceived in TiB{sub 2} sample fabricated by SPS at 1500 °C under 60 MPa pressure with a relative density of 96.7%. The microhardness and elastic modulus were measured as 27.4 GPa and 685.2 GPa, respectively. This sample revealed an improved oxidation resistance due to the formation of a thin oxidation layer on the surface when heated up to 1200 °C.

36 MATERIALS SCIENCE↗

Thermo-mechanical processing window for β phase recrystallization inTi-5Al-5Mo-5V-3Cr alloy

Highlights: • A processing window has been developed to obtain fine uniform recrystallized grains. • High deformation (90%) with annealing at intermediate temperature (950 °C) suggested • Dynamic recrystallization (Drx) should be avoided. • DRx reduces driving force for static rx. It gives bimodal distribution of grains. • Final deformation step should be in the α + β phase field. Ti-5Al-5Mo-5V-3Cr (Ti-5553) is a high strength β titanium alloy. It is now commonly used in thick section aerospace components. In general, the thermo-mechanical processing (TMP) of β titanium alloys done at high temperature to obtain uniformly recrystallized fine grain structure is one of the major challenges. Through this work, a TMP window for Ti-5553 (through systematic variation in % reduction and post deformation annealing temperature) has been developed to obtain fine uniformly recrystallized β grains. Grain size has been quantified on EBSD generated orientation maps, by applying stereological methods, image processing and automated reconstruction. Effects of % deformation and post deformation annealing temperature, as well as that of initial ingot size prior to deformation and the capacity of the forge on the static and dynamic recrystallization behavior, which eventually determine the final grain size distribution, have been illustrated.

36 MATERIALS SCIENCE↗

Orientation and morphology of Pt nanoparticles in γ-alumina processed via ion implantation and thermal annealing

Structure and chemistry of metal/metal-oxide interfaces are critical for many catalytic processes and sensing. Pristine interfaces of Pt and γ-Al 2 O 3 were fabricated using high-energy ion implantation and thermal processing. Amorphous regions of alumina develop in single crystal α-alumina during Pt+ implantation and an 800 °C thermal treatment crystalizes amorphized alumina to γ-Al 2 O 3 and allows Pt ions to precipitate within the developing γ-alumina, yielding Pt nanoparticle tetrahedra terminated by {111} surfaces. The phase of alumina that developed and the distribution, morphology, and orientation of Pt nanoparticles was determined using x-ray diffraction, Rutherford backscattering spectrometry, transmission electron microscopy and scanning transmission electron microscopy.

36 MATERIALS SCIENCE↗