Microstructure and mechanical properties of V–4Ti–4Cr alloy as a function of the chemical heat treatment regimes

The regularities of the formation of a heterophase structure and mechanical properties of V–4Ti–4Cr alloy as a function of thermomechanical and chemical heat treatments are studied. The regimes of thermomechanical treatment which provide the formation of a heterophase structure with a homogeneous volume distribution of oxycarbonitride nanoparticles with a size of about 10 nm and an increase in the volume content and thermal stability of this phase and which provide an increase in the temperature of alloy recrystallization are developed. The formation of the heterophase structure results in a substantial (up to 70%) increase in the short-term high-temperature strength of the alloy at T = 800°C. The increase in the strength is achieved while keeping a rather high level of plasticity.

36 MATERIALS SCIENCE↗

Microstructure, texture, and mechanical properties of friction stir welded commercial brass alloy

Microstructural evolution during friction stir welding of single-phase brass and corresponding mechanical properties were investigated. For this purpose, 2 mm thick brass plate was friction stir welded at a rotational speed of 450 rpm and traverse speed of 100 mm/min. The microstructure of the joint was studied using optical microscopy, scanning electron microscopy equipped with electron back scattered diffraction system, and scanning transmission electron microscopy. The mechanical properties were measured using hardness and tensile tests. The formation of subgrains and their transformation into new grains in conjunction with existence of A{sub 1}{sup ⁎}, A{sub 2}{sup ⁎} and C texture components revealed that the continuous dynamic recrystallization plays a dominant role in the microstructural evolution. However, grain boundary bulging, along with the formation of twin boundaries, and presence of the G texture component showed that the discontinues dynamic recrystallization may participate in the new grain formation. Furthermore, the different strengthening mechanisms, which caused the higher strength of the joint, were discussed. - Highlights: •Microstructural evolution during FSW of a single phase brass was investigated. •CDRX and DDRX were the main mechanisms of the grain structure formation during FSW. •GDRX and SRX were not contributed in grain structure formation. •The lamellas TBs were formed in the SZ of the joints. •Grain boundary, dislocation, and texture effects resulted in higher strength.

36 MATERIALS SCIENCE↗

Effect of rare-earth composition on microstructure and pinning properties of Zr-doped (Gd, Y)Ba{sub 2}Cu{sub 3}O{subx} superconducting tapes.

The effect of changing Gd + Y content from 1.2 to 1.6 in the precursor of (Gd,Y)Ba{sub 2}Cu{sub 3}O{sub 7} superconducting thin film tapes made by metal organic chemical vapor deposition (MOCVD) at a constant Gd:Y ratio and a fixed Zr content of 7.5% has been studied. The influence of changing the Gd:Y ratio from Gd = 0 to Y= 0 in 0.2 mol steps at a constant Gd + Y content of 1.2 in the precursor has also been investigated at a fixed Zr content of 7.5%. The critical current of these films is found to vary significantly as a function of rare-earth content as well as a function of rare-earth type. Even for a fixed Zr content, it is found that the critical current in the orientation of magnetic field parallel to the a-b plane and that in the orientation of field perpendicular to the a-b plane can be systematically varied with changing Gd + Y content as well as with changing Gd:Y ratio. The nanoscale defect structures along the a-b plane and along the c-axis are found to be sensitive to these changes in rare-earth content and type.

36 MATERIALS SCIENCE↗

Reel-to-Reel Heat Treatment, Microstructure, and Superconducting Properties of Jelly-Roll Nb{sub 3}Al Superconducting Wire

In this work, we utilized the jelly-roll method to make a single-filament Nb{sub 3}Al precursor long wire, combining with a homemade reel-to-reel rapid heating and quenching (RHQ) equipment, and consequently the high-performance Nb{sub 3}Al superconducting wires had been prepared. By investigating the heating current and wire moving speed, the optimized RHQ heat treatment conditions of this Nb{sub 3}Al wire were obtained. The results suggest that the T{sub c} for the Nb{sub 3}Al superconducting wire is up to 17.4 K and the non-Cu critical current density (non-Cu J{sub c}) reaches 1238 A/mm{sup 2} at 4.2 K and 12 T, which indicates the bcc-phase Nb–Al supersaturated solid solution has already been generated. Considering the Nb{sub 3}Al precursor wire with a large thickness of Al layer, about 690 nm, such high J{sub c} is quite unexpected. The SEM analysis presents that there is still some unreacted Nb and Nb{sub 2}Al phase in the superconducting wire, which may result from the inhomogeneity of Nb and Al foils. This work implies the Nb{sub 3}Al superconducting wire is promising to the application of high-field superconducting magnets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructural and photocatatlytic properties of Eu-doped mesporous titanium dioxide nanopaticles by sol–gel method

Highlights: ► Eu-doped TiO{sub 2} was prepared using sol–gel method in the presence of pluronic P123. ► Eu atoms were doped into the lattice of anatase TiO{sub 2}. ► Eu doping can increase the band gap of TiO{sub 2}. ► Eu-doped TiO{sub 2} exhibited much higher photocatalytic activity than undoped TiO{sub 2}. -- Abstract: The europium-doped mesoporous titanium dioxide nanoparticles (Eu-doped TiO{sub 2}) with the different Eu/Ti rations were prepared using sol–gel method in the presence of tir-block copolymer pluronic P123. The as-prepared catalysts were characterized by low-angle and wide-angle X-ray diffraction (XRD), high resolution transmission electron microscopy (HRTEM), N{sub 2} absorption–desorption, ultraviolet visible light spectroscopy (UV–vis) and X-ray photoelectron spectroscopy (XPS), respectively. The XRD analysis indicated that all as-prepared TiO{sub 2} samples were mainly anatase phase and mesoporous. The crystallite sizes were in the range 6–11 nm, in consistent with the results obtained form TEM images. HRTEM and XPS showed that the europium atoms were doped into the lattice of anatase TiO{sub 2}. Eu doping can not only increase the stability of mesoporous TiO{sub 2}, but also make the absorption edge position move toward shorter wavelength. The photodecomposition experiments showed that the photodegradation activity of Eu-doped TiO{sub 2} was higher than that of undoped TiO{sub 2}.

36 MATERIALS SCIENCE↗

Influencing mechanism of Al-containing Zn coating on interfacial microstructure and mechanical properties of friction stir spot welded Mg–steel joint

Highlights: • Al-containing Zn coating improved Mg–steel interfacial wettability during friction stir spot welding (FSSW). • Pre-existing Al{sub 5}Fe{sub 2} phase in coating on steel surface promoted Mg–steel metallurgical bonding. • A high tensile-shear load of 4.3 kN was obtained in FSSW AZ31–steel joint. - Abstract: 2.4 mm thick AZ31 Mg alloy sheet and 1.5 mm Q234 steel sheet with a hot-dipped Al-containing Zn coating were friction stir spot welded (FSSW) using a pinless tool. It was shown that the Al-containing Zn coating played a crucial role in joining the Mg alloy and steel during FSSW. The Zn coating observably improved the Mg–steel interfacial wettability during FSSW, and the Al{sub 5}Fe{sub 2} phase in the Zn coating on the steel substrate surface promoted the metallurgical bonding of Mg alloy and steel. It was confirmed that the Al{sub 5}Fe{sub 2} phase on the steel surface resulted from the reaction between the steel substrate and the Al in the Zn coating during hot-dipping, and was not related to the Al-containing Mg alloy substrate. The tensile-shear load of the FSSW Mg–steel joint reached 4.3 kN. The fracture of the joint occurred along the interface on the steel substrate side. The interface between the Al{sub 5}Fe{sub 2} layer and Mg alloy substrate was the weakest region of the Mg–steel joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Mechanical properties, deformation behavior and microstructure evolution of Ti-43Al-6Nb-1Mo-1Cr alloys

Highlights: • The alloys exhibit excellent high-temperature tensile properties. • Activation energy of deformation (Q) and n are 571 KJ/mol and 2.765, respectively. • The hot processing maps of strain 0.5 and 0.6 are displayed. • Phase transformations and microstructure evolution are explained in different conditions. • Three types of deformation mechanisms are exhibited at different temperature. - Abstract: The high-temperature properties, microstructure evolution and deformation behavior of a novel Ti-43Al-6Nb-1Mo-1Cr(at.%) alloy were studied in this paper. The ultimate tensile strength (UTS) and elongation (δ) were tested at 800, 850, and 900 °C, in which the excellent strength 551 MPa, 510 MPa, and 382 MPa, and elongation 2.9%, 12.7%, and 16.8% were exhibited, respectively. Isothermal compression tests were carried out in the temperature range of 1100–1250 °C and strain rate range of 0.001–1.0 s{sup − 1}. Based on dynamic materials model (DMM) and phase diagram, dynamic recrystallization mechanism and phase transformation during thermal deformation were clarified and the hot processing maps were calculated. The experimental results show that the values of stress exponent (n) and the apparent deformation activation energy (Q) of Ti-43Al-6Nb-1Mo-1Cr(at.%) were calculated to be 2.77 and 571 KJ/mol. Meanwhile, three various types of microstructure evolution in different deformation conditions were discussed and concluded.

36 MATERIALS SCIENCE↗

Influence of halide flux on the crystallinity, microstructure and thermoluminescence properties of CdSiO{sub 3}:Co{sup 2+} nanophosphor

Graphical abstract: TL glow curves of CdSiO{sub 3}:Co{sup 2+} different alkali flux (inset without adding flux). Display Omitted Highlights: ► CdSiO{sub 3}:Co{sup 2+} (1–7 mol%) nanocrystalline phosphors synthesized by combustion route. ► Flux effect on thermoluminescence behavior of CdSiO{sub 3}:Co{sup 2+} reported for first time. ► Addition of 2 wt% of flux would drastically enhance the TL properties. ► Well resolved single glow peak at ∼170 °C was recorded for all the samples. ► Among all the alkali flux, NaCl shows highest TL peak intensity. -- Abstract: CdSiO{sub 3}:Co{sup 2+} (1–7 mol %) nanophosphors have been prepared via solution combustion method with post calcination at 800 °C for 2 h for the first time. The formation of expected monoclinic phase was investigated by Powder X-ray diffraction (PXRD) measurements. The effect of different fluxes like NaF, NaCl, NH{sub 4}F and NH{sub 4}Cl on the crystallinity, phase and morphology of CdSiO{sub 3} was investigated in detail. The crystallinity of the samples can be greatly enhanced by using fluxes rather than increasing the calcination temperature. Scanning electronic micrograph (SEM) image shows that the powder morphologies are highly influenced by flux addition. The addition of 2 wt% of fluxes would drastically enhance the crystallinity when NaCl, NH{sub 4}F and NH{sub 4}Cl fluxes are used. A well resolved single thermoluminescent glow peak at ∼170 °C was recorded for all the samples. Among all the halide fluxes, NaCl flux was found to be the potential one in enhancing the TL peak intensity along with crystallinity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructure and Mechanical Properties of Friction Stir Process Derived Al-TiO{sub 2} Nanocomposite

Aluminum-based composites have many advantages over their conventional counterparts. A major problem in such composites is the clustering of particles in the matrix. Friction stir processing (FSP) can homogenize particle distribution in aluminum-based composites. In this study, unannealed TiO{sub 2} particles were used to prepare Al-TiO{sub 2} nanocomposite using FSP. The TiO{sub 2} particles, about 1 µm, were dispersed into an aluminum matrix by 6 passes of FSP. The TiO{sub 2} particles were fractured by multiple FSP passes, leading to a nano-size particle distribution in the matrix. Nanoscale dispersion was confirmed by scanning electron microscopy and transmission electron microscopy. The fractured TiO{sub 2} particles reacted with the aluminum matrix to form Al{sub 3}Ti intermetallic and Al{sub 2}O{sub 3} ceramic. The progression of the Al-TiO{sub 2} reaction from the fourth to the sixth pass of FSP was revealed by x-ray diffraction. Due to the nanoscale dispersion, the yield and ultimate tensile strength of the composite increased to 97 and 145 MPa, respectively. Ductility of the composite decreased marginally compared to the as-received aluminum. As the dispersed particles pin dislocations, the strain-hardening rate of the composite was considerably increased and the same was seen in the Kocks-Mecking plot. The TiO{sub 2} particles are mechanically activated due to their fracture during FSP, hence leading to reaction with the matrix. The particle refinement and dispersion lead to a homogeneous matrix with higher strength.

36 MATERIALS SCIENCE↗

Selective laser melting of 304L stainless steel: Role of volumetric energy density on the microstructure, texture and mechanical properties

The role of volumetric energy density on the microstructural evolution, texture and mechanical properties of 304L stainless steel parts additively manufactured via selective laser melting process is investigated. 304L is chosen because it is a potential candidate to be used as a matrix in a metal matrix composite with nanoparticles dispersion for energy and high temperature applications. The highest relative density of 99 %±0.5 was achieved using a volumetric energy density of 1400 J/mm 3 . Both XRD analysis and Scheil simulation revealed the presence of a small trace of the delta ferrite phase, due to rapid solidification within the austenitic matrix of 304L. Here, a fine cellular substructure ranged between 0.4–1.8 μm, was detected across different energy density values. At the highest energy density value, a strong texture in the direction of [100] was identified. At lower energy density values, multicomponent texture was found due to high nucleation rate and the existing defects. Yield strength, ultimate tensile strength, and microhardness of samples with a relative density of 99 % were measured to be 540 ± 15 MPa, 660 ± 20 MPa and 254 ± 7 HV, respectively and higher than mechanical properties of conventionally manufactured 304L stainless steel. Heat treatment of the laser melted 304L at 1200 °C for 2 h, resulted in the nucleation of recrystallized equiaxed grains followed by a decrease in microhardness value from 233 ± 3 HV to 208 ± 8 HV due to disappearance of cellular substructure.

304L stainless steel↗

Microstructure and mechanical properties of intragranular W-Cu/TiC-ZrC composite prepared by reactive melt infiltration at 1300 °C

Highlights: • W-Cu/TiC-ZrC composites with nano W dispersoids were prepared by reactive melt infiltration. • The nano-sized dispersoids were analyzed by TEM in detail. • The intragranular nano W dispersoids and ribbon like precipitates have toughening effects. - Abstract: Newly intragranular W-Cu/TiC-ZrC composites with nano W dispersoids in TiC matrix have been prepared by reactive melt infiltration at 1300 °C for 1 h in vacuum using molten Zr-Cu binary alloys and a (Ti{sub 0.75},W{sub 0.25})C solid solution powder as raw materials. The as-synthesized composites consist of major phases of W, Cu, TiC and ZrC. With the decrease of Zr content from 66 to 21 at.% in the Zr-Cu infiltrator, the reaction formed W phase in the composite has changed from micron-sized intergranular grains to nano-sized rounded inclusions in TiC{sub y} grains. The crystallographic orientation relationship at W and TiC interfaces are detected as:(0 1 1-bar ){sub W}//(1 1 1-bar ){sub TiC}&[0 1 1]{sub W}//[0 1 1]{sub TiC} and (4 1 1){sub W}//(4 2 4){sub TiC}&[0 1 1-bar ]{sub W}//[4 2-bar 3-bar ]{sub TiC}. Nano-sized lamellar structure with both W and Cu rich is detected to have super-lattice structure based on the TiC lattice. The elastic modulus, flexural strength, fracture toughness of the intragranular W-Cu/TiC-ZrC composite infiltrated with Zr{sub 14}Cu{sub 51} melt are 207.5 GPa, 457 MPa and 10.21 MPa∙m{sup 1/2}, respectively. The intragranular nano W dispersoids and ribbon like precipitates hinder crack propagation via crack deflection and bridging.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

PROCESSING, MICROSTRUCTURE AND MECHANICAL PROPERTY CORRELATION IN Al-B4C SURFACE COMPOSITE PRODUCED VIA FRICTION STIR PROCESSING

Friction stir processing (FSP) was employed to prepare surface composites (SC) composed of B4C particles in 5024 Al matrix. The processing parameters, such as hole pattern and geometry,and the number of FSP passes, were optimized to obtain uniform powder distribution. The micrographs revealed a homogeneous distribution of the particles with good interfacial bonding. The hardness of the composite was uniform across the processed region which again indicates the uniformity of powder distribution. The modulus of the surface composite was measured using strain gage and showed a significant improvement. This improvement in modulus lies in the load sharing capability from the soft matrix to the hard particles.

Aluminum MMC,↗

Effect of solvent/polymer infiltration and irradiation on microstructure and tensile properties of carbon nanotube yarns

Recently carbon nanotube (CNT) yarns have been gaining importance as an approach to harvest the excellent properties of the CNTs. However, the properties of CNT yarns at this stage are well below the expected value. Investigation of the structure of CNT yarns and possible approaches to enhance the strength and modulus are reported. Scanning electron microscopy and focused ion beam imaging reveal the inherently porous structure and poor orientation, emphasizing the need to enhance packing of CNT bundles in the yarns for increased strength and modulus. Densification of CNT yarn by toluene or polystyrene increases the strength by 140 or 172 % and modulus by 79 or 218 %, respectively, as compared to that of the pristine yarn. E-beam irradiation was investigated as a means to introduce crosslinking and enhanced internanotubes bonding to increase strength and modulus. However, the irradiation resulted in generation of defects and damages to the yarn contributing to reduction in strength and modulus. Raman spectroscopy studies on the irradiated samples reveal the change in bonding characteristics resulting in poor mechanical properties. As a result, denser packing of nanotubes and increased interaction without any damage is the key to improve the properties of CNT yarns.

36 MATERIALS SCIENCE↗

Advanced Process Possibilities in Friction Crush Welding of Aluminum, Steel, and Copper by Using an Additional Wire

Joining sheet metal can be problematic using traditional friction welding techniques. Friction crush welding (FCW) offers a high speed process which requires a simple edge preparation and can be applied to out-of-plane geometries. In this work, an implementation of FCW was employed using an additional wire to weld sheets of EN AW5754 H22, DC01, and Cu-DHP. The joint is formed by bringing together two sheet metal parts, introducing a wire into the weld zone and employing a rotating disk which is subject to an external force. The requirements of the welding preparation and the fundamental process variables are shown. Thermal measurements were taken which give evidence about the maximum temperature in the welding center and the temperature in the periphery of the sheet metals being joined. The high welding speed along with a relatively low heat input results in a minimal distortion of the sheet metal and marginal metallurgical changes in the parent material. In the steel specimens, this FCW implementation produces a fine grain microstructure, enhancing mechanical properties in the region of the weld. Aluminum and copper produced mean bond strengths of 77 and 69 pct to that of the parent material, respectively, whilst the steel demonstrated a strength of 98 pct. Using a wire offers the opportunity to use a higher-alloyed additional material and to precisely adjust the additional material volume appropriate for a given material alignment and thickness.

36 MATERIALS SCIENCE↗