Structural, thermodynamic, mechanical, and magnetic properties of FeW system

The Fe-W system is systematically investigated through a combined use of first-principles calculation, cluster expansion, special quasirandom structures, and experiments. It is revealed that the ferromagnetic state of BCC Fe-W solid solution has lower heat of formation than its nonmagnetic state within the entire composition range, and intermetallic λ-Fe{sub 2}W and μ-Fe{sub 7}W{sub 6} phases are energetically favorable with negative heats of formation. Calculations also show that the Fe-W solid solution has much lower coefficient of thermal expansion than its mechanical mixture, and that the descending sequence of temperature-dependent elastic moduli of each Fe-W solid solution is E > G > B. Moreover, magnetic state should have an important effect on mechanical properties of Fe-W phases, and electronic structures can provide a deeper understanding of various properties of Fe-W. The derived results agree well with experimental observations, and can clarify two experimental controversies regarding structural stability and magnetic property of Fe-W phases in the literature.

36 MATERIALS SCIENCE↗

Precipitation mechanism and mechanical properties of an ultra-high strength steel hardened by nanoscale NiAl and Cu particles

We report on the alloy design strategies, precipitation mechanism and mechanical properties of an ultra-high strength steel hardened by co-precipitation of nanoscale NiAl and Cu particles. The steel, developed through a computational-aided alloy design approach, exhibits a tensile strength of ~1.9 GPa, an elongation of ~ 10% and a reduction in area of ~ 40%. Atom probe tomography (APT) reveals an interesting type of co-precipitation mechanism of NiAl and Cu nanoparticles, in which the NiAl particles first come out of the supersaturated solid solution and the rejection of Cu solutes leads to the heterogeneous precipitation of Cu particles adjacent to the NiAl particles. The observed precipitation sequence of "supersaturated solid solution → NiAl → NiAl + Cu" is substantially different from the one previously reported in Cu-strengthened steels, which involves the process of "supersaturated solid solution → Cu → Cu + NiAl". The modulation of the precipitation sequence is attributed not only to the relatively high Ni/Cu and Al/Cu ratios but also the synergistic combination of Ni, Al, Mn and Cu additions in the steel. In addition, APT also reveals the precipitation of a small amount of nanoscale Fe 3 (Mo, W) 3 C-and NbC-type carbides. Lastly, the combination of the strengthening effects from the nanoscale NiAl particles, Cu particles and carbides contributes significantly to the overall ultra-high strength of the steel.

36 MATERIALS SCIENCE↗

Non-random cation distribution in hexagonal Al{sub 0.5}Ga{sub 0.5}PO{sub 4}

Based on powder X-ray diffraction and {sup 31}P Magic Angle Spinning Nuclear Magnetic Resonance (MAS NMR) investigations of mixed phosphate Al{sub 0.5}Ga{sub 0.5}PO{sub 4}, prepared by co-precipitation method followed by annealing at 900 deg. C for 24 h, it is shown that Al{sub 0.5}Ga{sub 0.5}PO{sub 4} phase crystallizes in hexagonal form with lattice parameter a=0.491(2) and c=1.106(4) nm. This hexagonal phase of Al{sub 0.5}Ga{sub 0.5}PO{sub 4} is similar to that of pure GaPO{sub 4}. The {sup 31}P MAS NMR spectrum of the mixed phosphate sample consists of five peaks with systematic variation of their chemical shift values and is arising due to existence of P structural units having varying number of the Al{sup 3+}/Ga{sup 3+} cations as the next nearest neighbors in the solid solution. Based on the intensity analysis of the component NMR spectra of Al{sub 0.5}Ga{sub 0.5}PO{sub 4}, it is inferred that the distribution of Al{sup 3+} and Ga{sup 3+} cations is non-random for the hexagonal Al{sub 0.5}Ga{sub 0.5}PO{sub 4} sample although XRD patterns showed a well-defined solid solution formation. - Graphical abstract: {sup 31}P MAS NMR pattern of hexagonal Al{sub 0.5}Ga{sub 0.5}PO{sub 4} solid solution.

36 MATERIALS SCIENCE↗

A General Strategy for Bandgap Engineering Via Anion‐Lattice Doping in High‐Entropy Oxides

Bandgap engineering is a critical tool for tailoring the electronic properties of functional materials, traditionally achieved by modifying the cation sublattice. Here, a generalizable strategy is introduced that leverages facile anion-lattice doping in high entropy materials to modulate the bandgap in high-entropy metal oxides (HEMOs). By incorporating nitrogen into a single-phase high-entropy metal oxide/nitride (HEMO:HEMN) solid solution, a substantial bandgap reduction is achieved from 3.55 eV (HEMO) to ≈2.46 eV (HEMO:HEMN), significantly enhancing electronic conductivity. Unlike conventional bandgap tuning approaches that rely on cation substitution or heterojunction formation, this method exploits anion-mediated entropy stabilization, enabling uniform bandgap narrowing across the entire solid solution. This anion-lattice engineering strategy is broadly applicable to high-entropy systems, providing a new pathway for designing energy materials with tailored electronic properties. The resulting HEMO:HEMN solid solution exhibits a tenfold increase in capacitance and capacity compared to HEMO in supercapacitor and lithium-ion battery tests, demonstrating the transformative potential of anion-driven bandgap modulation for next-generation energy storage and conversion technologies.

energy storage↗

Crystal structure and magnetic properties of titanium-based CuTi{sub 2−x}M{sub x}S{sub 4} and CuCr{sub 2−x}Ti{sub x}Se{sub 4} chalcospinels

CuTi{sub 2−x}M{sub x}S{sub 4} (M=Fe, Mn, Co; x=0.3, 0.5) and CuCr{sub 2−x}Ti{sub x}Se{sub 4} (x=0.3, 0.5, 0.7) chalcospinels were synthesized by conventional solid-state reactions. Their crystal structures were determined by single-crystal X-ray diffraction. All of the phases crystallized in cubic spinel-type structures (space group, Fd3{sup ¯}m). For all of the chalcospinel compounds, the edge-length distortion parameter (ELD) indicated that the most distorted polyhedron was Q[(Ti,M){sub 3}Cu], which displayed an ∼8% distortion from an ideal tetrahedron structure (Q=S or Se). The Mn-based thiospinel CuMn{sub 0.3}Ti{sub 1.7}S{sub 4} is paramagnetic, whereas the Fe-based thiospinels (CuTi{sub 2−x}Fe{sub x}S{sub 4}; x=0.3 and 0.7) are strongly antiferromagnetic due to their spin-glass states. The magnetic susceptibility measurements indicated ferromagnetic behavior for the selenospinels (CuCr{sub 2−x}Ti{sub x}Se{sub 4}; x=0.3, 0.5 and 0.7). - Graphical abstract: View along [1 0 0] of CuCr{sub 2−x}Ti{sub x}Se{sub 4} crystal structure showing tetrahedral and octahedral units. To the right, experimental X-ray powder diffraction pattern of CuCr{sub 1.7}Ti{sub 0.3}Se{sub 4} (top) in compared (in a like-mirror representation) to a simulated X-ray pattern from single-crystal data (bottom). - Highlights: • Chalcogenides belong to the family of compounds spinel-type. • Resolved single crystals of the solid solutions have space group Fd-3m. • The distortion of the tetrahedral and octahedral volume were calculated. • These solid solutions shows a ferromagnetic or spin-glass behavior.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Significantly enhanced ferroelectricity and magnetic properties in (Sr{sub 0.5}Ca{sub 0.5})TiO{sub 3}-modified BiFeO{sub 3} ceramics

BiFeO{sub 3} multiferroic ceramics were modified by introducing (Sr{sub 0.5}Ca{sub 0.5})TiO{sub 3} to form solid solutions. The single phase structure was easy to be obtained in Bi{sub 1−x}(Sr{sub 0.5}Ca{sub 0.5}){sub x}Fe{sub 1−x}Ti{sub x}O{sub 3} (x = 0.2, 0.25, 0.3, and 0.4) solid solutions. Rietveld refinement of X-ray diffraction data revealed a transition from rhombohedral R3c (x = 0.2, 0.25, and 0.3) to orthorhombic Pnma (x = 0.4). Current density-field (J-E) characteristics indicated that the leakage current density was reduced by three orders of magnitude in Bi{sub 1−x}(Sr{sub 0.5}Ca{sub 0.5}){sub x}Fe{sub 1−x}Ti{sub x}O{sub 3} ceramics. Both the ferroelectricity and magnetic properties were significantly enhanced in the present solid solutions. P-E hysteresis loop measurements with dynamic leakage current compensation methods showed the significantly enhanced ferroelectric properties for x = 0.25 and 0.3 and the paraelectric behavior for x = 0.4. The best ferromagnetic characteristics were achieved in the composition of x = 0.25, where the saturated M-H loop was determined with M{sub r} = 34.8 emu/mol. The improvement of ferroelectricity was mainly due to the suppressed leakage current, and the enhanced magnetism originated from the partial substitution of Fe{sup 3+} by Ti{sup 4+}, which destroyed its previous spiral structure to allow the appearance of a macroscopic magnetization.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and texture evolution of AZ31 alloy containing trace levels of strontium

The effect of low levels of Sr (0.01, 0.03, 0.05 wt.%) on the microstructure, mechanical properties and texture of AZ31 magnesium alloy has been investigated. Thermodynamic modeling has been used to study the effect of Sr on phase precipitation at different temperatures. Cooling curve analysis reveals a decrease in solidification superheat with the addition of 0.03 wt.% Sr to AZ31. The as-cast microstructures of the alloys have been studied using optical microscopy (OM) and electron probe micro analysis (EPMA). Results show the refining effect of Sr on the grain size and on the {beta}-Mg{sub 17}Al{sub 12} precipitates through growth poisoning and inoculation, respectively. To investigate the mechanical properties of the alloys, as-cast samples were compression tested at elevated temperatures. Hot compression peak stress ({sigma}{sub max}) and critical strain before recrystallization ({epsilon}{sub c}) initially drop but then increase. {sigma}{sub max} first decreases due to the depletion of Al from solid solution and then increases when the amount of the Al-Sr precipitates reach a significant amount. {epsilon}{sub c} drops due to the acceleration of dynamic recrystallization kinetics as a result of grain refinement. It increases with increasing Sr when the concentration Sr in solid solution is increased leading to dislocation pinning and retardation of recrystallization. X-ray texture measurements on the hot compressed and extruded samples show a decrease in maximum intensity of the basal pole figures with increasing Sr as a result of reduced twining and the changes in Al and Sr concentrations in solid solution. - Research Highlights: {yields} Microstructures/precipitates of AZ31+trace levels of Sr were examined by OM and EPMA. {yields} Thermodynamic calculations and cooling curve analysis were used to predict ppt formation. {yields} It has been shown that Sr refines the grains and Mg17Al12 precipitates. {yields} Mechanical properties and texture were studied using hot compression and X-ray diffraction. {yields} Different micro-mechanisms were responsible for mechanical and texture changes.

36 MATERIALS SCIENCE↗

Phase configuration, nanostructure evolution, and mechanical properties of unbalanced magnetron-sputtered Ti-C{sub x}-N{sub y} thin films

Ti-C{sub x}-N{sub y} thin films with different amounts of C incorporated into TiN{sub 0.87} were deposited on Si(100) substrates at 500 deg. C by reactive unbalanced dc magnetron sputtering. Their phase configuration, nanostructure, and mechanical behavior were investigated by x-ray diffraction (XRD), x-ray photoelectron spectroscopy (XPS), high-resolution transmission electron microscopy (HRTEM), and microindentation measurements. The results indicated that the atomic ratio of (C+N)/Ti played a crucial role in phase configuration, nanostructure evolution, and mechanical behavior. When the ratio was less than one, a nanocrystalline (nc-) Ti(C,N) solid solution was formed by dissolution of C into the TiN lattice. Both microhardness and residual compressive stress values increased with an increase of C content. When the C reached saturation, precipitation of small amounts of sp{sup 2} amorphous (a-) phase appeared with more C incorporation. Further increase of C content (up to {approx}19 at. % C) made the amorphous phase fully wet nanocrystallites, which resulted in the formation of nanocomposite thin films of {approx}5 nm nc-Ti(C,N) nanocrystallites separated by an {approx}0.5 nm amorphous phase comprised mainly of sp{sup 2} disordered C, graphite, and minor CN{sub x}. Thicker amorphous matrices and smaller sized grains followed when C content was further increased. The formation of nanocomposite structure greatly decreased both hardness and residual stress values of thin films. A hardness maximum was believed to be obtained at nc-Ti(C,N) solid solution containing the maximum C amount. Enhancement of the hardness value was attributed to solid solution effect and high residual stress value.

36 MATERIALS SCIENCE↗

Heteroepitaxial growth of cadmium carbonate at dolomite and calcite surfaces: Mechanisms and rates

Here, the systematic variation of rates and the mechanism of cadmium uptake on the (104) surface of dolomite (CaMg(CO 3 ) 2 ) were investigated using in situ and ex situ atomic force microscopy (AFM), ex situ specular X-ray reflectivity (XR), and ex situ X-ray fluorescence (XRF). Selected experiments were performed on the calcite (CaCO 3 ) (104) surface for comparison. Aqueous solutions of CdCl 2 , CaCl 2 , and NaHCO 3 , undersaturated with respect to calcite and supersaturated with respect to otavite (CdCO 3 ) and the (Cd x Ca 1-x )CO 3 solid solution, were reacted with dolomite surfaces for minutes to days. Calcite substrates were reacted with solutions containing 1-50 μM CdCl 2 , and with no added Ca or CO 3 . Thin carbonate films following the Stranski-Krastanov growth mode were observed on both substrates. Specular XR and XRF revealed the formation of nm-thick Cd-rich carbonate films that were structurally ordered with respect to the dolomite (104) plane. Epitaxial films adopted the calcite crystal structure with a d 104 - spacing (3.00 Å) larger than those of pure dolomite (2.88 Å) and otavite (2.95 Å) indicating either a solid solution with x approximate to 0.5, or a strained Cd-rich carbonate with a composition near that of otavite. The growth rate r of this phase increases with the initial supersaturation of the solution with respect to the solid solution, beta max, and follows the empirical relationship, as determined from XRF measurements, given by: r = 10 -4.88 ± 0.42 (β 2.29 ± 0.24 max - 1), (in units of atoms of Cd/Å 2 /h).The morphology of the overgrowth also varied with β max , as exemplified by AFM observations. Growth at step edges occurred over the entire β max range considered, and additional growth features including 3 Å high monolayer islands and ~ 25 Å high tall islands were observed when log β max > 1. On calcite, in situ XR indicated that this phase is similar to the Cd-rich overgrowth formed on dolomite and images obtained from X-ray reflection interface microscopy (XRIM) reveal the existence of laterally variable Cd-rich domains.

58 GEOSCIENCES↗

Development of a mechanistic thermal aging model for Grade 91

This report provides a summary on understanding and predicting the effects of long-term thermal aging on microstructure and tensile properties of G91 to corroborate the ASME Code rules in strength reduction due to elevated temperature service. The research is to support the design and long-term operation of G91 structural components in sodium-cooled fast reactors (SFRs). The report is a Level 2 deliverable in FY18 (M2NT-18AN050502061), under the Work Package NT-18AN05050206, “G91 Code Extension Testing” performed by the Argonne National Laboratory (ANL), as part of the Advanced Materials Development Program for Fast Reactors. The thermal aging study of G91 involves three types of thermally-aged specimens: (1) specimens machined from two heats of G91, G91-H1 and H30176 that have been tested for the Advanced Materials Development Programs in the past years. These specimens were aged at 550, 600, and 650°C for times up to ~64,000 h; (2) specimens fabricated from the heads of the archived crept specimens (13 in total) of six heats of G91, H5349, H30394, H30383, H10148, H30176. These specimens were aged at 427 - 538°C and for times up to 132,647 h; (3) specimens made from a tube removed from the Kingston coal-fired power plant after exposure for 155,000 h at 550°C. These three sets of specimens provide a comprehensive data set for understanding and predicting the effect of long-term thermal aging on microstructure and tensile properties of G91. Microstructural analysis of the thermally-aged G91 revealed that thermal aging causes significant microstructural changes: (1) the tempered martensite formed during tempering is unstable, and suffers significant recovery during aging, manifested by an increase in subgrain width, a decrease in subgrain length, and a decrease in subgrain aspect ratio (i.e. subgrains become more equiaxed) as the aging temperature and time increase. The subgrain recovery is facilitated by the reduction of dislocation density within subgrains; (2) M23C6 carbides in the as-received G91 are distributed along grain and subgrain boundaries and play an important role as pinning obstacles against subgrain coarsening. M23C6 carbides coarsen during aging, and the coarsening of M23C6 carbides reduces the pinning force on the boundaries; (3) MX carbonitrides in the as-received G91 are distributed uniformly within subgrains, providing the precipitation hardening effect. They coarsen with increasing aging temperature and time, but the coarsening rate is low; (3) a new phase, the Laves phase intermetallic forms during aging. The formation of the Laves phase removes the Mo solutes from the matrix, reducing the solid solution strengthening effect. The Laves phase particles grow rapidly once they are nucleated, and they precipitate primarily along boundaries. They may have a pinning effect on boundaries, but should provide little to the alloy strength. The evolution of each microstructural constituent during thermal aging can be well described by individual microstructural models. The estimated activation energy for MX coarsening was 175 kJ/mol, equivalent to the activation energy for boundary and core diffusion in a-Fe, while the estimated activation energy for subgrain coarsening was significantly lower, ~96 kJ/mol. Thermal aging of G91 results in the reduction in the yield stress and the ultimate tensile strength but has an insignificant effect on the uniform and total elongations. The reduction in tensile strength is more pronounced as the aging temperature and time increases. The in situ tensile tests with high-energy X-rays revealed that sub-boundary strengthening plays a dominant role, and the strengthening role of M23C6 particles may be accounted for by subgrian boundary hardening, and three strengthening mechanisms can be superimposed to describe the tensile strength of G91: subgrain boundary hardening, MX precipitation hardening, and Mo solid solution strengthening. A microstructure – strength model was establ

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effect of Cold Deformation and Heat Treatment on the Microstructure and Mechanical Behavior of High Entropy Alloy CuCrFeNi{sub 2}Al{sub 0.5}

CuCrFeNi{sub 2}Al{sub 0.5}, a high entropy alloy (HEA) with a single FCC phase, was deformed at room temperature and then heat treated. The small particles precipitated from the deformed FCC solid solution matrix after heating at 700 °C, softening the solid solution matrix. This outcome confirms that the microstructure of HEAs can be controlled by heat treatment in addition to controlling the chemical composition and the rate of cooling from liquid alloys. The hardness of the samples increased due to precipitation hardening, and the specimen heated at 700 °C with 10% predeformation had the highest hardness. As the predeformation increases, the precipitates tend to interweave in the network morphology. Meanwhile, grains in all specimens became more severely coarse after heat treatment at 1100 °C. Predeformation followed by annealing can obviously slow down the creep rate, indicating that annealing at an appropriate temperature can improve the mechanical properties of deformed HEA.

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Disorder in M n+1 AX n phases at the atomic scale

Atomic disordering in materials alters their physical and chemical properties and can subsequently affect their performance. In complex ceramic materials, it is a challenge to understand the nature of structural disordering, due to the difficulty of direct, atomic-scale experimental observations. Here we report the direct imaging of ion irradiation-induced antisite defects in M n+1 AX n phases using double CS-corrected scanning transmission electron microscopy and provide compelling evidence of order-to-disorder phase transformations, overturning the conventional view that irradiation causes phase decomposition to binary fcc-structured M n+1 AX n . With the formation of uniformly distributed cation antisite defects and the rearrangement of X anions, disordered solid solution γ-(M n+1 A)X n phases are formed at low ion fluences, followed by gradual transitions to solid solution fcc-structured (M n+1 A)X n phases. This study provides a comprehensive understanding of the order-to-disorder transformations in M n+1 AX n phases and proposes a method for the synthesis of new solid solution (M n+1 A)X n phases by tailoring the disorder.

36 MATERIALS SCIENCE↗

The stochastic model for ternary and quaternary alloys: Application of the Bernoulli relation to the phonon spectra of mixed crystals

To understand and interpret the experimental data on the phonon spectra of the solid solutions, it is necessary to describe mathematically the non-regular distribution of atoms in their lattices. It appears that such description is possible in case of the strongly stochastically homogenous distribution which requires a great number of atoms and very carefully mixed alloys. These conditions are generally fulfilled in case of high quality homogenous semiconductor solid solutions of the III–V and II–VI semiconductor compounds. In this case, we can use the Bernoulli relation describing probability of the occurrence of one n equivalent event which can be applied, to the probability of finding one from n configurations in the solid solution lattice. The results described in this paper for ternary HgCdTe and GaAsP as well as quaternary ZnCdHgTe can provide an affirmative answer to the question: whether stochastic geometry, e.g., the Bernoulli relation, is enough to describe the observed phonon spectra.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Compositionally controlled metal-insulator transition in Tl{sub 2-x}In{sub x}TeO{sub 6}

Tl{sub 2}TeO{sub 6} and In{sub 2}TeO{sub 6} are both known to crystallize in the Na{sub 2}SiF{sub 6}-type structure. We find Tl{sub 2}TeO{sub 6} is metallic, whereas In{sub 2}TeO{sub 6} is an insulator. We have prepared a complete Tl{sub 2-x}In{sub x}TeO{sub 6} series in a search for a compositionally controlled metal-insulator transition that might be expected if a complete solid solution can be obtained. Unit cell edges and volume vary monotonically with no indication of a miscibility gap. The metal-insulator transition occurs at an x value of about 1.4, which can be rationalized on a percolation model. No superconductivity could be detected down to 5 K. -- Graphical abstract: A complete solid solution between Tl{sub 2}TeO{sub 6} and In{sub 2}TeO{sub 6} is formed. A compositionally controlled metal-insulator transition occurs in Tl{sub 2-x}In{sub x}TeO{sub 6} at an x value of about 1.5. No superconductivity could be detected down to 5 K. Display Omitted Research highlights: {yields} A complete solid solution between Tl{sub 2}TeO{sub 6} and In{sub 2}TeO{sub 6} is formed. {yields} A compositionally controlled metal-insulator transition occurs in Tl{sub 2-x}In{sub x}TeO{sub 6} at an x value of about 1.5, which can be rationalized on a percolation model. {yields} No superconductivity could be detected down to 5 K.

36 MATERIALS SCIENCE↗

Electronic structure and atomic level complexity in Al 0.5 TiZrPdCuNi high-entropy alloy in glass phase

We present that high entropy alloys (HEAs), or concentrated solid solution alloys, are chemically complex metallic solid solutions in which five or more elements occupy the same crystallographic lattice sites with nearly equal compositions. The high degree of chemical disorder gives rise to considerable local lattice distortions, atomic-level stresses, and complex electronic structure, resulting in interesting properties. We calculated the electronic structure and the atomic-level stresses of Al x Ti y Zr y Pd y Cu y Ni y , x = 0.5, y = 1 (Al 0.5 TiZrPdCuNi) HEA in the glassy phase using the density functional theory (DFT) approach. We also briefly discuss the electronic structure in its crystalline phase. Whereas it has been reported recently that the crystalline phase of this HEA is obtained as a metastable phase during the crystallization of a glassy phase, the crystalline phase was found to be unstable at T = 0 in the DFT calculation. For this reason, we focus mainly on the glassy phase in this work. Lastly, the importance of charge transfer among elements on the atomic-level pressure and the role for atomic-level stresses to characterize the electronic and structural heterogeneity are discussed.

36 MATERIALS SCIENCE↗

Matrix isolation technique for the study of some factors affecting the partitioning of trace elements

The factors that affect the preferred positions of cations in ionic solid solutions were investigated utilizing vibrational spectroscopy. Solid solutions of the sulfate and chromate ions codoped with La(+3) and Ca(+2) in a KBr host lattice were examined as a function of the polyvalent cation concentration. The cation-anion pairing process was found to be random for Ca(+2), whereas the formation of La(+3)-SO4(-2) ion pairs with a C2 sub v bonding geometry is highly preferential to any type of La(+3)-CrO4(-2) ion pair formation. The relative populations of ion pair site configurations are discussed in terms of an energy-entropy competition model which can be applied to the partition of trace elements during magmatic processes.

Grzybowski, J. M.↗