Growth and surface modification of LaFeO3 thin films induced by reductive annealing
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
This thesis investigates the heat transfer aspects of the two-piston splat quench system by modifying surface roughness and by using copper and stainless steel platens. In additive manufacturing, specifically selective laser melting (SLM), metal is subjected to a very rapid heating and cooling that produces cooling rates in the range from 105-106 °C/s. This rapid solidification produces microstructures that deviate far from equilibrium. Splat quenching is an experimental method that produces rapidly solidified structures under cooling rates that are comparable to those found in additive manufacturing. The splat quenching approach allows for more efficient testing of the rapid solidification behavior of a wide variety of alloys. In this thesis, two platen characteristics, surface roughness and material thermal conductivity, were examined to determine their role in controlling the heat transfer and the subsequent cooling rate during splat quenching of austenitic stainless steel 316L. To that objective, 5 surface finishes were produced using metallographic techniques, from 7046-203 Å Rms. Copper and 316L stainless steel platen material were used to reach different levels of thermal conductance. The combination of these 2 variables created 10 scenarios, which were examined using, backscatter imaging, secondary imaging, and electron back scatter diffraction. Cooling rates were estimated using cell sizing obtained through electrolytic etching and secondary imaging. This thesis determined that both surface modification and changes in material type had a statistically significant impact on the cell sizes observed. Where material type far outweighed surface roughness in its effect on cell size.
Rare earth iron perovskites RFeO3, where R is a rare earth cation, exhibit an array of magnetic, catalytic, optical, and electrochemical properties. Here we study EuFeO3 films synthesized by molecular beam epitaxy to improve our understanding of the optical properties of ferrites. A combination of X-ray diffraction, X-ray reflectivity, Rutherford backscattering spectroscopy, and scanning transmission electron microscopy was used to characterize the film structure and cation composition. X-ray absorption spectroscopy confirms the nominal 3+ valence states of Eu and Fe. The optical properties of EuFeO3 were investigated using variable-angle spectroscopic ellipsometry between the photon energies of 1.25 and 5 eV. We find that EuFeO3 is a semiconductor with an onset of optical absorption near 2.5 eV. The absorption spectrum of EuFeO3 is blue-shifted with respect to LaFeO3 films, a result that is attributed to the structural differences between the two materials.
Ceramic oxides and carbides are promising matrices for the immobilization and/or transmutation of nuclear wastes, cladding materials for gas-cooled fission reactors and structural components for fusion reactors. For these applications there is a need of fundamental data concerning the behavior of nuclear ceramics upon irradiation. This article is focused on the presentation of a few remarkable examples regarding ion-beam modifications of nuclear ceramics with an emphasis on the mechanisms leading to damage creation and phase transformations. Results obtained by combining advanced techniques (Rutherford backscattering spectrometry and channeling, X-ray diffraction, transmission electron microscopy, Raman spectroscopy) concern irradiations in a broad energy range (from keV to GeV) with the aim of exploring both nuclear collision (Sn) and electronic excitation (Se) regimes. Finally, the daunting challenge of the demonstration of the existence of synergistic effects between Sn and Se is tackled by discussing the healing due to intense electronic energy deposition (SHIBIEC) and by reporting results recently obtained in dual-beam irradiation (DBI) experiments.
In most classic analytical models of linear stimulated scatter, light diffraction is omitted, a priori. However, modern laser optic typically includes a variant of the random phase plate [Y. Kato et al., Phys. Rev. Lett. 53, 1057 (1984)], resulting in diffraction limited laser intensity fluctuations - or localized speckles - which may result in explosive reflectivity growth as the average laser intensity approaches a critical value [H. A. Rose and D. F. DuBois, Phys. Rev. Lett. 72, 2883 (1994)]. Among the differences between stimulated Raman scatter (SRS) and stimulated Brillouin scatter is that the SRS scattered light diffracts more strongly than the laser light with increase of electron density. This weakens the tendency of the SRS light to closely follow the most amplified paths, diminishing gain. Let G{sub 0} be the one-dimensional power gain exponent of the stimulated scatter. In this paper we show that differential diffraction gives rise to an increase of G{sub 0} at the SRS physical threshold with increase of electron density up to a drastic disruption of SRS as electron density approaches one fourth of its critical value from below. For three wave interaction lengths not small compared to a speckle length, this is a physically robust Raman gap mechanism.
This paper discusses the nucleation behaviour of the CoSi to CoSi{sub 2} transformation from cobalt silicide thin films grown by deposition at elevated substrate temperatures ranging from 375 Degree-Sign C to 600 Degree-Sign C. A combination of channelling, real-time Rutherford backscattering spectrometry, real-time x-ray diffraction, and transmission electron microscopy was used to investigate the effect of the deposition temperature on the subsequent formation temperature of CoSi{sub 2}, its growth behaviour, and the epitaxial quality of the CoSi{sub 2} thus formed. The temperature at which deposition took place was observed to exert a significant and systematic influence on both the formation temperature of CoSi{sub 2} and its growth mechanism. CoSi films grown at the lowest temperatures were found to increase the CoSi{sub 2} nucleation temperature above that of CoSi{sub 2} grown by conventional solid phase reaction, whereas the higher deposition temperatures reduced the nucleation temperature significantly. In addition, a systematic change in growth mechanism of the subsequent CoSi{sub 2} growth occurs as a function of deposition temperature. First, the CoSi{sub 2} growth rate from films grown at the lower reactive deposition temperatures is substantially lower than that grown at higher reactive deposition temperatures, even though the onset of growth occurs at a higher temperature, Second, for deposition temperatures below 450 Degree-Sign C, the growth appears columnar, indicating nucleation controlled growth. Elevated deposition temperatures, on the other hand, render the CoSi{sub 2} formation process layer-by-layer which indicates enhanced nucleation of the CoSi{sub 2} and diffusion controlled growth. Our results further indicate that this observed trend is most likely related to stress and changes in microstructure introduced during reactive deposition of the CoSi film. The deposition temperature therefore provides a handle to tune the CoSi{sub 2} growth mechanism.
The microstructure developed during severe plastic deformation results in improved mechanical properties because of the decrease in domain sizes and accumulation of defects, mainly dislocation arrays. The characteristic deformation stages observed in low stacking fault energy (SFE) face centered cubic (FCC) materials are highly influenced by the development of the primary and secondary twinning that compete with dislocation glide. In this paper, a low SFE F138 stainless steel is deformed by equal channel angular pressing (ECAP) up to 4 passes at room temperature (RT) and at 300 °C to compare the grain refinement and twin boundary development with increasing deformation. Tensile tests were performed to determine the deformation stages reached by the material before and after ECAP deformation, and the resulting microstructure was observed by TEM. X-ray diffraction and EBSD, average technique the first and local the second one, were used to quantify the microstructural changes, allowing the determination of diffraction domain sizes, dislocation and stacking fault densities and misorientation indices, which lead to a complete analysis of the deformation introduced in the material, with comparative correlations between various microstructural parameters. - Highlights: • The microstructure of ECAP pressed F138 steel was studied using TEM, EBSD and XRD. • Increasing deformation reduced domain sizes and increased dislocation densities. • Dislocation array compactness and misorientation increased with higher deformation. • Largest dislocation densities, mostly screw, match with simultaneous activation of twins. • Several correlations among microstructural features and parameters have been disclosed.
Highlights: • Texture development of in-situ TiB{sub 2} particle reinforced Al matrix composites after cold rolling were characterized. • The sum of rolling texture volume fractions has been significantly reduced by the weak texture in particle deformation zone. • Recrystallization nuclei with the Cube and Rotated-Cube orientations were observed in the particle deformation zones. • Small TiB{sub 2} particles within Al grains kept the parallel relationship with surrounding matrix during the deformation. - Abstract: Texture development of particle-reinforced metal matrix materials (P-MMCs) has not been understood well, especially the effects of second-phase particles during the deformation. In this work, we have investigated the texture evolution of TiB{sub 2}/Al composites during cold rolling by Neutron Diffraction and EBSD analysis. Two forms of TiB{sub 2} particles influenced the texture evolution in different ways. The particle-clusters aggregated along grain boundaries led to a reduction of texture volume fraction; recrystallization nuclei with weak texture appeared around these particle-clusters. Small non-shearable TiB{sub 2} particles dispersed inside Al matrix contributed to strong Copper texture component at high strains; the individual particles rotated together with Al matrix during the deformation. These revealed effects of particles on the texture development in TiB{sub 2}/Al composites provide a reference for the texture control of P-MMCs.
Interface between ceramic particulate and matrix is known to control the response of the materials and functionality of the composite. Among numerous physical properties, grain structure of the materials has also played a significant role in defining the behaviour of metal matrix composites. Usually, silicon carbide (SiC) particles show poor interfacial wettability in aluminium melt. Herein, we were successfully synthesized magnesium oxide (MgO) and nanocrystalline magnesium aluminate (MgAl{sub 2}O{sub 4}) spinel coated silicon carbide (SiC) core-shell micro-composites through sol-gel technique to improve the wettability of dispersoids. Core-shell structures of submicron size were thoroughly investigated by various characterization techniques. Further, aluminium matrix composites incorporated with pristine SiC, MgO grafted SiC and MgAl{sub 2}O{sub 4} grafted SiC particles were fabricated by stir casting technique, respectively. Additionally, as-cast composites were processed via friction stir processing (FSP) technique to observe the influence of grain refinement on mechanical and damping properties. Electron back scattered diffraction (EBSD), Field emission scanning electron microscopy (FE-SEM) and X-ray energy dispersion spectroscopy (EDX) analysis were conducted for investigating grain size refinement, adequate dispersion, stability and de-agglomeration of encapsulated SiC particles in aluminium matrix. The mechanical as well as thermal cyclic (from − 100 to 400 °C) damping performance of the as-cast and friction stir processed composites were studied, respectively. Finally, the enhanced properties were attributable to reduced agglomeration, stabilization and proper dispersion of the tailored SiC particles Al matrix. - Highlights: •Synthesizing a novel coating layer of MgO and MgAl{sub 2}O{sub 4} spinel onto SiC particles •Significant improvement in UTS and hardness by reinforcing tailored SiC in Al •Significant grain refinements were obtained through FSP •SiC/MgAl{sub 2}O{sub 4}/Al exhibits ~ 61% higher storage modulus as compare to pure Al after FSP.
High temperature compressive deformation behaviors of as-cast Ti–43Al–4Nb–1.4W–0.6B alloy were investigated at temperatures ranging from 1050 °C to 1200 °C, and strain rates from 0.001 s{sup −1} to 1 s{sup −1}. Electron back scattered diffraction technique, scanning electron microscopy and transmission electron microscopy were employed to investigate the microstructural evolutions and nucleation mechanisms of the dynamic recrystallization. The results indicated that the true stress–true strain curves show a dynamic flow softening behavior. The dependence of the peak stress on the deformation temperature and the strain rate can well be expressed by a hyperbolic-sine type equation. The activation energy decreases with increasing the strain. The size of the dynamically recrystallized β grains decreases with increasing the value of the Zener–Hollomon parameter (Z). When the flow stress reaches a steady state, the size of β grains almost remains constant with increasing the deformation strain. The continuous dynamic recrystallization plays a dominant role in the deformation. In order to characterize the evolution of dynamic recrystallization volume fraction, the dynamic recrystallization kinetics was studied by Avrami-type equation. Besides, the role of β phase and the softening mechanism during the hot deformation was also discussed in details. - Highlights: • The size of DRXed β grains decreases with increasing the value of the Z. • The CDRX plays a dominant role in the deformation. • The broken TiB{sub 2} particles can promote the nucleation of DRX.
The tensile properties and microstructures of 1050 aluminum alloy prepared by equal channel angular pressing at cryogenic temperature (cryoECAP) after electric current annealing at 90–210 °C for 3 h were investigated by tensile test, electron back scattering diffraction (EBSD) and transmission electron microscopy (TEM). An unexpected annealing-induced strengthening phenomenon occurs at 90–210 °C, due to a significant decrease in the density of mobile dislocations after annealing, and thus a higher yield stress is required to nucleate alternative dislocation sources during tensile test. The electric current can enhance the motion of dislocations, lead to a lower dislocation density at 90–150 °C, and thus shift the peak annealing temperature from 150 °C to 120 °C. Moreover, the electric current can promote the migration of grain boundaries at 150–210 °C, result in a larger grain size at 150 °C and 210 °C, and thus causes a lower yield stress. The sample annealed with electric current has a lower uniform elongation at 90–120 °C, and the deviation in the uniform elongation between samples annealed without and with electric current becomes smaller at 150–210 °C. - Highlights: • An unexpected annealing-induced strengthening phenomenon occurs at 90–210 °C. • The d. c. current can enhance the motion of dislocations at 90–150 °C, and thus shift the peak annealing temperature from 150 °C to 120 °C. • The d. c. current can promote the grain growth at 150–210 °C, and thus cause a lower yield stress. • The DC annealed sample has a lower uniform elongation at 90–120 °C.
Highlights: • A new method to get orientation maps discriminating the gamma and gamma’ phases of Ni superalloys is described. • The method combines the iCHORD technique with secondary ion imaging. • The new method resolves precipitates down to 150 nm within a reasonable acquisition time. - Abstract: Because they exhibit very similar diffraction patterns, the γ and γ′ phases of nickel-based superalloys cannot be distinguished by the conventional EBSD technique alone. This paper presents an original method which discriminates those phases on an orientation map by exploiting their chemical differences. Performed with a Focused Ion Beam (FIB) microscope, the method is the combination of the ion CHanneling ORientation Determination technique (iCHORD) – recently developed by Langlois et al. [1] – with the chemical information obtained from Secondary Ion (SI) images. The performances of the method are compared to the EDS-EBSD coupling which also discriminates phases based on their chemical compositions. Applied filters, angular resolution, spatial resolution of the phase discrimination and acquisition time are discussed. It results that the iCHORD–SI combination offers an orientation map with an angular resolution slightly decreased compared to that of the EBSD technique, but with a good phase resolution (down to 150 nm) and within a reasonable acquisition time. Thus, the iCHORD–SI combination appears to be an interesting method for the crystallographic systems where phases are difficult to discriminate by the EBSD technique alone but present a significant chemical contrast.
In this study, AISI 321 austenitic stainless steel (ASS) was cryo-rolled and subsequently annealed at 650 and 800 °C to reverse BCC α′-martensite to FCC γ-austenite. The texture evolution associated with the reversion at the selected temperatures was investigated using high-resolution EBSD. After the reversion, TiC precipitates were observed to be more stable in 650 °C-annealed specimens than those reversed at 800 °C. {110} texture was mainly developed in specimens subjected to both annealing temperatures. However, specimens reversed at 650 °C have stronger texture than those annealed at 800 °C, even at the higher annealing time. The strong intensity of {110} texture component is attributed to the ability of AISI 321 ASS to memorize the crystallographic orientation of the deformed austenite, a phenomenon termed texture memory. The development of weaker texture in 800 °C-annealed specimens is attributed to the residual strain relief in grains, dissolution of grain boundary precipitates, and an increase in atomic migration along the grain boundaries. Based on the observed features of the reversed austenite grains and estimation from an existing model, it is suspected that the austenite reversion at 650 and 800 °C undergone diffusional and martensitic shear reversion, respectively.
Multimodal datasets of materials are rich sources of information which can be leveraged for expedited discovery of process–structure–property relationships and for designing materials with targeted structures and/or properties. For this data descriptor article, we provide a multimodal dataset of magnetron sputter-deposited molybdenum (Mo) thin films, which are used in a variety of industries including high temperature coatings, photovoltaics, and microelectronics. In this dataset we explored a process space consisting of 27 unique combinations of sputter power and Ar deposition pressure. Here, the phase, structure, surface morphology, and composition of the Mo thin films were characterized by x-ray diffraction, scanning electron microscopy, atomic force microscopy, and Rutherford backscattering spectrometry. Physical properties—namely, thickness, film stress and sheet resistance—were also measured to provide additional film characteristics and behaviors. Additionally, nanoindentation was utilized to obtain mechanical load-displacement data. The entire dataset consists of 2072 measurements including scalar values (e.g., film stress values), 2D linescans (e.g., x-ray diffractograms), and 3D imagery (e.g., atomic force microscopy images). An additional 1889 quantities, including film hardness, modulus, electrical resistivity, density, and surface roughness, were derived from the experimental datasets using traditional methods. Minimal analysis and discussion of the results are provided in this data descriptor article to limit the authors’ preconceived interpretations of the data. Overall, the data modalities are consistent with previous reports of refractory metal thin films, ensuring that a high-quality dataset was generated. The entirety of this data is committed to a public repository in the Materials Data Facility.
Rolling experiments were carried out on a ternary Mg–Zn–Ca alloy and its modification with zirconium. Short time annealing of as-rolled sheets is used to reveal the microstructure and texture development. The texture of the as-rolled sheets can be characterised by basal pole figures with split peak towards the rolling direction (RD) and a broad transverse angular spread of basal planes towards the transverse direction (TD). During annealing the RD split peaks as well as orientations in the sheet plane vanish whereas the distribution of orientations tilted towards the TD remains. It is shown in EBSD measurements that during rolling bands of twin containing structures form. During subsequent annealing basal orientations close to the sheet plane vanish based on a grain nucleation and growth mechanism of recrystallisation. Orientations with tilt towards the TD remain in grains that do not undergo such a mechanism. The addition of Zr delays texture weakening. - Highlights: • Ca in Mg–Zn-alloys contributes to a significant texture weakening during rolling and annealing. • Grain nucleation and growth in structures consisting of twins explain a texture randomisation during annealing. • Grains with transverse tilt of basal planes preferentially do not undergo a grain nucleation and growth mechanism. • Zr delays the microstructure and texture development.
The current work aims at proposing an EBSD-based indicator for fatigue damage of a Fe-3Si steel. At the same time direct observation of dislocation structures is provided by electron channelling contrast imaging (ECCI). The investigation consisted in processing the EBSD data from patterns collected on specimen subjected to low cycle fatigue. It revealed two different regimes depending on the applied total strain variation which is explained by the identification of the dislocations structures and their evolution. At low strain variation, strain accommodation occurs by planar glide of dislocations uniformly distributed throughout the grains. No misorientation evolution is observed. At higher strain variation, the vein-channel structure is observed within the grain and the wall-channel structure in the vicinity of grain boundaries. The misorientation between these two dislocation structures is evaluated at about 0.7° which is detected by the EBSD analyses and explains the increase of the different misorientation based criteria. The EBSD study enables also the prediction of crack initiation mode. Finally, this study points out the limits of the EBSD technique as no misorientation evolution is detected at small strain variation. Indeed, the lattice distortion is too weak to be detected by conventional EBSD. - Highlights: • Microstructure investigation of the fatigue behaviour of an iron-silicon steel • Use of cECCI to investigate the fatigue dislocations structures • Characterisation of local plastic accommodation through EBSD misorientation criteria.
Mechanical properties of steels depend on the phase constitutions of the final microstructures which can be related to the processing parameters. Therefore, accurate quantification of different phases is necessary to investigate the relationships between processing parameters, final microstructures and mechanical properties. Point counting on micrographs observed by optical or scanning electron microscopy is widely used as a phase quantification method, and different phases are discriminated according to their morphological characteristics. However, it is difficult to differentiate some of the phase constituents with similar morphology. Differently, for EBSD based phase quantification methods, besides morphological characteristics, other parameters derived from the orientation information can also be used for discrimination. In this research, a phase quantification method based on EBSD data in the unit of grains was proposed to identify and quantify the complex phase constitutions of a microalloyed steel subjected to accelerated coolings. Characteristics of polygonal ferrite/quasi-polygonal ferrite, acicular ferrite and bainitic ferrite on grain averaged misorientation angles, aspect ratios, high angle grain boundary fractions and grain sizes were analysed and used to develop the identification criteria for each phase. Comparing the results obtained by this EBSD based method and point counting, it was found that this EBSD based method can provide accurate and reliable phase quantification results for microstructures with relatively slow cooling rates. - Highlights: •A phase quantification method based on EBSD data in the unit of grains was proposed. •The critical grain area above which GAM angles are valid parameters was obtained. •Grain size and grain boundary misorientation were used to identify acicular ferrite. •High cooling rates deteriorate the accuracy of this EBSD based method.
Highlights: • The effects of LPSO/α-Mg interfaces on the dynamic recrystallization (DRX) behavior of Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} (at.%) alloy during indirect extrusion at 350 °C were investigated. • The LPSO/α-Mg interfaces in Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} alloy appeared as two groups, including the basal and non-basal LPSO/α-Mg interfaces, which have various effects on the DRX behavior of Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} alloy. • Compared with the basal LPSO/α-Mg interfaces, DRX grains are preferentially nucleated near the non-basal LPSO/α-Mg interfaces where there is higher V{sub GROD} and lower required energy E{sub s} for the DRX nucleation. - Abstract: Mg-Gd-Zn alloy, which contains a long period stacking ordered (LPSO) structure, has the potential to become a high-strength Mg alloy within the automotive and aerospace industries. Two types of LPSO/α-Mg interfaces in Mg{sub 96.5}Gd{sub 2.5}Zn{sub 1} (at.%) alloy were characterized, namely, basal and non-basal LPSO/α-Mg interfaces. The effects of LPSO/α-Mg interfaces on the dynamic recrystallization (DRX) behavior during indirect extrusion at 350 °C were investigated. The grain reference orientation deviation (GROD) value (V{sub GROD}), derived from EBSD, could qualitatively characterize the dislocation density within a grain and determine the presence of DRX grain nucleation. The results suggested that the areas around non-basal LPSO/α-Mg interfaces always have higher V{sub GROD} than do basal LPSO/α-Mg interfaces. In addition, the stored energy (E{sub s}) required for DRX nucleation on the non-basal LPSO/α-Mg interface is lower than that on the basal LPSO/α-Mg interface. This is a result of the flat, sharp basal LPSO/α-Mg interface compared to the faceted non-basal LPSO/α-Mg interface. Regardless of whether the LPSO structure/α-Mg matrix interface is coherent or not, non-basal LPSO/α-Mg interfaces are favorable nucleation sites for DRX grains due to the higher V{sub GROD} and lower required energy E{sub s}.