Search NASA⌕ Search

SEARCH · Search NASA

Results for “MAGNETRON SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 991 records · Page 55

The influence of interface on spin pumping effect in Ni{sub 80}Fe{sub 20} /Tb bilayer

Focusing on the interface effect of the Ni{sub 80}Fe{sub 20} (Py)/terbium (Tb) bilayer, the influence of interface on the magnetization dynamic damping is investigated systematically. Two series of Py (12 nm)/Tb (d nm) films with and without copper (Cu) (1 nm) interlayer are deposited on silicon (Si) substrates by DC magnetron sputtering at room temperature. From vibrating sample magnetometer (VSM) measurements, the saturation magnetization (M{sub s}) decreases with increasing Tb thickness in Py/Tb bilayer while the decrease of M{sub s} is suppressed efficiently by inserting a Cu layer with even 1 nm of thickness. From the frequency dependence of ferromagnetic resonance (FMR) linewidth, we can obtain the Gilbert damping coefficient (α), α is found to exhibit an extreme enhancement in comparison to the single Py layer and shows an increasing trend with increasing Tb thickness. By inserting the Cu layer, α decreases significantly. From theoretical fitting, the spin diffusion length (λ{sub SD}) and spin mixing conductance (g{sup ↑↓}) are determined. It shows that the interface structure influences the spin mixing conductance but not the spin diffusion length.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of intermetallic compounds on the thermal conductivity of Ti-Cu composites

Ti films were deposited by magnetron sputtering on polycrystalline Cu substrates. The samples were annealed at different temperatures and characterized by x-ray diffraction for phase identification, scanning electron microscopy, and energy dispersive spectrometry for microstructure and composition and transient thermoreflectance for thermal conductivity and interface thermal conductance. The results showed that the diffused layer of Ti in Cu contained intermetallic compounds and solid solution of Ti in Cu. The thermal conductivity of the diffused layer is reduced, and the thickness increased for higher annealing temperature. The interface thermal conductance also decreased for higher temperature of annealing. A stable Cu{sub 4}Ti phase was formed after annealing at 725 °C with thermal conductivity of 10 W m{sup −1} K{sup −1}. The interface thermal conductance between the intermetallic compound and the solid solution of Ti in Cu also was reduced to 30 MW m{sup −2} K{sup −1}. The effective thermal resistance of the diffused layer and the interface was found to increase for higher annealing temperature.

36 MATERIALS SCIENCE↗

Epitaxy, strain, and composition effects on metal-insulator transition characteristics of SmNiO{sub 3} thin films

SmNiO{sub 3} (SNO) thin films were deposited on LaAlO{sub 3} (LAO), SrTiO{sub 3}, SrLaAlO{sub 4}, Si, and Al{sub 2}O{sub 3} (sapphire) substrates by RF magnetron sputtering and studies were conducted to understand how film structure and composition influence the insulator-metal transition properties. It is observed that the compressive strain induces the insulator to metal transition (MIT), while tensile strain suppresses it. In the case of non-epitaxial films, semiconducting behavior is obtained on sapphire over a broad temperature range, while on heavily-doped Si substrate; an MIT is seen in out-of-plane resistance measurement. In addition, thickness dependence on the resistance behavior and nickel oxidation state has been examined for epitaxial SNO films on LAO substrates. Fine control of the MIT by modifications to the mismatch strain and thickness provides insights to enhance the performance and the functionality of these films for emerging electron devices.

36 MATERIALS SCIENCE↗

Exchange bias properties of [Co/CoO]{sub n} multilayers

In this study, the exchange bias properties of four polycrystalline multilayer stack samples of antiferromagnetic (AF) CoO and ferromagnetic (FM) Co in the form of [CoO/Co]{sub n} with n = 1, 2, 3, and 5 are reported. The samples were grown on top of Si (001) substrates by using magnetron sputtering method. X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM) were used to determine the structural properties of the samples. XPS measurements of cobalt oxide layer revealed the coexistence of different phases in cobalt oxide as CoO and Co{sub 3}O{sub 4}, the latter of which lowers the blocking temperature. The blocking temperature is also affected by the finite size scaling effects observed in AF layers. In-plane ferromagnetic resonance (FMR) measurements revealed uniaxial in-plane magnetic anisotropy for the samples. Low temperature vibrating sample magnetometer measurements provided exchange bias with a stepwise character. Observed steps are believed to be due to magnetization reversals of individual FM layers with varying thicknesses, each of which is pinned through two interfaces from above and below with two AFM layers, except the uppermost FM Co layer with a single AFM neighbor.

36 MATERIALS SCIENCE↗

Characterization and photoluminescence of Co-doped SiC films

Co-doped SiC films are fabricated on Si (100) substrates by radio frequency magnetron sputtering, and the crystal structure, composition, element valences, local structure, and photoluminescence of the films are studied. Crystal structure analysis identifies the film structure as 3C-SiC and shows that the Co dopant atoms form CoSi secondary phase compounds in the films. The composition and element valence analysis show that the Co dopant atoms substituting for C sites in the SiC lattice exist in the form of Co{sup 2+} ions, and that C clusters are present in the films, which increase in amount with increasing Co dopant concentration. The analysis of local structure reveals that Co clusters, CoO and Co{sub 3}O{sub 4}, are not present in the films, and CoSi secondary phase compounds exist. All of the films show a violet photoluminescence peak located at 413 nm, which becomes stronger with increased Co dopant concentration and annealing temperature, and is found to originate from the C clusters.

36 MATERIALS SCIENCE↗

Effect of annealing temperature on the structural and optical properties of CeO{sub 2}:Ni thin films

High quality Ni-doped CeO{sub 2} (CeO{sub 2}:Ni) thin films were deposited on glass substrates at room temperature by using radio frequency magnetron sputtering. The effect of annealing temperature on structural and optical properties of the CeO{sub 2}:Ni films was investigated. The structural, optical and vibrational properties of the films were determined using X-ray diffraction (XRD), photoluminescence spectrometer (PL) and Raman spectrometer. It was found that the as-deposited film has a fluorite cubic structure. By increasing annealing temperature from 100°C to 300°C, the crystalline quality of the thin films could be improved. The UV and visible band emissions were observed in the photoluminescence spectra, due to exciton, defect related emissions respectively. The micro-Raman results show the characteristic peak of CeO{sub 2} F{sub 2g} at 465 cm{sup −1} and 2L0 at 1142 cm{sup −1}. Defect peaks like D and 0 bands were observed at 641 cm{sup −1} and 548 cm{sup −1} respectively. It is found from the spectra that the peak intensity of the films increased with increase of annealing temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Correlative theoretical and experimental investigation of the formation of AlYB{sub 14} and competing phases

The phase formation in the boron-rich section of the Al-Y-B system has been explored by a correlative theoretical and experimental research approach. The structure of coatings deposited via high power pulsed magnetron sputtering from a compound target was studied using elastic recoil detection analysis, electron energy loss spectroscopy spectrum imaging, as well as X-ray and electron diffraction data. The formation of AlYB{sub 14} together with the (Y,Al)B{sub 6} impurity phase, containing 1.8 at. % less B than AlYB{sub 14}, was observed at a growth temperature of 800 °C and hence 600 °C below the bulk synthesis temperature. Based on quantum mechanical calculations, we infer that minute compositional variations within the film may be responsible for the formation of both icosahedrally bonded AlYB{sub 14} and cubic (Y,Al)B{sub 6} phases. These findings are relevant for synthesis attempts of all boron rich icosahedrally bonded compounds with the space group: Imma that form ternary phases at similar compositions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Influence of nanostructure on charge transport in RuO{sub 2} thin films

Polycrystalline thin films of RuO{sub 2} were grown on fused-quartz substrates and a parametric study was carried out to probe the influence of film nanostructure on the four-point Van der Pauw resistivity and Hall coefficient. The films were grown via reactive rf magnetron sputtering of a Ru target in an Ar/O{sub 2} plasma using deposition rates from 0.27 to 3.5 A/s and substrate temperatures from 16 to 500 deg. C Room-temperature resistivities of the RuO{sub 2} films ranged from 58 to 360 {mu}{Omega} cm. Upon first heating following deposition, some films showed decreasing resistivity with increasing temperature, but the resistivities also decreased upon subsequent cooling suggesting that the annealing treatment reduces the film defect density. The temperature coefficient of resistance was found to be small (<0.001 K{sup -1}) in agreement with previous investigations. Hall coefficient measurements of the polycrystalline thin films demonstrated that either n-type or p-type majority carriers can be present depending on deposition conditions and the resulting nanostructure, in contrast to single-crystal RuO{sub 2}, which is an n-type metal. Grain size and homogeneous strain within the films were measured by x-ray diffraction and are correlated to the majority carrier type.

36 MATERIALS SCIENCE↗

Manufacture, microstructure and mechanical properties of Mo-W-N nanostructured hard films

Mo{sub 1-x}W{sub x}N{sub y} (x = 0-0.67) hard films were fabricated on wafers of silicon and high speed steel by dc magnetron sputtering technique. The effect of tungsten concentration on the phase composition, microstructure, surface morphology, hardness, adhesion, and corrosion resistance of the films was studied by X-ray diffraction, scanning electron microscopy, nano-indentation, and scratch test. It was found that if the W concentration (x) in the film is in the range of 0-0.52, the films exhibit fcc (Mo,W)N{sub y} single phase where larger W atoms substituted Mo atoms in fcc MoN{sub y}. At higher x values (x > 0.52) the films exhibit a two-phase structure consisting of fcc (Mo,W)N{sub y} and pure bcc tungsten phase. The hardness of the Mo{sub 1-x}W{sub x}N{sub y} films increases at first with increasing x, and then decreases after passing a maximum. The maximum hardness of 47 GPa is obtained at x = 0.37 corresponding to an adhesion strength of 60 N. The Mo-W-N coated high speed steel has a lower corrosion current density and higher corrosion potential than the bare high speed steel substrates.

36 MATERIALS SCIENCE↗

Electronic structure of LiCoO{sub 2} thin films: A combined photoemission spectroscopy and density functional theory study

The electronic properties of LiCoO{sub 2} have been studied by theoretical band-structure calculations (using density functional theory) and experimental methods (photoemission). Synchrotron-induced photoelectron spectroscopy, resonant photoemission spectroscopy (ResPES), and soft x-ray absorption (XAS) have been applied to investigate the electronic structure of both occupied and unoccupied states. High-quality PES spectra were obtained from stoichiometric and highly crystalline LiCoO{sub 2} thin films deposited ''in situ'' by rf magnetron sputtering. An experimental approach of separating oxygen- and cobalt-derived (final) states by ResPES in the valence-band region is presented. The procedure takes advantage of an antiresonant behavior of cobalt-derived states at the 3p-3d excitation threshold. Information about the unoccupied density of states has been obtained by O K XAS. The structure of the Co L absorption edge is compared to semiempirical charge-transfer multiplet calculations. The experimental results are furthermore compared with band-structure calculations considering three different exchange potentials [generalized gradient approximation (GGA), using a nonlocal Hubbard U (GGA+U) and using a hybrid functional (Becke, three-parameter, Lee-Yang-Parr [B3LYP])]. For these different approaches total density of states and partial valence-band density of states have been investigated. The best qualitative agreement with experimental results has been obtained by using a GGA+U functional with U=2.9 eV.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Induced polarized state in intentionally grown oxygen deficient KTaO{sub 3} thin films

Deliberately oxygen deficient potassium tantalate thin films were grown by RF magnetron sputtering on Si/SiO{sub 2}/Ti/Pt substrates. Once they were structurally characterized, the effect of oxygen vacancies on their electric properties was addressed by measuring leakage currents, dielectric constant, electric polarization, and thermally stimulated depolarization currents. By using K{sub 2}O rich KTaO{sub 3} targets and specific deposition conditions, KTaO{sub 3-{delta}} oxygen deficient thin films with a K/Ta = 1 ratio were obtained. Room temperature X-ray diffraction patterns show that KTaO{sub 3-{delta}} thin films are under a compressive strain of 2.3% relative to KTaO{sub 3} crystals. Leakage current results reveal the presence of a conductive mechanism, following the Poole-Frenkel formalism. Furthermore, dielectric, polarization, and depolarization current measurements yield the existence of a polarized state below T{sub pol} {approx} 367 Degree-Sign C. A Cole-Cole dipolar relaxation was also ascertained apparently due to oxygen vacancies induced dipoles. After thermal annealing the films in an oxygen atmosphere at a temperature above T{sub pol}, the aforementioned polarized state is suppressed, associated with a drastic oxygen vacancies reduction emerging from annealing process.

36 MATERIALS SCIENCE↗

Epitaxial growth of tungsten layers on MgO(001)

Smooth single crystal W(001) layers were grown on MgO(001) substrates by magnetron sputtering at 900 °C. X-ray diffraction ω–2θ scans, ω-rocking curves, pole figures, and reciprocal space maps indicate a 45°-rotated epitaxial relationship: (001){sub W}‖(001){sub MgO} and [010]{sub W}‖[110]{sub MgO}, and a relaxed lattice constant of 3.167 ± 0.001 nm. A residual in-plane biaxial compressive strain is primarily attributed to differential thermal contraction after growth and decreases from −0.012 ± 0.001 to −0.001 ± 0.001 with increasing layer thickness d = 4.8–390 nm, suggesting relaxation during cooling by misfit dislocation growth through threading dislocation glide. The in-plane x-ray coherence length increases from 3.4 to 33.6 nm for d = 4.8–390 nm, while the out-of-plane x-ray coherence length is identical to the layer thickness for d ≤ 20 nm, but is smaller than d for d ≥ 49.7 nm, indicating local strain variations along the film growth direction. X-ray reflectivity analyses indicate that the root-mean-square surface roughness increases from 0.50 ± 0.05 to 0.95 ± 0.05 nm for d = 4.8–19.9 nm, suggesting a roughness exponent of 0.38, but remains relatively constant for d > 20 nm with a roughness of 1.00 ± 0.05 nm at d = 47.9 nm.

36 MATERIALS SCIENCE↗

Thickness dependent structural, magnetic and magneto-transport properties of epitaxial Nd{sub 0.50}Sr{sub 0.50}MnO{sub 3} thin films

We report the thickness-dependent structural, magnetic and magneto-transport properties in epitaxial Nd{sub 0.50}Sr{sub 0.50}MnO{sub 3} thin films (10 to 300nm) prepared by DC magnetron sputtering technique on single crystalline (001) oriented substrate LaAlO{sub 3}. X-ray diffraction pattern reveals the epitaxial growth of all the films and the out-of-plane lattice parameter of films were found to increase with thickness. As thickness of the film increases the paramagnetic insulator (PMI) to ferromagnetic metal (FMM) transition temperature (T{sub C}), charge ordered transition temperature (T{sub CO}) and magnetic moment were found to increase with a strong bifurcation in ZFC-FC magnetization. The asymmetry in the coercivity seen in field dependent magnetization loops (M-H loops) suggests the presence of exchange bias (EB) effect. While temperature dependent resistivity of films show the semiconducting nature for thickness 10-200nm in temperature range from 5-300K, the film of thickness 300nm shows the insulator to metal transition with transition temperature (T{sub IM}) at 175K. Temperature dependent low field magnetoresistance (LFMR) measured at 4kOe found to decrease with thickness and for high field magnetoresistance (HFMR) at 40kOe and 60kOe also show similar dependence and a crossover at intermediate temperature range in the magnitude of MR between 10nm and 200nm films at constant field. Colossal increase in magnetoresistance observed for 10nm film at low temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Growth and Structural, Magnetic, and Magnetooptical Properties of ZnO Films Doped with a Fe{sup 57} 3d Impurity

ZnO films obtained by high-frequency magnetron sputtering and doped with a Fe{sup 57} metallic 3d impurity by the diffusion method are studied. The type of local environment of Fe{sup 57} impurity atoms on varying the deposition parameters of ZnO films is determined by Mössbauer spectroscopy. It is established that the ground state of Fe{sup 57} impurity atoms corresponds to metallic iron in the magnetically ordered state and there is a small fraction of Fe{sup 57} atoms with a local environment corresponding to the complex oxide Fe{sub 3}O{sub 4}, having the magnetically ordered state; there is also a fraction of iron atoms in the paramagnetic state. The magnetic and magnetooptical parameters of the films were measured using magnetooptic Kerr effect. The spectral dependences of the polar magnetooptic Kerr effect in ZnO(Fe{sup 57}) films are measured in a photon energy range of 1.5–4.5 eV and simulated by the effective-medium method. It is established that ZnO(Fe{sup 57}) possess an easy-plane magnetic anisotropy with a magnetization lying in the film plane.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Mn doping on the structural, optical, and magnetic properties of In{sub 2}O{sub 3} films

(In{sub 1−x}Mn{sub x}){sub 2}O{sub 3} films were grown by radio frequency-magnetron sputtering technique. Effect of Mn doping on the structural, optical, and magnetic properties of films is investigated systematically. The detailed structure analyses suggest that Mn ions substitute for In{sup 3+} sites of the In{sub 2}O{sub 3} lattice in the valence of +2 states, and Mn-related secondary phases or clusters as the source of ferromagnetism is safely ruled out. All films show typical room temperature ferromagnetism. The saturation magnetization M{sub s} increases first, and then decreases, while carrier concentration n{sub c} decreases monotonically with Mn doping, implying that the ferromagnetism is not directly induced by the mediated carriers. The optical bandgap E{sub g} of films decreases monotonically with the increase of Mn concentration, and there exists a linear functional dependence between E{sub g} and n{sub c}{sup 2/3}, which is consistent with Burstein-Moss shift arguments. It can be concluded that the ferromagnetic order in Mn-doped In{sub 2}O{sub 3} films is intrinsic, arising from Mn atoms substitution for the In sites of In{sub 2}O{sub 3} lattice. The oxygen vacancies play a mediation role on the ferromagnetic couplings between the Mn ions.

36 MATERIALS SCIENCE↗

Effect of interfacial interactions on the thermal conductivity and interfacial thermal conductance in tungsten–graphene layered structure

Graphene film was deposited by microwave plasma assisted deposition on polished oxygen free high conductivity copper foils. Tungsten–graphene layered film was formed by deposition of tungsten film by magnetron sputtering on the graphene covered copper foils. Tungsten film was also deposited directly on copper foil without graphene as the intermediate film. The tungsten–graphene–copper samples were heated at different temperatures up to 900 °C in argon atmosphere to form an interfacial tungsten carbide film. Tungsten film deposited on thicker graphene platelets dispersed on silicon wafer was also heated at 900 °C to identify the formation of tungsten carbide film by reaction of tungsten with graphene platelets. The films were characterized by scanning electron microscopy, Raman spectroscopy, and x-ray diffraction. It was found that tungsten carbide film formed at the interface upon heating only above 650 °C. Transient thermoreflectance signal from the tungsten film surface on the samples was collected and modeled using one-dimensional heat equation. The experimental and modeled results showed that the presence of graphene at the interface reduced the cross-plane effective thermal conductivity and the interfacial thermal conductance of the layer structure. Heating at 650 and 900 °C in argon further reduced the cross-plane thermal conductivity and interface thermal conductance as a result of formation nanocrystalline tungsten carbide at the interface leading to separation and formation of voids. The present results emphasize that interfacial interactions between graphene and carbide forming bcc and hcp elements will reduce the cross-plane effective thermal conductivity in composites.

36 MATERIALS SCIENCE↗

Effect of Substrate Temperature on Structural, Morphological, Magnetic, and Electrical Properties of Fe{sub 2}CoSi Heusler Alloy Thin Films for Spin-Based Device Applications

Fe{sub 2}CoSi based Heusler alloy thin films are deposited on single crystal Si (111) substrate at different substrate temperatures varying from room temperature to 600 °C using ultrahigh vacuum DC magnetron sputtering. Structural analysis of the prepared thin films is carried out using GI-XRD measurement and it conform ordered L2{sub 1} crystal structure of the films deposited at 450 °C and above. The atomic force microscopic (AFM) images of Fe{sub 2}CoSi thin films exhibiting 3D-like growth on Si (111) substrate at varying temperatures. The magnetic property of the thin films is studied using vibrating sample magnetometer (VSM). At 450 °C of substrate temperature, the prepared thin film exhibits high saturation magnetization (M{sub s} = 948 emu/cc) and low coercivity (H{sub c} = 8 Oe). The self-energy magnetization of the film and its own field is very high, when the temperature of the substrate was maintained at 450 °C and switching field ratio for this film was obtained as ~ 0.9 due to its high crystallinity and atomic ordering. The electrical property of Fe{sub 2}CoSi thin film is investigated using four-probe technique and a positive magnetoresistive behavior was observed for thin film deposited at a substrate temperature of 450 °C which indicates the possible half-metallic nature at room temperature. The enhanced magnetic and electrical properties obtained for the thin film prepared at 450 °C substrate temperature is highly suitable for spin based device applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Novel hard, tough HfAlSiN multilayers, defined by alternating Si bond structure, deposited using modulated high-flux, low-energy ion irradiation of the growing film

Hf{sub 1−x−y}Al{sub x}Si{sub y}N (0 ≤ x ≤ 0.14, 0 ≤ y ≤ 0.12) single layer and multilayer films are grown on Si(001) at 250 °C using ultrahigh vacuum magnetically unbalanced reactive magnetron sputtering from a single Hf{sub 0.6}Al{sub 0.2}Si{sub 0.2} target in mixed 5%-N{sub 2}/Ar atmospheres at a total pressure of 20 mTorr (2.67 Pa). The composition and nanostructure of Hf{sub 1−x−y}Al{sub x}Si{sub y}N films are controlled by varying the energy E{sub i} of the ions incident at the film growth surface while maintaining the ion-to-metal flux ratio constant at eight. Switching E{sub i} between 10 and 40 eV allows the growth of Hf{sub 0.78}Al{sub 0.10}Si{sub 0.12}N/Hf{sub 0.78}Al{sub 0.14}Si{sub 0.08}N multilayers with similar layer compositions, but in which the Si bonding state changes from predominantly Si–Si/Si–Hf for films grown with E{sub i} = 10 eV, to primarily Si–N with E{sub i} = 40 eV. Multilayer hardness values, which vary inversely with bilayer period Λ, range from 20 GPa with Λ = 20 nm to 27 GPa with Λ = 2 nm, while fracture toughness increases directly with Λ. Multilayers with Λ = 10 nm combine relatively high hardness, H ∼ 24 GPa, with good fracture toughness.

36 MATERIALS SCIENCE↗