Search NASA⌕ Search

SEARCH · Search NASA

Results for “Coating”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,009 records · Page 56

Pyrolytic Carbon Coating Effects on Oxide and Carbide Kernels Intended for Nuclear Fuel Applications

The coating of nuclear fuel kernels with pyrolytic carbon (PyC) is a well-understood practice dating back over half a century. In spite of decades of studies related to these coatings, no study has yet investigated the effect of the PyC deposition coating process on the kernels themselves. In this study, the composition and crystallographic phase of kernel materials were observed to change after exposure to the thermal and chemical environment of PyC coating process. Specifically, the coating process increased the fraction of high carbon content phase within carbide microsphere kernels, with W 2 C containing microspheres driven towards WC, and UC containing microspheres driven towards UC 2 . Oxide microspheres consisted of a mixture of two crystalline phases. The monoclinic phase within yttria-stabilized zirconia microspheres was eliminated by the coating process resulting in a purely tetragonal phase. Hafnium oxide microspheres were more stable showing no detectable change in composition or crystal structure after coating.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of lithium coating on long pulse high performance plasma discharges in EAST

Control of impurities, fuel recycling and hydrogen content by lithium evaporative coatings and real-time lithium powder injection (LPI) in EAST are studied for high performance H-mode discharges of up to ~100 s. The results show that the lithium evaporative coatings significantly reduced both the low-Z impurity carbon and high-Z impurity tungsten as well as molybdenum concentration in the plasmas, and the impurities concentration significantly reduced with the accumulated lithium coatings and maintained well afterwards. Specifically the high-Z tungsten core impurity concentration was maintained between 3 ppm–15 ppm during the 101 s H-mode discharge, which is acceptable for the long pulse operation. In addition, real-time wall conditioning via LPI successfully reduced the core high-Z metal impurities by 50% during ~35 s long pulse H-mode discharge, exhibiting strong compatibility between real-time LPI with long pulse discharges. In addition, evaporative lithium coatings demonstrated fuel recycling control, with fuel recycling obviously reducing with lithium coatings and maintaining well afterwards. Also, the lithium evaporative coatings reduced the hydrogen minority species content, represented by the density ratio H/(H + D), from ~50% down to ~5% with accumulated lithium coatings; low hydrogen fraction improved the ICRF minority heating efficiency. Finally the real-time LPI reduced the recycling coefficient R global from 0.95 to 0.82. With these wall conditionings help, the plasma density controlled well during the 101 s long pulse H-mode discharge. Furthermore, these results provide valuable references on impurities, fuel recycling and hydrogen content control for future longer pulse high performance H-mode operation (≥400 s) in EAST and future fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Validation of the VUV-reflective coating for next-generation liquid xenon detectors

Abstract Coating detector materials with films highly reflective in the vacuum ultraviolet region improves sensitivity of the next-generation rare-event detectors that use liquid xenon. In this work, we investigate the MgF 2 -Al-MgF 2 coating designed to achieve high reflectance at 175 nm, the mean wavelength of liquid xenon (LXe) scintillation. The coating was applied to an unpolished, passivated copper substrate mimicking a realistic detector component of the proposed nEXO experiment, as well as to two unpassivated substrates with “high” and “average” levels of polishing. After confirming the composition and morphology of the thin-film coating using TEM and EDS, the samples underwent reflectance measurements in LXe and gaseous nitrogen (GN2). Measurements in LXe exposed the coated samples to -100°C for several hours. No peeling of the coatings was observed after several thermal cycles. Polishing is found to strongly correlate with the measured specular reflectance (R spec ). In particular, 5.8(5)% specular spike reflectance in LXe was measured for the realistic sample at 20° of incidence, while the values for similar angles of incidence on the high and average polish samples are 62.3(1.3)% and 27.4(7)%, respectively. At large angles (66°–75°), theR spec in LXe for the three samples increases to 23(5)%, 80(8)%, and 84(18)%, respectively. The R spec at around 45° was measured in both GN2 and LXe for average polish sample and shows a reasonable agreement. Importantly, the total reflectance of the samples is comparable and estimated to be 92(8)%, 85(8)%, and 83(8)% in GN2 for the realistic, average, and high polish samples, respectively. This is considered satisfactory for the next-generation LXe experiments that could benefit from using reflective films, such as nEXO and DARWIN, thus validating the design of the coating.

Instruments & Instrumentation↗

Quality of goat′s milk cheese as affected by coating with edible chitosan‐essential oil films

The effectiveness of applying chitosan coatings containing rosemary and oregano essential oils to cheeses was analysed. Cheeses were coated by immersing the samples two or three times successively in the different formulations. The ripening indexes, water loss, fungal growth and sensory properties of the coated and noncoated cheeses throughout ripening were evaluated. The coatings both prevented weight loss and improved the microbial safety. The lipolytic and proteolytic activities were reduced in coated cheese, which is in line with the antimicrobial effect of active coatings. Sensory evaluation revealed that the cheeses double‐coated with chitosan–oregano oil were the best evaluated in terms of aroma and flavour.

Cano Embuena, Amalia Isabel↗

Heavy-ion induced desorption of a TiZrV coated vacuum chamber bombarded with 5 MeV/u Ar{sup 8+} beam at grazing incidence

TiZrV nonevaporable getter (NEG) coated vacuum chambers is a new vacuum technology which is already used in many particle accelerators worldwide. This coating is also of interest for heavy-ion accelerator vacuum chambers. Heavy-ion desorption yields from an activated as well as a CO saturated NEG coated tube have been measured with 5 MeV/u Ar{sup 8+} beam. The sticking probability of the NEG film was obtained by using the partial pressure ratios on two sides of the NEG coated tube. These ratios were compared to results of modeling of the experimental setup with test particle Monte Carlo and angular coefficient methods. The partial pressures inside the saturated NEG coated tube bombarded with heavy ions were up to 20 times larger than those inside the activated one. However, the partial pressure of methane remained the same. The value of the total desorption yield from the activated NEG coated tube is 2600 molecules/ion. The desorption yields after saturation for CH{sub 4}, H{sub 2}, and CO{sub 2} were found to be very close to the yields measured after the activation, while CO increased by up to a factor of 5. The total desorption yield for the saturated tube is up to 7000 molecules/ion. The large value of the desorption yield of the activated NEG coated tube, an order of magnitude higher than the desorption yield from a stainless steel tube at normal incident angle, could be explained by the grazing incident angle.

36 MATERIALS SCIENCE↗

Analysis of laser damage tests on coatings designed for broad bandwidth high reflection of femtosecond pulses

We designed an optical coating based on TiO 2 /SiO 2 layer pairs for broad bandwidth high reflection (BBHR) at 45-deg angle of incidence (AOI), P polarization of femtosecond (fs) laser pulses of 900-nm center wavelength, and produced the coatings in Sandia’s large optics coater by reactive, ion-assisted e-beam evaporation. This paper reports on laser-induced damage threshold (LIDT) tests of these coatings. The broad HR bands of BBHR coatings pose challenges to LIDT tests. An ideal test would be in a vacuum environment appropriate to a high energy, fs-pulse, petawatt-class laser, with pulses identical to its fs pulses. Short of this would be tests over portions of the HR band using nanosecond or sub-picosecond pulses produced by tunable lasers. Such tests could, e.g., sample 10-nm-wide wavelength intervals with center wavelengths tunable over the broad HR band. Alternatively, the coating’s HR band could be adjusted by means of wavelength shifts due to changing the AOI of the LIDT tests or due to the coating absorbing moisture under ambient conditions. In conclusion, we had LIDT tests performed on the BBHR coatings at selected AOIs to gain insight into their laser damage properties and analyze how the results of the different LIDT tests compare.

36 MATERIALS SCIENCE↗

Laser damage comparisons of broad-bandwidth, high-reflection optical coatings containing TiO 2 , Nb 2 O 5 , or Ta 2 O 5 high-index layers

Broad bandwidth coatings allow angle of incidence flexibility and accommodate spectral shifts due to aging and water absorption. Higher refractive index materials in optical coatings, such as TiO 2 , Nb 2 O 5 , and Ta 2 O 5 , can be used to achieve broader bandwidths compared to coatings that contain HfO 2 high index layers. We have identified the deposition settings that lead to the highest index, lowest absorption layers of TiO 2 , Nb 2 O 5 , and Ta 2 O 5 , via e-beam evaporation using ion-assisted deposition. We paired these high index materials with SiO 2 as the low index material to create broad bandwidth high reflection coatings centered at 1054 nm for 45 deg angle of incidence and P polarization. Furthermore, high reflection bandwidths as large as 231 nm were realized. Laser damage tests of these coatings using the ISO 11254 and NIF-MEL protocols are presented, which revealed that the Ta 2 O 5 /SiO 2 coating exhibits the highest resistance to laser damage, at the expense of lower bandwidth compared to the TiO 2 /SiO 2 and Nb 2 O 5 /SiO 2 coatings.

36 MATERIALS SCIENCE↗

Lithium Vanadium Oxide (Li 1.1 V 3 O 8 ) Coated with Amorphous Lithium Phosphorous Oxynitride (LiPON): Role of Material Morphology and Interfacial Structure on Resulting Electrochemistry

In the present work, lithium vanadium oxide (Li 1.1 V 3 O 8 ) particles synthesized at two different temperatures were coated with an amorphous lithium phosphorous oxynitride (LiPON) film for the first time, and the effects of the LiPON coating on the electrochemistry of the Li 1.1 V 3 O 8 materials with different morphologies were systematically investigated by comparing uncoated Li 1.1 V 3 O 8 and Li 1.1 V 3 O 8 coated with LiPON of various thicknesses. Galvanostatic discharge-charge cycling revealed increased functional capacity for the LiPON-coated materials. Post-cycling electrochemical impedance spectroscopy showed that LiPON-coated Li 1.1 V 3 O 8 materials developed less interfacial resistance with extended cycling, rationalized by vanadium migration into the LiPON coating seen by electron energy loss spectra. Post-mortem quantitative analysis of the anodes revealed more severe vanadium dissolution for the more irregularly shaped Li 1.1 V 3 O 8 materials with less LiPON coverage. Thus, this study highlights the specific benefits and limitations of LiPON coatings for stabilizing a moderate voltage Li 1.1 V 3 O 8 cathode material under extended cycling in liquid electrolyte, and describes a generally applicable approach for comprehensive characterization of a composite electroactive material which can be used to understand interfacial transport properties in other functional systems.

25 ENERGY STORAGE↗

Optimization of thermal barrier coating performance and durability over a drive cycle

A methodology to thermo-mechanically optimize a piston thermal barrier coating over a full drive cycle was established. The optimization objective was to minimize the heat transfer to the engine wall while maintaining structural integrity of the coating. Over 800 candidate materials were investigated and the optimization required more than one million non-road transient drive cycle calculations; real materials were investigated to ensure a realizable result and the existence of thermal and mechanical properties. High computational efficiency was achieved using a recently developed analytical heat transfer technique for multilayer engine walls. An uncoupled approach was utilized for the optimization, wherein the gas temperature and heat transfer coefficient profiles from a fully coupled and calibrated baseline model over the 20-min drive cycle were employed. The coating/piston interface temperature was constrained to be below the maximum piston service temperature limit. The durability was assessed using a recently developed analytical coating delamination framework for engine in-cylinder coatings based on the energy release rate when a crack forms. Results are presented for a mechanically unconstrained optimization and for cases constrained to three fixed levels of drive-cycle maximum energy release rate, and also constrained by the individual material’s toughness. The best-performing coating materials identified were verified using the fully coupled system-level model, which compared well to the uncoupled predictions. A study on the effect of adding a sealing layer to some high-performing, but porous, coatings showed a reduction in fuel consumption benefit and an increased exhaust temperature over the cycle, but the system still outperformed the uncoated case. The results of the study elucidate the importance of including engine performance and mechanical failure considerations in thermal barrier coating design.

Engineering↗

Broadband, millimeter-wave antireflection coatings for large-format, cryogenic aluminum oxide optics

Here, we present two prescriptions for broadband (~77 -252 GHz), millimeter-wave antireflection coatings for cryogenic, sintered polycrystalline aluminum oxide optics: one for large-format (700 mm diameter) planar and plano–convex elements, the other for densely packed arrays of quasi-optical elements—in our case, 5 mm diameter half-spheres (called “lenslets”). The coatings comprise three layers of commercially available, polytetrafluoroethylene-based, dielectric sheet material. The lenslet coating is molded to fit the 150 mm diameter arrays directly, while the large-diameter lenses are coated using a tiled approach. We review the fabrication processes for both prescriptions, then discuss laboratory measurements of their transmittance and reflectance. In addition, we present the inferred refractive indices and loss tangents for the coating materials and the aluminum oxide substrate. We find that at 150 GHz and 300 K the large-format coating sample achieves (97±2)% transmittance, and the lenslet coating sample achieves (94±3)% transmittance.

36 MATERIALS SCIENCE↗

Managing Sn-Supply to Tune Surface Characteristics of Vapor-Diffusion Coating of Nb₃Sn

Nb₃Sn promises better RF performance (Q and E_{acc}) than niobium at any given temperature because of superior superconducting properties. Nb₃Sn-coated SRF cavities are now produced routinely by growing a few microns thick Nb₃Sn films inside Nb cavities via the tin vapor diffusion technique. Sn evaporation and consumption during the growth process notably affect the quality of the coating. Aiming at favorable surface characteristics that could enhance the RF performance, many coatings were produced by varying Sn sources and temperature profiles. Coupon samples were examined using different material characterization techniques, and a selected few sets of coating parameters were used to coat 1.3 GHz single-cell cavities for RF testing. The Sn supply’s careful tuning is essential to manage the microstructure, roughness, and overall surface characteristics of the coating. We summarize the material analysis of witness samples and discuss the performance of several Nb₃Sn-coated single-cell cavities linked to Sn-source characteristics and observed Sn consumption during the film growth process.

Pudasaini, U.↗

Feasibility of preparing patterned molybdenum coatings on bismuth telluride thermoelectric modules.

Molybdenum electrical interconnects for thermoelectric modules were produced by air plasma spraying a 30%CE%BCm size molybdenum powder through a laser-cut Kapton tape mask. Initial feasibility demonstrations showed that the molybdenum coating exhibited excellent feature and spacing retention (~170%CE%BCm), adhered to bismuth-telluride, and exhibited electrical conductivity appropriate for use as a thermoelectric module interconnect. A design of experiments approach was used to optimize air plasma spray process conditions to produce a molybdenum coating with low electrical resistivity. Finally, a molybdenum coating was successfully produced on a fullscale thermoelectric module. After the addition of a final titanium/gold layer deposited on top of the molybdenum coating, the full scale module exhibited an electrical resistivity of 128%CE%A9, approaching the theoretical resistivity value for the 6mm module leg of 112%CE%A9. Importantly, air plasma sprayed molybdenum did not show significant chemical reaction with bismuth-telluride substrate at the coating/substrate interface. The molybdenum coating microstructure consisted of lamellar splats containing columnar grains. Air plasma sprayed molybdenum embedded deeply (several microns) into the bismuth-telluride substrate, leading to good adhesion between the coating and the substrate. Clusters of round pores (and cracks radiating from the pores) were found immediately beneath the molybdenum coating. These pores are believed to result from tellurium vaporization during the spray process where the molten molybdenum droplets (2623%C2%B0C) transferred their heat of solidification to the substrate at the moment of impact. Substrate cooling during the molybdenum deposition process was recommended to mitigate tellurium vaporization in future studies.

Sarobol, Pylin↗

Mechanisms Underpinning Degradation of Protective Oxides and Thermal Barrier Coatings in High Hydrogen Content (HHC) - Fueled Turbines

The overarching goal of this research program has been to evaluate the potential impacts of coal-derived syngas and high-hydrogen content fuels on the degradation of turbine hot-section components through attack of protective oxides and thermal barrier coatings. The primary focus of this research program has been to explore mechanisms underpinning the observed degradation processes, and connections to the combustion environments and characteristic non-combustible constituents. Based on the mechanistic understanding of how these emerging fuel streams affect materials degradation, the ultimate goal of the program is to advance the goals of the Advanced Turbine Program by developing materials design protocols leading to turbine hot-section components with improved resistance to service lifetime degradation under advanced fuels exposures. This research program has been focused on studying how: (1) differing combustion environments – relative to traditional natural gas fired systems – affect both the growth rate of thermally grown oxide (TGO) layers and the stability of these oxides and of protective thermal barrier coatings (TBCs); and (2) how low levels of fuel impurities and characteristic non-combustibles interact with surface oxides, for instance through the development of molten deposits that lead to hot corrosion of protective TBC coatings. The overall program has been comprised of six inter-related themes, each comprising a research thrust over the program period, including: (i) evaluating the role of syngas and high hydrogen content (HHC) combustion environments in modifying component surface temperatures, heat transfer to the TBC coatings, and thermal gradients within these coatings; (ii) understanding the instability of TBC coatings in the syngas and high hydrogen environment with regards to decomposition, phase changes and sintering; (iii) characterizing ash deposition, molten phase development and infiltration, and associated corrosive/thermo-chemical attack mechanisms; (iv) developing a mechanics-based analysis of the driving forces for crack growth and delamination, based on molten phase infiltration, misfit upon cooling, and loss of compliance; (v) understanding changes in TGO growth mechanisms associated with these emerging combustion product streams; and (vi) identifying degradation resistant alternative materials (including new compositions or bi-layer concepts) for use in mitigating the observed degradation modes. To address the materials stability concerns, this program integrated research thrusts aimed at: (1) Conducting tests in simulated syngas and HHC environments to evaluate materials evolution and degradation mechanisms; assessing thermally grown oxide development unique to HHC environmental exposures; carrying out high-resolution imaging and microanalysis to elucidate the evolution of surface deposits (molten phase formation and infiltration); exploring thermo-chemical instabilities; assessing thermo-mechanical drivers and thermal gradient effects on degradation; and quantitatively measuring stress evolution due to enhanced sintering and thermo-chemical instabilities induced in the coating. (2) Executing experiments to study the melting and infiltration of simulated ash deposits, and identifying reaction products and evolving phases associated with molten phase corrosion mechanisms; utilizing thermal spray techniques to fabricate test coupons with controlled microstructures to study mechanisms of instability and degradation; facilitating thermal gradient testing; and developing new materials systems for laboratory testing; (3) Correlating information on the resulting combustion environments to properly assess materials exposure conditions and guide the development of lab-scale simulations of material exposures; specification of representative syngas and high-hydrogen fuels with realistic levels of impurities and contaminants, to explore differences in heat transfer, surface degradation, and deposit formation; and facilitating combustion rig testing of materials test coupons.

Mumm, Daniel↗

Low Thermal Conductivity, High Durability Thermal Barrier Coatings for IGCC Environments

Advanced thermal barrier coatings (TBC) are crucial to improved energy efficiency in next generation gas turbine engines. The use of traditional topcoat materials, e.g. yttria-stabilized zirconia (YSZ), is limited at elevated temperatures due to (1) the accelerated undesirable phase transformations and (2) corrosive attacks by calcium-magnesium-aluminum-silicate (CMAS) deposits and moisture. The first goal of this project is to use the Solution Precursor Plasma Spray (SPPS) process to further reduce the thermal conductivity of YSZ TBCs by introducing a unique microstructural feature of layered porosity, called inter-pass boundaries (IPBs). Extensive process optimization accompanied with hundreds of spray trials as well as associated SEM cross-section and laser-flash measurements, yielded a thermal conductivity as low as 0.62 Wm⁻¹K⁻¹ in SPPS YSZ TBCs, approximately 50% reduction of APS TBCs; while other engine critical properties, such as cyclic durability, erosion resistance and sintering resistance, were characterized to be equivalent or better than APS baselines. In addition, modifications were introduced to SPPS TBCs so as to enhance their resistance to CMAS under harsh IGCC environments. Several mitigation approaches were explored, including doping the coatings with Al₂O₃ and TiO₂, applying a CMAS infiltration-inhibiting surface layer, and filling topcoat cracks with blocking substances. The efficacy of all these modifications was assessed with a set of novel CMAS-TBC interaction tests, and the moisture resistance was tested in a custom-built high-temperature moisture rig. In the end, the optimal low thermal conductivity TBC system was selected based on all evaluation tests and its processing conditions were documented. The optimal coating consisted on a thick inner layer of YSZ coating made by the SPPS process having a thermal conductivity 50% lower than standard YSZ coatings topped with a high temperature tolerant CMAS resistant gadolinium zirconate Coating made by the SPPS process. Noteworthy was the fact that the YSZ to GZO interface made by the SPPS process was not the failure location as had been observed in APS coatings.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Degradation Mechanisms and Development of Protective Coatings for Thermal Energy Storage and High Temperature Fluid Containment Materials

This research addresses cost savings to achieve the SETO target of $15/kWh th for thermal energy storage and 6¢/kWh for levelized cost of energy. Next-generation solar power conversion systems require high-temperature, advanced fluids in the range of 600° to 900°C. The three major advanced fluid groups—supercritical CO 2 , liquid metal alloys, and molten salts—are very corrosive to common alloys used in vessels, heat exchangers, and piping at these temperatures. Understanding degradation mechanisms is essential for making recommendations on proper working conditions and suitable cost-effective coating materials for CSP applications at high temperatures. The implementation of the findings from this research will significantly reduce investment risk by increasing the lifetime of the CSP plant components. In the past, the majority of the hot corrosion evaluations have been performed for waste incinerators, gas turbine engines, and electric power generation (steam-generating equipment) applications for different materials, molten-salt systems, and coatings. Containment materials and resistant coatings for supercritical CO 2 , molten salts and liquid metal alloys have not being evaluated for CSP applications. We plan to understand the underlying degradation mechanisms to select protective approaches such as anodic passivation, cathodic protection, and coating designs.The novelty of the proposed research is the development of protective coatings and working conditions for materials in contact with high temperature TES and HTF. Current state-of-the-art materials and protection methods are non-existent. Novel approaches are: the use of graphite nanomaterials to enhance the non-wettability of the aggressive fluids with the coating; self-healing behavior of Si-coatings in liquid Al-Si alloys; anodic passivation in molten salts to protect metallic substrates and the modeling prediction of attack in liquid metal alloys.

14 SOLAR ENERGY↗

Microstructure Investigation and Mechanical Properties of Coated Zircaloy Cladding

Accident Tolerant Fuel concepts have been developed and tested in diverse research programs presently around the world. Industry teams have developed proprietary coating compositions and geometries, but significant knowledge gaps exist in terms of the resulting properties of the coating and the cladding and how those components impact each other in reactor conditions. Furthermore, the national laboratory and university teams currently studying the industry concepts are limited in their ability to freely disseminate and discuss results obtained on commercial coatings. The Advanced Fuels Campaign is therefore working to develop an understanding of ‘generic’ coatings applied to commercial nuclear cladding alloys free of these constraints. This milestone report provides insights in the microstructure of a 7-micrometer Cr coating on Zircaloy-2 and a 5- micrometer coating on Zry-4 as reference materials. SEM and TEM methods were utilized to describe and identify the interface, while nanoindentation was used to determine hardness and E-Moduli of coating and cladding material. This milestone summarizes the acquired knowledge to build a necessary verified foundation for future simulation and qualification efforts.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of Standardized Property Requirements, Measurement Methods, and Reporting Guidance for Coatings

The diverse research programs presently in progress around the world have advanced a large number of coated cladding concepts to various stages of maturity. Industry teams have developed leading coating compositions and geometries, but significant disparity exists in the importance placed on different coating properties, as well as the applicability and standardization of the various methods used to measure these properties. This milestone report provides an initial assessment of the most important coating properties and the experimental methods available for their determination to lay the foundation for standardized reporting and development of comprehensive datasets for modeling efforts. This report has determined that the residual stress of the coating is the most crucial property to investigate, yet it has received minimal attention to date due to a knowledge gap about the growth and formation of the brittle Laves phase under reactor conditions. The significance of residual stress of the coating is further enhanced by its connection and interdependence with other important properties like creep and coating failure mechanisms. This milestone proposes an importance rating for residual stress properties and their associated measurement techniques to fill in knowledge. Furthermore, techniques to investigate the outlined properties are discussed, and their capabilities and limitations are illustrated to provide guidance on their use.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

High Temperature Thermal Barrier Coating Evaluation of Yttrium Aluminum Garnet for Gas Turbine Applications

The Solution Precursor Spray Process (SPPS) process has been shown to overcome the durability and property challenges of applying yttrium aluminum garnet (YAG) coating for high temperature thermal barrier coating (TBC) applications (1200°C+) but only limited testing has been performed in representative application environments. In this study, YAG coatings were developed to optimize microstructure and tailor properties for combustion components in an industrial gas turbine. Thermal conductivity, erosion resistance and furnace cycling durability were used to validate YAG properties against the standard yttria-stabilized zirconia coating (YSZ). Graded and multi-layered microstructures were applied to enhance performance while maintaining durability. Further YAG process development was required to replicate coating properties and optimize deposition on more complex fuel injector nozzle and combustion liner components. Rig testing of both components was performed and compared against the baseline YSZ coating validating the high temperature capability and lower thermal conductivity of the SPPS YAG coating. The components in both tests were cycled for a minimum of ten cycles with the fuel injector test targeting a higher operating temperature while the combustor liner operated at standard conditions. A development engine test is planned to further validate performance in a gas turbine engine of this promising material.

36 MATERIALS SCIENCE↗