At least 1,027 records · Page 57

Comprehensive study of the p-type conductivity formation in radio frequency magnetron sputtered arsenic-doped ZnO film

Arsenic doped ZnO and ZnMgO films were deposited on SiO{sub 2} using radio frequency magnetron sputtering and ZnO-Zn{sub 3}As{sub 2} and ZnO-Zn{sub 3}As{sub 2}-MgO targets, respectively. It was found that thermal activation is required to activate the formation of p-type conductivity. Hall measurements showed that p-type films with a hole concentration of {approx}10{sup 17} cm{sup -3} and mobility of {approx}8 cm{sup 2} V{sup -1} s{sup -1} were obtained at substrate temperatures of 400-500 deg. C The shallow acceptor formation mechanism was investigated using x-ray photoelectron spectroscopy, positron annihilation, low temperature photoluminescence, and nuclear reaction analysis. The authors suggest that the thermal annealing activates the formation of the As{sub Zn}-2V{sub Zn} shallow acceptor complex and removes the compensating hydrogen center.

36 MATERIALS SCIENCE↗

DC reactive magnetron sputtering, annealing, and characterization of CuAlO{sub 2} thin films

CuAlO{sub x} thin films were prepared at three substrate temperatures (T{sub S}=60, 300, and 600 deg. C) and two oxygen partial pressures (P{sub O{sub 2}}=0.5 and 2 mTorr) via dc reactive magnetron sputtering from Cu-Al 50-50 at. % alloy targets and subsequent annealing. As-deposited films with P{sub O{sub 2}}=0.5 mTorr were oxygen deficient; although the delafossite structure formed upon annealing, electrical properties were poor. Films deposited with P{sub O{sub 2}}=2 mTorr transformed into the delafossite structure and exhibited p-type conductivity after annealing under N{sub 2} at temperatures T{sub A}{>=}750 deg. C. Conductivity generally increased with increasing T{sub S} and decreasing T{sub A}. A special case of P{sub O{sub 2}}=2 mTorr and low T{sub S} (60 deg. C) resulted in a partially crystalline oxide phase that transformed into the delafossite structure at T{sub A}=700 deg. C and yielded the highest conductivity of 1.8 S cm{sup -1}. In general, a T{sub A} near the phase formation boundary led to an increase in conductivity. Low-temperature hydrothermal annealing was also investigated and shown to produce mixed phase films exhibiting the delafossite structure along with CuO, AlOOH, and Al{sub 2}O{sub 3}.

36 MATERIALS SCIENCE↗

Highly textured growth of AlN films on sapphire by magnetron sputtering for high temperature surface acoustic wave applications

Piezoelectric aluminum nitride films were deposited onto 3 in. [0001] sapphire substrates by reactive magnetron sputtering to explore the possibility of making highly (002)-textured AlN films to be used in surface acoustic wave (SAW) devices for high temperature applications. The synthesized films, typically 1 {mu}m thick, exhibited a columnar microstructure and a high c-axis texture. The relationship between the microstructures and process conditions was examined by x-ray diffraction (XRD), transmission electron microscopy, and atomic force microscopy analyses. The authors found that highly (002)-textured AlN films with a full width at half maximum of the rocking curve of less than 0.3 deg. can be achieved under high nitrogen concentration and moderate growth temperature, i.e., 250 deg. C. The phi-scan XRD reveals the high in-plane texture of deposited AlN films. The SAW devices, based on the optimized AlN films on sapphire substrate, were characterized before and after an air annealing process at 800 deg. C for 90 min. The frequency response, recorded after the annealing process, confirmed that the thin films were still strong in a high temperature environment and that they had retained their piezoelectric properties.

36 MATERIALS SCIENCE↗

Effects of thermal annealing on the microstructure of sputtered Al{sub 2}O{sub 3} coatings

The morphology and microstructure of Al{sub 2}O{sub 3} thin films deposited by pulsed direct current magnetron sputtering were studied in the as-grown state and after vacuum annealing at 1000 deg. C for 12 h using transmission electron microscopy. For the coating deposited under low ion bombardment conditions, the film consists of small {gamma}- and/or {delta}-Al{sub 2}O{sub 3} grains embedded in an amorphous matrix. The grain size at the region close to the interface to the substrate was much larger than that of the remaining layer. Growth of the {gamma}-Al{sub 2}O{sub 3} phase is promoted during annealing but no transformation to {alpha}-Al{sub 2}O{sub 3} was detected. For high-energetic growth conditions, clear evidence for {gamma}-Al{sub 2}O{sub 3} formation was found in the upper part of the coating with grain size much larger than for low-energetic growth, but the film was predominately amorphous at the interface region. Annealing resulted in the transformation of {gamma}-Al{sub 2}O{sub 3} to {alpha}-Al{sub 2}O{sub 3}, while the mainly amorphous part crystallized to {gamma}-Al{sub 2}O{sub 3}.

36 MATERIALS SCIENCE↗

Effects of temperature and near-substrate plasma density on the structural and electrical properties of dc sputtered germanium thin films

Germanium thin films were deposited by dc reactive magnetron sputtering as a function of substrate temperature and ion flux using an unbalanced magnetron with an external magnetic field. The ion flux and energy distribution were measured using a retarding field energy analyzer (RFEA), a flat probe with a guard ring, and cylindrical Langmuir probes. The RFEA ion flux, the flat probe saturation currents, and the ion densities inferred from the cylindrical probe data are in very good agreement over a wide range of plasma densities, which were varied both by the external coil current and discharge power. The RFEA ion energy distributions are in good agreement with the plasma potentials inferred from the cylindrical probes, and suggest that the nonuniformity of the plasma in the vicinity of the substrate holder should be considered in the interpretation of probe results in these systems. The deposited films were characterized by x-ray diffraction, Raman spectroscopy, optical transmission, resistivity, and Hall effect measurements. Under low ion bombardment conditions, an abrupt onset of the crystalline phase with respect to temperature is observed in the Raman and x-ray diffraction measurements, and the crystal quality increases with increasing temperature above the transition temperature. The transition is also accompanied by a sharp decrease in film resistivity. The microcrystalline films have a strong preferential orientation in the (220) direction, and are p type with carrier densities in the range 10{sup 18} cm{sup -3} and mobilities in the range 15-30 cm{sup 2}/V-s. The structural and electronic properties of the films are sensitive to the ion flux. Near the transition temperature the effects of increasing ion flux can be attributed to the small temperature rise that accompanies the higher plasma density. At higher temperatures the increased ion flux results in a more random crystallographic orientation, with significantly lower carrier concentrations and only slightly lower carrier mobilities, implying either a reduction in acceptor defect density and/or the creation of compensating n-type defects.

36 MATERIALS SCIENCE↗

Effect of substrate temperature on the properties of transparent conductive ZnO:Al thin films prepared by RF sputtering

Transparent conductive ZnO:Al thin films were successfully deposited on glass substrates via radio frequency sputtering with a ceramic target in ambient argon. X-ray diffraction, profilometry, Hall-effect measurement, and spectrophotometry were employed to investigate the structural, electrical, and optical properties of films. The electrical and optical properties were found to be strongly dependent on the crystalline quality, grain size, and thickness of the films. X-ray diffraction spectra indicated that the crystalline quality of the films improved and grains became larger with increasing substrate temperature. Transmission spectra revealed that films possessed a higher transmittance in the visible range with an increase of the substrate temperature, but the band gap did not broaden obviously. Films with a resistivity of about 2.66 x 10{sup -4}{Omega} cm and an average transmittance above 90% in the visible range were obtained at the optimum temperature of 450 deg. C.

36 MATERIALS SCIENCE↗

Compositional study of vacuum annealed Al doped ZnO thin films obtained by RF magnetron sputtering

Aluminum doped zinc oxide (AZO) thin films were obtained by RF magnetron sputtering. The effects of deposition parameters such as power, gas flow conditions, and substrate heating have been studied. Deposited and annealed films were characterized for composition as well as microstructure using x ray photoelectron spectroscopy and x ray diffraction. Films produced were polycrystalline in nature. Surface imaging and roughness studies were carried out using SEM and AFM, respectively. Columnar grain growth was predominantly observed. Optical and electrical properties were evaluated for transparent conducting oxide applications. Processing conditions were optimized to obtain highly transparent AZO films with a low resistivity value of 6.67 x 10{sup -4}{Omega} cm.

36 MATERIALS SCIENCE↗

Deposition of novel nanocomposite films by a newly developed differential pumping co-sputtering system

A differential pumping co-sputtering system was developed to facilitate a controlled, but flexible fabrication of multifunctional nanocomposite films with compositions not limited by thermodynamic restrictions. This system features a multichamber design with a differential pumping system. Dividing atmospheres with this set up greatly reduced the cross-contamination between chambers, and each material could be co-deposited by rapid rotation of the substrate. The clearance between the substrate holder and the chamber was set at 1-2 mm, and the conductance of the clearance was examined roughly using conductance equations for typical types of orifices. It was found that the potential difference (PD) value of the clearance between the two chambers was less than 0.01; the gas flow between the two chambers through the clearance thus appears to be a practical molecular flow. The PD value, where P is a pressure (Pa) and D is a diameter of an orifice or a pipe (m), is a gas flow indicator or parameter obtained from an equation of Knudsen number. The changes in the oxygen partial pressure and glow discharge plasma in the left chamber were investigated using a process gas monitor (PGM) and optical emission spectroscope (OES) by introducing different gases to each chamber. The PGM results revealed that the cross-contamination of oxygen from the other chamber was suppressed to 10 {+-} 3% of the original. In addition, the OES measurement for glow discharge plasma did not detect substantial oxygen contamination from the other chamber. Using the newly developed system, an AlN/SiO{sub x} nanocomposite film consisting of B4-type AlN and amorphous SiO{sub x} was obtained successfully.

36 MATERIALS SCIENCE↗

Tribological behavior of Ti-Al-Si-C-N hard coatings deposited by hybrid arc-enhanced magnetron sputtering

Ti-Al-Si-C-N hard coatings are deposited on high speed steel by hybrid arc-enhanced magnetron sputtering, and the hardness, adhesion, and tribological behavior are studied. On account of the nanocomposite structure, the coatings possess hardness of more than 30 GPa. Failure of the coating during the scratch test is due to the buckling and wedge spallation failure mechanism. Compared to Ti-Al-Si-N, the presence of C in the Ti-Al-Si-C-N coatings leads to reduced friction coefficient and wear rate, indicating effective lubrication rendered by amorphous C. According to the wear tracks examined by scanning electron microscopy, the wear mechanism can be explained by plowing abrasion.

36 MATERIALS SCIENCE↗

In/ITO whisker and optoelectronic properties of ITO films deposited by ion beam sputtering

ITO films were deposited on a glass substrate using ion beam sputtering, with oxygen flow rates from 0.5 to 2 sccm. The films consisted of randomly oriented ITO nanoparticles and metallic indium (In) with {l_brace}101{r_brace} facets, following the specific crystallographic relationship of [010]{sub In}//[110]{sub ITO}; (001){sub In}//(001){sub ITO} with habit planes (100){sub In}//(011){sub ITO}, when fabricated using a low oxygen flow rate. Oxygen flow rate in excess of 2.0 sccm results in the growth of amorphous films. The epitaxial In nanoparticles probably act as seeds for the development of curved ITO whiskers as small as 10 nm and extend up to 100 nm in length along the [100] direction, with poorly defined shape, possibly due to the tapering and bending of the whisker to form a tilt boundary about the [011] zone axis of the ITO. The ITO whisker growth was facilitated by the In globular tips in the vapor-liquid-solid growth mechanism. The films prepared using a series of oxygen flow rates showed different chemical-bonding states, electric resistivity and optical transparency; as a result of phase and microstructural changes.

36 MATERIALS SCIENCE↗

Evaporation-assisted high-power impulse magnetron sputtering: The deposition of tungsten oxide as a case study

The deposition rate during the synthesis of tungsten trioxide thin films by reactive high-power impulse magnetron sputtering (HiPIMS) of a tungsten target increases, above the dc threshold, as a result of the appropriate combination of the target voltage, the pulse duration, and the amount of oxygen in the reactive atmosphere. This behavior is likely to be caused by the evaporation of the low melting point tungsten trioxide layer covering the metallic target in such working conditions. The HiPIMS process is therefore assisted by thermal evaporation of the target material.

36 MATERIALS SCIENCE↗

Magnetron-sputter epitaxy of {beta}-FeSi{sub 2}(220)/Si(111) and {beta}-FeSi{sub 2}(431)/Si(001) thin films at elevated temperatures

{beta}-FeSi{sub 2} thin films have been grown on Si(111) and Si(001) substrates by magnetron-sputter epitaxy at 700 Degree-Sign C. On Si(111), the growth is consistent with the commonly observed orientation of [001]{beta}-FeSi{sub 2}(220)//[1-10]Si(111) having three variants, in-plane rotated 120 Degree-Sign with respect to one another. However, on Si(001), under the same growth conditions, the growth is dominated by [-111]{beta}-FeSi{sub 2}(431)//[110]Si(001) with four variants, which is hitherto unknown for growing {beta}-FeSi{sub 2}. Photoelectron spectra reveal negligible differences in the valance-band and Fe2p core-level between {beta}-FeSi{sub 2} grown on Si(111) and Si(001) but an apparent increased Si-oxidization on the surface of {beta}-FeSi{sub 2}/Si(001). This phenomenon is discussed and attributed to the Si-surface termination effect, which also suggests that the Si/Fe ratio on the surface of {beta}-FeSi{sub 2}(431)/Si(001) is larger than that on the surface of {beta}-FeSi{sub 2}(220)/Si(111).

36 MATERIALS SCIENCE↗

Biaxial texture development in aluminum nitride layers during off-axis sputter deposition

Polycrystalline aluminum nitride (AlN) layers were deposited by pulsed-dc reactive magnetron sputtering from a variable deposition angle {alpha} = 0 Degree-Sign -84 Degree-Sign in 5 mTorr pure N{sub 2} at room temperature. X-ray diffraction pole figure analyses show that layers deposited from a normal angle ({alpha} = 0 Degree-Sign ) exhibit fiber texture, with a random in-plane grain orientation and the c-axis tilted by 42 Degree-Sign {+-} 2 Degree-Sign off the substrate normal, yielding wurtzite AlN grains with the {l_brace}1012{r_brace} plane approximately parallel ({+-}2 Degree-Sign ) to the substrate surface. However, as {alpha} is increased to 45 Degree-Sign , two preferred in-plane grain orientations emerge, with populations I and II having the c-axis tilted toward and away from the deposition flux, by 53 Degree-Sign {+-} 2 Degree-Sign and 47 Degree-Sign {+-} 1 Degree-Sign off the substrate normal, respectively. Increasing {alpha} further to 65 Degree-Sign and 84 Degree-Sign , results in the development of a single population II with a 43 Degree-Sign {+-} 1 Degree-Sign tilt. This developing biaxial texture is attributed to a competitive growth mode under conditions where the adatom mobility is sufficient to cause intergrain mass transport, but insufficient for the thermodynamically favored low energy {l_brace}0001{r_brace} planes to align parallel to the layer surface. Consequently, AlN nuclei are initially randomly oriented and form a kinetically determined crystal habit exposing {l_brace}0001{r_brace} and {l_brace}1120{r_brace} facets. The expected direction of its highest growth rate is 49 Degree-Sign {+-} 5 Degree-Sign tilted relative to the c-axis, in good agreement with the 42 Degree-Sign -53 Degree-Sign measured tilt. The in-plane preferred orientation for {alpha} > 0 Degree-Sign is well explained by the orientation dependence in the cross section of the asymmetric pyramidal nuclei to capture directional deposition flux. The observed tilt is ideal for shear mode electromechanical coupling, which is maximized at 48 Degree-Sign .

36 MATERIALS SCIENCE↗

Surface characterization of Zr/Ti/Nb tri-layered films deposited by magnetron sputtering on Si(111) and stainless steel substrates

Among metallic materials, commercially pure titanium and titanium alloys are very often used as biomaterials for implants. Among these alloys, titanium-aluminum-vanadium alloy Ti-6 A-4 V is one of the most commonly used due to its excellent biocompatibility and ability to allow bone-implant integration. A new class of Ti alloys employs Zr for solid-solution hardening and Nb as {beta}-phase stabilizer. Metals such as Ti, Nb, and Zr-known as valve metals-usually have their surfaces covered by a thin oxide film that forms spontaneously in air. This oxide film constitutes a barrier between the metal and the medium. The Ti-Nb-Zr alloys have mechanical and corrosion resistance characteristics which make them suitable for use as implants. Tri-layered films of Ti-Nb-Zr were deposited on both Si(111) and stainless steel (SS) substrates using dc magnetron sputtering equipment, under an argon atmosphere according to the following methodology: a 100 nm thick layer of Nb was deposited on the substrate, followed by a 200 nm thick layer of Ti, and finally a 50 nm thick layer of Zr, on top of the multilayer stack. The morphology and chemical composition of the films were analyzed by atomic force microscopy (AFM), x-ray photoelectron spectroscopy (XPS), and time-of-flight secondary ion mass spectrometry (ToF-SIMS). AFM images showed that the Zr/Ti/Nb tri-layer films presented nanostructured grains and low roughness. The ToF-SIMS depth profiles confirmed the formation of a three-layered film on Si(111) with well-defined and sharp interfaces between the layers, while the deposition on the stainless steel substrate caused slight intermixing at the different alloy/Nb, Nb/Ti and Ti/Zr interfaces, reflecting the greater roughness of the raw substrate. The XPS results for the Zr/Ti/Nb layers deposited on Si(111) and SS confirmed that the outermost layer consisted of Zr only, with a predominance of ZrO{sub 2}, as the metal layer is passivated in air. An oxidation treatment of 1000 Degree-Sign C in air for 1 h for the multilayer stacks caused some dewetting with Si(111) films, and alloying in the layers. The latter effect was more pronounced for the stainless steel substrate.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of Ti–B–C–N–Si nanocomposite films deposited by unbalanced magnetron sputtering

Quinary Ti–B–C–N–Si nanocomposite thin films were deposited on AISI 304 stainless steel substrates by d.c. unbalanced magnetron sputtering from a TiB{sub 2}–TiC compound target and a pure Si target. The relationship between microstructure and mechanical properties of the films was investigated in terms of the nanosized crystallites/amorphous system. The synthesized Ti–B–C–N–Si films were characterized using x-ray diffraction, x-ray photoelectron spectroscopy, atomic force microscopy, and high resolution transmission electron microscopy. The results showed that the Ti–B–C–N–Si films were nanocomposites composed of nanosized TiB{sub 2}, TiC, and TiSi{sub 2} crystallites (2-3 nm in size) embedded in an amorphous matrix. The addition of Si to the Ti–B–C–N film led to precipitation of nanosized crystalline TiSi{sub 2} and percolation of amorphous SiC phases. The Ti–B–C–N–Si films with up to 7 at. % Si content presented high hardness (≥35 GPa), H/E (≥0.0095), and W{sub e} (>50%) with compressive residual stress (∼0.5 GPa). A systematic investigation on the microstructure and mechanical properties of Ti–B–C–N–Si films containing different Si contents is reported.

36 MATERIALS SCIENCE↗

Nanoscale compositional analysis of NiTi shape memory alloy films deposited by DC magnetron sputtering

The formation of surface oxide layer as well as compositional changes along the thickness for NiTi shape memory alloy thin films deposited by direct current magnetron sputtering at substrate temperature of 300 °C in the as-deposited condition as well as in the postannealed (at 600 °C) condition have been thoroughly studied by using secondary ion mass spectroscopy, x-ray photoelectron spectroscopy, and scanning transmission electron microscopy-energy dispersive x-ray spectroscopy techniques. Formation of titanium oxide (predominantly titanium dioxide) layer was observed in both as-deposited and postannealed NiTi films, although the oxide layer was much thinner (8 nm) in as-deposited condition. The depletion of Ti and enrichment of Ni below the oxide layer in postannealed films also resulted in the formation of a graded microstructure consisting of titanium oxide, Ni{sub 3}Ti, and B2 NiTi. A uniform composition of B2 NiTi was obtained in the postannealed film only below a depth of 200–250 nm from the surface. Postannealed film also exhibited formation of a ternary silicide (Ni{sub x}Ti{sub y}Si) at the film–substrate interface, whereas no silicide was seen in the as-deposited film. The formation of silicide also caused a depletion of Ni in the film in a region ∼250–300 nm just above the film substrate interface.

36 MATERIALS SCIENCE↗

Physical properties of epitaxial ZrN/MgO(001) layers grown by reactive magnetron sputtering

Single-crystal ZrN films, 830 nm thick, are grown on MgO(001) at 450 °C by magnetically unbalanced reactive magnetron sputtering. The combination of high-resolution x-ray diffraction reciprocal lattice maps, high-resolution cross-sectional transmission electron microscopy, and selected-area electron diffraction shows that ZrN grows epitaxially on MgO(001) with a cube-on-cube orientational relationship, (001){sub ZrN}‖(001){sub MgO} and [100]{sub ZrN}‖[100]{sub MgO}. The layers are essentially fully relaxed with a lattice parameter of 0.4575 nm, in good agreement with reported results for bulk ZrN crystals. X-ray reflectivity results reveal that the films are completely dense with smooth surfaces (roughness = 1.3 nm, consistent with atomic-force microscopy analyses). Based on temperature-dependent electronic transport measurements, epitaxial ZrN/MgO(001) layers have a room-temperature resistivity ρ{sub 300K} of 12.0 μΩ-cm, a temperature coefficient of resistivity between 100 and 300 K of 5.6 × 10{sup −8}Ω-cm K{sup −1}, a residual resistivity ρ{sub o} below 30 K of 0.78 μΩ-cm (corresponding to a residual resistivity ratio ρ{sub 300Κ}/ρ{sub 15K} = 15), and the layers exhibit a superconducting transition temperature of 10.4 K. The relatively high residual resistivity ratio, combined with long in-plane and out-of-plane x-ray coherence lengths, ξ{sub ‖} = 18 nm and ξ{sub ⊥} = 161 nm, indicates high crystalline quality with low mosaicity. The reflectance of ZrN(001), as determined by variable-angle spectroscopic ellipsometry, decreases slowly from 95% at 1 eV to 90% at 2 eV with a reflectance edge at 3.04 eV. Interband transitions dominate the dielectric response above 2 eV. The ZrN(001) nanoindentation hardness and modulus are 22.7 ± 1.7 and 450 ± 25 GPa.

36 MATERIALS SCIENCE↗

Mechanical and transparent conductive properties of ZnO and Ga-doped ZnO films sputtered using electron-cyclotron-resonance plasma on polyethylene naphtalate substrates

Transparent conductive ZnO and Ga-doped ZnO (GZO) films were deposited on polyethylene naphtalate (PEN) sheet substrates using electron cyclotron resonance plasma sputtering. Both ZnO and GZO films were highly adhesive to the PEN substrates without inserting an intermediate layer in the interface. When compared at the same thickness, the transparent conductive properties of GZO films on PEN substrates were only slightly inferior to those on glass substrates. However, the carrier concentration of ZnO films on PEN substrates was 1.5 times that of those on glass substrates, whereas their Hall mobility was only 60% at a thickness of 300 nm. The depth profile of elements measured by secondary ion mass spectroscopy revealed the diffusion of hydrocarbons out of the PEN substrate into the ZnO film. Hence, doped carbons may act as donors to enhance carrier concentration, and the intermixing of elements at the interface may deteriorate the crystallinity, resulting in the lower Hall mobility. When the ZnO films were thicker than 400 nm, cracks became prevalent because of the lattice mismatch strain between the film and the substrate, whereas GZO films were free of cracks. The authors investigated how rolling the films around a cylindrical pipe surface affected their conductive properties. Degraded conductivity occurred at a threshold pipe radius of 10 mm when tensile stress was applied to the film, but it occurred at a pipe radius of 5 mm when compressive stress was applied. These values are guidelines for bending actual devices fabricated on PEN substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗