Search NASA⌕ Search

SEARCH · Search NASA

Results for “microstructural properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,027 records · Page 57

Effect of deposition pressure on the microstructure and thermoelectric properties of epitaxial ScN(001) thin films sputtered onto MgO(001) substrates

Four epitaxial ScN(001) thin films were successfully deposited on MgO(001) substrates by dc reactive magnetron sputtering at 2, 5, 10, and 20 mTorr in an Ar/N2 ambient atmosphere at 650 °C. The microstructure of the resultant films was analyzed by x-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Electrical resistivity, electron mobility and concentration were measured using the room temperature Hall technique, and temperature dependent in-plain measurements of the thermoelectric properties of the ScN thin films were performed. The surface morphology and film crystallinity significantly degrade with increasing deposition pressure. The ScN thin film deposited at 20 mTorr exhibits the presence of <221> oriented secondary grains resulting in decreased electric properties and a low thermoelectric power factor of 0.5 W/m-K² at 800 K. ScN thin films grown at 5 and 10 mTorr are single crystalline, yielding the power factor of approximately 2.5 W/m-K² at 800 K. The deposition performed at 2 mTorr produces the highest quality ScN thin film with the electron mobility of 98 cm² V⁻¹ s⁻¹ and the power factor of 3.3 W/m-K² at 800 K.

36 MATERIALS SCIENCE↗

The Effect of Arc Current on Microstructure and Mechanical Properties of Hybrid LasTIG Welds of High-Strength Low-Alloy Steels

A hybrid laser-tungsten inert gas (LasTIG) welding system was applied for 3-mm-thick S460MC and S700MC high-strength low-alloy steel sheet butt welding with the aim to reduce the cooling rate compared with laser welding. The effect of the electric current was evaluated. Increasing arc current led to the increase of fused metal and heat-affected-zone (HAZ) dimensions. Fused metal grains were larger whereas the microhardness increase toward the base metal was lower at higher currents in this region. Microhardness peaks corresponding to the coarse-grained HAZ were reduced at higher currents for S460MC but were almost not affected in S700MC. The tensile strength of both the laser weld and LasTIG welds was comparable to the base metal for both alloys.

36 MATERIALS SCIENCE↗

Interfacial Microstructure and Mechanical Properties of Friction Stir Welded Joints of Commercially Pure Aluminum and 304 Stainless Steel

In the present investigation, friction stir welding of commercially pure aluminum and 304 stainless steel was carried out at varying tool rotational speeds from 200 to 1000 rpm in steps of 200 rpm using 60 mm/min traverse speed at 2 (degree) tool tilt angle. Microstructural characterization of the interfacial zone was carried out using optical microscope and scanning electron microscope. Energy-dispersive spectroscopy indicated the presence of FeAl{sub 3} intermetallic phase. Thickness of the intermetallic layer increased with the increase in tool rotational speed. X-ray diffraction studies indicated the formation of intermetallic phases like FeAl{sub 2}, Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}, and FeAl{sub 3}. A maximum tensile strength of ~ 90% that of aluminum along with ~ 4.5% elongation was achieved with the welded sample at tool rotational speed of 400 rpm. The stir zone showed higher hardness as compared to base metals, heat affected zone, and thermo-mechanically affected zone due to the presence of intermetallics. The maximum hardness value at the stir zone was achieved at 1000 rpm tool rotational speed.

36 MATERIALS SCIENCE↗

Chemical composition, microstructure, and hygroscopic properties of aerosol particles at the Zotino Tall Tower Observatory (ZOTTO), Siberia, during a summer campaign

In this study we describe the hygroscopic properties of accumulation- and coarse-mode aerosol particles sampled at the Zotino Tall Tower Observatory (ZOTTO) in Central Siberia (61° N; 89° E) from 16 to 21 June 2013. The hygroscopic growth measurements were supplemented with chemical analyses of the samples, including inorganic ions and organic/elemental carbon. In addition, the microstructure and chemical composition of aerosol particles were analyzed by X-ray micro-spectroscopy (STXM-NEXAFS) and transmission electron microscopy (TEM). A mass closure analysis indicates that organic carbon accounted for 61 and 38% of PM in the accumulation mode and coarse mode, respectively. The water soluble fraction of organic matter was estimated to be 52 and 8% of PM in these modes. Sulfate, predominantly in the form of ammoniated sulfate, was the dominant inorganic component in both size modes: ~ 34% in the accumulation vs. ~ 47% in the coarse mode. The hygroscopic growth measurements were conducted with a filter-based differential hygroscopicity analyzer (FDHA) over the range of 5–99.4% RH in the hydration and dehydration operation modes. The FDHA study indicates that both accumulation and coarse modes exhibit pronounced water uptake approximately at the same RH, starting at ~ 70%, while efflorescence occurred at different humidities, i.e., at ~ 35% RH for submicron particles vs. ~ 50% RH for supermicron particles. This ~ 15% RH difference was attributed to higher content of organic material in the submicron particles, which suppresses water release in the dehydration experiments. The kappa mass interaction model (KIM) was applied to characterize and parameterize non-ideal solution behavior and concentration-dependent water uptake by atmospheric aerosol samples in the 5–99.4% RH range. Based on KIM, the volume-based hygroscopicity parameter, &kappa; v , was calculated. The &kappa; v, ws value related to the water soluble (ws) fraction was estimated to be ~ 0.15 for the accumulation mode and ~ 0.36 for the coarse mode, respectively. The obtained &kappa; v, ws for the accumulation mode is in good agreement with earlier data reported for remote sites in the Amazon rain forest (&kappa; v &approx; 0.15) and a Colorado boreal forest (&kappa; v &approx; 0.16). We used the Zdanovskii–Stokes–Robinson (ZSR) mixing rule to predict the chemical composition dependent hygroscopicity, &kappa; v, p . The obtained &kappa; v, p values overestimate the experimental FDHA-KIM-derived &kappa; v, ws by factors of 1.8 and 1.5 for the accumulation and coarse modes, respectively. This divergence can be partly explained by incomplete dissolution of the hygroscopic inorganic compounds resulting from kinetic limitations due to a sparingly soluble organic coating. The TEM and STXM-NEXAFS results indicate that aged submicron (>300 nm) and supermicron aerosol particles possess core-shell structures with an inorganic core, and are enriched in organic carbon at the mixed particle surface. The direct FDHA kinetic studies provide a bulk diffusion coefficient of water of ~ 10 &minus;12 cm 2 s &minus;1 indicating a semi-solid state of the organic-rich phase leading to kinetic limitations of water uptake and release during hydration and dehydration cycles. Overall the present ZOTTO data set, obtained in the growing season, has revealed a strong influence of organic carbon on the hygroscopic properties of the ambient aerosols. The sparingly soluble organic coating controls hygroscopic growth, phase transitions, and microstructural rearrangement processes. The observed kinetic limitations can strongly influence the outcome of experiments performed on multi-second time scales, such as the commonly applied HTDMA (Hygroscopicity Tandem Differential Mobility Analyzer) and CCNC (Cloud Condensation Nuclei Counter) measurements.

54 ENVIRONMENTAL SCIENCES↗

Influence of Packing Atmosphere on the Microstructures and Transport Properties of Bi-2223/AgAu Tapes

Oxygen partial pressure was the key factor to tune the phase evolution mechanism of Bi-2223 system. In order to investigate the influence of packing atmosphere on the phase formation rate of Bi-2223, microstructures‚ and the current capacity of final tapes‚ 37-filamentary Bi-2223/AgAu tapes were fabricated by powder-in-tube (PIT) process, and the powder packing process operated in the glove box under different atmosphere of pure O{sub 2}‚ air, and N{sub 2}–7.5%O{sub 2}, with the oxygen partial pressure of 100%‚ 25%, and 7.5%, respectively. With different packing atmosphere, the phase formation rate of Bi-2223 increased obviously during the first heat treatment process (HT1). While, based on the same HT1 process, the maximum Bi-2223 phase content was obtained in the tapes with packing atmosphere of N{sub 2}–7.5%O{sub 2}‚ which should be attributed to the suitable Bi-2223 content and distribution. Due to the improvement of superconducting phase content and better texture structure, the critical current density increased with decreasing oxygen partial pressure of packing atmosphere and the maximum value of 19.9 kA/cm{sup 2} was reached. Moreover‚ the in-field current capacities of these Bi-2223/AgAu tapes have also been enhanced with low oxygen partial pressure in packing atmosphere, attributed to the improvements of intergrain connectivity.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructural and wear properties of sputtered carbides and silicides

Sputtered Cr3C2, Cr3Si2, and MoSi2 wear-resistant films (0.05 to 3.5 microns thick) were deposited on metal and glass surfaces. Electron transmission, electron diffraction, and scanning electron microscopy were used to determine the microstructural appearance. Strong adherence was obtained with these sputtered films. Internal stresses and defect crystallographic growth structures of various configurations within the film have progressively more undesirable effects for film thicknesses greater than 1.5 microns. Sliding contact and rolling element bearing tests were performed with these sputtered films. Bearings sputtered with a duplex coating (0.1-micron-thick undercoating of Cr3Si2 and subsequently 0.6-micron coating of MoS2) produced marked improvement over straight MoS2 films.

Spalvins, T.↗

Microstructural and wear properties of sputtered carbides and silicides

Sputtered Cr3C2, Cr3Si2, and MoSi2 wear-resistant films (0.05 to 3.5 microns thick) were deposited on metal and glass surfaces. Electron transmission, electron diffraction, and scanning electron microscopy were used to determine the microstructural appearance. Strong adherence was obtained with these sputtered films. Internal stresses and defect crystallographic growth structures of various configurations within the film have progressively more undesirable effects for film thicknesses greater than 1.5 microns. Sliding contact and rolling-element bearing tests were also performed with these sputtered films.

Spalvins, T.↗

Relationship between microstructure and mechanical properties of M50 ultra-high strength steel via quenching-partitioning-tempering process

Highlights: • The impact energy of M50 steels treated by QPT process increases by 35–93% than QT. • Cracks distribution inside impact fracture specimens is studied by 3D X-ray tomography. • The work indicates that QPT process can be applied to high-C steel with little Si. Novel quenching-partitioning-tempering (Q-P-T) and traditional quenching-tempering (Q-T) processes are conducted for M50 ultra-high strength steel. An excellent combination of strength and toughness is obtained via the Q-P-T process. The highest impact absorption energy of the Q-P-T specimen increases by 93% compared to the Q-T specimen. However, the yield and ultimate tensile strength of Q-P-T specimens are almost the same as those of Q-T specimens. Microstructure analysis indicates that the maximum fraction of retained austenite in the Q-P-T specimen is 7.5%, which is much higher than that in the Q-T (2.0%) specimen. Meanwhile, more fine cracks appear in the fracture Q-P-T specimen. The precipitation of fine and diffuse ω phase, Fe{sub 3}C and Cr{sub 23}C{sub 6} is observed during the partitioning process. The present work also reveals that the Q-P-T/Q-P process can be applied to high‑carbon steel with little Si or Al.

36 MATERIALS SCIENCE↗

Effect of calcination temperature on microstructure and magnetic properties of Ni{sub 0.5}Zn{sub 0.25}Cu{sub 0.25} Fe{sub 2}O{sub 4} nanoparticles synthesized by sol-gel method

This paper examines the effect of calcination process on the structural and magnetic properties material nanostructure composite of Ni{sub 0Ð}œ‡{sub 5}Zn{sub 0Ð}œ‡{sub 25}Cu{sub 0.25} Fe{sub 2}O{sub 4} ferrites. The samples were successfully prepared by sol-gel method at different calcination temperature, which are 600°C, 700°C, 800°C and 900°C. Morphological investigation, average crystallite size and microstructure of the material were examined by using X-ray diffraction (XRD) and confirmed by high resolution transmission electron microscope (HRTEM) and field emission scanning electron microscope (FESEM). The effects of calcination temperature on the magnetic properties were calculated by using vibrating sample magnetometer (VSM). The XRD result shows single-phase cubic spinel structure with interval average size 5.9-38 nm, and grain size microstructure of the material was increasing with temperature increases. The highest magnetization saturation was reached at a temperature 800°C with value 53.89 emu/g, and the value coercive force (Hc) was inversely with the grain size.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and Mechanical Properties of Copper Billets Fabricated by the Repetitive Extrusion and Free Forging Process

In the present study, with the aim of obtaining a weakened texture, grain refinement and improved mechanical properties, copper billets were successfully fabricated using the severe plastic deformation method of repetitive extrusion and free forging (REFF) without using any additional tools or devices. The evolution of the microstructure, texture and mechanical behavior of the ultrafine grain copper billets over an increasing number of REEF cycles was also systematically studied. Our results show that the effective strain per REFF process was ε = 2.35. After two cycles of REFF process, the sum effective strain became ε = 4.7, leading to high efficiency of grain refinement. The grain size was refined from 50 to 0.8 μm; the yield strength was increased to 462 MPa, and we obtained a weakened texture in the pure copper billets. By increasing the number of cycles, the grain refinement ability was decreased, and the texture was thus strengthened further. Therefore, two cycles of REFF were a reasonable process for producing ultrafine-grained copper billets.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Study of microstructure and electrical properties of bulk YBCO prepared by melt textured growth technique

Bulk YBCO components were prepared using Melt Texture Growth (MTG) technique. Components were fabricated using MTG by addition of Y{sub 2}BaCuO{sub 5} (Y211) and Ag to YBCO, which leads to improved grain size without affecting superconducting properties. Green compacts prepared by cold isostatic pressing were pre-sintered at 930°C before subjecting melt texturing. Cooling rates lower than 1 °C.h{sup −1} was used, in between (peritectic) temperature of about 995 and 1025°C, to obtain large grained components. Microstructure studies in details were carried out by Scanning Electron Microscope (SEM), Electron Probe Micro Analysis (EPMA), Orientation Imaging Microscope (OIM) and TEM correlated with electrical properties like Critical current density (J{sub c})

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A Comparative Study on Microstructure, Mechanical and Tribological Properties of A4, AE41, AS41 and AJ41 Magnesium Alloys

Microstructure, tensile and wear properties of as-cast A4 (Mg-4Al), AE41 (Mg-4Al-0.5Ce-0.5La), AS41 (Mg-4Al-1Si) and AJ41 (Mg-4Al-1Sr) alloys were investigated, and the results were compared with each other in this study. Microstructures were investigated by XRD, optical and scanning electron microscopes. Tensile tests were conducted at both room and elevated temperatures. Tribological properties were examined by pin-on-disk wear tests under different applied loads. Microstructure characterizations revealed that the volume fraction of second phases considerably increased by alloying additions of 1 wt.% Ce/La, Si and Sr. The microstructure of A4 alloy consisted of α-Mg grains and divorced β-Mg{sub 17}Al{sub 12} phases. After individual alloying additions of 1 wt.% Ce/La, Si and Sr, the secondary phases were primarily replaced by needle-shaped and massive blocky-shaped Al{sub 11}(Ce,La){sub 3} phases in AE41 alloy, Chinese-script-type Mg{sub 2}Si phases in AS41 alloy and divorced globular-like and massive blocky-shaped Al{sub 4}Sr and (Mg,Al){sub 17}Sr{sub 2} phases in AJ41 alloy. The tensile tests showed that at both room and elevated temperatures alloying additions of 1 wt.% Ce/La, Si and Sr resulted in an increase in the strength but a decrease in the ductility. Among the studied alloys, AS41 alloy exhibited the best strength. Wear test results showed that AE41 and AJ41 alloys similarly exhibited the best wear resistance owing to the presence of hard and dense intermetallics. Abrasion was the main wear mechanism under low applied loads while delamination, adhesion and oxidation mechanisms were majorly observed under high applied loads.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of the AA7075 Tube Fabricated using Shear Assisted Processing and Extrusion (ShAPE)

Shear Assisted Processing and Extrusion (ShAPE) experimental setup and tooling were adopted for extruding thin-walled AA7075 aluminum tube from as-cast non-homogenized billet material in a single run. The mechanical and microstructural characterizations were performed on the extrudate in the as-extruded condition without subsequent heat treating. It was shown that the ShAPE process developed a significantly refined microstructure with uniform and almost equiaxed grain structure on both hoop and axial cross-sections of the extrudate as well as through the thickness of the material. The pole figures and inverse pole figures of the EBSD data showed an strong shear texture development, and it was found out that axial shear is the dominant deformation mechanism in the regions near the inner surface of the tube, while combined axial and torsional shears are the two dominant modes of deformation near the outer surface of the extrudate. As for the mechanical properties, there was an increase of 150% and 73% in the yield and ultimate strengths of the tube produced using ShAPE process, respectively, and a 18% decrease in maximum uniform plastic elongation compared to the conventionally extruded AA7075-O tube.

Shear Assisted Processing and Extrusion, Friction ↗

Analyzing the Effect of CeB{sub 6} on Microstructure and Mechanical Properties of High-Speed Steel Consolidated by Powder Metallurgy

By adding various amounts of CeB{sub 6}, high-speed steel (M3:2) was consolidated by powder metallurgy in the form of sintering. The addition of CeB{sub 6} improved the density of the sintered steel and the formation of M{sub 6}C phase in microstructure. It is speculated that CeB{sub 6} was decomposed into boron and cerium. Boron atoms were enriched in M{sub 6}C carbide phases, but cerium atoms were mainly clustered on grain boundary while they were converted to oxides, whereby the mechanical properties were improved. For example, upon the sintering at 1210 °C, relative density ~ 98.5% and average grain size ~ 18 μm were obtained with CeB{sub 6} content at 0.3 wt.%. Excellent mechanical properties, e.g., the Rockwell hardness ~ 52 HRC, flexural strength ~ 3.05 GPa, and fracture toughness ~ 40.92 MPa m{sup 1/2}, were achieved in the sample containing 0.3 wt.% CeB{sub 6}, which implies accordingly remarkable increases by 23.5, 38.1, and 23.7%, of the properties compared with those in the sample free of CeB{sub 6}.

36 MATERIALS SCIENCE↗

Manufacture, microstructure and mechanical properties of Mo-W-N nanostructured hard films

Mo{sub 1-x}W{sub x}N{sub y} (x = 0-0.67) hard films were fabricated on wafers of silicon and high speed steel by dc magnetron sputtering technique. The effect of tungsten concentration on the phase composition, microstructure, surface morphology, hardness, adhesion, and corrosion resistance of the films was studied by X-ray diffraction, scanning electron microscopy, nano-indentation, and scratch test. It was found that if the W concentration (x) in the film is in the range of 0-0.52, the films exhibit fcc (Mo,W)N{sub y} single phase where larger W atoms substituted Mo atoms in fcc MoN{sub y}. At higher x values (x > 0.52) the films exhibit a two-phase structure consisting of fcc (Mo,W)N{sub y} and pure bcc tungsten phase. The hardness of the Mo{sub 1-x}W{sub x}N{sub y} films increases at first with increasing x, and then decreases after passing a maximum. The maximum hardness of 47 GPa is obtained at x = 0.37 corresponding to an adhesion strength of 60 N. The Mo-W-N coated high speed steel has a lower corrosion current density and higher corrosion potential than the bare high speed steel substrates.

36 MATERIALS SCIENCE↗

Changes in the microstructure and mechanical properties of additively manufactured AlSi10Mg alloy after exposure to elevated temperatures

Highlights: • Elevated temperatures above 120 °C brought changes to the AM AlSi10Mg alloy. • A maximum hardness state obtained at 160 °C/5 h was thoroughly tested. • Hardness increased by 15% and TYS by 5%, but elongation dropped by 60%. • Pure Si precipitates were responsible for the observed changes. - Abstract: The additive manufacture (AM) of the AlSi10Mg alloy has become the subject of considerable attention, especially for production of complex parts in engines. Because such parts can be exposed to elevated temperatures during operation, material stability is very important, but as yet little is known about it in relation to AM. Here, we studied changes of the AlSi10Mg alloy produced by selective laser melting (SLM) after its exposure to temperatures between 120 and 180 °C. At each temperature, hardness evolution was measured, with hardness increasing over time. The maximum hardness state obtained at 160 °C was selected for further studies comprising microstructural analysis by scanning and transmission electron microscopy, chemical composition analysis and mechanical properties assessment. Transmission microscopy revealed nano-scale acicular precipitates that caused a slight increase in the yield strength of the alloy together with a significant drop in elongation. Electron energy loss spectroscopy (EELS) and energy dispersive spectroscopy (EDS) showed that the precipitates surprisingly consisted of pure Si. To provide a comparison, conventional regimes of heat treatment (stress-relief and T6) were applied. Despite a considerable loss in mechanical performance, thermal instability was no longer observed. Overall, our results indicate that operating temperatures are a key factor in ensuring the smooth operation of AM parts of the AlSi10Mg alloy. In respect to that, we offer recommendations for their industrial use.

36 MATERIALS SCIENCE↗