Effects of B additions in FePt and FePt:C films

B was co-sputtered with FePt films, leading to a granular structure; however, in addition to segregating at grain boundaries, local bonding of Fe-B was formed, which suppressed the ordering of FePt and thus degraded the perpendicular anisotropy. A boron capping layer was deposited on FePt:C (28 vol. %) films and B diffused into FePt:C grain boundaries during post-annealing. FePt:(B, C) films revealed a reduced grain size of 5.5 nm and perpendicular coercivity of 2T. Co-additions of B and C into FePt films may provide an alternative tuning knob to manipulate the microstructure and magnetic anisotropy of FePt films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of capping material on interfacial ferromagnetism in FeRh thin films

The role of the capping material in stabilizing a thin ferromagnetic layer at the interface between a FeRh film and cap in the nominally antiferromagnetic phase at room temperature was studied by x-ray magnetic circular dichroism in photoemission electron microscopy and polarized neutron reflectivity. These techniques were used to determine the presence or absence of interfacial ferromagnetism (FM) in films capped with different oxides and metals. Chemically stable oxide caps do not generate any interfacial FM while the effect of metallic caps depends on the element, showing that interfacial FM is due to metallic interdiffusion and the formation of a ternary alloy with a modified antiferromagnetic to ferromagnetic transition temperature.

36 MATERIALS SCIENCE↗

Local atomic structure inheritance in Ag{sub 50}Sn{sub 50} melt

Local structure inheritance signatures were observed during the alloying process of the Ag{sub 50}Sn{sub 50} melt, using high-temperature X-ray diffraction and ab initio molecular dynamics simulations. The coordination number N{sub m} around Ag atom is similar in the alloy and in pure Ag melts (N{sub m} ∼ 10), while, during the alloying process, the local structure around Sn atoms rearranges. Sn-Sn covalent bonds were substituted by Ag-Sn chemical bonds, and the total coordination number around Sn increases by about 70% as compared with those in the pure Sn melt. Changes in the electronic structure of the alloy have been studied by Ag and Sn K-edge X-ray absorption spectroscopy, as well as by calculations of the partial density of states. We propose that a leading mechanism for local structure inheritance in Ag{sub 50}Sn{sub 50} is due to s-p dehybridization of Sn and to the interplay between Sn-s and Ag-d electrons.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Enhancement of exchange bias and training effect in ion-beam sputtered Fe{sub 46}Mn{sub 54}/Ni{sub 81}Fe{sub 19} bilayers

We present a remarkable enhancement by 300% of the exchange-bias field at room temperature, without affecting the coercivity value, via optimum magnetic annealing (250 °C/3 kOe) in ion-beam sputtered FeMn(30 nm)/NiFe(10 nm) bilayers. This specific behavior has been attributed to a higher degree of γ-FeMn(111) orientation that offers more interfacial FeMn moments to get pinned with the moments of the adjacent NiFe layer. Unlike the absence of training effect at room temperature, a pronounced training effect and an accompanying magnetization reversal asymmetry are evidenced upon field cooling below 50 K due to the presence of biaxial exchange induced anisotropy across the interdiffused FeMn/NiFe interface. The present findings not only have technological significance but also are of relevance to the understanding of interfacial spin disorder and frustration in these exchange-biased systems.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Co{sub 2}FeAl Heusler thin films grown on Si and MgO substrates: Annealing temperature effect

10 nm and 50 nm Co{sub 2}FeAl (CFA) thin films have been deposited on MgO(001) and Si(001) substrates by magnetron sputtering and annealed at different temperatures. X-rays diffraction revealed polycrystalline or epitaxial growth (according to CFA(001)[110]//MgO(001)[100] epitaxial relation) for CFA films grown on a Si and on a MgO substrate, respectively. For these later, the chemical order varies from the A2 phase to the B2 phase when increasing the annealing temperature (T{sub a}), while only the A2 disorder type has been observed for CFA grown on Si. Microstrip ferromagnetic resonance (MS-FMR) measurements revealed that the in-plane anisotropy results from the superposition of a uniaxial and a fourfold symmetry term for CFA grown on MgO substrates. This fourfold anisotropy, which disappears completely for samples grown on Si, is in accord with the crystal structure of the samples. The fourfold anisotropy field decreases when increasing T{sub a}, while the uniaxial anisotropy field is nearly unaffected by T{sub a} within the investigated range. The MS-FMR data also allow for concluding that the gyromagnetic factor remains constant and that the exchange stiffness constant increases with T{sub a}. Finally, the FMR linewidth decreases when increasing T{sub a}, due to the enhancement of the chemical order. We derive a very low intrinsic damping parameter (1.1×10{sup −3} and 1.3×10{sup −3} for films of 50 nm thickness annealed at 615 °C grown on MgO and on Si, respectively)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Correlation between medium-range order structure and glass-forming ability for Al-based metallic glasses

To clarify the correlation of medium-range order (MRO) structure with glass forming ability (GFA) of Al-based metallic glasses, Al{sub 86}Ni{sub 14-a}Y{sub a} (a = 2∼9 at. %) metallic glasses were analyzed by x-ray diffraction in detail and further verified by synchrotron high-energy x-ray diffraction. The prepeak that reflects the MRO structural evolution was found to be much sensitive to alloy composition. We have proposed an icosahedral supercluster MRO structure model in Al-TM (transition metal)-RE (rare earth metal) system, which consists of 12 RE(TM)-centered clusters on the vertex of icosahedral supercluster, one RE(TM)-centered clusters in the center, and TM(RE) atoms located at RE(TM)-centered cluster tetrahedral interstices in the icosahedral supercluster. It was indicated that the MRO structural stability mainly depends on the interaction of efficient dense packing and electrochemical potential equalization principle. The Al{sub 86}Ni{sub 9}Y(La){sub 5} alloys present good GFA due to the combination of the two structural factors.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Low beryllium content Zr-based bulk metallic glass composite with plasticity and work hardenability

A modified Zr-based bulk metallic glass matrix composite Zr{sub 47.67}Cu{sub 40}Ti{sub 3.66}Ni{sub 2.66}Be{sub 6} has been produced by increasing the contents of elements of Zr and Cu with higher Poisson ratio and reducing the contents of Ti, Ni, and Be elements with lower Poisson ratio based on famous metallic glass former Vitreloy 1. A compressive yielding strength of 1804 MPa, fracture strength of 1938 MPa and 3.5% plastic strain was obtained for obtained metallic glass composite. Also, work-hardening behavior was observed during compressive experiment which was ascribed to the interaction of the in situ precipitated CuZr phase and shear bands.

36 MATERIALS SCIENCE↗

Magnetic behaviors in melt spun Fe{sub 52−x}Mn{sub 23+x}Ga{sub 25} (x = 0–3) ribbons

The effect of volume fraction of B2-type ferromagnetic (FM) phase on magnetic behavior of melt-spun Fe{sub 52−x}Mn{sub 23+x}Ga{sub 25} (x = 0, 1, 2, and 3) ribbons has been investigated. X-ray diffraction (XRD) results show that the volume fraction of the B2 phase is decreased, accompanied by the increased antiferromagnetic (AFM) fcc phase, with increasing x. The magnetization isotherms of these ribbons at different temperatures demonstrate that there exists a critical field H{sub CR} from AFM to FM state, and the H{sub CR} decreases and vanishes finally with increasing temperature. High exchange bias field (H{sub EB}) at 10 K through a cooling field at H{sub CR} from 300 K could be found and correlated to the volume fraction of B2-type FM phase. Both H{sub CR} and H{sub EB} are increased with decreasing the amount of B2-type FM phase. The H{sub CR} is increased from 20 kOe for x = 0 to 50 kOe for x = 3, and H{sub EB} is increased from 0.9 kOe for x = 0 to 2.5 kOe for x = 2. The latter phenomenon might be attributed to the change of exchange interactions at FM/AFM interfaces due to the change of proportion of FM and AFM phase at low temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of metastable crystal structure for Co-Pt alloy thin film by x-ray diffraction

Co{sub 50}Pt{sub 50} and Co{sub 75}Pt{sub 25} (at. %) alloy epitaxial films with the close-packed plane parallel to the substrate surface are prepared on MgO(111) substrates with and without Ti(0001) underlayer at 300 °C. The structural properties are investigated by using a combination of out-of-plane, in-plane, and pole-figure x-ray diffractions. The crystal structure is determined by taking into account the order degree and the atomic stacking sequence of close-packed plane. Formation of a metastable ordered fcc-based L1{sub 1}-CoPt phase is recognized for the Co{sub 50}Pt{sub 50} film deposited on MgO(111) substrate, whereas a metastable ordered hcp-based B{sub h}-CoPt phase is involved in the Co{sub 50}Pt{sub 50} film deposited on Ti(0001) underlayer in addition to an L1{sub 1}-CoPt phase. The Co{sub 75}Pt{sub 25} film deposited on MgO(111) consists of a mixture of ordered hcp-based phases of B{sub h}-CoPt and D0{sub 19}-Co{sub 3}Pt. An accurate order degree is calculated by comparing the out-of-plane superlattice and fundamental reflection data. A simplified method for estimating the order degree, where there are only two kinds of parameter: intensity ratio of superlattice to fundamental reflection and out-of-plane lattice spacing, is also proposed. The order degree estimated by the simplified method agrees in a small error less than a few percentages with the accurate value.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Mixing antiferromagnets to tune NiFe-[IrMn/FeMn] interfacial spin-glasses, grains thermal stability, and related exchange bias properties

Spintronics devices and in particular thermally assisted magnetic random access memories require a wide range of ferromagnetic/antiferromagnetic (F/AF) exchange bias (EB) properties and subsequently of AF materials to fulfil diverse functionality requirements for the reference and storage. For the reference layer, large EB energies and high blocking temperature (T{sub B}) are required. In contrast, for the storage layer, mostly moderate T{sub B} are needed. One of the present issues is to find a storage layer with properties intermediate between those of IrMn and FeMn and in particular: (i) with a T{sub B} larger than FeMn for better stability at rest-T but lower than IrMn to reduce power consumption at write-T and (ii) with improved magnetic interfacial quality, i.e., with reduced interfacial glassy character for lower properties dispersions. To address this issue, the EB properties of F/AF based stacks were studied for various mixed [IrMn/FeMn] AFs. In addition to EB loop shifts, the F/AF magnetic interfacial qualities and the AF grains thermal stability are probed via measurements of the low- and high-temperature contributions to the T{sub B} distributions, respectively. A tuning of the above three parameters is observed when evolving from IrMn to FeMn via [IrMn/FeMn] repetitions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Heat assisted magnetic recording with patterned FePt recording media using a lollipop near field transducer

In heat-assisted magnetic recording, optical energy is transferred to a small optical spot on the recording media using a near field transducer. In this study, a scattered field finite difference time domain simulation is used to analyze the performance of a lollipop transducer in heat assisted magnetic recording on both a patterned FePt media and a continuous thin film. To represent wear, sharp corners of the peg are approximated with curved ones, which are found to narrow the track width without excessive loss of intensity. Compared with continuous media, the patterned media exhibits higher energy efficiency and a better concentrated optical beam spot. This effect is due to the near field effects of patterned media on the performance of the transducer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Ag addition to L1{sub 0} FePt and L1{sub 0} FePd films grown by molecular beam epitaxy

L1{sub 0} ordered FePt-Ag (5 nm) and FePd-Ag (5 nm) films were grown on MgO (001) substrate at temperatures of 250–400 °C by using molecular beam epitaxy method, and their crystal and surface structures, perpendicular magnetic anisotropies and Curie temperatures were investigated. In the case of FePt-Ag, Ag addition with the amount of 10–20 at. % was effective to promote L1{sub 0} ordering and granular growth, resulting in the increase of the perpendicular magnetic anisotropy and coercivity of the FePt-Ag films. On the other hand, in the case of FePd-Ag, Ag addition changed the surface morphology from island to continuous film associated with the reductions of its coercivity and perpendicular anisotropy. The variations of lattice constants and Curie temperature with Ag addition were significantly different between FePt-Ag and FePd-Ag. For FePd-Ag, the c and a axes lattice spacings and Curie temperature gradually changed with increasing Ag content, while they unchanged for FePt-Ag. These results suggest the possibility of the formation of FePdAg alloy in FePd-Ag, while Ag segregation in FePt-Ag.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Large grain growth of Ge-rich Ge{sub 1−x}Sn{sub x} (x ≈ 0.02) on insulating surfaces using pulsed laser annealing in flowing water

We investigate Sn incorporation effects on the growth characteristics of Ge-rich Ge{sub 1−x}Sn{sub x} (x < 0.02) on SiO{sub 2} crystallized by pulsed laser annealing (PLA) in air and water. Despite the very low Sn content of 2%, Sn atoms within the GeSn layers play a role in preventing ablation and aggregation of the layers during these PLA. Raman and electron backscatter diffraction measurements demonstrate achievement of large-grain (∼800 nmϕ) growth of Ge{sub 0.98}Sn{sub 0.02} polycrystals by using PLA in water. These polycrystals also show a tensile-strain of ∼0.68%. This result opens up the possibility for developing GeSn-based devices fabricated on flexible substrates as well as Si platforms.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

X-ray nano-diffraction study of Sr intermetallic phase during solidification of Al-Si hypoeutectic alloy

The evolution of strontium (Sr) containing intermetallic phase in the eutectic reaction of Sr-modified Al-Si hypoeutectic alloy was studied with high energy synchrotron beam source for nano-diffraction experiments and x-ray fluorescence elemental mapping. Contrary to popular belief, Sr does not seem to interfere with the Twin Plane Re-entrant Edge (TPRE) growth mechanism of eutectic Si, but evolves as the Al{sub 2}Si{sub 2}Sr phase during the eutectic reaction at the boundary between the eutectic Si and Al grains.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Time resolved imaging of magnetization dynamics in hard disk writer yokes excited by bipolar current pulses

A partially built hard disk writer structure with a NiFe/CoFe/Ru/NiFe/CoFe synthetic antiferromagnetic (SAF) yoke was studied by time and vector resolved scanning Kerr microscopy. All three time dependent components of the magnetization were recorded simultaneously as a bipolar current pulse with 1 MHz repetition rate was delivered to the coil. The component of magnetization parallel to the symmetry axis of the yoke was compared at the pole and above a coil winding in the centre of the yoke. The two responses are in phase as the pulse rises, but the pole piece lags the yoke as the pulse falls. The Kerr signal is smaller within the yoke than within the confluence region during pulse cycling. This suggests funneling of flux into the confluence region. Dynamic images acquired at different time delays showed that the relaxation is faster in the centre of the yoke than in the confluence region, perhaps due to the different magnetic anisotropy in these regions. Although the SAF yoke is designed to support a single domain to aid flux conduction, no obvious flux beaming was observed, suggesting the presence of a more complicated domain structure. The SAF yoke writer hence provides relatively poor flux conduction but good control of rise time compared to single layer and multi-layered yokes studied previously.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Deformation and fracture behavior of composite structured Ti-Nb-Al-Co(-Ni) alloys

Tensile ductility of the Ti-based composites, which consist of a β-Ti phase surrounded by ultrafine structured intermetallics, is tunable through the control of intermetallics. The two Ti-based alloys studied exhibit similar compressive yield strength (about 1000 MPa) and strain (about 35%–40%) but show a distinct difference in their tensile plasticity. The alloy Ti{sub 71.8}Nb{sub 14.1}Ni{sub 7.4}Al{sub 6.7} fractures at the yield stress while the alloy Ti{sub 71.8}Nb{sub 14.1}Co{sub 7.4}Al{sub 6.7} exhibits about 4.5% of tensile plastic deformation. To clarify the effect of microstructure on the deformation behavior of these alloys, tensile tests were carried out in the scanning electron microscope. It is shown that the distribution as well as the type of intermetallics affects the tensile ductility of the alloys.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Sign change of exchange bias in [Pt/Co]{sub 3}/IrMn multilayer

The properties of exchange bias in a multilayer of [Pt(1.0 nm)/Co(1.0 nm)]{sub 2}/Pt(t{sub Pt} nm)/Co(1.0 nm)/ IrMn(12.0 nm) were investigated with a variation of Pt layer thickness, t{sub Pt}. For t{sub Pt} ≤ 1.6 nm, it was typically observed that Co layers were ferromagnetically coupled while IrMn layer exhibited negative exchange bias. With increasing Pt thickness, antiferromagnetic (AF) interlayer coupling strength increased and caused AF spin configuration between the Co layers. With further increasing of Pt thickness (t{sub Pt} = 2.5 nm), the exchange bias between Co and IrMn layers was changed from negative to positive. Therefore, a large enhancement of AF interlayer coupling induced the sign change of exchange bias from negative to positive and resulted in a drastic change of switching behavior in a magnetization reversal. Both extraordinary Hall-effect and magnetoresistance were measured to verify the exchange bias direction and spin configurations upon magnetization reversal.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural, magnetic, and electron transport properties of Mn{sub 3−x}Pt{sub x}Sn (x = 0, 0.5, 1) nanomaterials

The structural, magnetic, and electron-transport properties of Mn{sub 3−x}Pt{sub x}Sn (x = 0, 0.5, 1) nanomaterials prepared by arc-melting, melt-spinning, and annealing were investigated. It was found that the hexagonal structure is the most stable structure for Mn{sub 3}Sn and the samples show an antiferromagnetic spin order at room temperature. The Pt-containing samples are mainly tetragonal but contain a small amount of other impurity phases, including hexagonal Mn{sub 3}Sn and Mn{sub 2}Sn. At room temperature, the Pt-containing samples show ferri- or ferromagnetic spin order with a Curie temperature of about 370 K. The measured high-field magnetization and anisotropy constant for Mn{sub 2}PtSn are 405 emu/cm{sup 3} and 2.6 Mergs/cm{sup 3}, respectively. The samples are all highly conducting with metallic electron transport and show a substantial negative magnetoresistance.

36 MATERIALS SCIENCE↗