Search NASA⌕ Search

SEARCH · Search NASA

Results for “cycle performance”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,045 records · Page 58

High-Pressure Oxygen Generation for Outpost EVA

Low Lunar Orbit (LLO) poses unique thermal challenges for the orbiting space craft, particularly regarding the performance of the radiators. The emitted infrared (IR) heat flux from the lunar surface varies drastically from the light side to the dark side of the moon. Due to the extremely high incident IR flux, especially at low beta angles, a radiator is oftentimes unable to reject the vehicle heat load throughout the entire lunar orbit. One solution to this problem is to implement Phase Change Material (PCM) Heat Exchangers. PCM Heat Exchangers act as a "thermal capacitor, storing thermal energy when the radiator is unable to reject the required heat load. The stored energy is then removed from the PCM heat exchanger when the environment is more benign. Because they do not use an expendable resource, such as the feed water used by sublimators and evaporators, PCM Heat Exchangers are ideal for long duration Low Lunar Orbit missions. The Advanced Thermal Control project at JSC is completing a PCM heat exchanger life test to determine whether further technology development is warranted. The life test is being conducted on four nPentadecane, carbon filament heat exchangers. Fluid loop performance, repeatability, and measurement of performance degradation over 2500 meltfreeze cycles will be performed and reported in the current document.

Jeng, Frank↗

Impact of Charge Methodology upon the Performance of Lithium Ion Cells

This viewgraph gives an overview on the impact of charge methodology upon the performance of lithium ion cells. Charge characteristics are given on the following: (1) lithium ion prototype cells, including charge rate characteristics at different temperatures, the effect of charge methodology upon cycle life performance, the effect of charge voltage upon cell performance; (2) three-electrode cells; and (3) lithium-ion eight-cell batteries.

lithium ion cells↗

Importance of the (n,gamma) Cm-247 Evaluation on Neutron Emission in Fast Reactor Fuel Cycle Analysis

As part of the GNEP program, it is envisioned to build a fast reactor for the transmutation of minor actinides. The spent nuclear fuel from the current fleet of light water reactors would be recycled, the current baseline is the UREX+1a process, and would act as a feed for the fast reactor. As the fuel is irradiated in a fast reactor a certain quantity of minor actinides would thus build up in the fuel stream creating possible concerns with the neutron emission of these minor actinides for fuel transportation, handling and fabrication. Past neutronic analyses had not tracked minor actinides above Cm-246 in the transmutation chain, because of the small influence on the overall reactor performance and cycle parameters. However, when trying to quantify the neutron emission from the recycled fuel with high minor actinide content, these higher isotopes play an essential role and should be included in the analysis. In this paper, the influence of tracking these minor actinides on the calculated neutron emission is presented. Also presented is the particular influence of choosing a different evaluated cross section data set to represent the minor actinides above Cm-246. The first representation uses the cross-sections provided by MC2-2 for all isotopes, while the second representation uses infinitely diluted ENDF/BVII.0 cross-sections for Cm-247 to Cf-252 and MC2-2 for all other isotopes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Imaging of 3D morphological evolution of nanoporous silicon anode in lithium ion battery by X-ray nano-tomography

Nanostructured silicon with its high theoretical capacity and ability to accommodate volume expansion has attracted great attention as a promising anode material for Lithium ion (Li-ion) batteries. Liquid metal dealloying method, is a novel method to create nanoporous silicon (np-Si). The assembled Li-ion batteries based on such np- Si anode can be cycled beyond 1500 cycles, in 1000 mA h/g constant capacity cycling mode with consistent performance; however, it suffers from degradation after ~ 460 cycles, while being cycled under 2000 mA h/g. To reveal the failure mechanism and differences in the morphological evolution in different capacity cycling modes in the np-Si anode, we conducted synchrotron X-ray nano-tomography studies. The three dimensional (3D) morphological evolution was visualized and quantified as a function of the number of cycles and cycling capacities. By comparing the 3D morphology under each cycling condition and correlating these 3D morphological changes with cycling-life performance, we elucidate the failure mechanism of the np-Si electrodes resulting from a mesoscopic to macroscopic deformation, involving volume expansion and gradual delamination. In particular, the shorter cycling life in higher-capacity cycling mode stems from particle agglomeration. Overall, while the nanoporous structure can accommodate the volume expansion locally, these mesoscopic and macroscopic deformations ultimately result in heterogeneous stress distribution with faster delamination. As a result, the work thus sheds the light on the importance to consider the structural evolution at the mesoscopic and macroscopic scales, while designing nano-structured energy storage materials for enhanced performances, particularly for long cycling-life durability.

25 ENERGY STORAGE↗

Capacity decline of ambient temperature secondary Li-TiS2 cells

The main objective of the study described was to identify the causes responsible for the capacity losses observed during cycling of secondary Li-TiS2 cells. Experimental Li-TiS2 cells were fabricated and tested for their cycle life performance. The open circuit voltage of the cells was monitored during the rest period between the charging and discharging. The polarization at the Li and TiS2 electrodes was also monitored during cycling. Cycled cells were disassembled and the cathodes were analyzed by various analytical techniques. The results of the study indicate that the observed capacity loss is almost entirely due to the increased polarization of the TiS2 electrode with cycling. The electrolyte was found to degrade during cycling and the degradation products were found to deposit at the TiS2 electrode, which probably lead to the higher polarization.

Subbarao, S.↗

Performance measurement for information systems: Industry perspectives

Performance measurement has become a focal topic for information systems (IS) organizations. Historically, IS performance measures have dealt with the efficiency of the data processing function. Today, the function of most IS organizations goes beyond simple data processing. To understand how IS organizations have developed meaningful performance measures that reflect their objectives and activities, industry perspectives on IS performance measurement was studied. The objectives of the study were to understand the state of the practice in IS performance techniques for IS performance measurement; to gather approaches and measures of actual performance measures used in industry; and to report patterns, trends, and lessons learned about performance measurement to NASA/JSC. Examples of how some of the most forward looking companies are shaping their IS processes through measurement is provided. Thoughts on the presence of a life-cycle to performance measures development and a suggested taxonomy for performance measurements are included in the appendices.

Bishop, Peter C.↗

EDF's used fuel management french policy - 15199

Regarding back-end fuel cycle, EDF's strategy, implemented from the very beginning of French nuclear production, consists in reprocessing of used fuel; decision to recycle plutonium in French PWR was taken from 1984. This reprocessing and recycling strategy, relying on existing industrial facilities (AREVA La Hague and Melox plants), has proven to be reliable and efficient. Treatment leads to a stabilization of used fuel total inventory in interim storage. Vitrification process ensures a safe packaging for high level and long-lived waste under a reduced volume. Recycling of fissile materials saves natural uranium requirements. Concentration of Pu in MOX used fuel leaves open the option to reuse it for starting next Generation IV systems beyond 2040. In 2008, EDF and AREVA, supported by French Government, agreed on commercial terms covering long term fuel reprocessing and recycling (up to 2040). Currently, EDF fuel management strategy relies on flow equilibrium in order to respect fuel cycle consistency and sustainability. The underlying principle is to strictly adjust separated plutonium production to recycling possibilities (i.e. licensed reactors and MOX fuel fabrication facilities). Given that fuel cycle policy, any trend in NPP core management that may impact the fuel cycle should be anticipated within times in order to avoid technical or administrative incompatibilities, and guarantee a high level of safety and robustness. In collaboration with industrial operators, EDF have to perform periodic 'Cycle Impact' analyses and report to the French Nuclear Safety Authority (ASN); next exercise is scheduled by the end of 2016. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Thermomechanical and sequential stress performance of photovoltaic backsheets

Photovoltaic backsheet technology is utilized to protect the interior components of solar modules from environmental stress as well as provide electrical insulation to the module. The growing demand for solar energy and longer module service life requirements have brought backsheet performance into focus. Despite being a protective packaging material, many backsheets have exhibited failure in the field, limiting the performance and service life of entire modules. Most backsheets consist of multiple polymeric layers laminated together using adhesives. A new backsheet, with a high performance polyamide structure, has been developed as the solution to module failure. Primarily, it contains a unique polyamide-ionomer alloy targeted at improved weather resistance. In this study, several photovoltaic industry standard backsheets, and the novel polyamide compositions of multilayered backsheets fabricated from the coextrusion process, were examined using thermomechanical analysis (TMA). The coefficient of thermal expansion (CTE) for entire backsheets and their constituent layers was used to model the thermomechanical behavior of various backsheet constructions. Subsequently, thermal cycling was performed in the TMA to examine the intrinsic thermal behavior of the backsheets. Thermal cycling in the TMA indicates the resilience and dimensional stability in the coextruded structures as opposed to the laminated structures. Lastly, results from a Module Accelerated Sequential Testing (MAST), are included to show the mechanical integrity of these backsheets after sequential exposure to stressors including damp heat, ultra-violet (UV) light radiation, and thermal cycling. The laminate backsheets deteriorated extensively after sequential exposure to these stressors, while the novel coextruded structures retained their physical properties.

14 SOLAR ENERGY↗

Addition of Chloroform in a Solvent-in-Salt Electrolyte: Outcomes in the Microscopic Dynamics in Bulk and Confinement

Solvent-in-salt electrolytes (SISEs) are a promising alternative to the electrolytes currently used in commercial devices. Despite the SISEs’ advantages, their utilization is not yet realized due to the poor mobility of their chemical species. Here, we explore this problem by adding chloroform to a SISE formed by acetonitrile and a Li-salt. First, we performed illustrative cycling experiments to highlight the potential of this approach. Then, we focused on the description of the microscopic dynamics of the electrolytes and exposed the relevant aspects to be considered for their optimal performance. While the conductivity at low temperatures may be enhanced by the addition of chloroform, only subtle changes occur at room temperature. As revealed by molecular dynamics simulations and quasielastic neutron scattering (QENS) experiments, this effect is related to the preservation of the structure expected for a highly concentrated solution and promotion of the formation of ionic aggregates. These outcomes occur despite the increase in the overall mobility of the chemical species. The dynamics of the electrolytes in porous carbon was also investigated using QENS. In these circumstances, low concentrations of chloroform lead to diffusivities of the molecular species higher than those observed for the bulk electrolytes. As chloroform’s concentration increases, no further changes in the diffusivities are observed. Nonetheless, chloroform is mostly immobilized on the carbon surfaces and this behavior may be intensified at compositions closer to the eutectic mixture.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of electronically passivating surfaces to enhance battery performance

For many decades, lithium metal batteries (LMBs) have been studied for their high energy density, though they suffer from high reactivity, which safety concerns such as explosions and fires. These events can occur as a result of degradation due to redox reactions and lithium morphology that evolve during cycling. Mostly, the failure is caused by the electrolyte degradation leading to the creation of a solid electrolyte interphase (SEI), which tends to induce electron leakage, lithium dendrite growth, and capacity decay. SEI formation is practically inevitable. This work investigated the minimization of degradation events by modifying different battery configurations. Modifications were made by exchanging electrolytes, electrode surfaces, and even annexing innovative components. Our goal is to achieve a configuration where Li-ion transfer is facilitated, and electron transfer is limited which would enable a longer lithium metal battery life cycle. When performing these modifications and testing their electrochemical performance, a current reduction was observed when the electrodes were spontaneously coated with preformed SEI. Herein several classes of artificial SEI layers are explored for their ability to form passivating layers through use of a redox active molecule.

25 ENERGY STORAGE↗

Projection Analysis for ATR Irradiation of the AFC-FAST Experiment

Analyses of the Advanced Fuels Campaign Fission Accelerated Steady-state Test (AFC-FAST) in the Advanced Test Reactor are presented. A detailed methodology was employed to better account for uncertainties in the planned power and duration of sequential reactor loading cycles. By performing coupled depletion analyses at multiple power levels and durations, the differences in experiment heating outputs can be found. The effects of these uncertainties upon multiple experiment configurations were assessed in an effort to streamline the process of planning for and documenting future irradiations. In conclusion, the data generated from this work have been used to help inform assumptions on subsequent projections to perform only a nominal case depletion.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mg segregation in Mg-rich Mg-Ni switchable mirror studied by Rutherford backscattering, elastic recoil detection analysis, and nuclear reaction analysis

Pd/Mg{sub 3.3}Ni films were prepared by dc sputtering deposition on three different substrates of glass, diamondlike carbon/Si, and Si. Hydrogenation and dehydrogenation cycles were performed on these samples simultaneously. The optical switching property due to the hydrogenation and dehydrogenation was monitored by the transmission of laser light via the glass substrate. The switching ability was totally lost after 120 cycles. We made comparative study of the composition change between the new (as-deposited) and old (after 120 switching cycles) samples by Rutherford backscattering (RBS), elastic recoil detection analysis (ERDA), and nuclear reaction analysis (NRA). From the RBS results we found out the segregation of a Mg layer between the Pd cap layer and the rest of the Mg-Ni layer. At the Pd/Mg interface in the old sample, thin MgO layer formed probably during the dehydrogenation process with O{sub 2}. ERDA showed that there is much hydrogen in the old sample. NRA displayed the depth profiles of hydrogen distribution in the old sample. It is revealed that much hydrogen is accumulated at the interface between the Pd cap layer and the segregated Mg layer. It can be concluded that the formations of oxide and hydride of the segregated Mg layer are the main reasons for the degradation of the Mg{sub 3.3}Ni switchable mirror.

36 MATERIALS SCIENCE↗

Degradation of Commercial Lithium-Ion Cells as a Function of Chemistry and Cycling Conditions

Energy storage systems with Li-ion batteries are increasingly deployed to maintain a robust and resilient grid and facilitate the integration of renewable energy resources. However, appropriate selection of cells for different applications is difficult due to limited public data comparing the most commonly used off-the-shelf Li-ion chemistries under the same operating conditions. This article details a multi-year cycling study of commercial LiFePO 4 (LFP), LiNi x Co y Al 1–x–y O 2 (NCA), and LiNi x Mn y Co 1–x–y O 2 (NMC) cells, varying the discharge rate, depth of discharge (DOD), and environment temperature. The capacity and discharge energy retention, as well as the round-trip efficiency, were compared. Even when operated within manufacturer specifications, the range of cycling conditions had a profound effect on cell degradation, with time to reach 80% capacity varying by thousands of hours and cycle counts among cells of each chemistry. The degradation of cells in this study was compared to that of similar cells in previous studies to identify universal trends and to provide a standard deviation for performance. All cycling files have been made publicly available at batteryarchive.org, a recently developed repository for visualization and comparison of battery data, to facilitate future experimental and modeling efforts.

25 ENERGY STORAGE↗

Impacts of Recycling Time on Fuel Cycle Transition

The purpose of this work is to show the importance of assumptions regarding the recycling time for time-dependent fuel cycle scenarios that involve transition from the current state of the U.S. fuel cycle to cycles based on continuous recycling via fast reactors. The recycling time is defined here as the total time between when the fuel is discharged from the reactor core and when its recovered heavy metals (HM) are recycled back into the core as part of the fresh/new fuel. The main processes occurring within the recycling time include cooling, separations, and fuel fabrication. The minimum recycling time required for fast reactor fuel largely depends on the minimum cooling time, which will be longer if discharged fuel needs to be moved to a centrally-located separations facility. A longer cooling time is needed for the heat load and fuel characteristics to reach safer levels for handling and transportation. Therefore, if the separation and fabrication facilities were co-located with reactors on-site, then the total recycling time could be reduced by several years. For fuel cycle transition scenarios in which external fissile materials (Pu or TRU) are limiting, these longer recycling times may prolong the transition to the continuous recycling system of fast reactors as well as impact the fuel cycle system performance during the transition. Therefore, in order to demonstrate the quantitative impacts of these recycling time assumptions, an example scenario of transition to the fast reactor fleet with continuous recycle was modeled in the fuel cycle systems code DYMOND. It must be emphasized that this is a point study that demonstrates how a longer recycling time can impact the rate of transition under specific conditions and assumptions. For alternative scenarios, such as those in which there are no fissile material constraints, there are likely no significant impacts due to recycling time. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Honeycomb-Layered Oxide Cathode for Sodium-Ion Batteries with Suppressed P3-O1 Phase Transition

Mg–substituted Na 3 Ni 2–x Mg x SbO 6 cathode materials are synthesized via a scalable high–temperature solid–state method to improve the cyclability of the honeycomb–layered oxide cathode in sodium–ion batteries. Here, the partial substitution of Ni 2+ by Mg 2+ in the transition–metal layer suppresses the electrochemically unfavorable P3–O1 transition and enlarges the lattice parameters to bring improved performance with respect to capacity retention, Coulombic efficiency, and Na (de)intercalation kinetics.

25 ENERGY STORAGE↗

Water-Based Electrode Manufacturing and Direct Recycling of Lithium-Ion Battery Electrodes—A Green and Sustainable Manufacturing System

It is critical to develop a low-cost and environmentally friendly system to manufacture and recycle lithium-ion batteries (LIBs) as the demand on LIBs keeps increasing dramatically. Conventional LIB cathodes are manufactured using N-methyl-2-pyrrolidone as the solvent, which is expensive, highly toxic, flammable, and energy intensive to produce and recover. Ideally, a close-loop industrial supply chain should be built, in which the batteries are manufactured, market harvested, and recycled with minimal external toxic solvent through the whole system. This work demonstrates a green and more sustainable manufacturing method for LIBs where no hazardous organic solvent is used during electrode manufacturing and recycling. The electrodes fabricated via water-based processing demonstrate comparable rate performance and cycle life to the ones from conventional solvent-based processing. Utilization of a water-soluble binder enables recovering the cathode compound from spent electrodes using water, which is successfully regenerated to deliver comparable electrochemical performance to the pristine one.

25 ENERGY STORAGE↗

Improved performance through tight coupling of redox cycles of sulfur and 2,6-polyanthraquinone in lithium–sulfur batteries

Lithium–sulfur (Li–S) batteries offer high theoretical capacity and energy density; however, complex nanoengineered cathodes have been required to suppress the unwanted polysulfide shuttling. The textural complexity of such electrodes hinders detailed understanding of their function, impeding the development of new materials. In this report, the redox-active polymer 2,6-polyanthraquinone (PAQ) was incorporated into the cathode. The presence of this polymer improves capacity retention in galvanostatic cycling and inhibits Li corrosion and S deposition. In conclusion, we show that redox reactions of this polymer are strongly coupled to the S redox cycle and hypothesize that the observed improvements in the performance originate from the electrocatalytic inhibition of polysulfide shuttling in this system.

25 ENERGY STORAGE↗

Mid-Infrared Reflectance Imaging of Thermal-Barrier Coatings

An apparatus for mid-infrared reflectance imaging has been developed as means of inspecting for subsurface damage in thermal-barrier coatings (TBCs). The apparatus is designed, more specifically, for imaging the progression of buried delamination cracks in plasma-sprayed yttria-stabilized zirconia coatings on turbine-engine components. Progression of TBC delamination occurs by the formation of buried cracks that grow and then link together to produce eventual TBC spallation. The mid-infrared reflectance imaging system described here makes it possible to see delamination progression that is invisible to the unaided eye, and therefore give sufficiently advanced warning before delamination progression adversely affects engine performance and safety. The apparatus (see figure) includes a commercial mid-infrared camera that contains a liquid-nitrogen-cooled focal plane indium antimonide photodetector array, and imaging is restricted by a narrow bandpass centered at wavelength of 4 microns. This narrow wavelength range centered at 4 microns was chosen because (1) it enables avoidance of interfering absorptions by atmospheric OH and CO2 at 3 and 4.25 microns, respectively; and (2) the coating material exhibits maximum transparency in this wavelength range. Delamination contrast is produced in the midinfrared reflectance images because the introduction of cracks into the TBC creates an internal TBC/air-gap interface with a high diffuse reflectivity of 0.81, resulting in substantially higher reflectance of mid-infrared radiation in regions that contain buried delamination cracks. The camera is positioned a short distance (.12 cm) from the specimen. The mid-infrared illumination is generated by a 50-watt silicon carbide source positioned to the side of the mid-infrared camera, and the illumination is collimated and reflected onto the specimen by a 6.35-cm-diameter off-axis paraboloidal mirror. Because the collected images are of a steady-state reflected intensity (in contrast to the transient thermal response observed in infrared thermography), collection times can be lengthened to whatever extent needed to achieve desired signal-to-noise ratios. Each image is digitized, and the resulting data are processed in several steps to obtain a true mid-infrared reflectance image. The raw image includes thermal radiation emitted by the specimen in addition to the desired reflected radiation. The thermal-radiation contribution is eliminated by subtracting the image obtained with the illumination off from the image obtained with the illumination on. A flat-field correction is then made to remove the effects of non-uniformities in the illumination level and pixel-to-pixel variations in sensitivity. This correction is performed by normalizing to an image of a standard object that has a known reflectance at a wavelength of 4 microns. After correction, each pixel value is proportional to the reflectance (at a wavelength of 4-microns) at the corresponding location on the specimen. Mid-infrared reflectance imaging of specimens that were thermally cyc led for different numbers of cycles was performed and demonstrated t hat mid-infrared reflectance imaging was able to monitor the gradual delamination progression that occurs with continued thermal cycling . Reproducible values were obtained for the reflectance associated w ith an attached and fully delaminated TBC, so that intermediate refle ctance values could be interpreted to successfully predict the numbe r of thermal cycles to failure.

Edlridge, Jeffrey I.↗