Study of advanced composite structural design concepts for an arrow wing supersonic cruise configuration, task 3

A structural design study was conducted to assess the relative merits of structural concepts using advanced composite materials for an advanced supersonic aircraft cruising at Mach 2.7. The configuration and structural arrangement developed during Task I and II of the study, was used as the baseline configuration. Allowable stresses and strains were established for boron and advanced graphite fibers based on projected fiber properties available in the next decade. Structural concepts were designed and analyzed using graphite polyimide and boron polyimide, applied to stiffened panels and conventional sandwich panels. The conventional sandwich panels were selected as the structural concept to be used on the wing structure. The upper and lower surface panels of the Task I arrow wing were redesigned using high-strength graphite polyimide sandwich panels over the titanium spars and ribs. The ATLAS computer system was used as the basis for stress analysis and resizing the surface panels using the loads from the Task II study, without adjustment for change in aeroelastic deformation. The flutter analysis indicated a decrease in the flutter speed compared to the baseline titanium wing design. The flutter analysis indicated a decrease in the flutter speed compared to the baseline titanium wing design. The flutter speed was increased to that of the titanium wing, with a weight penalty less than that of the metallic airplane.

Source record↗

Synthesis of perfluoroalkylene aromatic diamines

Analogues of methylene dianilines were synthesized, in which the methylene group between the two aromatic nuclei was replaced by various perfluoroalkylene linkage. The hydrolytic thermal, and thermal oxidative stabilities of PMR Polyimides derived from these diamines were determined. Three types of PMR Polyimide discs were fabricated from the dimethyl ester of 3,3', 4,4'-benzophenonetetracarboxylic acid, the methyl ester of 5-norbornene-2,3-dicarboxylic acid, and one of the following three diamines: methyl dianiline, 1,3-bis(4-aminophenyl)hexafluoropropane, and 2,2-bis(4-aminophenyl)hexafluoropropane. The polyimide based on 2,2-bis(4-aminophenyl)hexafluoropropane exhibited the best hydrolytic, thermal, and thermal oxidative stability as determined by moisture uptake and thermogravimetric analysis.

Paciorek, K. L.↗

High temperature adhesives for bonding Kapton

Experimental polyimide resins have been developed and evaluated as potential high temperature adhesives for bonding Kapton polyimide film. Lap shear strengths of 'Kapton'/'Kapton' bonds were obtained as a function of test temperature, adherend thickness, and long term aging at 575K (575 F) in vacuum. Glass transition temperatures of the polyimide/'Kapton' bondlines were monitored by thermomechanical analysis.

Saint Clair, A. K.↗

Solvent resistant thermoplastic aromatic poly(imidesulfone) and process for preparing same

A process for preparing a thermoplastic poly(imidesulfone) is disclosed. This resulting material has thermoplastic properties which are generally associated with polysulfones but not polyimides, and solvent resistance which is generally associated with polyimides but not polysulfones. This system is processable in the 250 to 350 C range for molding, adhesive and laminating applications. This unique thermoplastic poly(imidesulfone) is obtained by incorporating an aromatic sulfone moiety into the backbone of an aromatic linear polyimide by dissolving a quantity of a 3,3',4,4'-benzophenonetetracarboxylic dianhydride (BTDA) in a solution of 3,3'-diaminodiphenylsulfone and bis(2-methoxyethyl)ether, precipitating the reactant product in water, filtering and drying the recovered poly(amide-acid sulfone) and converting it to the poly(imidesulfone) by heating.

St.clair, T. L.↗

High density circuit technology, part 2

A multilevel metal interconnection system for very large scale integration (VLSI) systems utilizing polyimides as the interlayer dielectric material is described. A complete characterization of polyimide materials is given as well as experimental methods accomplished using a double level metal test pattern. A low temperature, double exposure polyimide patterning procedure is also presented.

Wade, T. E.↗

Development of partially fluorinated resin apex seals

Partially fluorinated polyimides were prepared and molded in the form of discs and pins for test as potential apex seal materials for advanced rotary combustion engines. The polyimides were formulated from the diamine 2,2-bis 4-(4-aminophenoxy)phenyl hexafluoropropane (4-BDAF) and the dianhydrides of pyromellitic acid (PMDA) and benzophenonetetracarboxylic acid (BTDA). Tribological testing was performed at sliding speeds of 0.31 to 11.6 m/s and at temperatures of from 298K to 573K. It is shown that the carbon fiber filled polyimides, particularly the 80/20 compositions, have an excellent balance of wear/friction at 573K. The unfilled, 80/20 and 60/40 compositions indicate an unusual combination of high friction and low wear which may be advantageous in such applications as brakes and traction drives.

Green, H. E.↗

Process for preparing solvent resistant, thermoplastic aromatic poly(imidesulfone)

A process for preparing a thermoplastic poly(midesulfone) is disclosed. This resulting material has thermoplastic properties which are generally associated with polysulfones but not polyimides, and solvent resistant which is generally associated with polyimides but not polysulfones. This system is processable in the 250 to 350 C range for molding, adhesive and laminating applications. This unique thermoplastic poly(imidesulfone) is obtained by incorporating an aromatic sulfone moiety into the backbone of an aromatic linear polyimide by dissolving a quantity of a 3,3',4,4'-benzophenonetetracarboxylic dianhydride (BTDA) in a solution of 3,3'-diaminodiphenylsulfone and bis(2-methoxyethyl)ether, precipitating the reactant product in water, filtering and drying the recovered poly(amide-acid sulfone) and converting it to the poly(imidesulfone) by heating.

St.clair, T. L.↗

Ion beam sputter-deposited thin film coatings for protection of spacecraft polymers in low Earth orbit

Ion beam sputter-deposited thin films of Al2O3, SiO2, and a codeposited mixture of predominantly SiO2 with small amounts of a fluoropolymer were evaluated both in laboratory plasma ashing tests and in space on board shuttle flight STS-8 for effectiveness in preventing oxidation of polyimide Kapton. Measurements of mass loss and optical performance of coated and uncoated polyimide samples exposed to the low Earth orbital environment are presented. Optical techniques were used to measure loss rates of protective films exposed to atomic oxygen. Results of the analysis of the space flight exposed samples indicate that thin film metal oxide coatings are very effective in protecting the polyimide. Metal oxide coatings with a small amount of fluoropolymer codeposited have the additional benefit of great flexibility.

Banks, B. A.↗

Development of an impact- and solvent-resistant thermoplastic composite matrix, phase 3

The polyimide from BTDA 1,6-hexanediamine and m-phenylenediamine was selected from a prior study for the present study. Methods to prepare prepreg which would provide low void composites at low molding pressures from the thermoplastic polyimide were studied. Cresol solutions of the polyimide were applied to a balanced weave carbon fabric and the cresol removed prior to composite molding. Low void composites were prepared from smoothed prepregs at high pressures (34.5 MPa) and temperatures as low as 260 C. Lower molding pressures lead to higher void composites. Need for a lower melt viscosity in the neat resin is suggested as a requirement to achieve low void composites at low pressures. Some mechanical properties are included.

Delano, C. B.↗

Prepreg cure monitoring using diffuse reflectance-FTIR

An in situ diffuse reflectance-Fourier transform infrared technique was developed to determine infrared spectra of graphite fiber prepregs as they were being cured. A bismaleimide, an epoxy, and addition polyimide matrix resin prepregs were studied. An experimental polyimide adhesive was also examined. Samples were positioned on a small heater at the focal point of diffuse reflectance optics and programmed at 15 F/min while FTIR spectra were being scanned, averaged, and stored. An analysis of the resulting spectra provided basic insights into changes in matrix resin molecular structure which accompanied reactions such as imidization and crosslinking. An endo-exothermal isomerization involving reactive end-caps was confirmed for the addition polyimide prepregs. The results of this study contribute to a fundamental understanding of the processing of composites and adhesives. Such understanding will promote the development of more efficient cure cycles.

Young, P. R.↗

High-temperature Adhesive Development and Evaluation

High-temperature adhesive systems are evaluated for short and long-term stability at temperatures ranging from 232C to 427C. The resins selected for characterization include: NASA Langley developed polyphenylquinoxaline (PPQ), and commercially available polyimides (PI). The primary method of bond testing is single lap shear. The PPQ candidates are evaluated on 6A1-4V titanium adherends with chromic acid anodize and phosphate fluoride etch surface preparations. The remaining adhesives are evaluated on 15-5 PH stainless steel with a sulfuric acid anodize surface preparation. Preliminary data indicate that the PPQ adhesives tested have stability to 3000 hours at 450F with chromic acid anodize surface preparation. Additional studies are continuing to attempt to improve the PPQ's high-performance by formulating adhesive films with a boron filler and utilizing the phosphate fluoride surface preparation on titanium. Evaluation of the polyimide candidates on stainless-steel adherends indicates that the FM-35 (American Cyanamid), PMR-15 (U.S. Polymeric/Ferro), TRW partially fluorinated polyimide and NR 150B2S6X (DuPont) adhesives show sufficient promise to justify additional testing.

Hendricks, C. L.↗

The 371 deg C mechanical properties of graphite/polyimide composites

A series of condensation polyimides based on pyromellitic dianhydride is synthesized and evaluated for potential application at 371 C. Several three-and four-ring benzenoid diamine systems containing oxygen bridging groups are investigated. Thermomechanical analysis of neat resin specimens indicate that the polyimide prepared from the dimethyl ester of pyrometallitic acid (PMDE) and 2,2-bis4-(4'-aminophenoxy) phenyl]-1,1,1,3,3,3- hexafluoropropane (BDAF) is the only resin system which has a glass transition temperature (Tg) above 371 C. The Tg of the PMDE/BDAF polyimide is found to be 390 C after a postcure air at 371 C for 24 hr. Unidirectional composites are fabricated from the PMDE/BDAF system and unsized Celion 6000 graphite fibers. Final cure temperatures in the range of 371 to 427 C with an applied pressure of 10.34 to 13.78 MPa are investigated. The void content of the composites ranges from 4.6 to 8.6 percent. Composites cured at 399 C under a pressure of 10.34 MPa and postcured in air at 371 C for 24 hr exhibit the highest 371 C interlaminar shear strength (ILSS, 40.7 MPa) and flexural strength (758 MPa). The thermo-oxidative stability of the composites is determined by subjecting specimens to isothermal exposure at 371 C in air at atmospheric pressure, as well as a pressure of 0.52 MPa. Specimens exposed at atmospheric pressure exhibit a weight loss of 12 percent after 200 hr of exposure and 88 percent retention of its original 371 C ILSS. In contrast, the specimens exposed at 0.52 MPa pressure exhibit a comparable weight loss after only 72 hr, and a 71 percent retention of its original 371 C ILSS.

Delvigs, P.↗

Ion beam sputter-deposited thin film coatings for protection of spacecraft polymers in low earth orbit

Ion beam sputter-deposited thin films at Al2O3, SiO2, and a codeposited mixture of predominantly SiO2 with small amounts of fluoropolymer were evaluated both in laboratory plasma ashing tests and in space on board Shuttle flight STS-8 for effectiveness in preventing oxidation of polyimide Kapton. Measurements of mass loss and optical performance of coated and uncoated polyimide samples exposed to the low earth orbital environment are presented. Optical techniques were used to measure loss rates of protective films exposed to atomic oxygen. Results of the analysis of the space flight exposed samples indicate that thin film metal oxide coatings are very effective in protecting the polyimide. Metal oxide coatings with a small amount of fluoropolymer codeposited have the additional benefit of great flexibility.

Banks, B. A.↗

Preparation of bis(4-(3,4 dimethylene pyrrolidyl) phenyl) methane as a high temperature reactive oligomer

A major goal in the field of high temperature polymers was to prepare aromatic polyimides that can be easily fabricated with the required thermal and physical properties for aerospace applications. Recent research was directed to achieve polyimides that are: soluable in a common organic solvent; melt-processable; and thermally curable without the evolution of volatile by-products. A monomer, N-phenyl 3,4-dimethylene pyrrolidine, that can be modified to form a bis (exocyclodiene) I for the preparation of polyimides by the Diels-Alder process was developed. Preparation of high temperature polymeric materials by Diels-Alder polymerization that will maintain their integrity and toughness during long exposure time at elevated temperature is sought.

Ottenbrite, Raphael M.↗

Development of an impact- and solvent-resistant thermoplastic composite matrix, phase 4

Polyimides from BTDA with m-phenylenediamine and three aliphatic diamines were prepared in cresol and characterized. Characterization tests included compression strength and modulus, stressed solvent resistance, and melt-flow tests. Efforts to reduce the molecular weights of these polymers by either stoichiometric imbalance or phthalic anhydride end capping produced opacity in the polymer moldings when the stoichiometry was less than 99 percent. Use of 2,4-diaminotoluene in place of the m-phenylenediamine allowed clear polymer moldings to be obtained at all stoichiometries by end capping or stoichiometric imbalance. After melt-flow/molecular-weight studies, carbon fabric composites were prepared from three polyimide compositions containing BTDA, 2,4-diaminotoluene and two aliphatic diamines. Flexural strengths of two of the resins were in excess of 689 MPa (100 ksi) at both room temperature and 93 C. The polyimide from BTDA was selected for scale-up and neat resin characterization tests. The Tg of this polymer was 233 C.

Delano, C. B.↗

Polymer Lubricants For Use In Vacuum

Report describes tests of lubricating properties of 10 polymer-based materials - in particular, polyimides - in vacuum. Commercially available materials, in forms of solid bodies and films on metals, were tested on pin-on-disk apparatus in vacuum. Best low-wear, low-friction material was 80 PMDA/20 BTDA solid-body polyimide. Friction and wear properties of most polyimides so good in vacuum that solid-lubricant additives not necessary.

Fusaro, Robert L.↗

Evaluation of two bisimide additives in LARC-TPI adhesive

The processability of aromatic polyimides can be improved by the addition of bis (amide) acids or bisimides to LARC-TPI. These low molecular weight additives apparently lower the melt viscosity of aromatic polyimides without affecting the glass transition temperature. Well-consolidated, fiber reinforced composites were fabricated using this technology. LARC-TPI can be processed as a thermoplastic polyimide to form high strength bonds, however, this is generally accomplished by processing at relatively high bonding pressures. An adhesive investigation is presented on the effects of two bisimide additives to LARC-TPI in an attempt to improve the bonding process by lowering the viscosity of the material to achieve improved bond strength properties. Apparently, the high flow which is exhibited by the additives when they melt, tended to be masked by the more viscous LARC-TPI.

Progar, Donald J.↗

Surface characterization and adhesion of oxygen plasma-modified LARC-TPI

LARC-TPI, an aromatic thermoplastic polyimide, was exposed to an oxygen plasma as a surface pretreatment for adhesive bonding. Chemical and physical changes which occurred in the polyimide surface as a result of the plasma treatment were investigated using X-ray photoelectron spectroscopy (XPS), infrared reflection-absorption spectroscopy (IR-RAS), contact-angle analysis, ellipsometry, and high resolution SEM. A 180-deg peel test with an acrylate-based pressure sensitive adhesive as a flexible adherent was utilized to study the interactions of the plasma-treated polyimide surface with other polymeric materials. The surface characterization and adhesion testing results showed that the oxygen plasma treatment, while creating a more hydrophilic, polar surface, also caused chain scission, resulting in the formation of a weak boundary layer which inhibited adhesion.

Chin, J. W.↗