Precipitation of dopants on acceptor-doped LaMnO3±δ revealed by defect chemistry from first principles

Perovskite oxides degrade at elevated temperatures while precipitating dopant-rich particles on the surface. A knowledge-based improvement of surface stability requires a fundamental and quantitative understanding of the dopant precipitation mechanism on these materials. We propose that dopant precipitation is a consequence of the variation of dopant solubility between calcination and operating conditions in solid oxide fuel cells (SOFCs) and electrolyzer cells (SOECs). To study dopant precipitation, we use 20% (D = Ca, Sr, Ba)-doped LaMnO3+δ (LDM20) as a model system. We employ a defect model taking input from density functional theory calculations. The defect model considers the equilibration of LDM20 with a reservoir consisting of dopant oxide (DO), peroxide (DO2), and O2 in the gas phase. The equilibrated non-stoichiometry of the A-site and B-site as a function of temperature, T, and oxygen partial pressure, p(O2), reveals three regimes for LDM20: A-site deficient (oxidizing conditions), A-site rich (atmospheric conditions), and near-stoichiometric (reducing conditions). Assuming an initial A/B non-stoichiometry, we compute the dopant precipitation boundaries in a p–T phase diagram. Our model predicts precipitation both under reducing (DO) and under highly oxidizing conditions (DO2). We found precipitation under anodic, SOEC conditions to be promoted by large dopant size, while under cathodic, SOFC conditions precipitation is promoted by initial A-site excess. The main driving forces for precipitation are oxygen uptake by the condensed phase under oxidizing conditions and oxygen release assisted by B-site vacancies under reducing conditions. Possible strategies for mitigating dopant precipitation under in electrolytic and fuel cell conditions are discussed.

Hess, Franziska (ORCID:000000024460643X)↗

Critical Parameter Identification of Fuel-Cell Models Using Sensitivity Analysis

Numerical modeling has been a vital tool in proton-exchange-membrane fuel-cell (PEMFC) analysis; however, the predictive capabilities of these models depend on the input physical parameters, several of which are either not experimentally measured or have large scatter in measured values. This article presents an uncertainty propagation-based sensitivity analysis to identify the model parameters that impact the model predictions most. A comprehensive 2-D membrane electrode assembly (MEA) model is used to perform local sensitivity analysis at multiple operating conditions, which encompass the range of environments and operating conditions a cell can encounter. While at lower humidities, cathode kinetics and membrane-ohmic-loss related parameters are crucial, gas transport and porous-media saturation behavior are more important at humidified conditions. Several of these findings are different from previous studies presented in literature. Identifying the crucial parameters helps focus future material and cell optimization studies as well as experimental studies to quantify these parameters with higher accuracy.

25 ENERGY STORAGE↗

Wind energy system time-domain (WEST) analyzers

A portable analyzer which simulates in real time the complex nonlinear dynamics of horizontal axis wind energy systems was constructed. Math models for an aeroelastic rotor featuring nonlinear aerodynamic and inertial terms were implemented with high speed digital controllers and analog calculation. This model was combined with other math models of elastic supports, control systems, a power train and gimballed rotor kinematics. A stroboscopic display system graphically depicting distributed blade loads, motion, and other aerodynamic functions on a cathode ray tube is included. Limited correlation efforts showed good comparison between the results of this analyzer and other sophisticated digital simulations. The digital simulation results were successfully correlated with test data.

Dreier, M. E.↗

The temporal development of hollow cathode discharges

The temporal development of hollow cathode discharges was studied by means of electrical and optical diagnostic techniques. The results indicate that the discharge develops in two stages. The initial breakdown occurs along the longest straight path of the system, i.e., from the anode to the bottom of the cathode hole. This predischarge is confined to a narrow filament along the axis and carries a current of up to hundreds of milliamperes. The resulting distortion of the electric field in the cathode hole is assumed to cause a radial breakdown from the filamentary plasma on the axis to the edge of the cathode hole. After this second breakdown, an increase in current by more than three orders of magnitude is observed. Measurements with axial magnetic fields support the two-stage model.

Ngo, Mai T.↗

Evaluating Risk Of Failure With Limited Information

Report describes probabilistic failure assessment (PFA). Developed for application to spaceflight systems for sufficient testing of hardware to ensure reliability not feasible. However, must be ascertained that critical failure modes extremely unlikely to occur during service. PFA applied to any failure mode described by quantitative models of physics and mechanics of failure phenomena, such as fatigue crack in initiation or propagation in structures, leakage of seals, wear in bearings, and erosion of arcjet thrustor cathodes.

Moore, N. R.↗

Modeling the dynamic behavior of proton-exchange membrane fuel cell

A two-phase transient model that incorporates the permanent hysteresis observed in the experimentally measured capillary pressure of GDL has been developed. The model provides explanation for the difference in time constant between membrane hydration and dehydration observed in the HFR experiment conducted at LANL. When there is liquid water at the cathode catalyst layer, time constant of the water content in the membrane is closely tied to that of liquid water saturation in the CCL, as the vapor is already saturated. The water content in the membrane will not reach steady state as long as the liquid water flow in the CCL is not at steady state. Also, Increased resistance to proton transport in the membrane is observed when the cell voltage is stepped down to a very low value.

30 DIRECT ENERGY CONVERSION↗

Emission properties and back-bombardment for CeB{sub 6} compared to LaB{sub 6}

The emission properties of CeB{sub 6} compared to LaB{sub 6} thermionic cathodes have been measured using an electrostatic DC gun. Obtaining knowledge of the emission properties is the first step in understanding the back-bombardment effect that limits wide usage of thermionic radio-frequency electron guns. The effect of back-bombardment electrons on CeB{sub 6} compared to LaB{sub 6} was studied using a numerical simulation model. The results show that for 6 μs pulse duration with input radio-frequency power of 8 MW, CeB{sub 6} should experience 14% lower temperature increase and 21% lower current density rise compared to LaB{sub 6}. We conclude that CeB{sub 6} has the potential to become the future replacement for LaB{sub 6} thermionic cathodes in radio-frequency electron guns.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electrode Mesoscale as a Collection of Particles: Coupled Electrochemical and Mechanical Analysis of NMC Cathodes

Battery electrodes are composed of polydisperse particles and a porous, composite binder domain. These materials are arranged into a complex mesostructure whose morphology impacts both electrochemical performance and mechanical response. We present image-based, particle-resolved, mesoscale finite element model simulations of coupled electrochemical-mechanical performance on a representative NMC electrode domain. Beyond predicting macroscale quantities such as half-cell voltage and evolving electrical conductivity, studying behaviors on a per-particle and per-surface basis enables performance and material design insights previously unachievable. Voltage losses are primarily attributable to a complex interplay between interfacial charge transfer kinetics, lithium diffusion, and, locally, electrical conductivity. Mesoscale heterogeneities arise from particle polydispersity and lead to material underutilization at high current densities. Particle-particle contacts, however, reduce heterogeneities by enabling lithium diffusion between connected particle groups. While the porous composite binder domain (CBD) may have slower ionic transport and less available area for electrochemical reactions, its high electrical conductivity makes it the preferred reaction site late in electrode discharge. Mesoscale results are favorably compared to both experimental data and macrohomogeneous models. This work enables improvements in materials design by providing a tool for optimization of particle sizes, CBD morphology, and manufacturing conditions.

42 ENGINEERING↗

New Secondary Batteries Using Electronically Conductive Polymer Cathodes

A Li/Polypyrrole secondary battery was designed and built, and the effect of controlling the morphology of the polymer on enhancement of counterion diffusion in the polymer phase was explored. The experimental work was done at Colorado State University, while the mathematical modeling of the battery was done at Texas A and M University. Manuscripts and publications resulting from the project are listed.

Martin, Charles R.↗

Measurement and modeling of electric field and space-charge distributions in obstructed helium discharge

Axial and radial variations of electric field have been measured in dielectric shielded 0.025 m diameter parallel plate electrode with 0.0065 m gap for 1.6 mA, 2260 V helium dc discharge at 1.75 Torr. The axial and radial electric field profiles have been measured from the Stark splitting of 2{sup 1}S→11 {sup 1}P transition through collision induced fluorescence from 4{sup 3}D→2{sup 3}P. The electric field values showed a strong radial variation peaking to 500 kV/m near the cathode radial boundary, and decreasing to about 100 kV/m near the anode edge, suggesting the formation of an obstructed discharge for this low nd condition, where n is the gas density and d is the gap distance. The off-axis Stark spectra showed that the electric field vector deviates from normal to the cathode surface which permits longer path electron trajectories in the inter-electrode gap. Also, the on-axis electric field gradient was very small and off-axis electric field gradient was large indicating a radially non-uniform current density. In order to obtain information about the space charge distribution in this obstructed discharge, it was modeled using the 2-d axisymmetric Poisson solver with the COMSOL finite element modeling program. The best fit to the measured electric field distribution was obtained with a space charge variation of ρ(r) = ρ{sub 0}(r/r{sub 0}){sup 3}, where ρ(r) is the local space charge density, ρ{sub 0} = 6 × 10{sup −3} Coulomb/m{sup 3}, r is the local radial value, and r{sub 0} is the radius of the electrode.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

High–Energy Earth–Abundant Cathodes with Enhanced Cationic/Anionic Redox for Sustainable and Long–Lasting Na–Ion Batteries

Layered iron/manganese-based oxides are a class of promising cathode materials for sustainable batteries due to their high energy densities and earth abundance. However, the stabilization of cationic and anionic redox reactions in these cathodes during cycling at high voltage remain elusive. Here, an electrochemically/thermally stable P2-Na 0.67 Fe 0.3 Mn 0.5 Mg 0.1 Ti 0.1 O 2 cathode material with zero critical elements is designed for sodium-ion batteries (NIBs) to realize a highly reversible capacity of ≈210 mAh g –1 at 20 mA g –1 and good cycling stability with a capacity retention of 74% after 300 cycles at 200 mA g –1 , even when operated with a high charge cut-off voltage of 4.5 V versus sodium metal. Combining a suite of cutting-edge characterizations and computational modeling, it is shown that Mg/Ti co-doping leads to stabilized surface/bulk structure at high voltage and high temperature, and more importantly, enhances cationic/anionic redox reaction reversibility over extended cycles with the suppression of other undesired oxygen activities. This work fundamentally deepens the failure mechanism of Fe/Mn-based layered cathodes and highlights the importance of dopant engineering to achieve high-energy and earth-abundant cathode material for sustainable and long-lasting NIBs.

25 ENERGY STORAGE↗

Status of the NEXT Long-Duration Test After 23,300 Hours of Operation

The NASA s Evolutionary Xenon Thruster (NEXT) program is developing the next-generation ion propulsion system with significant enhancements beyond the state-of-the-art in ion propulsion to provide future NASA science missions with enhanced mission capabilities at a low total development cost. As part of a comprehensive thruster service life assessment utilizing both testing and analyses, a Long-Duration Test (LDT) was initiated in June 2005, to verify the NEXT propellant throughput capability to a qualification-level of 450 kg, 1.5 times the anticipated throughput requirement of 300 kg per thruster from mission analyses. The LDT is being conducted with a modified, flight-representative NEXT engineering model ion thruster, designated EM3. As of July 2009, the thruster has accumulated 23,300 h of operation with extensive durations at the following input powers: 6.9, 4.7, 1.1, and 0.5 kW. The thruster has processed 427 kg of xenon surpassing the NSTAR propellant throughput demonstrated during the extended life testing of the Deep Space 1 flight spare ion thruster and approaching the NEXT development qualification throughput goal. The NEXT LDT has demonstrated a total impulse of 16.0 10(exp 6) N/s; the highest total impulse ever demonstrated by an ion thruster. Thruster performance tests are conducted periodically over the entire NEXT throttle table with input power ranging 0.5 to 6.9 kW. Thruster performance parameters including thrust, input power, specific impulse, and thruster efficiency have been nominal with little variation to date. The NSTAR first-failure mode, accelerator aperture erosion leading to electron backstreaming, has been mitigated in the NEXT design. The severe NSTAR discharge cathode assembly erosion has been mitigated by a graphite keeper in the NEXT thruster. Tracking of the NEXT first failure mode, charge-exchange ion impingement on the accelerator grid causing hexagonal groove erosion, is consistent with model predictions and indicates thruster life greater than or equal to 750 kg throughput. This paper presents the status, performance data, and wear characteristics of the NEXT LDT to date.

Herman, Daniel A.↗

Rechargeability and economic aspects of alkaline zinc-manganese dioxide cells for electrical storage and load leveling

Batteries based on manganese dioxide (MnO2) cathodes are good candidates for grid-scale electrical energy storage, as MnO2 is low-cost, relatively energy dense, safe, water-compatible, and non-toxic. Alkaline Zn-MnO2 cells, if cycled at reduced depth of discharge (DOD), have been found to achieve substantial cycle life with battery costs projected to be in the range of $100 to 150 per kWh (delivered). Commercialization of rechargeable Zn-MnO2 batteries has in the past been hampered due to poor cycle life. In view of this, the work reported here focuses on the long-term rechargeability of prismatic MnO2 cathodes at reduced DOD when exposed to the effects of Zn anodes and with no additives or specialty materials. Over 3000 cycles is shown to be obtainable at 10% DOD with energy efficiency >80%. The causes of capacity fade during long-term cycling are also investigated and appear to be mainly due to the formation of irreversible manganese oxides in the cathode. Analysis of the data indicates that capacity loss is rapid in the first 250 cycles, followed by a regime of stability that can last for thousands of cycles. A model has been developed that captures the behavior of the cells investigated using measured state of charge (SOC) data as input. An approximate economic analysis is also presented to evaluate the economic viability of Zn-MnO2 batteries based on the experiments reported here. (C) 2014 Elsevier B.V. All rights reserved.

Ingale, ND↗

Developing extreme fast charge battery protocols – A review spanning materials to systems

Extreme fast charging (XFC) has become a focal research point in the lithium-battery community over the last several years. As adoption of electric vehicles increases, fast charging has become a key driver in enhancing consumer recharge experience. Recently, the research community has made significant improvements in developing charge protocols to support XFC. New charge protocol designs derived using a combination of advanced, physically derived models, and electrochemical and secondary characterization methods, increase charge acceptance and decrease aging. By coordinating these methods and modifying protocols to account for different material constraints, including lithium plating and cathode particle degradation, novel charge protocols have increased the energy accepted during charging by over 25% in 10 min and increased the charge acceptance prior to a constant-voltage step by approximately 3x. Here, we review several charge-protocol advances, aging factors which are enhanced by XFC and advances which will enable adoption of XFC capable vehicles. These advances include implementing machine learning and other detection algorithms to reduce and classify lithium plating, which is known to significantly degrade cell performance and reduce cell life. The review concludes by discussing full-system fast charge requirements, including electric vehicle service equipment needs for implementing XFC protocols.

25 ENERGY STORAGE↗

Data-driven design of electrolyte additives supporting high-performance 5 V LiNi 0.5 Mn 1.5 O 4 positive electrodes

LiNi 0.5 Mn 1.5 O 4 (LNMO) is a high-capacity spinel-structured material with an average lithiation/de-lithiation potential at ca. 4.6–4.7 V vs Li + /Li, far exceeding the stability limits of electrolytes. An efficient way to enable LNMO in lithium-ion batteries is to reformulate an electrolyte composition that stabilizes both graphitic (Gr) negative electrode with solid-electrolyte-interphase and LNMO with cathode-electrolyte-interphase. In this study, we select and test a diverse collection of 28 single and dual additives for the Gr||LNMO battery system. Subsequently, we train machine learning models on this dataset and employ the trained models to suggest 6 binary compositions out of 125, based on predicted final area-specific-impedance, impedance rise, and final specific-capacity. Such machine learning-generated new additives outperform the initial dataset. This finding not only underscores the efficacy of machine learning in identifying materials in a highly complicated application space but also showcases an accelerated material discovery workflow that directly integrates data-driven methods with battery testing experiments.

batteries↗

Corrosion inhibition of mild steel in acidic media using newly synthesized heterocyclic organic molecules: Correlation between inhibition efficiency and chemical structure

The corrosion inhibition of mild steel in 5% HCl solutions by some new synthesized organic compounds namely 3-(2-methoxyphenyl) 5-mercapto-1. 2. 4-triazole (2-MMT), 3-(3-methoxyphenyl) 5-mercapto-1. 2. 4-triazole (3-MMT) and 3-(2-hydroxyphenyl) 5-mercapto-1. 2. 4-triazole (2-HMT) was investigated using weight loss and potentiostatic polarization techniques. These measurements reveal that the inhibition efficiency obtained by these compounds increased by increasing their concentration. The inhibition efficiency follows the order 2-MMT >3-MMT >2-HMT. Polarization studies show that these compounds are of the mixed type but dominantly act as a cathodic inhibitors for mild steel in 5% HCl solutions. These inhibitors function through adsorption following Langmuir isotherm. Activation energy and Gibbs free energy for adsorption of inhibitors are calculated. Molecular modeling has been conducted to correlate the corrosion inhibition properties with the calculated quantum chemical parameters.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Coupling of transit time instabilities in electrostatic confinement fusion devices

A model of the behavior of transit time instabilities in an electrostatic confinement fusion reactor is presented in this letter. It is demonstrated that different modes are excited within the spherical cathode of a Farnsworth fusor. Each of these modes is dependent on the fusion products as well as the acceleration voltage applied between the two electrodes and they couple to a resulting oscillation showing non-linear beat phenomena. This type of instability is similar to the transit time instability of electrons between two resonant surfaces but the presence of ions and the occurring fusion reactions alter the physics of this instability considerably. The physics of this plasma instability is examined in detail for typical physical parameter ranges of electrostatic confinement fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Determining the Length Scale of Transport Impedances in Li-Ion Electrodes: Li(Ni 0.33 Mn 0.33 Co 0.33 )O 2

Battery cathodes are complex multiscale, multifunctional materials. The length scale at which the dominant impedance arises may be difficult to determine even with the most advanced experimental characterization efforts, and thus modeling can play an important role in analysis. Discharge and voltage relaxation curves, interrogated with theory, are used to distinguish between transport impedance that arise on the scale of the active crystal and on the scale of agglomerates (secondary particles) comprised of nanoscale crystals. Model-selection algorithms are applied to determine that the agglomerate scale is dominant in the Li Ni 0.33 Mn 0.33 Co 0.33 O 2 electrode studied here. Furthermore, conditions where the agglomerate and crystal-scale models yield distinct simulation results are demonstrated, providing approaches that can be applied to other systems.