Search NASA⌕ Search

SEARCH · Search NASA

Results for “Melting”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,063 records · Page 59

Effect of Heat Treatment on the Properties of CoCrMo Alloy Manufactured by Selective Laser Melting

To obtain medical implants with better mechanical properties, it is necessary to conduct studies on the heat treatment process of the selective laser melting (SLM) manufacturing parts. The differential scanning calorimetry method was used to study the heat treatment process of the phase transition of SLM CoCrMo alloy parts. The tensile properties were tested with a tensile test machine, the quantity of carbide precipitated after heat treatment was measured by energy-dispersive x-ray spectroscopy, and the tensile fracture morphology of the parts was investigated using SEM. The obtained results were: Mechanical properties in terms of elongation and tensile strength of CoCrMo alloy manufactured by SLM that had been heat-treated at 1200 °C for 2 h followed by cooling with water were not only higher than the national standard but also higher than the experimental results of the same batch of castings. The mechanism of fracture of parts manufactured by SLM without heat treatment was brittle fracture, whereas parts which had been heat-treated at 1200 °C for 2 h combined with water cooling and at 1200 °C for 1 h with furnace cooling suffered ductile fracture. This study provides the basis for defining the applications for which CoCrMo alloys manufactured by SLM are suitable within the field of medical implants.

36 MATERIALS SCIENCE↗

Processing Parameter Effects on Residual Stress and Mechanical Properties of Selective Laser Melted Ti6Al4V

Selective laser melting (SLM) process is characterized by large temperature gradients resulting in high levels of residual stress within the additively manufactured metallic structure. SLM-processed Ti6Al4V yields a martensitic microstructure due to the rapid solidification and results in a ductility generally lower than a hot working equivalent. Post-process heat treatments can be applied to SLM components to remove in-built residual stress and improve ductility. Residual stress buildup and the mechanical properties of SLM parts can be controlled by varying the SLM process parameters. This investigation studies the effect of layer thickness on residual stress and mechanical properties of SLM Ti6Al4V parts. This is the first-of-its kind study on the effect of varying power and exposure in conjunction with keeping the energy density constant on residual stress and mechanical properties of SLM Ti6Al4V components. It was found that decreasing power and increasing exposure for the same energy density lowered the residual stress and improved the % elongation of SLM Ti6Al4V parts. Increasing layer thickness resulted in lowering the residual stress at the detriment of mechanical properties. The study is based on detailed experimental analysis along with finite element simulation of the process using ABAQUS to understand the underlying physics of the process.

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Build Orientation Effects on Texture and Mechanical Properties of Selective Laser Melting Inconel 718

The production of components via selective laser melting (SLM) metal additive manufacturing results in microstructures unique to the process that are highly dependent on laser processing parameters and orientation of part geometry relative to the build direction. This study investigates the variation in tensile properties of SLM Inconel 718 at varying angles with respect to build direction. ASTM E8 tensile specimens were built in XY, Z, and B+45 from Z orientations to near-net shape, HIP and heat treated, and tensile tested at room temperature. Orientation dependence of mechanical properties was observed; Z samples had the lowest strength and highest elongation, while XY samples had the highest strength and lowest elongation. Optical, SEM, and EBSD analysis were conducted to probe for microstructure variation that could be the cause of the difference in mechanical properties. Analysis of pole figures and grain maps suggests a preferred grain texture and twinning orientation that aligns with the build direction, which may contribute to the anisotropic enhancement in ductility.

36 MATERIALS SCIENCE↗

The Effects of Sc Addition on the Microstructure and Mechanical Properties of Be-Al Alloy Fabricated by Induction Melting

This study investigated the alloying effects of 0.4 wt.% Sc on the microstructure, mechanical properties, and fracture behavior of a cast Be-Al alloy prepared by vacuum induction melting. The micromechanics of Sc-containing secondary-phase particles (SPs) were characterized by nanoindentation, and the fracture behavior of the alloy was investigated via tensile fractography and optical metallography. The addition of 0.4 wt.% Sc significantly modified the alloy microstructure by decreasing the secondary dendritic arm spacing (SDAS), weakening the dendritic structure of Be, and producing an equiaxed/cellular alloy microstructure with refined Be grains. Sc alloying increased the Vickers hardness by 36%, elastic modulus by 28%, yield strength by 35%, ultimate strength by 52%, but decreased the elongation from 3.6 to 2.9%. Sc-containing SPs had a higher elastic modulus, yield strength, microhardness, and a lower plasticity index than the Be and Al matrices, resulting in interface separation during the fracture process. SPs located at the Be/Al interfaces did not act as microcrack sources for the matrices, whereas highly faceted SPs within the Be grains induced microcrack formation and decreased the elongation. The failure mode of the cast Be-Al-0.4Sc alloy still involved the brittle cleavage failure of Be regions and ductile dimple failure of Al regions, which was not the case with the cast Be-Al alloy.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Properties of 24CrNiMoY Alloy Steel Fabricated by Selective Laser Melting

24CrNiMoY alloy steel samples were fabricated by selective laser melting (SLM), and a phase transformation model was established to study the alloy steel microstructural evolution. Meanwhile, microhardness and tensile properties of 24CrNiMoY alloy steel prepared by different laser energy densities (E{sub v}) were investigated. Results indicate that the microstructural evolution of 24CrNiMoY alloy steel is consistent with the phase transformation model. The main microstructure changed from martensite to bainite with the increase in thermal cycle numbers. In addition, a suitable E{sub v} plays an important role in refining the bainite structure and improving the alloy steel properties. When the E{sub v} decreases from 210 to 140 J/mm{sup 3}, the bainite lath width reduces from 1.7 to 0.6 μm. Simultaneously, the relative density, tensile strength and microhardness of the fabricated samples increase first and decrease later. 24CrNiMoY alloy steel sample prepared by 160 J/mm{sup 3} has fine mechanical properties: The tensile strength is 850 MPa and microhardness is 360 HV{sub 0.2}.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure Evolution and Mechanical Properties of Selective Laser Melted Inconel 718 Alloy

The microstructure characteristics of the selective laser melted Inconel 718 alloy under as-deposited, homogenization + solution + aging (HSA) and solution + aging (SA) conditions were studied. The anisotropy and heterogeneity of mechanical properties under different conditions were also investigated. Under the as-deposited condition, the morphology and size of the grains are heterogeneous. The dendrite structures which grow nearly perpendicular to the molten pool traces, accompanying interdendritic Laves phase, can be observed within the grains. The dendrite structure completely disappeared, and the Laves phases embedded in the interdendritic regions also dissolved into the matrix to precipitate γ′ and γ″ phases after heat treatments. Fully recrystallized grains were obtained under the HSA condition, while only incomplete recrystallized grains were obtained under the SA condition. However, the characteristics of γ′ and γ″ phases are very similar under the HSA and SA conditions. Significant improvement in strength after heat treatments was due to the dissolution of undesirable Laves phase and the precipitation of γ′ and γ″ phases. For all the three conditions, different tensile properties were observed depending on the orientation of the specimens. The scatter of mechanical properties is notable, and heat treatments increased the scatter of mechanical properties.

36 MATERIALS SCIENCE↗

A Study on the Microstructures and Properties of Selective Laser Melted Babbitt Metals

Babbitt metal cubes were prepared by means of selected laser melting (SLM) process using Sn—11% Sb—6% Cu alloy powders; their microstructures were studied using optical microscope (OM), SEM, EDS, XRD and DSC; and their mechanical properties were tested using Vickers hardness and tensile methods. The results show that fully dense Babbitt metal components can be prepared by using appropriate SLM process parameters and an interlayer staggered laser scanning strategy. Anisotropy characteristics appear in both the microstructure and mechanical properties of SLM-Babbitt cubic specimens. The average hardness was in the range of 32.5 HV0.05 to 35.3 HV0.05. Both tensile strength and elongation were somewhat higher in a direction parallel to the laser scanning speed (Y axis) than in a direction perpendicular to the laser scanning speed (X axis). The strengthening mechanism is suggested to include solid solution strengthening of oversaturated Sb in the Sn matrix, as well as dispersion strengthening of finely dispersed SnSb and Cu{sub 6}Sn{sub 5} particles. The overgrown acicular Cu{sub 6}Sn{sub 5} phases at low laser scanning speeds and void formation at higher laser scanning speeds seriously deteriorate the mechanical properties of the SLM-Babbitt specimens.

36 MATERIALS SCIENCE↗

Melt Pool and Heat Treatment Optimization for the Fabrication of High-Strength and High-Toughness Additively Manufactured 4340 Steel

Additively manufactured (AM) components offer superior design flexibility compared to their conventionally manufactured counterparts, and optimizing processing parameters is key to achieving high-quality depositions with desirable and predictable mechanical properties. This study was focused on 4340 steel fabricated using laser powder bed fusion (LPBF), and 42 laser power and scan speed combinations have been systematically investigated to determine an optimized melt pool geometry that would ensure fully-dense parts. The AM material was compared with a wrought 4340 equivalent and studied in two customized heat treated conditions, optimized for strength and toughness, respectively. The microstructures of the as-fabricated and heat treated AM and wrought materials were characterized to assess differences introduced by the layer-by-layer fabrication process and subsequent heat treatment. Tensile properties of both materials were also evaluated and demonstrate that the AM materials offer equal or superior properties compared to the wrought equivalents. Differences in fracture surface morphologies indicate the distinct failure mechanisms associated with the materials’ characteristic microstructures, and the role of inclusions in the failures was studied to elucidate these differences. Complementary to the experimental investigations, the dataset was leveraged to make recommendations for future design of experiments to optimize AM build parameters in other material systems. A statistical Monte Carlo analysis was used to predict the interpolation error produced using reduced datasets and to enable informed processing parameters selection. These findings are discussed to make recommendations for the use of AM materials for high-integrity structural applications.

36 MATERIALS SCIENCE↗

Microstructure Development in Electron Beam-Melted Inconel 718 and Associated Tensile Properties

During the electron beam melting (EBM) process, builds occur at temperatures in excess of 800°C for nickel-base superalloys such as Inconel 718. When coupled with the temporal differences between the start and end of a build, a top-to-bottom microstructure gradient forms. Characterized in this study is the microstructure gradient and associated tensile property gradient that are common to all EBM Inconel 718 builds. From the characteristic microstructure elements observed in EBM Inconel 718 material, the microstructure gradient can be classified into three distinct regions. Region 1 (top of a build) and is comprised of a cored dendritic structure that includes carbides and Laves phase within the interdendritic regions. Region 2 is an intermediate transition zone characterized by a diffuse dendritic structure, dissolution of the Laves phase, and precipitation of δ needle networks within the interdendritic regions. The bulk structure (Region 3) is comprised of a columnar grain structure lacking dendritic characteristics with δ networks having precipitated within the grain interiors. Mechanically at both 20°C and 650° C, the yield strength, ultimate tensile strength, and elongation at failure exhibit the general trend of increasing with increasing build height.

36 MATERIALS SCIENCE↗

Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization

Selective Laser Melted Ti-6Al-4V (as-SLMed) exhibits decreased yield strength, increased work hardening, and increased ductility after heat treatment at 730 degrees C (HT-730) or 900 degrees C (HT-900) for 2 h. To understand the change of mechanical properties, in situ high energy X-ray diffraction (HEXRD) is used to examine the phase composition, load partitioning, slip system activity, and dislocation density evolution in all three specimens. The as-SLMed specimen is dominated by martensitic α'. After heat treatment, α' partly or fully decomposes into α+β, reducing the yield strength. In HT-730, beta precipitates with confined size show much higher lattice strain than the α'/α matrix during deformation; in HT-900, the lattice strain difference is mostly eliminated. This is a key reason for the increased ductility in HT-900. From the anisotropic lattice strain development, basal slip is identified as the easiest slip system in α'/α. Using an elasto-plastic self-consistent (EPSC) model, the critical resolved shear stress ratio between prismatic slip and basal slip (CRSS prism /CRSS basal ) is estimated to be 1.31 and 1.16 in the as -SLMed and the HT-900 specimens, respectively. Further, the alpha phase in HT-900 is able to activate multiple slip systems and accumulate more dislocations during plastic deformation. This explains why HT-900 has better ductility and higher work hardening rate than the other two specimens.

36 MATERIALS SCIENCE↗

Transmission electron microscopy of the rapid solidification microstructure evolution and solidification interface velocity determination in hypereutectic Al-20at.%Cu after laser melting

The evolution of rapid solidification (RS) microstructure and solidification interface velocity has been studied experimentally by in-situ transmission electron microscopy and postmortem characterization for hypereutectic Al-20at.%Cu (37 wt.%Cu) after laser melting. Four morphologically distinct regions formed via growth modes changing from θ-Al 2 Cu phase dendrites to eutectic cell growth, possibly α-Al dendrite growth (α-cell), banded growth, and α-Al plane front growth. Tendency for faceting and low capacity for solute trapping limited the θ-phase dendrite growth to solidification interface velocity v < 0.07 m/s. Consequently, formation of pro-eutectic micro-constituent was suppressed, and RS microstructure formation was dominated by eutectic, α-cell, and banded morphology grains for the Al-20at.%Cu alloy. Eutectic growth operated for interface velocity of 0.1 m/s ≤ v < 0.3 m/s, with a transition from regular lamellar, 2-λ and 1-λ mode to a dense irregular morphology dominated by α-phase at v = 0.3 m/s. Interface temperature calculations indicated feasibility of α-cell growth mode for 0.3 m/s ≤ v < 0.7 m/s. Banded growth occurred for 0.7 m/s ≤ v < 1.3 m/s. Plane front α-phase growth was evident for interface velocities v ≥ 1.3 m/s. Previous work on rapid solidification microstructure development in hypereutectic Al-Cu alloys reported a regime of α-cell growth subsequently to eutectic and prior to transition to banded growth for Al-19at.%Cu (36 wt.%Cu), while for Al-22at.%Cu (40 wt.%Cu) eutectic growth transitioned directly to α-plane front growth without emergence of a banded regime. Finally, based on the current study the disappearance of the banded growth regime occurs for a composition larger than 20at.%Cu.

36 MATERIALS SCIENCE↗

Synthesis of a 316L stainless steel-copper composite by laser melting

This paper demonstrates a laser melting method to produce a metal matrix composite with a higher thermal conductivity compared to 316 L stainless steel using a Jettable Cu ink. A novel canister was used to control the oxygen level during laser processing to emulate a hybrid inkjet-powder bed fusion technique for doping the stainless steel powder bed with Cu precursor ink. Here, the thermal conductivity of the composite was found to be 187% higher than that of 316 L stainless steel, while the microhardness decreased by 39%. Microstructural results show opportunities to further enhance the thermal conductivity and mechanical properties of the composite by eliminating interfacial cracking.

36 MATERIALS SCIENCE↗

Experimental comparison of residual stresses for a thermomechanical model for the simulation of selective laser melting

Selective laser melting (SLM) is an additive manufacturing process in which multiple, successive layers of metal powders are heated via laser in order to build a part. Modeling of SLM requires consideration of the complex interaction between heat transfer and solid mechanics. Here, the present work describes the authors initial efforts to validate their first generation model. In particular, the comparison of model-generated solid mechanics results, including both deformation and stresses, is presented. Additionally, results of various perturbations of the process parameters and modeling strategies are discussed.

42 ENGINEERING↗

Infiltration studies of additive manufacture of WC with Co using binder jetting and pressureless melt method

Additive manufacturing (AM) of tungsten carbide-cobalt (WC-Co) is explored starting with WC preforms shaped with binder jet additive manufacturing (BJAM) followed by melt infiltration of Co. The research objective is to demonstrate the ability to net-shape WC-Co composites through BJAM of a WC preform followed by backfilling with cobalt via pressureless infiltration. This method also has the potential to minimize shrinkage and grain growth compared to other AM techniques. The effects of sintering, Co content, and infiltration time on the net shaping and properties of processed composites are shown. The best shaped material had an average grain size of 5.1 μm, 32 vol.% Co, density of 98.54% theoretical, fracture toughness of 23.2 MPa m 1/2 , and hardness of 9.0 GPa. Data presented illustrates that the proposed approach results in favorable ceramic-metal (cermet) properties and is viable for fabricating cermets of other material combinations. Furthermore successful AM of cermets provides complex geometries, high throughout, and low costs.

36 MATERIALS SCIENCE↗

Multi-scale computational modeling of residual stress in selective laser melting with uncertainty quantification

Selective laser melting (SLM) is a powder-based additive manufacturing technique which creates parts by fusing together successive layers of powder with a laser. The quality of produced parts is highly dependent on the proper selection of processing parameters, requiring significant testing and experimentation to determine parameters for a given machine and material. Computational modeling could potentially be used to shorten this process by identifying parameters through simulation. However, simulating complete SLM builds is challenging due to the difference in scale between the size of the particles and laser used in the build and the size of the part produced. Often, continuum models are employed which approximate the powder as a continuous medium to avoid the need to model powder particles individually. While computationally expedient, continuum models require as inputs effective material properties for the powder which are often difficult to obtain experimentally. Building on previous works which have developed methods for estimating these effective properties along with their uncertainties through the use of detailed models, this work presents a part scale continuum model capable of predicting residual thermal stresses in an SLM build with uncertainty estimates. Model predictions are compared to experimental measurements from the literature.

42 ENGINEERING↗

Quantitatively accounting for the effects of surface topography on the oxidation kinetics of additive manufactured Hastelloy X processed by electron beam melting

In this work, the effects of surface roughness on the high-temperature corrosion of nickel-based superalloy X produced through electron-beam melting (EBM) additive manufacturing were studied. Surface area of samples in the rough, as-fabricated condition was measured using a 2D cross-section image analysis technique and a 3D image analysis technique. To verify the accuracy of surface area measurements, oxidation testing of samples in the as-fabricated and polished conditions was performed; polished sample oxidation curves were then compared to the as-fabricated sample oxidation curves before and after being adjusted using obtained surface area measurements. It was found that the 2D technique accurately measured surface area and accounted for the overlapping features present on EBM sample surfaces, whereas the 3D technique did not. Further, it was also observed that oxidation kinetics were moderately faster on the alloy X samples in the as-fabricated condition than for the polished condition.

36 MATERIALS SCIENCE↗

Registration and fusion of large-scale melt pool temperature and morphology monitoring data demonstrated for surface topography prediction in LPBF

In-situ monitoring technologies for laser powder bed fusion (LPBF) additive manufacturing often face one key challenge, extracting the ultrafast melt pool (MP) signatures for understanding the localized part properties. Further, the spatial information of each monitored MP signature is essential for correlating the MP – part property. This spatial information is often unavailable especially from commercial LPBF printers. Many MP monitoring methods have been reported and utilized. However, very few of these have the MP’s spatial information. To overcome this challenge, in this work we report a method for spatially registering the key MP signatures (MP intensity, temperature, and area) to the monitored print parts. The MP signatures are obtained from our coaxial high-speed single-camera based two-wavelength imaging pyrometry (STWIP) system and the MP spatial information is obtained from an off-axis camera system. A machine learning aided image analysis method is employed to retrieve the spatial distribution of MPs within the corresponding part’s coordinates system. Then, the MP signature maps (MPSMs) are reconstructed by mapping the STWIP measured MP signatures to the registered MP coordinates. Further, a long short-term memory (LSTM) neural network is developed for estimating the layer surface topography from the registered MPSMs. The obtained results indicate that the layer surface topography can be more accurately estimated by using MP temperature signature rather than MP intensity and/or area signatures as in common practice. Finally, our developed methods for MP monitoring, registration, and MP-surface topography prediction offer advanced capabilities for the online detection of process anomalies and part defects.

36 MATERIALS SCIENCE↗