Thermal and fragility studies on microwave synthesized K{sub 2}O-B{sub 2}O{sub 3}-V{sub 2}O{sub 5} glasses
Glasses with composition xK{sub 2}O–60B{sub 2}O{sub 3}–(40-x) V{sub 2}O{sub 5} (15 ≤ x ≤ 39 mol %) was prepared by an energy efficient microwave method. The heat capacity change (ΔC{sub p}) at glass transition (T{sub g}), width of glass transition (ΔT{sub g}), heat capacities in the glassy (C{sub pg}) and liquid (C{sub pl}) state for the investigated glasses were extracted from Modulated Differential Scanning Calorimetry (MDSC) thermograms. The width of glass transition is less than 30°C, indicating that these glasses belongs to fragile category. Fragility functions [NBO]/(V{sub m}{sup 3}T{sub g}) and (ΔC{sub p}/C{sub pl})increases with increasing modifier oxide concentration. Increase in fragility is attributed to the increasing coordination of boron. Further, addition of K{sub 2}O creates NBOs and the flow mechanism involves bond switching between BOs and NBOs. Physical properties exhibit compositional dependence and these properties increase with increasing K{sub 2}O concentration. The observed variations are qualitatively analyzed.